ELECTROPLATING DEVICE AND ELECTROPLATING METHOD
20240279838 ยท 2024-08-22
Assignee
Inventors
- Hui Wang (Shanghai, CN)
- Hongchao Yang (Shanghai, CN)
- Jian Wang (Shanghai, CN)
- Yinuo Jin (Shanghai, CN)
- Yi Shi (Shanghai, CN)
- Zheng Zhang (Shanghai, CN)
Cpc classification
C25D21/00
CHEMISTRY; METALLURGY
C25D17/06
CHEMISTRY; METALLURGY
C25D17/00
CHEMISTRY; METALLURGY
International classification
C25D17/00
CHEMISTRY; METALLURGY
Abstract
Disclosed in an embodiment of the present invention is an electroplating device, comprising an electroplating tank, a clamp, a positioning cylinder and an anode, wherein the positioning cylinder is located in the electroplating tank; the positioning cylinder is open at one end; the anode is located inside the positioning cylinder, and the positioning cylinder comes in contact with the anode in a sealing manner; and in the entire surface region of the anode, only a first surface comes in contact with an electroplating solution, and the first surface is parallel and opposite to a substrate, with the center of the first surface being aligned with the center of the substrate, and the size of the first surface being similar to that of an effective electroplating region of the substrate. By means of the electroplating device, an electric field generated by the anode is uniformly distributed on the surface of the substrate, thereby improving the uniformity of the electroplating height on the surface of the substrate. Further disclosed in an embodiment of the present invention is an electroplating method using the electroplating device.
Claims
1. An electroplating device, comprising: an electroplating tank, configured to contain an electroplating solution; a clamp, configured to hold a substrate; a positioning cylinder, located in the electroplating tank, one end of the positioning cylinder being open; and an anode, located inside the positioning cylinder, wherein the positioning cylinder comes in contact with the anode in a sealing manner, and in the entire surface region of the anode, only a first surface comes in contact with the electroplating solution, the first surface being parallel and opposite to the substrate, with the center of the first surface being aligned with the center of the substrate, and the size of the first surface being similar to that of an effective electroplating region of the substrate.
2. The electroplating device according to claim 1, wherein the positioning cylinder comes in contact with a second surface of the anode in a sealing manner, the second surface is perpendicular to the first surface.
3. The electroplating device according to claim 1, wherein the positioning cylinder is arranged vertically, the inner wall of the positioning cylinder is provided with at least one ring of sealing member, the sealing member comes in contact with at least the edge of the first surface in a sealing manner, the sealing member has a certain height in the vertical direction.
4. The electroplating device according to claim 1, further comprising a driving device and a controller, the driving device being connected to the anode and the controller respectively, the controller regularly calculates the change in distance between the first surface of the anode and the substrate and controls the driving device, the driving device drives the anode to move toward the substrate to make the distance between the first surface of the anode and the substrate reach a set value.
5. The electroplating device according to claim 4, wherein the anode is arranged vertically, the anode consists of more than two small anodes assembled in horizontal direction, the bottom of the anode is provided with an anode support plate, the driving device is located below the anode support plate, the output shaft of the driving device is connected to the anode support plate.
6. The electroplating device according to claim 1, wherein the electroplating tank is provided with a gas inlet for introducing air or oxygen into the electroplating solution.
7. The electroplating device according to claim 1, further comprising a driving device, a sensor and a controller, the driving device being connected to the anode and the controller respectively, the sensor being connected to the controller, the sensor being arranged on the electroplating tank and configured to detect the position of the first surface of the anode, and sending a first signal or a second signal to the controller according to the detection result, the controller controlling the driving device according to the received first signal or second signal, the driving device driving the anode to move toward the substrate until the distance between the first surface of the anode and the substrate reaches a set value.
8. The electroplating device according to claim 7, wherein the sensor is an infrared sensor, comprising a sending sensor and a receiving sensor, the electroplating tank is provided with two view windows, the infrared light emitted by the sending sensor are received by the receiving sensor through the view windows.
