METHOD FOR ENHANCED INTERVENTIONAL IMAGING FOR CRACKS IN HYDRAULIC FRACTURING TEST OF ROCKS

20180306736 ยท 2018-10-25

Assignee

Inventors

Cpc classification

International classification

Abstract

A method for enhanced interventional imaging for cracks, improving the precision in observing cracks in rock hydraulic fracturing test, benefiting for scientifically understanding regular pattern of development of hydraulically fractured cracks in rocks. The technical solution comprises: hydraulically fracturing the rock with aqueous solutions containing nanoscale interventional contrast-enhanced agent which has a high atomic number; forming hydraulically fractured cracks, wherein the difference in mass attenuation coefficient / of x-ray between the cracks and the rock is improved by the interventional contrast-enhanced agent in the cracks, moreover, the difference in mass energy absorption coefficient .sub.en/ of x-ray between the cracks and the rock is improved, then the linear attenuation coefficient of the reception of detector is changed, improving the imaging resolution for hydraulically fractured cracks in the rock.

Claims

1. A system for high precision imaging for cracks in a rock hydraulic fracturing test, comprising: a laboratorial x-ray industrial CT, a high precision rotary platform and a hydraulic fracturing testing machine for rocks provided on the high precision rotary platform, wherein the hydraulic fracturing testing machine for rocks includes a support device, a peripheral pressurizing device, an axial pressurizing device and a high pressure water pump, wherein the support device is used for clamping a rock sample to be fractured, the peripheral pressurizing device is disposed to surround the rock sample and used for applying pressure on periphery of the rock sample, the axial pressurizing device is provided below the support device and used for applying axial pressure to the rock sample, the high pressure water pump is used for delivering interventional contrast-enhanced agent into the rock sample to form cracks within the rock sample, wherein the laboratorial x-ray industrial CT is used for forming a CT image of the cracks within the rock sample, wherein the interventional contrast-enhanced agent is a dispersed nano bismuth solution which is made by the following steps: stirring a dispersant with a mass fraction of 5%, a nano bismuth powder with a mass fraction of 20% and a polyethylene glycol with a mass fraction of 75% for a first time period via a high speed rotor instrument, and vibrating them for a second time period via an ultrasonic vibrator.

2. The system as defined by claim 1, wherein the particle diameters of the nano bismush is 40-50 nm.

3. The system as defined by claim 2, wherein the first time period is 10 minutes, and the second time period is 30 minutes.

4. The system as defined by claim 3, wherein the support device includes an upper spacer and a lower spacer, the upper spacer and the lower spacer support the rock sample from upper and lower sides of the rock sample respectively.

5. The system as defined by claim 4, wherein the peripheral pressurizing device includes a triaxial cylinder surrounding the rock sample and a peripheral pressurizing pump in communication with the triaxial cylinder, and the peripheral pressurizing pump supplies power for the triaxial cylinder to apply peripheral pressure to the rock sample.

6. The system as defined by claim 5, wherein the axial pressurizing device includes an axial actuator disposed on the high precision rotary platform and a self-balancing piston disposed on the axial actuator, and the axial actuator applies axial pressure to the rock sample through the self-balancing piston.

7. The system as defined by claim 6, wherein the laboratorial x-ray industrial CT includes an x-ray source and a CT detector, the x-ray source is used for emitting x-ray beam, and the CT detector is used for receiving the x-ray beam penetrating the rock sample and forming a CT image based on a distribution of linear attenuation coefficient of the x-ray beam.

8. A method for high precision imaging for cracks in rock hydraulic fracturing test, realized by the system of claim 7, wherein the method comprises following steps: Step 1, putting the rock sample between the upper spacer and the lower spacer; Step 2, peripherally pressurizing the rock sample by means of the triaxial cylinder and the peripheral pressurizing pump; Step 3, axially pressurizing the rock sample by means of the self-balancing piston and the axial actuator; Step 4, supplying the interventional contrast-enhanced agent into the rock sample by means of the high pressure pump to form the fractured cracks; Step 5, at the same time when Steps 2, 3 and 4 being executed, rotating the high precision rotary platform; Step 6, after the cracks being formed within the rock sample, penetrating the rock sample by the x-ray beam emitted from the x-ray source, and receiving the x-ray beam penetrating the rock sample and forming a CT image based on a distribution of linear attenuation coefficient of the x-ray beam by the CT detector.

Description

BRIEF DESCRIPTION OF DRAWINGS

[0012] FIG. 1 is an exemplary diagram showing a system for imaging cracks in a rock, where

[0013] 1: rock sample;

[0014] 2: upper spacer;

[0015] 3: lower spacer;

[0016] 4: spherical pedestal;

[0017] 5: triaxial cylinder;

[0018] 6: fractured cracks;

[0019] 7: peripheral pressuring pump;

[0020] 8: upper cavity of self-balancing piston;

[0021] 9: lower cavity of self-balancing piston;

[0022] 10: self-balancing piston 10;

[0023] 11: axial actuator 11;

[0024] 12: high precision rotary platform;

[0025] 13: high pressure water pump containing interventional contrast-enhanced agent;

[0026] 14: x-ray source;

[0027] 15: detector;

[0028] 16: detector post;

[0029] 17: x-ray source post;

[0030] 18: x-ray beam;

[0031] 19: foundation base;

DESCRIPTION OF EMBODIMENTS

[0032] 1. First, formulating an interventional contrast-enhanced agent for cracks at a certain concentration: stirring a dispersant with a mass fraction of 5%, a nano bismuth powder with a mass fraction of 20%, and a polyethylene glycol with a mass fraction of 75% for 10 min via a high speed rotor instrument, and vibrating them for 30 min via an ultrasonic vibrator to obtain a dispersed nano bismuth solution, wherein the particle diameters of the nano bismush is 40-50 nm, then adding the interventional contrast-enhanced agent into the high pressure water pump 13. [0033] 2. The hydraulic fracturing testing machine is disposed on the high precision rotary platform 12, the rock sample 1 is disposed between the upper spacer 2 and the lower spacer 3, the spherical pedestal 4 reduces the end face effect of the rock sample 1 when loading, the triaxial cylinder 5 and the peripheral pressuring pump 7 implement peripheral pressure loading for the rock sample 1, and the upper cavity 8 of the self-balancing piston, the lower cavity 9 of the self-balancing piston, the self-balancing piston 10 and the axial actuator 11 ensure implementation of axial loading for the rock sample 1, when the hydraulic fracturing testing machine for rocks is loaded for peripheral pressure, axial compression and hydraulic fracturing, the rotary platform 12 rotates at a certain rate. [0034] 3. Running the laboratorial x-ray industrial CT, an x-ray beam 18 emitted from the x-ray source 14 penetrates the rock sample 1, the x-rays after penetration are received by the detector 15, and a CT image is formed based on a distribution of linear attenuation coefficient. [0035] 4. Pressing the interventional contrast-enhanced agent into the rock sample 1, fracturing the rock sample 1 to form fractured cracks 6 in the rock sample 1, which are filled with a nanogold aqueous solution, utilizing the principle of the interventional contrast-enhanced agent, which improves the difference in mass attenuation coefficient / between different substances, i.e., increases the difference in mass energy absorption coefficient .sub.en/ between different substances, affecting the process of x-ray projection, to change the linear attenuation coefficient of the reception of the detector 15, and then to improve the imaging resolution of the hydraulically fractured cracks 6 in the rock.