HIGH-DENSITY FLUIDIZED BED SYSTEMS HEAT BALANCE
20220356405 · 2022-11-10
Assignee
Inventors
Cpc classification
C10G2300/1044
CHEMISTRY; METALLURGY
C10G2300/104
CHEMISTRY; METALLURGY
International classification
Abstract
Methods for catalytic cracking hydrocarbon mixture have been disclosed. A hydrocarbon mixture having an initial boiling temperature of 30° C. to 70° C. is catalytically cracked in the presence of a catalyst to produce one or more olefins and/or one or more aromatics. The catalytic cracking is conducted such that the amount of coke formed on the catalyst is at least 5 wt. % (based on total weight of spent catalyst). The catalyst from the catalytic cracking step is then regenerated to produce regenerated catalyst.
Claims
1. A method of producing olefins and/or aromatics, the method comprising: contacting a hydrocarbon mixture having an initial boiling point of 30° C. to 70° C. with catalyst particles of a catalyst bed, in a reactor, under reaction conditions effective to produce one or more olefins and/or one or more aromatics; and regenerating the catalyst particles, in response to coke content of the catalyst bed being at least 5 wt. %.
2. The method of claim 1, wherein the catalyst is regenerated in response to coke content of the catalyst bed being at least 10 wt.
3. The method of 1, wherein the reaction conditions include a superficial gas velocity in a range of 2 to 7 m/s.
4. The method of 1, wherein the one or more olefins are selected from the group consisting of ethylene, propylene, 1-butene, 2-butene and isobutene, or combinations thereof.
5. The method of 1, wherein the one or more aromatics are selected from the group consisting of benzene, toluene and xylene, or combinations thereof.
6. The method of 1, further comprising: prior to the regenerating step, determining coke content of the catalyst bed; and removing the catalyst particles from the reactor.
7. The method of claim 6, wherein the regenerating comprises flowing a regenerating gas comprising oxygen to the regenerator.
8. The method of claim 6, wherein the regenerating is conducted at a regeneration temperature of 550 to 850° C.
9. The method of 1, wherein the catalyst bed includes a circulating fluidized catalyst bed.
10. The method of 1, wherein the catalyst bed has a diameter to height ratio in a range of 0.05 to 3.6.
11. The method of 1, wherein the reactor comprises baffles therein configured to control back mixing in the catalyst bed.
12. The method of 1, wherein the reaction conditions include a residence time in a range of 5 to 120 minutes.
13. The method of 1, wherein the reaction conditions include a reaction temperature of 500 to 800° C. and a reaction pressure of 0.9 to 3 atm.
14. The method of claim 2, wherein the catalyst bed includes a circulating fluidized catalyst bed.
15. The method of claim 2, wherein the catalyst bed has a diameter to height ratio in a range of 0.05 to 3.6.
16. The method of claim 2, wherein the reactor comprises baffles therein configured to control back mixing in the catalyst bed.
17. The method of claim 2, wherein the reaction conditions include a residence time in a range of 5 to 120 minutes.
18. The method of claim 2, wherein the reaction conditions include a reaction temperature of 500 to 800° C. and a reaction pressure of 0.9 to 3 atm.
19. The method of claim 1, wherein the reaction conditions include a reaction temperature of 500° C. and a reaction pressure of 3 atm.
20. The method of claim 1, wherein the reaction conditions include a reaction temperature of 800° C. and a reaction pressure of 0.9 atm.