9. The electroplating device according to claim 7, wherein the sensor is a tactile sensor with an elastic contact, the contact of the tactile sensor is installed on the positioning cylinder, when the distance between the first surface of the anode and the substrate is greater than the set value, the first surface of the anode does not contact the contact, at this time, the driving device drives the anode to move toward the substrate to make the first surface of the anode come into contact with the contact.
10. The electroplating device according to claim 7, wherein the inner wall of the positioning cylinder is provided with at least one O-shaped sealing ring, and the at least one O-shaped sealing ring comes in contact with the edge of the first surface in a sealing manner.
11. The electroplating device according to claim 7, wherein the positioning cylinder is arranged vertically, the inner wall of the positioning cylinder is provides with an upper sealing ring, a lower sealing ring and an annular groove, a water inlet channel and a water outlet channel are provided in the positioning cylinder, the upper sealing ring comes in contact with the edge of the first surface in a sealing manner, the lower sealing ring is located below the upper sealing ring, the annular groove is located between the upper sealing ring and the lower sealing ring, the top of the water inlet channel is connected to the annular groove, and the bottom of the water inlet channel is connected to a water inlet pump, the water inlet pump is used to transport liquid from the outside into the annular groove, the top of the water outlet channel is connected to the annular groove, the bottom of the water outlet channel is connected to a water outlet pump, the water outlet pump is used to discharge the liquid in the annular groove to the outside.
12. An electroplating method, comprising: set a positioning cylinder in an electroplating tank, place an anode inside the positioning cylinder, wherein the inner wall of the positioning cylinder comes in contact with the anode in a sealing manner, so that in the surface region of the anode, only a first surface of the anode is in contact with electroplating solution, the first surface of the anode is parallel and opposite to the substrate, with the center of the first surface of the anode being aligned with to the center of the substrate; set a driving device in the electroplating tank, wherein the driving device is contacted to the anode, calculate or detect the change in distance between the first surface of the anode and the substrate, and control the driving device moving to make the anode move toward the substrate until the distance between the first surface of the anode and the substrate reaches a set value.
13. The electroplating method according to claim 12, further comprising introducing air or oxygen into the electroplating solution.
Description
BRIEF DESCRIPTION OF THE DRAWINGS
[0021]
[0022]
[0023]
[0024]
[0025]
[0026]
[0027]
[0028]
[0029]
[0030]
[0031]
[0032]
[0033]
[0034]
[0035]
DETAILED DESCRIPTION OF EMBODIMENTS
[0036] In order to explain the technical content, structural features, objects and effects of the present invention in detail, the following will be described in detail in combination with the embodiments and drawings.
[0037]
[0038] As shown in
[0039] In addition, as shown in
[0040] In order to uniformly distribute the electric field intensity between the anode and the substrate, the present invention improves the design of the electroplating device and method, as shown in the following embodiments.
Embodiment 1
[0041] As shown in
[0042] Regarding the effective electroplating region of the substrate 402, this region refers to an region where metal is deposited. For example, when a circular substrate 402 with a diameter of 300 mm is held by the clamp 409, there is an annular region with a width of 1.5 mm on the edge of the substrate 402 that is wrapped by a lip seal of the clamp 409, this annular region will not be deposited with metal, so the diameter of the effective electroplating region of the substrate 402 is 297 mm.
[0043] As shown in
[0044] In this embodiment, a ring of sealing member 405 is provided on the inner wall of the positioning cylinder 404, and the sealing member 405 comes in contact with at least the top of the side surface of the anode 401 in a sealing manner, so that the electroplating solution 403 does not leak to the side surface of the anode 401 and consume the side surface of the anode 401. Since the upper surface 410 of the anode 401 gradually decreases during the electroplating process, while usually a new anode is replaced before the anode 401 is entirely consumed, the sealing member 405 has at least a certain height in the vertical direction. This height can be a height that can ensure that the edge of the upper surface 410 of the anode 401 comes always in contact with the positioning cylinder 404 in a sealing manner.
