Anti-counterfeit medium, method for manufacturing the same and method for preventing counterfeiting
10300731 ยท 2019-05-28
Assignee
Inventors
Cpc classification
B42D25/391
PERFORMING OPERATIONS; TRANSPORTING
B32B37/14
PERFORMING OPERATIONS; TRANSPORTING
B32B2554/00
PERFORMING OPERATIONS; TRANSPORTING
B32B7/12
PERFORMING OPERATIONS; TRANSPORTING
B42D25/351
PERFORMING OPERATIONS; TRANSPORTING
B32B2307/42
PERFORMING OPERATIONS; TRANSPORTING
International classification
B32B37/14
PERFORMING OPERATIONS; TRANSPORTING
B42D25/351
PERFORMING OPERATIONS; TRANSPORTING
B32B7/02
PERFORMING OPERATIONS; TRANSPORTING
G07D7/00
PHYSICS
B32B7/12
PERFORMING OPERATIONS; TRANSPORTING
Abstract
An anti-counterfeit medium, a method for manufacturing the same and a method for preventing counterfeiting are provided. The anti-counterfeit medium includes a retardation layer having birefringence and a reflection layer, and identification data is recorded in the anti-counterfeit medium. The identification data is divided into a plurality of partial images, and a plurality of transparent areas which correspond to the plurality of partial images are disposed adjacent to each other in the same plane so as to form the retardation layer, the plurality of transparent areas having optical axes which are oriented in different directions from each other in a rotation direction. The identification data includes biometric information.
Claims
1. An anti-counterfeit medium in which identification data is recorded, comprising: a retardation layer having birefringence; a reflection layer, wherein the identification data is divided into a plurality of partial images, and a plurality of transparent areas which correspond to the plurality of partial images are disposed adjacent to each other in a same plane so as to form the retardation layer, the plurality of transparent areas having optical axes which are oriented in different directions from each other in a rotation direction, and the identification data includes biometric information, wherein the identification data comprises first identification data and second identification data being recorded in the retardation layer, wherein the retardation layer includes at least a first image corresponding to a portion of the first identification data, at least a second image corresponding to a portion of the second identification data, and at least one third image which corresponds to a portion in which the first identification data and the second identification data are overlapped, the at least one third image being recorded in a transparent area of the plurality of transparent areas, wherein the anti-counterfeit medium is configured to display a first synthesized image corresponding to the second identification data, when viewed at a first angle, wherein the anti-counterfeit medium is configured to display a second synthesized image corresponding to a portion of the first identification data, when viewed at a second angle, and wherein each of the plurality of partial images comprises incomplete portions of the biometric information, the incomplete portions corresponding to fragments of the images.
2. The anti-counterfeit medium of claim 1, wherein the non-biometric information includes a character string or a symbol string; and wherein the anti-counterfeit medium is configured to be capable of individually displaying the first and second identification data.
3. The anti-counterfeit medium of claim 2, wherein part of the first identification data and part of the second identification data are recorded in at least one transparent area of the plurality of transparent areas.
4. The anti-counterfeit medium of claim 3, wherein the retardation layer includes a plurality of transparent areas, at least two of the transparent areas having optical axes oriented in different directions from each other.
5. The anti-counterfeit medium of claim 4, wherein the plurality of transparent areas comprises a first transparent area, a second transparent area, a third transparent area, and a fourth transparent area, and wherein the third image corresponds to a portion in which the first identification data and the second identification data are overlapped is recorded in the fourth transparent area.
6. The anti-counterfeit medium of claim 5, wherein the fourth transparent area is adjacent to the first transparent area and opposite to the second transparent area in the rotation direction.
7. The anti-counterfeit medium of claim 6, wherein: the reflection layer has a thickness of 500 , and the retardation layer has a thickness of retardation value of /4.
8. The anti-counterfeit medium of claim 1, wherein the base layer comprises cellophane or nylon.
9. The anti-counterfeit medium of claim 1, wherein the reflection layer comprises Sn, Cr, Ni, Cu, Au or a compound thereof.