Description
BRIEF DESCRIPTION OF THE DRAWINGS
[0022] For a more complete understanding, reference is now made to the following descriptions taken in conjunction with the accompanying drawings, in which:
[0023]
DETAILED DESCRIPTION OF THE INVENTION
[0024] Currently, the catalytic cracking processes for producing olefins and/or aromatics suffer several drawbacks that limit the production efficiency and increase the production for olefins and aromatics. In particular, the catalyst regenerating process of the conventional catalytic cracking methods may not produce sufficient heat for the catalytic cracking process, resulting in low production efficiency for olefins and aromatics. Adding fuel to increase the temperature of the catalyst may be able to mitigate the problem. However, this can increase the production cost for olefins and aromatics and reduce the catalyst stability or catalyst life time. The present invention provides a solution to this problem. The solution is premised. on a method of catalytic cracking hydrocarbons that includes catalytically cracking naphtha until the spent catalyst contains at least 5 wt. % coke, and regenerating the spent catalyst by burning the coke. The heat released from coke burning is used to provide sufficient heat for the catalytic cracking reaction. This disclosed method is capable of mitigating the problem of conventional catalytic cracking processes that gets insufficient reaction heat. Additionally, the catalytic cracking reactor used in the disclosed method can include internal baffles to control the back mixing and gas distribution in the reactor, resulting in improved heat distribution and, consequently, improved production efficiency for olefins and aromatics. These and other non-limiting aspects of the present invention are discussed in further detail in the following section.
Method of Producing Olefins and/or Aromatics
[0025] Methods of catalytic cracking hydrocarbons to produce olefins and aromatics have been discovered. The methods may be capable of mitigating the issue of insufficient heat generated by catalyst regeneration for the conventional catalytic cracking processes. As shown in
[0026] According to embodiments of the invention, as shown in block 101, method 100 includes contacting a hydrocarbon mixture having an initial boiling point of 30° C. to 70° C. with catalyst particles of a catalyst bed under reaction conditions effective to produce one or more olefins and/or one or more aromatics. In embodiments of the invention, the hydrocarbon mixture includes light naphtha (initial boiling point of 10° C. and final boiling point 70° C.), heavy naphtha (initial boiling point of 71° C. and final boiling point 200° C.), or full range naphtha (initial boiling point of 25° C. and final boiling point 204° C.). Non-limiting examples of the catalyst particles include ZSM-5, Y-Zeolite, Beta-Zeolite, SAPO-34, all zeolite and dual function catalyst with a “zeolite and metallic” composition, or combinations thereof. In embodiments of the invention, the catalyst particles may have a particle density of 800 to 1300 kg/m.sup.3 and all ranges and values there between including ranges of 800 to 900 kg/m.sup.3, 900 to 1000 kg/m.sup.3, 1000 to 1100 kg/m.sup.3, 1100 to 1200 kg/m.sup.3, and 1200 to 1300 kg/m.sup.3. In embodiments of the invention, the contacting at block 101 is conducted in a fluidized bed reactor. The fluidized bed reactor may comprise a fluidized catalyst bed having a catalyst fraction volume of 5 to 15% and all ranges and values there between including 5 to 6%, 6 to 7%, 7 to 8%, 8 to 9%, 9 to 10%, 10 to 11%, 11 to 12%, 12 to 13%, 13 to 14%, and 14 to 15%. The one or more olefins produced in the contacting step at block 101 may include light olefins comprising ethylene, propylene, 1-butene, 2-butene, isobutene, or combinations thereof. The one or more aromatics produced in the contacting step at block 101 may include benzene, toluene, xylene, or combinations thereof.
[0027] In embodiments of the invention, the fluidized bed reactor is a circulating fluidized bed reactor. The circulating fluidized bed reactor may have a fluidized bed having diameter to height ratio in a range of 0.05 to 3.6 and all ranges and values there between including ranges of 0.05 to 0.10, 0.10 to 0.20, 0.20 to 0.30, 0.30 to 0.40, 0.40 to 0.50, 0.50 to 0.60, 0.60 to 0.70, 0.70 to 0.80, 0.80 to 0.90, 0.90 to 1.0, 1.0 to 1.5, 1.5 to 2.0, 2.0 to 2.5, 2.5 to 3.0, and 3.0 to 3.6. In embodiments of the invention, the fluidized bed reactor includes one or more internal baffles disposed therein. The internal baffles may be configured to guide the catalyst particles and hydrocarbon in the fluidized bed reactor and control the back mixing in the fluidized bed reactor. In embodiments of the invention, the control of the back mixing in the fluidized bed reactor is configured to control light olefins to BTX ratio in a product stream from the fluidized bed reactor. The internal baffles may be further configured to improve gas distribution in the fluidized bed and improve contact between the catalyst particles and hydrocarbons. The internal baffles may be further configured to improve heat distribution in the catalyst bed.
