Canvas flocking diamond picture

11524520 · 2022-12-13

Assignee

Inventors

Cpc classification

International classification

Abstract

The disclosure discloses a canvas flocking diamond picture, and relates to the technical field of canvas flocking diamond picture devices and making methods, solving the problem that the gray cloth of diamond canvas is shrunk after encountering water so that the diamond picture becomes uneven. The picture frame is internally provided with a protective film and a canvas, and the protective film is located at one side of the canvas; the upper end surface of the canvas is provided with a flash layer; an ink-receiving layer is arranged under the flash layer; an upper back cover layer is arranged under the ink-receiving layer; a cingico layer is arranged under the upper back cover layer; a lower back cover layer is arranged under the cingico layer; a flocking layer is arranged under the lower back cover layer, and the flocking layer is located on the lower end surface of the canvas; an adhesive layer is arranged between the lower back cover layer and the flocking layer.

Claims

1. A method for producing a canvas diamond picture, comprising: providing a canvas defining a first side and a second side opposite the first side; wetting a chemical fiber oxford cloth layer arranged on a first side of the canvas; after wetting the chemical fiber oxford cloth layer, drying the chemical fiber oxford cloth layer at a temperature of 190° C. to mitigate shrinking and flatting a surface of the chemical fiber oxford cloth layer; coating and sealing holes and gaps on a back surface of the chemical fiber oxford cloth layer with waterborne waterproof acrylic acid to form a lower back cover layer; uniformly brushing a layer of adhesive glue on the lower back cover layer to form an adhesive layer; attaching a fibrous layer to the adhesive layer on the second side of the canvas opposite the first side of the canvas; coating and sealing holes and gaps on a front surface of the chemical fiber oxford cloth layer with waterborne waterproof acrylic acid to form an upper back cover layer; coating waterborne waterproof acrylic emulsion on the upper back cover layer, and performing drying at a temperature of 150° C. to form an ink-receiving layer; forming a flash layer on the ink-receiving layer; printing patterns of a picture on the flash layer; and smearing oily glue at a place where the patterns are printed after printing.

2. The method of claim 1, further comprising of attaching a lower end surface of the upper back cover layer to an upper end surface of the chemical fiber oxford cloth layer.

3. The method of claim 1, further comprising attaching a lower end surface of the chemical fiber oxford cloth layer to an upper end surface of the lower back cover layer.

4. The method of claim 1, further comprising fixedly connecting the ink-receiving layer with the upper back cover layer.

5. The method of claim 1, wherein attaching the fibrous layer to the adhesive layer includes spraying woolen on the adhesive layer to form a flocking layer.

6. The method of claim 1, further comprising providing the fibrous layer as a flocking layer.

7. A method for producing a canvas diamond picture, comprising: providing a canvas defining a first side and a second side opposite the first side; wetting a chemical fiber oxford cloth layer arranged on a first side of the canvas; after wetting the chemical fiber oxford cloth layer, drying the chemical fiber oxford cloth layer to mitigate shrinking and flatting a surface of the chemical fiber oxford cloth layer; coating and sealing holes and gaps on a back surface of the chemical fiber oxford cloth layer with waterborne waterproof acrylic acid to form a lower back cover layer; brushing a layer of adhesive glue on the lower back cover layer to form an adhesive layer; attaching a fibrous layer to the adhesive layer on the second side of the canvas opposite the first side of the canvas; coating and sealing holes and gaps on a front surface of the chemical fiber oxford cloth layer with waterborne waterproof acrylic acid to form an upper back cover layer; coating waterborne waterproof acrylic emulsion on the upper back cover layer, and performing drying at a temperature of 150° C. to form an ink-receiving layer; smearing paillettes on the ink-receiving layer to form a flash layer; and printing patterns of a picture on the flash layer; and smearing oily glue at a place where the patterns are printed after printing.

8. The method of claim 7, further comprising attaching a lower end surface of the upper back cover layer to an upper end surface of the chemical fiber oxford cloth layer.

9. The method of claim 7, further comprising attaching a lower end surface of the chemical fiber oxford cloth layer to an upper end surface of the lower back cover layer.