10. The anti-counterfeit medium of claim 1, further comprising a relief forming layer between the retardation layer and the reflection layer.
11. The anti-counterfeit medium of claim 1, wherein the reflection layer comprises polytetrafluoroethylene.
12. The anti-counterfeit medium of claim 1, wherein the first identification data is biometric information and the second identification data is non-biometric information.
13. A method for manufacturing an anti-counterfeit medium, comprising the steps of: providing a reflection layer; supporting the reflection layer and a retardation layer on a base layer; dividing identification data to be recorded into a plurality of partial images and wherein the identification data includes biometric information; and providing a plurality of transparent areas each of which corresponds to a corresponding one of the plurality of partial images to be disposed adjacent to each other in a same plane so as to form the retardation layer, the plurality of transparent areas having birefringence and having optical axes which are oriented in different directions from each other in a rotation direction, and wherein the identification data comprises first identification data and second identification data being recorded in the retardation layer, wherein the retardation layer includes at least a first image corresponding to a portion of the first identification data, at least a second image corresponding to a portion of the second identification data, and at least one third image which corresponds to a portion in which the first identification data and the second identification data are overlapped, the at least one third image being recorded in a transparent area of the plurality of transparent areas, wherein the anti-counterfeit medium is configured to display a first synthesized image corresponding to the second identification data, when viewed at a first angle, wherein the anti-counterfeit medium is configured to display a second synthesized image corresponding to a portion of the first identification data, when viewed at a second angle, and wherein each of the plurality of partial images comprises incomplete portions of the biometric information, the incomplete portions corresponding to fragments of the images.
14. The method for manufacturing an anti-counterfeit medium of claim 13, wherein the base layer comprises cellophane or nylon.
15. The method for manufacturing an anti-counterfeit medium of claim 13, wherein the reflection layer comprises Sn, Cr, Ni, Cu, Au or a compound thereof.
16. The method for manufacturing an anti-counterfeit medium of claim 13, further comprising disposing a relief forming layer between the retardation layer and the reflection layer.
17. The method for manufacturing an anti-counterfeit medium of claim 13, wherein the reflection layer comprises polytetrafluoroethylene.
18. The method for manufacturing an anti-counterfeit medium of claim 13, wherein: part of the first identification data and part of the second identification data are recorded in at least one transparent area of the plurality of transparent areas.
19. The method for manufacturing an anti-counterfeit medium of claim 13, wherein: the plurality of transparent areas comprises a first transparent area, a second transparent area, a third transparent area, and a fourth transparent area, and the third image corresponds to a portion in which the first identification data and the second identification data are overlapped is recorded in the fourth transparent area, and the fourth transparent area is adjacent to the first transparent area and opposite to the second transparent area in the rotation direction.
20. The method for manufacturing an anti-counterfeit medium of claim 19, wherein: the reflection layer has a thickness of 500 , and the retardation layer has a thickness of retardation value of /4.
21. The method of claim 13, wherein the first identification data is biometric information and the second identification data is non-biometric information.
22. A method for preventing counterfeiting, comprising the steps of: providing the anti-counterfeit medium of claim 1; and observing the anti-counterfeit medium via a polarizing plate.
Description
BRIEF DESCRIPTION OF THE DRAWINGS
(1)
(2)
(3)
(4)
(5)
(6)
(7)
(8)
(9)
(10)
(11)
(12)
(13)
(14)
(15)
(16)
(17)
(18)
(19)
(20)
(21)
(22)
(23)
(24)
DESCRIPTION OF REPRESENTATIVE EMBODIMENTS
(25) With reference to the drawings, an anti-counterfeit medium according to an embodiment of the present invention will be described below in detail.
(26)
(27) The retardation layer 2 may be made of a material having birefringence. Birefringence means that refractive indices of an object are different depending on the optical axis direction, and accordingly, light which travels through such an object has different speeds. As a result, retardation occurs due to the different travelling speeds in the light which has passed through the object. For example, the material may be a liquid crystal material.
