TWO-LAYER FABRIC FOR UNWOVEN FABRIC

20190136422 ยท 2019-05-09

    Inventors

    Cpc classification

    International classification

    Abstract

    The object of the present invention is to provide a two-layer fabric for manufacturing a unwoven fabric which can reduce the sticking of the fiber generated upon the manufacturing of the unwoven fabric, while add the excellent lateral rigidity, the excellent diagonal rigidity, and the excellent sheet supportability to the two-layer fabric for manufacturing the unwoven fabric.

    In the two-layer fabric for manufacturing the unwoven fabric comprising a right surface side layer consisting of wefts of the right surface side and warps of the right surface side, and a back surface side layer consisting of wefts of the back surface side and warps of the back surface side, the two-layer fabric for manufacturing the unwoven fabric further comprises a first pair of wefts in which a binding warp on the right surface side serving as a binding yarn and a binding warp on the back surface side serving as a binding yarn are arranged in a substantially vertical direction, a second pair of warps in which a warp on the right surface side and a warp on the back surface side are arranged in a vertical direction to be overlapped with each other, and a third pair of warps in which two warps on the right surface side are arranged adjacent to each other.

    Claims

    1. In the two-layer fabric for manufacturing the unwoven fabric comprising a right surface side layer consisting of wefts of the right surface side and warps of the right surface side, and a back surface side layer consisting of wefts of the back surface side and warps of the back surface side, the two-layer fabric for manufacturing the unwoven fabric further comprises a first pair of wefts in which a binding warp on the right surface side serving as a binding yarn and a binding warp on the back surface side serving as a binding yarn are arranged in a substantially vertical direction, a second pair of warps in which a warp on the right surface side and a warp on the back surface side are arranged in a vertical direction to be overlapped with each other, and a third pair of warps in which two warps on the right surface side are arranged adjacent to each other.

    2. The two-layer fabric for manufacturing the unwoven fabric according to claim 1, wherein a perfect structure of said two-layer fabric for manufacturing the unwoven fabric includes sixteen warps, said sixteen warps comprises two sets of said first pairs of warps, four sets of said second pair of warps, and two sets of said third pair of warps.

    3. The two-layer fabric for manufacturing the unwoven fabric according to claim 1, wherein the diameters of the warps constituting said first pair of warps, said second pair of warps, and said third pair of warps are between 0.30 mm and 0.50 mm, and the diameters of the wefts on the back surface side are between 0.30 mm and 0.70 mm.

    4. The two-layer fabric for manufacturing the unwoven fabric according to claim 1, the two-layer fabric for manufacturing the unwoven fabric is formed to be endless by opposed ends of the warps being joined by a loop joint manner.

    5. The two-layer fabric for manufacturing the unwoven fabric according to claim 1, a portion of, or all of at least said second pair of warps are formed by a carbon line.

    6. The two-layer fabric for manufacturing the unwoven fabric according to claim 1, wherein the weaving structure of the fabric on the right surface side and the fabric on the back surface side is formed by a plain weaving.

    Description

    BRIEF EXPLANATION OF DRAWINGS

    [0027] FIG. 1 is a design view showing a complete structure of the two-layer fabric for manufacturing the unwoven fabric of the present invention in a first embodiment.

    [0028] FIG. 2 is a schematic view showing a vertical cross section taken along the warps in FIG. 1.

    EMBODIMENT OF INVENTION

    [0029] The structure and the effect of the two-layer fabric for manufacturing the unwoven fabric of the present invention will now be described. Thereafter, the embodiment of the two-layer fabric for manufacturing the unwoven fabric of the present invention will be explained in detail.

    [0030] The two-layer fabric for manufacturing the unwoven fabric of the present invention is formed by a right surface side fabric consisting of wefts of the right surface side and warps of the right surface side, and a back surface side fabric consisting of wefts of the back surface side and warps of the back surface side being bound by a binding yarn on the right surface side serving as a binding yarn and a binding warp on the back surface side serving as a binding yarn.

