Mineral composition for generating small water clusters, a small water cluster generating device and a seawater desalination equipment using the same, and a small water cluster generating method
10272357 ยท 2019-04-30
Inventors
Cpc classification
B01D3/34
PERFORMING OPERATIONS; TRANSPORTING
C02F2305/00
CHEMISTRY; METALLURGY
International classification
B01D3/34
PERFORMING OPERATIONS; TRANSPORTING
Abstract
A mineral composition for generating small water clusters, a small water cluster generating device and a seawater desalination equipment using the same and a small water cluster generating method are provided. The mineral composition includes a tourmaline, a quartz, a bleaching earth, a dolomite, a shale, and a porcelain clay. The small water cluster generating device includes the mineral composition and an energy supplying unit for supplying energy. The seawater desalination equipment includes the mineral composition, a heat supplying unit, and a cooling unit. The small water cluster generating method includes using the mineral composition on water or a solution and providing the energy.
Claims
1. A mineral composition for generating small water clusters, comprising: a tourmaline, wherein the weight percent of the tourmaline based on the total weight of the mineral composition is 10 wt %; a quartz, wherein the weight percent of the quartz based on the total weight of the mineral composition is 10 wt %; a bleaching earth, wherein the weight percent of the bleaching earth based on the total weight of the mineral composition is 30 wt %; a dolomite, wherein the weight percent of the dolomite based on the total weight of the mineral composition is 15 wt %; a shale, wherein the weight percent of the shale based on the total weight of the mineral composition is 15 wt %; and a porcelain clay, wherein the weight percent of the porcelain clay based on the total weight of the mineral composition is between 20 wt %.
2. The mineral composition of claim 1, wherein the mineral composition is made by sintering at temperature between 300 C. and 500 C. over 1 hour.
3. The mineral composition of claim 1, wherein the mineral composition is able to absorb an energy and emit a short-wavelength light wave.
4. The mineral composition of claim 1, wherein the energy is selected from the group consisting of heat energy, electromagnetic energy, luminous energy, radiant energy, and a combination thereof.
5. The mineral composition of claim 1, wherein the wavelength of the short-wavelength light wave is 430 m.
6. A small water cluster generating device comprising the mineral composition of claim 1.
7. A small water cluster generating method, comprising: providing the mineral composition of claim 1 in water or a solution; and providing an energy to the mineral composition.
8. The method of claim 7 wherein the mineral composition is able to absorb the energy and emit a short-wavelength light wave.
9. The method of claim 8, wherein the energy is selected from the group consisting of heat energy, electromagnetic energy, luminous energy, radiant energy, and a combination thereof.
10. The method of claim 8, wherein the wavelength of the short-wavelength light wave is 430 m.
Description
BRIEF DESCRIPTION OF THE DRAWINGS
(1)
(2)
(3)
(4)
(5)
DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENT
(6) The mineral composition of the present invention includes a tourmaline, a quartz, a bleaching earth, a dolomite, a shale, and a porcelain clay, wherein the weight percent of the tourmaline based on the total weight of the mineral composition is between 5 wt % and 15 wt %; the weight percent of the quartz based on the total weight of the mineral composition is between 5 wt % and 15 wt %; the weight percent of the bleaching earth based on the total weight of the mineral composition is between 25 wt % and 35 wt %; the weight percent of the dolomite based on the total weight of the mineral composition is between 15 wt % and 20 wt %. The weight percent of the shale based on the total weight of the mineral composition is between 15 wt % and 20 wt %; the weight percent of the porcelain clay based on the total weight of the mineral composition is between 5 wt % and 25 wt %. In the preferred embodiment, the weight percent of the tourmaline based on the total weight of the mineral composition is 10 wt %, the weight percent of the quartz based on the total weight of the mineral composition is 10 wt %, the weight percent of the bleaching earth based on the total weight of the mineral composition is 30 wt %, the weight percent of the dolomite based on the total weight of the mineral composition is 15 wt %, the weight percent of the shale based on the total weight of the mineral composition is 15 wt %, and the weight percent of the porcelain clay based on the total weight of the mineral composition is 20 wt %. In the preferred embodiment, The mineral composition is made by sintering at temperature between 300 C. and 500 C. over 1 hour. In a different embodiment, however, the temperature and time for sintering the mineral composition can be varied depending on the composition, the amount of content, and the manufacturing requirement.