10. The method of claim 7, further comprising fixedly connecting the ink-receiving layer with the upper back cover layer.

11. The method of claim 7, wherein attaching the fibrous to the adhesive layer includes spraying woolen on the adhesive layer to form a flocking layer.

Description

DESCRIPTION OF THE DRAWINGS

(1) FIG. 1 is a front view of a canvas flocking diamond picture according to the disclosure;

(2) FIG. 2 is a structural diagram of a canvas flocking diamond picture according to the disclosure; and

(3) FIG. 3 is a structural diagram of a flowchart of use method steps according to the disclosure.

(4) In drawings, 1, picture frame; 2, protective film; 3, canvas; 4, flash layer; 5, ink-receiving layer; 6, upper back cover layer; 7, cingico layer; 8, lower back cover layer; 9, adhesive layer; 10, flocking layer.

DETAILED DESCRIPTION OF PREFERRED EMBODIMENTS

(5) Next, the technical solution in embodiments of the disclosure will be clearly and completely described in combination with drawings in embodiments of the disclosure, apparently, the described embodiments are only one part of embodiments of the disclosure but not all the embodiments.

(6) Referring to FIGS. 1-3, an embodiment provided by the disclosure is as follows: a canvas flocking diamond picture comprises a picture frame 1, wherein, the picture frame 1 is internally provided with a protective film 2 and a canvas 3, and the protective film 2 is located at one side of the canvas 3; the upper end surface of the canvas 3 is provided with a flash layer 4; an ink-receiving layer 5 is arranged under the flash layer 4; an upper back cover layer 6 is arranged under the ink-receiving layer 5; a cingico layer 7 is arranged under the upper back cover layer 6; a lower back cover layer 8 is arranged under the cingico layer 7; a flocking layer 10 is arranged under the lower back cover layer 8, and the flocking layer 10 is located on the lower end surface of the canvas 3; an adhesive layer 9 is arranged between the lower back cover layer 8 and the flocking layer 10.

(7) Further, the lower end surface of the upper back cover layer 6 is attached to the upper end surface of the cingico layer 7.

(8) Further, the lower end surface of the cingico layer 7 is attached to the upper end surface of the lower back cover layer 8.

(9) Further, the ink-receiving layer 5 is fixedly connected with the upper back cover layer 6.

(10) Further, a method for producing the canvas flocking diamond picture comprises the following steps:

(11) step 1: after wetting a cingico layer 7 made of chemical fiber oxford cloth, drying the wet cloth at a high temperature of 190° C. to take an effect of preventing shrinking and flatting the cloth surface, thereby completing the sizing of gray cloth;

(12) step 2: coating and sealing holes and gaps on the back surface of the cingico layer 7 with waterborne waterproof environmental-friendly acrylic acid to form a lower back cover layer 8;

(13) step 3: uniformly brushing a layer of adhesive glue on the lower back cover layer 8 to form an adhesive layer 9, and paving woolens on the adhesive layer 9 in a manner of spraying to form a flocking layer 10;

(14) step 4: coating and sealing holes and gaps on the front surface of the cingico layer 7 with waterborne waterproof environmental-friendly acrylic acid to form an upper back cover layer 6;

(15) step 5: coating waterborne waterproof environmental-friendly acrylic emulsion on the surface of the upper back cover layer 6, and drying at a high temperature of 150° C. to form a film, namely, an ink-receiving layer 5;

(16) step 6: smearing paillettes on the ink-receiving layer 5 to form a flash layer 4; and

(17) step 7: printing the patterns of the diamond picture on the flash layer 4, and smearing oily environmental-friendly glue at a place where the patterns are printed after printing.

(18) It is apparent for those skilled in the art that the disclosure is not limited to details of the above exemplary embodiment and can be achieved in other particular forms without departing from the spirit or basic features of the disclosure. Thus, regardless of which points, embodiments should be deemed as being exemplary and non-limiting. The scope of the disclosure is defined by appended claims rather than the above description, and therefore it is intended that all changes coming within the meanings and scope of equivalent elements of claims are included in the disclosure. Any reference numbers in claims should not be considered as limiting the involved claims.