    [0031] In the two-layer fabric for manufacturing the unwoven fabric of the present invention, the binding yarn on the right surface side serving as a binding yarn and the binding warp on the back surface side serving as a binding yarn are arranged in a substantially vertical direction, a second pair of warps in which a warp on the right surface side and a warp on the back surface side are arranged in a vertical direction to be overlapped with each other, and a third pair of warps in which two warps on the right surface side are arranged adjacent to each other.

    [0032] Here, a binding yarn on the right surface side serving as a binding yarn is to be defined to be the yarn which serves as a binding yarn by weaving the warp originally serving as the warp on the right surface side as an arrangement of the warp in a perfect structure of the two-layer fabric for manufacturing the unwoven fabric, with the weft on the back surface side from the back surface side, while a binding yarn on the back surface side serving as a binding yarn is to be defined to be the yarn which serves as a binding yarn by weaving the warp originally serving as the warp on the back surface side as an arrangement of the warp in a perfect structure of the two-layer fabric for manufacturing the unwoven fabric, with the weft on the right surface side from the right surface side.

    [0033] In addition, in the first pair of warps, one binding yarn on the right surface side passes above the weft on the right surface side and passes below the weft on the back surface side at a position where it originally passes above the weft on the right surface side as a plain weaving fabric to be woven with each other. At said position, other binding yarn on the back surface side passes above the weft on the right surface side to be woven with each other. In other words, two binding yarns alternately complements knuckles on the right surface side to form the plain weaving structure.

    [0034] Further, the second pair of warps forms a pair by the warps on the right surface side and the warps on the back surface side being vertically arranged. By weaving a right surface side layer with a back surface side layer, the two-layer fabric for manufacturing the unwoven fabric of the present invention can obtain the properties required for the fabric such as the lateral rigidity, the diagonal rigidity at a high level. Still further, since the two-layer fabric for manufacturing the unwoven fabric of the present invention does not include a binding structure, so that a tension of the fibers can be alleviated.

    [0035] In addition, the technical feature of the present invention lies in the fact that a single warp on the right surface side among tow warps on the right surface side constituting the third pair of the warps forms a fabric on the right surface side by the yarns originally constituting the warps on the back surface side as a whole structure being woven with the weft on the right surface side.

    [0036] Such being the case, in the two-layer fabric for manufacturing the unwoven fabric of the present invention, the number of the warps on the right surface side of the fabric becomes larger than that of the warps on the back surface side by making the third pair of the warps an essential element, so that the surface density is increased, whereby a supporting force at the intersection can be largely alleviated. In addition, since the number of the warps on the back surface side is small, the air permeability and the dehydration can be improved.

    [0037] Further, the sticking of the fiber which is the technical problem for the conventional technology can be improved by means of the warps of the second pair of the warps emerging on the right surface side and the third pair of the warps.

    [0038] Still further, in the two-layer fabric for manufacturing the unwoven fabric of the present invention, it is preferred that a perfect of the structure of the fabric on the right surfaces side and the fabric on the back surface side be formed by a plain weaving method.

    [0039] Here, in the present invention, the perfect structure is defined to be a minimum unit the repetition of which forms the fabric structure, in other words, the unit is repeated in right and left directions, and in upper and lower directions to form the fabric.

    [0040] In the present invention the weft with a large or small diameter can be used despite of the fact that the surface structure is formed by the plain weaving. In the structure of the conventional fabric for the unwoven fabric, the surface density is reduced if a weft with a large diameter is adopted for the plain weaving structure. However, in the present invention, since the first, second, third pairs of warps include the warps, the surface density can be enhanced by adopting the wefts with a large diameter for the weft on the back surface side and the weft on the back surface side with a diameter small than the former weft. In addition, the air permeability can be enhanced by adopting the weft with a large diameter for the weft on the right surface side and the weft with a small diameter for the weft on the back surface side. More specifically, the difference of the diameter between the weft on the right surface side and the weft on the back surface side may be within +?20% of the diameter of the weft on the right surface side. If the diameter of the weft on the right surface side and that on the back surface side exceeds 20%, the balance of the network can be deteriorated, or it becomes technically difficult to form a loop.