(28) Orienting the optical axis of the retardation layer 2 in one direction may be achieved by drawing a film or applying a rubbing process to a film. In drawing a film, the optical axis is oriented in the drawing direction of the film. In a rubbing process of a film, the optical axis is oriented in the rubbing direction. A uniaxially oriented liquid crystal may be obtained by applying liquid crystal on an orientation film which is treated with orientation process in any unidirection. The orientation process of orientation film for orienting a liquid crystal material may be performed by, for example, a rubbing orientation method or an optical orientation method. A retardation value may be determined depending on the index of birefringence and the film thickness of liquid crystal.
(29) The rubbing orientation method is a method of directly rubbing the base material by using a cloth or rubbing an orientation film formed by applying polymer solution on the base material by using a cloth. This method uses an alteration in property of the surface of the base material or the surface of the orientation film which occurs in the rubbing direction and liquid crystal molecules are aligned in the rubbing direction. The orientation film may be made of polyimide, PVA or the like.
(30) The optical orientation method is a method of irradiating light having anisotropy such as polarized light or irradiating non-polarized light in an oblique direction to the orientation film, thereby inducing re-alignment or anisotropic chemical reaction of molecules in the orientation film. This method uses that liquid crystal molecules which are aligned by providing anisotropy to the orientation film. Mechanisms of providing optical orientation may include using the anisotropy of azobenzene derivatives, photodimerization or cross-linkage of derivatives of cinnamic acid ester, coumarin, chalcone and benzophenone, and photodegradation of polyimide.
(31) When the orientation film is used as described above, a known technique such as gravure coating method or micro gravure coating method may be used for the orientation film.
(32) The retardation layer 2 may be obtained by providing a liquid crystal material on an oriented film, a film treated by a rubbing process, or an orientation film treated by an orientation process. Liquid crystal materials may include photo-curable liquid crystal monomers having acrylate on both ends of the mesogenic group, EB or UV curable polymer liquid crystal, polymer liquid crystal having mesogenic groups for the polymer main chain, and liquid crystal polymer in which the molecular main chain itself is oriented. After those liquid crystals being applied, a heat treatment may be performed at a temperature slightly lower than the N-I point at which phase transition occurs so as to promote orientation.
(33)
(34) On the other hand, a second image 10, which is the other of two partial images that are obtained by dividing identification data into two parts, is transferred to the transferred object 6 at an angle shown in
(35) The first image 7 and the second image 10 can be transferred by using a thermal head 25 as shown in
(36) The transferred first transparent area 8 and its optical axis 9, and the transferred second transparent area 12 and its optical axis 13 have a relationship as shown in
(37) The anti-counterfeit medium of
(38)
(39) The first image 16, the second image 17, and the third image 18 are transferred while the transferred object 6 is rotated by different rotation angles. The first image 16 is transferred with the rotation angle of the transferred object 6 being .sub.0=0 so as to obtain a first transparent area. The second image 17 is transferred with the rotation angle of the transferred object 6 being .sub.1=60 so as to obtain a second transparent area. The third image 18 is transferred with the rotation angle of the transferred object 6 being .sub.2=30 so as to obtain a third transparent area. The first to third transparent areas are disposed adjacent to each other in the same plane, thereby forming a single retardation layer 2.
(40) The anti-counterfeit medium having the identification data divided as shown in
(41)
(42) The first image 20 corresponds to a portion of the second identification data (that is, character string) which is not overlapped with the first identification data (that is, facial image).
(43) The second image 21 corresponds to a portion in which neither the first identification data (that is, facial image) nor the second identification data (that is, character string) is recorded.
(44) The third image 22 corresponds to a portion of the first identification data (that is, facial image) which is not overlapped with the second identification data (that is, character string).
(45) The fourth image 23 corresponds to a portion in which the first identification data (that is, facial image) and the second identification data (that is, character string) are overlapped.