[0045] A material of the positioning cylinder 404 can be metal, rigid insulating materials, etc., that does not participate in electrochemical reactions. The inner wall of the positioning cylinder 404 can be provided with a groove, and the sealing member 405 can be embedded in the groove.
Embodiment 2
[0046] As shown in
[0047] The remaining structures are the same as those in embodiment 1, and will not be repeated here.
Embodiment 3
[0048] As shown in
[0049] The inner wall of the positioning cylinder 804 is provided with an O-shaped sealing ring 805, the O-shaped sealing ring 805 comes in contact with the top of the side wall of the anode 801 in a sealing manner, such that in the surface region of the anode 801, only the upper surface 810 of the anode 801 is in contact with the electroplating solution 803, so the electric field generated by anode 801 is emitted entirely from the upper surface 810. The anode 801 may be cylindrical, and the size B of the upper surface 810 of the anode 801 is similar to the size A of the effective electroplating region of the substrate 802, so the size of the cross-section of the electric field generated by the anode 801 is the same (absolutely the same or approximately the same) as the size A of the effective electroplating region of the substrate 802, thus, the uniformity of the electric field distribution can be improved, so that the electric field intensity at each place of the effective electroplating region of the substrate 402 can be close to each other, thereby improving the uniformity of the electroplating height on the surface of the substrate 802.
[0050] Regarding the effective electroplating region of the substrate 802, this region refers to an region where metal is deposited. For example, when a circular substrate 802 with a diameter of 200 mm is held by the clamp 809, there is an annular region with a width of 1 mm on the edge of the substrate 802 that is wrapped by a lip seal of the clamp 809, this annular region will not be deposited with metal, so the diameter of the effective electroplating region of the substrate 802 is 198 mm.
[0051] The sensor 8012 is fixed to the outer wall of the electroplating tank 808, and the sensor 8012 detects whether the upper surface 810 of the anode 801 is located at a set height, so that the distance between the upper surface 810 of the anode 801 and the substrate 802 is maintained at a set value. Specifically, the sensor 8012 is flush with the upper surface 810 of the anode 801, and the upper surface 810 of the anode 801 is detected by the sensor 8012.
[0052] To prevent contamination or damage to the sensor 8012 from electroplating solution overflowing from the electroplating tank 808, a cover may be disposed over the sensor 8012.
[0053] The anode 801 consists of more than two small anodes assembled in a horizontal direction, and the bottom of the anode 801 is provided with an anode support plate 8010. The driving device 8011 is located below the anode support plate 8010, and the output shaft of the driving device 8011 is connected to the anode support plate 8010.
[0054] The controller 8013 is connected to the sensor 8012 and the driving device 8011 respectively.
[0055] During the electroplating process, the anode 801 is gradually consumed, and since the upper surface 810 of the anode 801 is consumed uniformly, the shape of the upper surface 810 always remains unchanged, and therefore the size of the cross-section of the electric field generated by the anode 801 remains unchanged. When the height of the upper surface 810 of the anode 801 is reduced, it cannot be detected by the sensor 8012, at this time, the sensor 8012 sends a first signal to the controller 8013, and after the controller 8013 receiving the first signal, the controller 8013 sends a command to the driving device 8011 to cause the output shaft of the driving device 8011 to move, raising the anode 801 up slowly until the sensor 8012 detects the upper surface 810 of the anode 801 again, at this time, the sensor 8012 sends a second signal to the controller 8013, and after the controller 8013 receiving the second signal, the controller 8013 sends a command to the driving device 8011, and the driving device 8011 stops moving. This allows the upper surface 810 of the anode 801 to always remain at the set height and the distance between the upper surface 810 of the anode 801 and the substrate 802 to be constant, making the process results more stable and not changing with the consumption of the anode.