    [0041] In the two-layer fabric for manufacturing the unwoven fabric of the present invention, the air permeability can the surface smoothness can be adjusted by setting the difference of the diameter between the weft on the right surfaces side and the weft on the back surface side to be within +?20%.

    [0042] The general yarn used for the lower surface side fabric can be polyester, polyamide, polyphenylene sulfide, polypropylene, aramid, polyether ketone, polyethylene naphthalate, polytetrafluoroethylene, etc.

    [0043] The configuration of the yarn includes, in addition to monofilaments, multifilaments, spun yarns, finished yarns subjected to crimping or bulking such as so-called textured yarn, bulky yarn and stretch yarn, and yarns obtained by intertwining them. As the cross-section of the yarn, not only circular form but also square or short form such as stellar form, or elliptical or hollow form can be used.

    [0044] The material of the yarns can be freely selected, and is not limited to the specific material.

    [0045] The configuration of the yarn includes, in addition to monofilaments, multifilaments, spun yarns, finished yarns subjected to crimping or bulking such as so-called textured yarn, bulky yarn and stretch yarn, and yarns obtained by intertwining them. As the cross-section of the yarn, not only circular form but also square or short form such as stellar form, or elliptical or hollow form can be used. The material of the yarn can be selected freely and usable examples of it include polyester, polyamide, polyphenylene sulfide, polyvinylidene fluoride, polypropylene, aramid, polyether ketone, polyethylene naphthalate, polytetrafluoroethylene, cotton, wool and metal. Of course, yarns obtained using copolymers or incorporating or mixing the above-described material with a substance selected depending on the intended purpose may be used.

    [0046] Since the yarn constituting the fabric for unwoven fabric generally includes a high rigidity, polyester monofilaments with excellent dimension stability may be preferably adopted.

    [0047] Further, in the present invention, a carbon line can be used for a portion of, or all of the second pair of the warps. Upon the manufacturing of the unwoven fabric, the wire can be electrically charged by static electricity. In such a case, since the wire and the fiber of the unwoven fabric electrically charged repel each other, the unwoven fabric cannot be formed on the wire. Such being the case, the static electricity can be removed by adopting a carbon line for a portion of, or all of the second pair of the warps.

    [0048] In this connection, the present invention encompasses a case where the carbon line is used for a yarn except of the second pair of warps (the weft on the right surfaces side or the back surface side).

    [0049] A specific limitation is not put on the diameter of the yarn constituting the fabric, however, it is preferred that the diameter of the warps on the right surface side or the weft on the right surface side constituting a layer on the right surface side be comparatively small in order to make the surface if the fabric fine and smooth. In addition, since the back surface contacting the machine or the roll needs to possess a rigidity or a wear resistance, it is preferred that the diameter of the weft on the back surface side or the warps on the back surface side be comparatively large. Theses diameters may be selected, in view of an application, a circumstance in which the fabric is used, the ratio of the number of the upper wefts to that of the lower wefts.

    [0050] It is preferred that the two-layer fabric for manufacturing the unwoven fabric of the present invention be made an endless type by connecting the opposed longitudinal ends on a loop joint manner.

    [0051] Here, in the loop joint, a loop can be formed with at least one weft at the end portion of the fabric being left. Further, in the above formed loop, a loop for joining can be formed by folding back all of, or a portion of the warps at the one, or the both end portions of the fabric to form a loop, and appropriately weaving the formed loop with the weft.

    [0052] A common hole for inserting a core line below the weft may formed by making a plurality of loops bite.

    [0053] Now, the embodiments of the present invention will be described below with reference to the drawings. Here, the design view corresponds to the complete structure of the fabric defining the minimum unit to be repeated of the fabric structure. The fabric recited in the claims corresponds to this complete structure. The final product is completed by combining any number of such complete structures in the longitudinal direction and the direction perpendicular to the longitudinal direction.

    [0054] In each of the design views, the warp is indicated by a reference number such as 1, 2, 3 . . . .