(46) The first image 20, the second image 21, the third image 22, and the fourth image 23 are transferred while the transferred object 6 is rotated by different rotation angles. The first image 20 is transferred with the rotation angle of the transferred object 6 being 0=0 so as to obtain a first transparent area. The second image 21 is transferred with the rotation angle of the transferred object 6 being .sub.2=67.5 so as to obtain a second transparent area. The third image 22 is transferred with the rotation angle of the transferred object 6 being .sub.2=45 so as to obtain a third transparent area. The fourth image 23 is transferred with the rotation angle of the transferred object 6 being .sub.3=22.5 so as to obtain a fourth transparent area. The first to fourth transparent areas are disposed adjacent to each other in the same plane, thereby forming a single retardation layer 2.
(47) The anti-counterfeit medium having the identification data divided as shown in
(48) A first rotation angle of the verifier 15 shown in
(49) A second rotation angle of the verifier 15 shown in
(50) A third rotation angle of the verifier 15 shown in
(51) A fourth rotation angle of the verifier 15 shown in
(52) Although the retardation layer 2 of the transfer foil 1 is described as the retardation layer which is oriented in a uniaxial direction, a transfer foil which has a multi-axial retardation layer may be used. Alternatively, a plurality of transfer foils each of which have different optical axis directions with a retardation layer which is oriented in uniaxial direction may be provided and used as necessary. However, the retardation layer having the optical axis oriented in a uniaxial direction allows for reduction of manufacturing processes, and thus reduction of manufacturing cost.
(53) The retardation value is preferably , for example, when a linear polarizer is used for the verifier 15 and the reflection layer 3 is incorporated into the transfer foil 1. Further, the retardation value is effective when a transparent substrate is used for the transferred object 6 and a linear polarizer is disposed on the back surface of the transferred object 6, and a linear polarizer is used for the verifier 15. Further, the retardation value is effective, for example, when a transparent substrate is used for the transferred object 6 and a circular polarizer is disposed on the back surface of the transferred object 6, and a circular polarizer is used for the verifier 15. In any of those cases, any of the retardation values , , may be used.
(54) The base material 5 may be a non-oriented film formed by extruding or casting, an oriented film formed by drawing or the like. The oriented film may be either a uniaxially oriented film or a biaxially oriented film.
(55) Those non-oriented film and oriented film may be made of a material such as cellophane, polycarbonate (PC), polyethylene (PE), polypropylene (PP), polyolefin (PO), ethylene vinyl alcohol (EVOH), polyvinyl alcohol (PVA), polyvinyl chloride, polyethylene naphthalate (PEN), polyethylene terephthalate (PET), nylon, acrylic resin, and triacetyl cellulose (TAC) film.
(56) When the oriented film is used, an orientation process for the above retardation layer 2 may not be necessary. However, when the non-oriented film is used, a rubbing process or orientation process of the orientation film needs to be performed.
(57) The reflection layer 3 may be made of any metal material such as Al, Sn, Cr, Ni, Cu, Au, Ag or a compound thereof.
(58) Further, a transparent reflection layer 3 which is substantially transparent to light vertical to a film surface but has a reflective property to oblique light depending on the refractive index may be used as a single layer or multilayer. Examples for the material of the transparent reflection layer 3 may include, but are not limited to, ceramics such as FE2O3, TiO2, CdS, CeO2, ZnS, PbCl2, CdO, WO3, SiO, Si2O3, In2O3, PbO, Ta2O3, ZnO, ZrO2, MgO, SiO2, MgF2, CeF3, CaF2, AlF3, Al2O3, GaO and organic polymers such as polyethylene, polypropylene, polytetrafluoroethylene, polymethyl methacrylate, polystyrene.
(59) Methods for forming the reflection layer 3 may be a known method as appropriate, for example, a vacuum deposition method, sputtering method, and CVD method. Alternatively, ink having a light reflection effect may be applied by a known printing method.
(60) Further, the reflection layer 3 may be formed along a relief forming layer. A method for forming the reflection layer 3 along a relief structure may include providing a relief forming layer in advance, duplicating a fine concave-convex pattern by applying heat and pressure by using a relief type press plate formed of a fine concave-convex pattern of a relief hologram or a grating which uses light interference, and then forming the reflection layer 3 by using a known method such as a vacuum deposition method. The relief forming layer may be disposed between the retardation layer 2 and the reflection layer 3.
