Method of Constructing Composite Stiffened Building Materials
20240293995 ยท 2024-09-05
Inventors
Cpc classification
B32B15/20
PERFORMING OPERATIONS; TRANSPORTING
B32B2305/30
PERFORMING OPERATIONS; TRANSPORTING
B32B2250/42
PERFORMING OPERATIONS; TRANSPORTING
B32B3/30
PERFORMING OPERATIONS; TRANSPORTING
B32B7/12
PERFORMING OPERATIONS; TRANSPORTING
B32B21/02
PERFORMING OPERATIONS; TRANSPORTING
B32B21/14
PERFORMING OPERATIONS; TRANSPORTING
International classification
B32B7/12
PERFORMING OPERATIONS; TRANSPORTING
B32B38/00
PERFORMING OPERATIONS; TRANSPORTING
Abstract
This patent is a new method of constructing composite stiffened building materials. Conventional door construction materials are made of solid wood, MDF, or LVL. Solid wood tends to move over time and is very heavy. MDF and LVL core doors tend to be extremely heavy and both have a tendency to delaminate or move over time, especially when exposed to moisture. This new method of building stile and rail doors will create lasting stile and rail doors of any size last without warping and remaining high strength, lightweight, and rigid. The stiles, or horizontal members, and rails, or vertical members, can be made of honeycomb core, laminated alternating wood products and stiffening materials like the Composite Stiffener, U.S. Patent No. 63/313,649.
The composite stiffener comprises of multiple layers (at least 2) of aluminum, formica, plastic, sheet metals, fiberglass, or other strengthening materials: plywood, vencer, multiple layers of veneer, MDF, or other wood products for adequate bonding surface; and honeycomb core, paper core, hollow core, or other filler materials. The materials listed above can alternate and be adhered with an adhesive. Once the adhesive is fully cured, the layers of materials can be cut length-wise or width-wise perpendicular to the width edge of the sandwiched materials. Thickness of the section being cut is determined by the thickness of the core used in the panel the composite stiffener is intended for. The section that was previously cut off, is the composite stiffener, to be placed with the end grain to each surface of the panel requiring the stiffener. With the end grain of the stiffener facing the inner surface of the panel, or the stiffener layers are perpendicular to the surface of the panel, ensures the panel containing the stiffener will remain straight and not warp, bend, twist, or otherwise fail.
The composite stiffener material can have lumber adhered to at least two sides with any adhesive. Skin material can be adhered to the top and bottom faces of the composite stiffener core material. Skin material can be flat building materials such as plywood, vencer, multiple layer vencer, MDF, HPL, formica, plastics, aluminum, metals, fiberglass, or other flat building materials. This creates the composite stiffened building materials like stiles and rails material. They can be profiled to fit together with the desired amount of panels.
Claims
1. The composite stiffened building materials comprises of multiple layers (at least 2) of aluminum, formica, plastic, sheet metals, fiberglass, or other strengthening materials: plywood, veneer, multiple layers of veneer, MDF, or other wood products for adequate bonding surface; and honeycomb core, paper core, hollow core, or other filler materials. The materials listed above can alternate and be adhered with an adhesive. Once the adhesive is fully cured, the layers of materials can be cut length-wise or width-wise perpendicular to the width edge of the sandwiched materials. Thickness of the section being cut is determined by the thickness of the core used in the panel the composite stiffener is intended for. The section that was previously cut off, is the composite stiffener, to be placed with the end grain to each surface of the panel requiring the stiffener. With the end grain of the stiffener facing the inner surface of the panel, or the stiffener layers are perpendicular to the surface of the panel, ensures the panel containing the stiffener will remain straight and not warp, bend, twist, or otherwise fail.
2. In accordance of claim 1, the composite stiffened building materials can be used in a wide variety of applications as conventional lumber can be used. This can replace conventional lumber products such as dimensional lumber, studs, posts, beams, door frames, window frames, or any other building materials.
3. In accordance with claim 1, the composite building material can be sandwiched between at least two pieces of lumber, metal, plastic, fiberglass, HPL, MDF, or other flat sheet goods. The top and bottom surfaces can have a skin material adhered. Skin material can be any flat sheet building materials. The skin applied will greatly increase the shear strength of the composite stiffened building materials.
4. In accordance with claim 1, the composite stiffened building material can be profiled with any shape, like tongue and groove, to be made into stile and rail doors, doors with glass inserts, doors with raised panels, door frames, window frames, and many more applications.
Description
SHORT FIGURE DESCRIPTION OF DRAWINGS
[0014]
[0015]
[0016]
[0017]
[0018]
[0019]
[0020]
[0021]
[0022]
[0023]
[0024]
[0025]
DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0026] The composite stiffened building material is comprised of at least two layers of aluminum, formica, plastic, sheet metals, fiberglass, or other strengthening materials: plywood, vencer, multiple layers of vencer, MDF, or other wood products for adequate bonding surface; and honeycomb core, paper core, hollow core, or other filler materials. The alternating layers of lumber 1-1 and stiffening material 1-2 can be adhered together to form a block