[0056] It is also possible to infer the height change value of the upper surface 810 of the anode 801 based on the anode metal consumption calculated regularly by controller, so as to control the driving device 8011 to raise the upper surface 810 of the anode 801 up to the initial position. The anode metal consumption is related to factors such as electroplating current, power-on time, electroplating efficiency, etc., and the specific calculation method can be referred to the disclosed text of Japanese patent with Publication No. JP1983113399A. The amplitude of each action of the driving device 8011 should be as small as possible to prevent the upper surface 810 of the anode 801 from detaching from the O-shaped sealing ring 805, resulting in sealing failure.
[0057] As shown in
[0058] In this embodiment, the sensor 8012 is an infrared sensor, comprising a sending sensor and a receiving sensor. Both sides of the electroplating tank 808 are provided with view windows, if the infrared light emitted by the sending sensor passes through the view windows and is sensed by the receiving sensor on the other side, the upper surface 810 of the anode 801 is below the set height, at this time, the anode 801 needs to be raised to make the upper surface 810 of the anode 801 reach the set height.
[0059] In other embodiments, the sensor 8012 can also be a tactile sensor with an elastic contact, the contact of the sensor 8012 is installed on the top of the positioning cylinder 804. When the anode 801 is located below the set height, the contact is not in contact with the upper surface 8109 of the anode 801, at this time, the anode 801 needs to be raised to make the upper surface 8109 of the anode 801 contact with the contact.
[0060] The number of the O-shaped sealing ring 805 can be more than two.
Embodiment 4
[0061] As shown in
[0062] The inner wall of the positioning cylinder 904 is provides with an upper sealing ring 9051, a lower sealing ring 9052, annular groove 9014, and a water inlet channel 9015 and a water outlet channel 9016 are provided in the positioning cylinder 904. The upper sealing ring 9051 comes in contact with the top of the side wall of the anode 901 in a sealing manner, so that in the surface region of the anode 901, only the upper surface 910 of the anode 901 is in contact with the electroplating solution 903, so the electric field generated by the anode 901 is emitted entirely from the upper surface 910. The anode 901 may be cylindrical, and the size B of the upper surface 910 of the anode 901 is similar to the size A of the effective electroplating region of the substrate 902, so the size of the cross-section of the electric field generated by the anode 901 is the same (absolutely the same or approximately the same) as the size A of the effective electroplating region of the substrate 902, thus, the uniformity of the electric field distribution can be improved, so that the electric field intensity at each place of the effective electroplating region of the substrate 902 can be made close to each other, thereby improving the uniformity of the electroplating height on the surface of the substrate 902.
[0063] As shown in
[0064] The sensor 9012 is fixed to the outer wall of the electroplating tank 908, and the sensor 8012 detects whether the upper surface 910 of the anode 901 is located at a set height, so that the distance between the upper surface 910 of the anode 901 and the substrate 902 is maintained at a set value. Specifically, the sensor 9012 is flush with the upper surface 910 of the anode 901, and the upper surface 910 of the anode 901 is detected by the sensor 9012.
[0065] To prevent contamination or damage to the sensor 9012 from electroplating solution overflowing from the electroplating tank 908, a cover may be provided over the sensor 9012.
[0066] The anode 901 consists of more than two small anodes assembled in a horizontal direction, and the bottom of the anode 901 is provided with the anode support plate 9010. The driving device 9011 is located below the anode support plate 9010, and the output shaft of the driving device 9011 is connected to the anode support plate 9010.
[0067] The controller 9013 is connected to the sensor 9012 and the driving device 9011 respectively.