(61) The relief forming layer is preferably made of a material having a good thermoformability, resistance to uneven pressing, and formability of clear reproduction image. For example, thermo-plastic resin such as acryl-based resin, epoxy-based resin, cellulose-based resin and vinyl-based resin, thermosetting resin such as urethane resin containing acryl polyol, polyester polyol or the like having a reactive hydroxyl group with polyisocyanate added and cross-linked as a cross-linking agent, melamine-based resin and phenol-based resin, UV or EB curable resin such as epoxy (meta)acryl, and urethane (meta)acrylate may be used alone or in combination thereof. Alternatively, any resin other than described above may be used as appropriate as long as it may form a diffractive structure pattern.
(62) The adhesive layer 4 is made of a heat-sensitive adhesive which exhibits adhesiveness when heat is applied. The adhesive layer 4 is formed by providing a resin having such ability on the substrate by using gravure coater, microgravure coater, roll coater or the like. Materials which may be used are thermoplastic resin such as acrylic resin, vinyl chloride-vinyl acetate copolymer, epoxy, and EVA.
(63) A release layer may be disposed between the base material 5 and the retardation layer 2. The release layer may be a resin alone, or a resin with lubricating agent being added. Examples of resin may include thermoplastic resin, thermosetting resin, moisture curable resin, UV curable resin, and EB curable resin. For example, acrylic resin, polyester resin, or polyamide-imide resin may be used. Further, examples of lubricating agent may include wax such as polyethylene powder or carnauba wax. Those may be used for the release layer formed on the base material 5 by using a known method such as gravure printing method or microgravure method.
(64) The transferred object 6 may be transparent or opaque. Materials for the transferred object 6 may include, for example, paper, plastic, metal, ceramics, and glass.
(65) The inputted identification data may be divided into N parts as the first to Nth images. Each of the images may be thermally transferred to the transferred object 6 by using a thermal head as the first to Nth transparent areas while being rotated by an angle of .sub.n=90/Nn (n=N1, N2, . . . , 1).
(66) For example, in an example of binarized image shown in
(67) In an example of image divided into three parts shown in
(68) As a result, when the verifier 15 is held at a specific angle as shown in
(69) In an example of an image divided into four parts to exhibit two images shown in
(70) The number of pieces into which the data is divided is not specifically limited, and data may be divided as appropriate depending on the inputted data and the type of desired latent image. The inputted data may be one image, two overlapped image as described above, or an image having a gradation of tones.
(71) The inputted data may be an image including personal information. The personal information includes personal authentication information which is used for personal authentication. The personal information may be classified as, for example, biometric information and non-biometric information.
(72) The biometric information is information regarding biological characteristics and derived from an image or a pattern in a plane which is specific to the individual. For example, biometric information is at least one image or pattern of face, fingerprint, iris, vein and the like.
(73) The non-biometric information is personal information other than biometric information, which is particularly a character string or symbol string. For example, non-biometric information may be at least one of name, date of birth, age, blood type, gender, nationality, address, permanent address, phone number, department and title. Non-biometric information may include typed characters, handwritten characters such as signature read by machine, or both of them.
(74) As described above, in this embodiment, the identification data including biometric information is divided into a plurality of partial images, and the plurality of partial images are provided as a plurality of transparent areas having different optical axis directions. Accordingly, the anti-counterfeit medium which is a polarized latent image device can be more difficult to counterfeit.
(75) Examples 1 to 3 according to an embodiment of the present invention were fabricated for confirmation.
Example 1
(76) Lumirror 19F60 was provided as the base material 5, and the surface of the base material was rubbed by a rubbing cloth in the feeding direction of the raw sheet. The UV curable liquid crystal UCL-008 manufactured by DIC corporation was applied by microgravure coating to form a thickness of retardation value of /4, and UV-cured in oxygen atmosphere. As a result, the retardation layer having the optical axis in the feeding direction was obtained.