    [0055] The weft is indicated by a reference number to which is attached such as 1, 2, 3 . . . . the yarn on the right surface side is indicated by a reference number to which U is attached, while the yarn on the back surface side is indicated by a reference number to which L is attached such as 1U, 2L . . . . In addition, the binding warp yarn binding the fabric on the right surface side with the fabric on the back surface is indicated by a reference number to which b is attached.

    [0056] In each of the design views, a symbol ? indicates that the yarn constituting the one on the back surface side in the first pair of warps is arranged above the weft on the right surface side, a symbol x indicates that the binding yarn on the right surface side serving as a binding yarn in the first pair of warps, and the warps on the right surface side in the second pair of warps and the third pair of warps are arranged above the weft on the right surface side, a symbol ? indicates that the binding yarn on the right surface side serving as a binding yarn in the first pair of warps is arranged below the weft on the back surface side, and a symbol ? indicates that the binding yarn on the back surface side serving as a binding yarn in the first pair of warps, and the warps on the back surface side in the second pair of warps and the third pair of warps are arranged below the weft on the back surface side.

    [0057] In the explanation of the embodiment, a knuckle is defined to be a portion of a warp which passes above or below one or more wefts to protrude toward the right surface side, and a crimp is defined to be a floating portion of a weft formed on the right surface side by passing above or below a plurality of warps.

    First Embodiment

    [0058] FIG. 1 is a design view showing a complete structure of the two-layer fabric for manufacturing the unwoven fabric of the present invention in a first embodiment. FIG. 2 is a schematic view showing a vertical cross section taken along the warps in FIG. 1. In FIG. 1, since warps on the right surface side of a third pair of warps (4U and 4L, 8U and 8L) are aligned with each other, they are illustrated by dividing two rows for the clarity.

    [0059] The two-layer fabric of the first embodiment in FIG. 1 is a plain weaving structure constituted by a first pair of warps (1Ub and 1Lb), two sets of a second pair of warps (2U and 2L, 3U and 3L), a third pair of warps (4U and 3L), a first pair of warps (5Ub and 5Lb), two sets of a second pair of warps (6U and 6L, 7U and 7L), a third pair of warps (8U and 8L), and the wefts on the right surface side (1U, 2U, 3U, 4U) and wefts on the back surface side (1L, 2L, 3L, 4L).

    [0060] As shown in FIG. 2, the warp 1Ub on the right surface side serving as a binding yarn and constituting a first pair of warps passes below the weft 1L on the back surface side to form a knuckle on the back surface side, and passes between the weft 2U on the right surface side and the weft 2L on the back surface side and passes above the weft 3U on the right surface side to form a knuckle on the right surface side, and passes between the weft 4U on the right surface side and the weft 4L on the back surface side to be woven with each other.

    [0061] In addition, the warp 1Lb on the back surface side serving as a binding yarn and constituting a first pair of warps passes above the weft 1U on the right surface side to form a knuckle on the right surface side, and passes between the weft 2U on the right surface side and the weft 2L on the back surface side and passes below the weft 3L on the back surface side to form a knuckle on the back surface side, and passes between the weft 4U on the right surface side and the weft 4L on the back surface side to be woven with each other.

    [0062] In addition, the warp 2U on the right surface side constituting a second pair of warps passes below the weft 1U on the right surface side, and passes above the weft 2U on the right surface side to form a knuckle on the right surface side, and passes below the weft 3U on the right surface side and above the weft 4U on the right surface side to be woven with each other so as to form a knuckle on the right surface side again.

    [0063] In addition, the warp 3U on the right surface side constituting a second pair of warps passes above the weft 1U on the right surface side to form a knuckle on the right surface side, and passes below the weft 2U on the right surface side and above the weft 3U on the right surface side to form a knuckle on the right surface side again, and passes below the weft 4U on the right surface side to be woven with each other.

    [0064] In addition, the warp 3L on the back surface side constituting a second pair of warps passes below the weft 1L on the back surface side to form a knuckle on the back surface side, and passes above the weft 2L on the back surface side and below the weft 3L on the back surface side to form a knuckle on the back surface side again, and passes between the weft 4L on the back surface side and the weft 4L on the back surface side to be woven with each other.