[0068] During the electroplating process, the anode 901 is gradually consumed, and since the upper surface 910 of the anode 901 is consumed uniformly, the shape of the upper surface 910 always remains unchanged, and therefore the size of the cross-section of the electric field generated by the anode 901 remains unchanged. When the height of the upper surface 910 of the anode 901 is reduced, it cannot be detected by the sensor 9012, at this time, the sensor 9012 sends a first signal to the controller 9013, and after the controller 9013 receiving the first signal, the controller 9013 sends a command to the driving device 9011 to cause the output shaft of the driving device 9011 to move, raising the anode 901 up slowly until the sensor 9012 detects again the upper surface 910 of the anode 901, at this time, the sensor 9012 sends a second signal to the controller 9013, and after the controller 9013 receiving the second signal, the controller 9013 sends a command to the driving device 9011, and the driving device 9011 stops moving. This allows the upper surface 910 of the anode 901 to always remain at the set height and the distance between the upper surface 910 of the anode 901 and the substrate 902 to be constant, making the process results more stable and not changing with the consumption of the anode.
[0069] It is also possible to infer the height change value of the upper surface 910 of the anode 901 based on the anode metal consumption calculated regularly by controller, so as to control the driving device 9011 to raise the upper surface 910 of the anode 901 up to the initial position.
[0070] In this embodiment, the sensor 9012 is an infrared sensor, comprising a sending sensor and a receiving sensor. Both sides of the electroplating tank 908 are provided with view windows. If the infrared light emitted by the sending sensor passes through the view windows and is sensed by the receiving sensor on the other side, the upper surface 910 of the anode 901 is below the set height, at this time, the anode 901 needs to be raised to make the upper surface 910 of the anode 901 reach the set height.
Embodiment 5
[0071] As shown in
Embodiment 6
[0072] As shown in
Embodiment 7
[0073] This embodiment provides an electroplating method, comprising: [0074] set a positioning cylinder in an electroplating tank, place an anode inside the positioning cylinder, wherein the inner wall of the positioning cylinder comes in contact with the anode in a sealing manner, so that in the surface region of the anode, only a first surface of the anode is in contact with electroplating solution, the first surface of the anode is parallel and opposite to the substrate and the size of the first surface of the anode is similar to that of the effective electroplating region of the substrate, with the center of the first surface of the anode being aligned with to the center of the substrate; [0075] set a distance between the first surface of the anode and the substrate; [0076] calculate the change in distance between the first surface of the anode and the substrate, drive the anode to move toward the substrate until the distance between the first surface of the anode and the substrate reaches a set value.
Embodiment 8
[0077] This embodiment provides an electroplating method, comprising: [0078] set a positioning cylinder in an electroplating tank, place an anode inside the positioning cylinder, wherein the inner wall of the positioning cylinder comes in contact with the anode in a sealing manner, so that in the surface region of the anode, only a first surface of the anode is in contact with electroplating solution, the first surface of the anode is parallel and opposite to the substrate and the size of the first surface of the anode is similar to that of the effective electroplating region of the substrate, with the center of the first surface of the anode being aligned with to the center of the substrate; [0079] set a distance between the first surface of the anode and the substrate; [0080] detect the position of the first surface of the anode through a sensor and send signal to a controller; [0081] when the distance between the first surface of the anode and the substrate exceeds the set value, the sensor sends a first signal to the controller, after the controller receiving the first signal, the controller sends a command to the driving device, and the driving device drives the anode to move toward the substrate until the distance between the first surface of the anode and the substrate is equal to the set value, at this time, the sensor sends a second signal to the controller, after the controller receiving the second signal, the controller sends a command to the driving device, and the driving device stops moving.
[0082] In order to make the metal ions in the electroplating solution more stable, a gas inlet is opened in the electroplating tank and air or oxygen is introduced into the electroplating solution, and the metal ions are fully oxidized and converted into more stable metal ions under the action of oxygen.
[0083] In summary, the present invention, by means of the above-described embodiments and related illustrations, has specifically and in detail disclosed the relevant technology, so that those skilled in the art can be implemented accordingly. The above-mentioned embodiments are only used to illustrate the present invention, and are not used to limit the present invention, the scope of rights of the present invention shall be defined by the Claims of the invention. Changes in the number of components or substitution of equivalent components as described herein shall still be within the scope of the present invention.