Method and apparatus for manufacturing a wrinkled net
11518124 ยท 2022-12-06
Assignee
Inventors
Cpc classification
A47K7/02
HUMAN NECESSITIES
International classification
Abstract
A method for manufacturing a wrinkled net includes the step of guiding a net body between two opposed first rollers where the first rollers are rotated to primarily wrinkle the net body, the step of guiding the net body in between two second rollers where the second rollers are rotated to pressurize the net body and heat is generated by friction between the second rollers and the net body to soften the net body, the step of collecting the softened net body in a container where portions of the softened net body are squeezed against one another, and the step of releasing the wrinkled net body from the container after a predetermined period of time in which the portions of the softened the net body are squeezed against one another in the container.
Claims
1. A method for manufacturing a wrinkled net, comprising the steps of: a) guiding a net body between two opposed first rollers where said first rollers are rotated to primarily wrinkle said net body; b) guiding said net body in between two second rollers where said second rollers are rotated to pressurize said net body and heat is generated by friction between said second rollers and said net body to soften said net body without using a heating element; c) collecting the softened said net body in a container where portions of the softened said net body are squeezed against one another; and d) releasing the wrinkled said net body from said container after a predetermined period of time in which the said portions of the softened said net body are squeezed against one another in said container.
2. The method as claimed in claim 1, wherein said net body is deformed under the pressure of said two second rollers such that the wrinkles formed in the surface of said net body in step b) are more pronounced than in step a).
3. The method as claimed in claim 1, wherein an interval between said two second rollers is less than an interval between said two first rollers.
4. The method as claimed in claim 1, wherein a rotational speed of said two second rollers is higher than a rotational speed of said two first rollers.
5. An apparatus for the implementation of the method for manufacturing a wrinkled net as claimed in claim 1, comprising: a container comprising an inlet and an outlet; two opposed second rollers disposed adjacent to said inlet of said container and spaced apart from each other by a predetermined interval; and two opposed first rollers located on the same side of said container as said two second rollers and maintain a distance between said two second rollers, said two first rollers being spaced apart from each other by a predetermined interval.
6. The apparatus as claimed in claim 5, wherein the interval between said two second rollers is less than the interval between said two first rollers.
7. The apparatus as claimed in claim 5, wherein a rotational speed of said two second rollers is higher than a rotational speed of said two first rollers.
8. The apparatus as claimed in claim 5, further comprising a cover plate pivotally connected to said container and biasable between a closed position where said cover plate closes said outlet and an open position where said cover plate is opened from said outlet.
9. The apparatus as claimed in claim 5, further comprising a weight mounted to said cover plate and used to hold said cover plate in said closed position.
Description
BRIEF DESCRIPTION OF THE DRAWINGS
(1)
(2)
(3)
(4)
(5)
(6)
DETAILED DESCRIPTION OF THE INVENTION
(7) The Applicant first describes here, in the entire specification, including the preferred embodiment described below and the claims of the patent application, the nouns relating to directionality are based on the directions in the drawings. In the following preferred embodiment and the drawings, the same reference numerals are used to refer to the same or similar elements or structural features thereof.
(8) Referring to
(9) The container 20 has an inlet 21 and an outlet 22.
(10) The two second rollers 30 are disposed adjacent to the inlet 21 of the container 20. The two first rollers 32 are located on the same side of the container 20 as the two second rollers 30 and maintain a distance between the two second rollers 30. In addition, the interval between the two second rollers 30 is less than the interval between the two first rollers 32, and the rotational speed of the two second rollers 30 is higher than the rotational speed of the two first rollers 32.
(11) The cover plate 23 is pivotally connected to the container 20 and biasable between a closed position P1 (see
(12) The weight 25 is hung on a cantilever rod 24, and one end of the cantilever rod 24 is connected to the outer side of the cover plate 25, so that the cover plate 23 is held in the closed position P1 by the torque generated by the weight 25.
(13) Referring to
(14) Step a): As shown in
(15) Step b): As shown in
(16) Step c): As shown in
(17) Step d): As shown in
(18) As can be seen from the above, the manufacturing method of the present invention softens the net body 40 by means of friction heating, and prolongs the time during which the net body 40 is pressed and deformed in the container 20, thereby increasing the degree of squeezing of the net body 40 in the container 20 and making the surface wrinkle effect better. Therefore, the bathing products made by the net body 40 (such as the bathing ball 44 shown in