FIXING ELEMENT FOR COMPONENTS OF AN ASSEMBLY
20190024697 ยท 2019-01-24
Inventors
- Jean-Philippe MAUREL (Colomiers, FR)
- Frederic LABAL (ROUFFIAC-TOLOSAN, FR)
- Jean-luc Martres (Saint-Jory, FR)
Cpc classification
F16B33/008
MECHANICAL ENGINEERING; LIGHTING; HEATING; WEAPONS; BLASTING
F16B35/00
MECHANICAL ENGINEERING; LIGHTING; HEATING; WEAPONS; BLASTING
International classification
F16B33/00
MECHANICAL ENGINEERING; LIGHTING; HEATING; WEAPONS; BLASTING
F16B33/06
MECHANICAL ENGINEERING; LIGHTING; HEATING; WEAPONS; BLASTING
Abstract
A fixing element for components of an assembly, comprising a rod which is formed by a cylindrical shaft and an end, the rod being a metal component which is at least partially surface-treated by means of anode oxidation and coated over at least a portion of the cylindrical shaft with a lubricating coating. Such a fixing element enables the electrical continuity to be ensured with the components during mounting with moderate interference in the assembly.
Claims
1. An aircraft assembly, comprising: a first component; a second component; and a metal rod comprising a cylindrical shaft and an end for securing the first and second components, the metal rod comprising: a first region that is at least partially surface-treated by means of anode oxidation; and a second region coated over at least a portion thereof with a lubricating coating.
2. The aircraft assembly of claim 1, wherein the cylindrical shaft comprises: at least a first strip that extends a length of the cylindrical shaft and which is surface-treated by means of anode oxidation; and at least a second strip that extends the length of the cylindrical shaft and which is coated with the lubricating coating.
3. The aircraft assembly of claim 2 wherein the cylindrical shaft comprises: a plurality of first strips that are surface-treated by means of anode oxidation; and a plurality of second strips that are coated with a lubricating coating, the first and second strips extending over angular sectors that are distributed around the periphery of the cylindrical shaft.
4. The aircraft assembly of claim 3, wherein the oxidation is a sulfur anode oxidation.
5. The aircraft assembly of claim 4, wherein the metal rod comprises a cylindrical shaft and an end, and wherein a section between the cylindrical shaft and the end is frustroconical.
6. The aircraft assembly of claim 5 wherein the frustoconical section is threaded.
7. The aircraft assembly of claim 4 wherein the anode oxidation is substantially 0.5 microns thick.
8. The aircraft assembly of claim 4 wherein the lubricant coating is substantially 5 microns thick.
9. The aircraft assembly of claim 4 wherein the metal rod is titanium.
10. A method for treating a fixing element that secures an aircraft assembly, the fixing assembly including a rod comprised of a cylindrical shaft, an end section, and an intermediate connecting section, the method comprising: coating at least a first portion of the cylindrical shaft with a lubricant.
11. The method of claim 10 further comprising anode oxidizing at least a second portion of the cylindrical shaft.
Description
BRIEF DESCRIPTION OF THE DRAWINGS
[0019] The various embodiments will hereinafter be described in conjunction with the following drawing figures, wherein like numerals denote like elements, and:
[0020]
[0021]
[0022]
[0023]
[0024]
[0025]
[0026]
[0027]
[0028]
DETAILED DESCRIPTION
[0029] The following detailed description is merely exemplary in nature and is not intended to limit the present disclosure or the application and uses of the present disclosure. Furthermore, there is no intention to be bound by any theory presented in the preceding background or the following detailed description.
[0030] Various embodiments of a fixing element for components of an assembly will now be described with reference to
[0031]
[0032] The cylindrical shaft 12 has a diameter which is substantially greater than the diameter of the threaded end 13 so that the rod 11 comprises a frustoconical connection portion I5 between the cylindrical shaft 12 and the end 13. The fixing element 10 is a metal component and may be produced, for example, from titanium. The use of titanium is particularly preferred for its properties of conductivity and corrosion resistance. Of course, there may be used other metal materials, for example, a nickel alloy of the type Inconel?. In this embodiment, the head 14 and the end 13 of the rod 11 are covered with a lubricating coating R.
[0033] The cylindrical shaft 12 comprises both a portion that is coated with a lubricating coating R and a portion that is surface-treated by means of anode oxidation O or the like. As can clearly be seen in
[0034] The strips that are surface-treated by means of anode oxidation O and the strips that are coated with a lubricating coating R extend over angular sectors of the periphery of the cylindrical shaft 12. In the embodiment illustrated in
[0035] Treatment by means of anode oxidation results in good electrical conductivity at the rod 11 and in particular at the cylindrical shaft 12 of the fixing element 10.