[0028] According to embodiments of the invention, the reaction conditions at block 101 include a superficial gas velocity in the catalyst bed in a range of 2 to 7 m/s and all ranges and value there between including ranges of 2 to 3 m/s, 3 to 4 m/s, 4 to 5 m/s, 5 to 6 m/s, and 6 to 7 m/s. The reaction conditions at block 101 may include a residence time of 5 to 120 min (minutes) and all ranges and values there between including ranges of 5 to 10 min, 10 to 15 min, 15 to 20 min, 20 to 25 min, 25 to 30 min, 30 to 35 min, 35 to 40 min, 40 to 45 min, 45 to 50 min, 50 to 55 min, 55 to 60 min, 60 to 65 min, 65 to 70 min, 70 to 75 min, 75 to 80 min, 80 to 85 min, 85 to 90 min, 90 to 95 min, 95 to 100 min, 100 to 105 min, 105 to 110 min, 110 to 115 min, and 115 to 120 min. The reaction conditions at block 101 may further include a reaction temperature of 500 to 800° C. and all ranges and values there between including ranges of 500 to 510° C., 510 to 520° C., 520 to 530° C., 530 to 540° C., 540 to 550° C., 550 to 560° C., 560 to 570° C., 570 to 580° C., 580to 590° C., 590 to 600° C., 600 to 610° C., 610 to 620° C., 620 to 630° C., 630 to 640° C., 640 to 650 ° C., 650 to 660° C., 660 to 670° C., 670 to 680° C., 680 to 690° C., 690 to 700° C., 700 to 710° C., 710 to 720° C., 720 to 730° C., 730 to 740° C., 740 to 750° C., 750 to 760° C., 760 to 770° C., 770 to 780° C., 780 to 790° C., and 790 to 800° C. The reaction conditions at block 101 may further still include a reaction pressure of 0.9 to 3 atm and all ranges and values there between including ranges of 0.9 to 1.2 atm, 1.2 to 1.5 atm, 1.5 to 1.8 atm, 1.8 to 2.1 atm, 2.1 to 2.4 atm, 2.4 to 2.7 atm, 2.7 to 3.0 atm.
[0029] According to embodiments of the invention, method 100 includes determining coke content the catalyst bed, as shown in block 102. Coke content of the catalyst bed may increase with duration of the contacting step at block 101. According to embodiments of the invention, as shown in block 103, method 100 includes removing the catalyst particles from the reactor. At block 103, the catalyst particles can be transported from the reactor to a catalyst regenerator. In embodiments of the invention, the reactor is a fluidized bed reactor and the catalyst is separated from a reaction mixture comprising the products produced in the contacting step at block 101, prior to being transported to the catalyst regenerator. In embodiments of the invention, the reaction mixture and the catalyst are separated in a cyclone separation units comprising one or more cyclonic separators.