(7) The mineral composition is able to absorb an energy and emits a short-wavelength light wave to break the water clusters into smaller water clusters. More particularly, the energy is selected from the group consisting of heat energy, electromagnetic energy, luminous energy, radiant energy, and a combination thereof. After absorbing the energy, the mineral composition emits the short-wavelength light wave to break the water clusters, wherein the wavelength of the short-wavelength light wave is 430 m. The short-wavelength light wave makes water molecules become individual having low frequency oscillations and hence breaks the hydrogen bond between the water molecules. Furthermore, the water clusters are broken to form small water clusters.
(8) Accordingly, the present invention provides a small water cluster generating device. As the embodiment shown in
(9) As the embodiment shown in
(10) The mineral composition of the present can be further used in seawater desalination. As the embodiment shown in
(11) As the embodiment shown in
(12) As the embodiment shown in
(13) Furthermore, the first section 710 and the second section 720 can be isolated in the distillation chamber 700 by the heat exchanging unit 500. Since the first section has the feeding seawater having lower temperature, the second section has the heating unit 333 heated discharging water vapor 620 having higher temperature, and the heat exchanging unit 500 is disposed between the first section 710 and the second section 720, the temperature of the heat exchanger 500 would be between the feeding seawater 610 and the heating unit 333 heated discharging water vapor 620. In other words, for the feeding seawater 610, the side of the heat exchanging unit 500 corresponding to the first section 710 has higher temperature and is able to serve as a heat supplying unit 300 for supplying heat energy. For discharging water vapor 620 heated by the heating unit 333, the side of the heat exchanging unit 500 corresponding to the second section 720 has lower temperature and is able to serve as a cooling unit 400 for absorbing heat energy. In accordance with the above design, the energy efficiency can be raised.
(14) On the other hand, the mineral composition 100 is able to absorb the heat energy released by the heat supplying unit 300 of the heat exchanging unit 500 and emits the short-wavelength light wave to make water molecules in the feeding seawater 610 become individual having low frequency oscillations, hence breaks the hydrogen bond between the water molecules and makes the water clusters form small water clusters. Thus, other materials originally included between the water clusters, such as sodium, calcium, magnesium, and other ions, are separated from the water molecules. Accordingly, the content of sodium, calcium, magnesium, and other ions in the discharging water vapor 620 are decreased, therefore improving the purity of the formed desalination water. In one embodiment, the desalination water formed by using the seawater desalination equipment 900 of the present invention has sodium less than 5 ppm.
(15) As the embodiment shown in
(16) In different embodiments, the mineral composition of the present invention can also be used in different kinds of seawater desalination equipment. For example, when applying the mineral composition of the present invention in reverse osmosis membrane type seawater desalination equipment, the mineral composition is able to emit the short-wavelength light wave to break the water clusters in the feeding seawater and form small water clusters. Thus, other materials originally included between the water clusters, such as sodium, calcium, magnesium, and other ions, are separated from the water molecules. Accordingly, it decreases the possibility of the water clusters passing through the reverse osmosis membrane together with sodium, calcium, magnesium, and other ions and therefore improves the purity of the formed desalination water.
(17) As the embodiment shown in
(18) Step 1010 involves the step of using the above mentioned mineral composition on water or a solution.
(19) In the preferred embodiment, the method further includes step 1030 of providing an energy, wherein the mineral composition is able to absorb the energy and emit a short-wavelength light wave. The energy is selected from the group consisting of heat energy, electromagnetic energy, luminous energy, radiant energy, and a combination thereof. The wavelength of the short-wavelength light wave is 430 m.
(20) Although the preferred embodiments of the present invention have been described herein, the above description is merely illustrative. Further modification of the invention herein disclosed will occur to those skilled in the respective arts and all such modifications are deemed to be within the scope of the invention as defined by the appended claims.