(77) Then, the reflection layer 3 made of aluminum was formed on the retardation layer. The reflection layer 3 was formed by a vacuum deposition method to have a thickness of 500 . Then, acrylic resin as the adhesive layer 4 was applied on the entire surface by microgravure coating, and the transfer foil 1 was obtained.
(78) Then, a photo of a person was taken, and immediately divided into two parts by binarization. The first image 7 was transferred as shown in
Example 2
(79) Lumirror 19F60 was provided as the base material 5, and the surface of the base material was rubbed by a rubbing cloth in the feeding direction of the raw sheet. The UV curable liquid crystal UCL-008 manufactured by DIC corporation was applied by microgravure coating to form a thickness of retardation value of /2, and UV-cured in oxygen atmosphere. As a result, the retardation layer having the optical axis in the feeding direction was obtained. Then, acrylic resin as the adhesive layer 4 was applied on the entire surface of the retardation layer by microgravure coating, and the transfer foil 1 was obtained.
(80) Then, the inputted identification data was divided into three parts to form the first image 16 to the third image 18 as shown in
(81) Then, a linear polarizer was disposed on the back surface of the anti-counterfeit medium, and the anti-counterfeit medium was observed by using the verifier 15. As a result, although not visually observed, the latent images 19a, 19b, 19c as shown in
Example 3
(82) Lumirror 19F60 was provided as the base material 5, and the surface of the base material was rubbed by a rubbing cloth in the feeding direction of the raw sheet. The UV curable liquid crystal UCL-008 manufactured by DIC corporation was applied by microgravure coating to form a thickness of retardation value of /4, and UV-cured in oxygen atmosphere. As a result, the retardation layer having the optical axis in the feeding direction was obtained.
(83) Then, the reflection layer 3 made of aluminum was formed on the retardation layer 2. The reflection layer 3 was formed by a vacuum deposition method to have a thickness of 500 . Then, acrylic resin as the adhesive layer 4 was applied on the entire surface by microgravure coating, and the transfer foil 1 was obtained.
(84) A photo of a person was taken, and binarized to obtain a person positive image. Further, TP1234 was inputted, and then, the person positive image and two types of data of TP1234 were combined and divided into four images as shown in
(85) Then, the anti-counterfeit medium was observed by using the verifier 15. When the verifier 15 was held and rotated to a specific angle as shown in
(86) Further, the present invention is not limited to the above embodiment, and various alterations can be made without departing from the spirit in each of the implementation phases. Further, the above embodiment includes various phases of the invention. Accordingly, various inventions can be extracted from appropriate combinations of a plurality of disclosed components.
(87) For example, even if some elements are deleted from all the elements described in the embodiment, the configuration with some elements deleted is regarded as the invention as long as the problem described in the section of technical problem can be solved and an effect described in the section of solution to problem can be obtained.
(88) According to the present invention, a transfer foil and anti-counterfeit medium capable of easily forming of identification information while achieving easy judgment of identification information and prevention of counterfeiting and falsification of identification information can be provided. The anti-counterfeit medium according to the present invention can be applied to various cards such as credit cards, cash cards, member cards, employee cards, prepaid cards and driver's licenses, various paper certificates such as gift certificates, gift coupons and stock certificates, application forms, receipts, various slips such as carbon copy slips, various booklets such as passports, passbooks and pension books, as well as covers of books and notebooks and displays such as panels. The retardation layer may be bonded to a part of or the entire surface of the transferred object.
REFERENCE SIGNS LIST
(89) 1 . . . transfer foil 2 . . . retardation layer 3 . . . reflection layer 4 . . . adhesive layer 5 . . . base material 6 . . . transferred object 7 . . . first image of data divided into two parts 8 . . . first transparent area 9 . . . optical axis of first transparent area 10 . . . second image of data divided into two parts 12 . . . second transparent area 13 . . . optical axis of second transparent area 14a, 14b . . . latent image which appears when verifier is held over anti-counterfeit medium of