[0030] In embodiments of the invention, as shown in block 104, method 100 includes regenerating the catalyst particles, in response to coke content of the catalyst bed being at least 5 wt. %, preferably at least 10 wt. %, more preferably at least 15 wt. %, based on total weight of the catalyst. In embodiments of the invention, regenerating at block 104 includes flowing, under regenerating conditions, a regenerating gas through catalyst particles in the catalyst regenerator. The regenerating gas may include oxygen, air, or combinations thereof. At block 104, regenerating conditions may include a regenerating temperature of 550 to 850° C. and all ranges and values there between including ranges of 550 to 600° C., 600 to 650° C., 650 to 700° C., 700 to 750° C., 750 to 800° C., and 800 to 850° C. The regenerating conditions at block 104 may further include flowing regenerating gas on turbulent fluidization regime with less than 2 m/s velocity. In embodiments of the invention, the regenerating at block 104 may restore sufficient heat to the regenerated catalyst for catalytically cracking the hydrocarbon mixture at a reaction temperature of 500 to 800° C. The regenerated catalyst may be transported back to the reactor for catalytic cracking.
[0031] Although embodiments of the present invention have been described with reference to blocks of
[0032] The systems and processes described herein can also include various equipment that is not shown and is known to one of skill in the art of chemical processing. For example, some controllers, piping, computers, valves, pumps, heaters, thermocouples, pressure indicators, mixers, heat exchangers, and the like may not be shown.
[0033] In the context of the present invention, at least the following 13 embodiments are described. Embodiment 1 is a method of producing olefins and/or aromatics. The method includes contacting a hydrocarbon mixture having an initial boiling point of 30° C. to 70° C. with catalyst particles of a catalyst bed, in a reactor, under reaction conditions effective to produce ogle or more olefins and/or one or more aromatics. The method further includes regenerating the catalyst particles, in response to coke content of the catalyst bed being at least 5 wt. %. Embodiment 2 is the method of embodiment 1, wherein the catalyst is regenerated in response to coke content of the catalyst bed being at least 10 wt. %. Embodiment 3 is the method of either of embodiments 1 or 2, wherein the reaction conditions include a superficial gas velocity in a range of 2 to 7 m/s. Embodiment 4 is the method of any of embodiments 1 to 3, wherein the one or more olefins include ethylene, propylene, 1-butene, 2-butene, isobutene, or combinations thereof. Embodiment 5 is the method of any of embodiments 1 to 4, wherein the one or more aromatics include benzene, toluene, xylene, or combinations thereof. Embodiment 6 is the method of any of embodiments 1 to 5, further including, prior to the regenerating step, determining coke content of the catalyst bed, and removing the catalyst particles from the reactor. Embodiment 7 is the method of embodiment 6, wherein the regenerating includes flowing a regenerating gas containing oxygen to the regenerator. Embodiment 8 is the method of either of embodiments 6 or 7, wherein the regenerating is conducted at a regeneration temperature of 550 to 850° C. Embodiment 9 is the method of any of embodiments 1 to 8, wherein the catalyst bed includes a circulating fluidized catalyst bed. Embodiment 10 is the method of any of embodiments 1 to 9, wherein the catalyst bed has a diameter to height ratio in a range of 0.05 to 3.6. Embodiment 11 is the method of any of embodiments 1 to 10, wherein the reactor includes baffles therein configured to control back mixing in the catalyst bed. Embodiment 12 is the method of any of embodiments 1 to 11, wherein the reaction conditions include a residence time in a range of 5 to 120 minutes. Embodiment 13 is the method of any of embodiments 1 to 12, wherein the reaction conditions include a reaction temperature of 500 to 800° C. and a reaction pressure of 0.9 to 3 atm.
[0034] Although embodiments of the present application and their advantages have been described in detail, it should be understood that various changes, substitutions and alterations can be made herein without departing from the spirit and scope of the embodiments as defined by the appended claims. Moreover, the scope of the present application is not intended to be limited to the particular embodiments of the process, machine, manufacture, composition of matter, means, methods and steps described in the specification. As one of ordinary skill in the art will readily appreciate from the above disclosure, processes, machines, manufacture, compositions of matter, means, methods, or steps, presently existing or later to be developed that perform substantially the same function or achieve substantially the same result as the corresponding embodiments described herein may be utilized. Accordingly, the appended claims are intended to include within their scope such processes, machines, manufacture, compositions of matter, means, methods, or steps.