[0036] The surface-treatment of a metal rod by means of anode oxidation of a metal rod is known and does not need to be further described herein. However, in so far as only a portion of the surface of the cylindrical shaft 12 of rod 11 is surface-treated by means of anode oxidation, a cover or mask will be required on the portions of the fixing element which are not subjected to anode oxidation. The thickness of the surface-treatment by means of anode oxidation is approximately 0.5 ?m. It should be noted that in the embodiment of
[0037] The lubricating coating R comprises, for example, a coating based on phenolic resin. It may, for example, be comprised of a coating based on phenolic resin that includes anti-corrosion pigments and/or lubrication pigments. Such a coating is, in particular, marketed under the mark HI-KOTE? and, for example, under the name HI-KOTE? INC.
[0038] Insofar as only one portion of the fixing element 10, and in particular of the rod 11, is coated with the lubricating coating R, it will be applied, for example, by means of atomization or of immersion, using a protective cover or mask applied to the portions of the rod 11 that are not covered with the lubricating coating R. The thickness of the lubricating coating R on the rod 11 is approximately 5 ?m.
[0039] Of course, when the cylindrical shaft 12 comprises a strip that is surface-treated by means of anode oxidation O and a strip that is coated with the lubricating coating R, the arrangement of the longitudinal strips around the cylindrical shaft 12 is not limited to the embodiment described above. For example, the cylindrical shaft 12 may comprise only one strip that is surface-treated by means of anode oxidation O and only one strip that is coated with the lubricating coating R, these strips thus each extending over an angular sector of 180?. Furthermore, in an embodiment in that the cylindrical shaft 12 comprises two strips that are surface-treated by means of anode oxidation O and two strips that are coated with a lubricating coating R, each strip may extend over angular sectors of 90?. In other embodiments, the two strips that are coated with a lubricating coating R may extend over angular sectors that are between 30 and 90?, and the two strips that are treated by means of anode oxidation O may extend over angular sectors between 90 and 150?, respectively. Such an arrangement assures good electrical conductivity when the fixing element 10 is mounted in an assembly.
[0040] Alternatively, the two strips that are coated with a lubricating coating R may extend over angular sectors between 90 and 150?, respectively, and the two strips that have been processed by means of anode oxidation O may extend over angular sectors between 30 and 90?, respectively. This arrangement may provide the assembly of the fixing element 10 with moderate interference.
[0041] In still other embodiments, the number of strips processed by means of anode oxidation O and the number of strips coated with the lubricating coating R are not limited to two but may be greater, for example three or four. Other embodiments are illustrated, for example, in
[0042] In
[0043] In the embodiment illustrated in
[0044] Another embodiment will now be described with reference to
[0045] Longitudinal strips of portions of cylindrical shaft 12 processed by means of anode oxidation O, and portions of cylindrical shaft 12 coated with lubricating coating R may be similar to those described above with reference to
[0046]
[0047] According to an alternative embodiment described in
[0048] The fixing element 10 thus described according to different embodiments enables at least two components P1, P2 to be fixed to each other, as illustrated in
[0049] When a fixing element 10 is mounted by means of interference, the portions of the cylindrical shaft 12 covered with a lubricating coating R promote the sliding action and thus the assembly with moderate interference of the fixing element 10 in a hole that is provided for this purpose in the components P1, P2 of the assembly. Furthermore, the surface components processed by means of anode oxidation ensure electrical continuity between the fixing element 10 and the components P 1, P2, thus ensuring the protection of the assembly against phenomena linked with lightning strikes, in particular in the region of the head 14 of fixing element 10.
[0050] In order to obtain good electrical conductivity between the fixing element 10 and the components P1, P2 of the assembly, it is desirable that the surface-area occupied by the lubricating coating R on the rod portion 11 accommodated in the last assembly component, and in this instance the component P2, not exceed 50% of the inner surface-area of the hole produced in the last component P2. In this manner, when the lubricating coating R is arranged in an annular manner on the rod 11 of the fixing element 10, the width of the lubricating coating R in the longitudinal direction X of the fixing element 10 is less than or equal to half of the thickness of the last assembly component P2 also measured in the longitudinal direction X of the fixing element 10.
[0051] When the lubricating coating R extends in accordance with one or more strips along the length of the cylindrical shaft 12 of the fixing element 10, the cumulative surface-area of the lubricating coating strips R is less than or equal to 50% of the annular portion of the cylindrical shaft 12.
[0052] While at least one exemplary embodiment has been presented in the foregoing detailed description, it should be appreciated that a vast number of variations exist. It should also be appreciated that the exemplary embodiment or exemplary embodiments are only examples, and are not intended to limit the scope, applicability, or configuration of the present disclosure in any way. Rather, the foregoing detailed description will provide those skilled in the art with a convenient road map for implementing an exemplary embodiment, it being understood that various changes may be made in the function and arrangement of elements described in an exemplary embodiment without departing from the scope of the present disclosure as set forth in the appended claims and their legal equivalents.