    [0065] In addition, the warp 4U on the right surface side constituting a third pair of warps passes below the weft 1U on the right surface side and above the weft 2U on the right surface side to form a knuckle on the right surface side, and passes below the weft 3U on the right surface side and above the weft 4U on the right surface side to be woven with each other so as to form a knuckle on the right surface side again.

    [0066] In addition, the warp 4U on the right surface side constituting a third pair of warps passes above the weft 1U on the right surface side to form a knuckle on the right surface side, and passes below the weft 2U on the right surface side and above the weft 3U on the right surface side to form a knuckle on the right surface side, and passes below the weft 4U on the right surface side to be woven with each other.

    [0067] In addition, the warp 5Ub on the right surface side serving as a binding yarn and constituting a first pair of warps passes between the weft 1U on the right surface side and the weft 1L on the back surface side and passes above the weft 2U on the right surface side to form a knuckle on the right surface side, and passes between the weft 3U on the right surface side and the weft 3L on the back surface side and below the weft 4L on the back surface side to a knuckle on the back surface side.

    [0068] In addition, the warp 5Lb on the back surface side serving as a binding yarn and constituting a first pair of warps passes between the weft 1U on the right surface side and the weft 1L on the back surface side and passes below the weft 2L on the back surface side to form a knuckle on the back surface side, and passes between the weft 3U on the right surface side and the weft 3L on the back surface side and above the weft 4U on the right surface side to a knuckle on the right surface side.

    [0069] In addition, the right surface side warp 6U consisting the second pair of warps passes above the right surface side weft 1U to form a knuckle on the right surface side, and passes below the right surface side weft 2U and above the right surface side weft 3U to form a knuckle on the right surface again, and passes below the right surface side weft 4U to be woven with each other. Further, the right surface side warp 6L consisting the second pair of warps passes below the back surface side weft 1L to form a knuckle on the back surface side, and passes above the back surface side weft 2L and below the back surface side weft 3L to form a knuckle on the back surface again, and passes above the back surface side weft 4L to be woven with each other.

    [0070] Further, the right surface side warp 7U consisting the second pair of warps passes below the right surface side weft 1U and above the right surface side weft 2U to form a knuckle on the right surface side, and passes below the right surface side weft 3U and above the right surface side weft 4U to form a knuckle on the right surface again. In addition, the back surface side warp 7L consisting the second pair of warps passes above the back surface side weft 1L and below the back surface side weft 2L to form a knuckle on the back surface side, and passes above the back surface side weft 3L and below the back surface side weft 4L to form a knuckle on the back surface again.

    [0071] In addition, the right surface side warp 8U constituting the third pair of warps passes above the right surface side weft 1U to form a knuckle on the right surface side, and passes below the right surface side weft 2U and above the right surface side weft 3U to form a knuckle on the right surface side again, and passes below the right surface side weft 4U to be woven with each other. Further, the right surface side warp 8U constituting the third pair of warps passes below the right surface side weft 1U and above the right surface side weft 2U to form a knuckle on the right surface, and passes below the right surface side weft 3U and above the right surface side weft 4U to form a knuckle on the right surface side again.

    [0072] The two-layered fabric for manufacturing the unwoven fabric of the first embodiment forms a plain weaving pattern by adopting the above structure. The surface density on the fabric supporting the unwoven fabric can be kept uniform and the sheet supportability can be improved by regularly forming the plain weaving pattern on the surface.

    [0073] In addition, the force supporting the intersection generated on the knuckle of the binding yarn on the right surface side can be alleviated as the entire fabric by arranging three sets of the second pair of warps and the third pair of the warps between two first pair of warps existing the complete structure, so that the sticking of the fibers can be restricted.

    [0074] Further, the rigidity of the fabric can be enhanced by aligning two sets of the second pair of warps, so that the lateral rigidity of the fabric and the diagonal rigidity of the fiber can be improved without a need to arrange auxiliary wefts, etc. inside the fabric.