Abstract
A flash-free mold assembly (100) is provided. The mold assembly comprises a first plate (110) and a second plate (112) adapted to be superimposed on the first plate to define a mold space therein. The first plate comprises one or more projections (120, 122) surrounding the mold space, and the second plate is adapted to be superimposed on the first plate such that it primarily contacts the one or more projections of the first plate.
Claims
1. A mold assembly for use in the manufacture of an article of footwear, the mold assembly comprising: a first plate having a plate surface and at least one mold cavity, the first plate having one or more projections extending upward from the plate surface and surrounding the at least one mold cavity, wherein the plate surface surrounds the one or more projections; and a second plate operably coupled to the first plate and adapted to be superimposed on the first plate to define a mold space therein, wherein when the second plate is superimposed on the first plate, the second plate is adapted to primarily contact the one or more projections of the first plate, wherein the mold assembly is effective to mold the article of footwear, the article of footwear comprising at least a top surface, a bottom surface, and a side surface having a continuous skin at the intersection of the first plate and the second plate.
2. The mold assembly of claim 1, wherein the one or more projections completely surround the mold cavity.
3. The mold assembly of claim 1, wherein the one or more projections comprise two projections.
4. The mold assembly of claim 1, wherein the plate surface entirely surrounds the one or more projections of the first plate.
5. The mold assembly of claim 1, wherein the first plate is constructed of a material that deforms to a first degree in response to a fixed force, and wherein the second plate is constructed of a material that deforms to a second degree in response to the fixed force.
6. The mold assembly of claim 5, wherein the first degree of deformation of the first plate is less than the second degree of deformation of the second plate in response to the fixed force.
7. The mold assembly of claim 1, wherein the first plate is constructed of steel.
8. The mold assembly of claim 1, wherein the second plate is constructed of either aluminum or bronze.
9. The mold assembly of claim 1, wherein the second plate further comprises one or more vent apertures in communication with the mold space when the second plate is superimposed on the first plate.
10. The mold assembly of claim 1, wherein the second plate further comprises one or more depressions adapted to receive the one or more projections of the first plate when the second plate is superimposed on the first plate.
11. A molded article of footwear having the following features: a top surface; a bottom surface; and a side surface, the side surface having a continuous skin at an intersection of a first plate and a second plate of a mold assembly.
12. The molded article of footwear of claim 11, wherein the molded article of footwear comprises a midsole.
13. The molded article of footwear of claim 11, wherein the molded article of footwear comprises one of an outsole or a combination midsole/outsole.
14. A method of molding an article of footwear comprising the steps of: providing a fixed quantity of moldable compound; providing a mold assembly effective to form the article of footwear; and molding the article of footwear, the article of footwear having a top surface, a bottom surface, and a side surface having a continuous skin at an intersection of a first plate and a second plate of the mold assembly.
15. The method of molding of claim 14, wherein the first plate of the mold assembly comprises a plate surface and at least one mold cavity, the first plate having one or more projections extending upward from the plate surface and surrounding the at least one mold cavity, wherein the plate surface surrounds the one or more projections; and wherein the second plate is operably coupled to the first plate and is adapted to be superimposed on the first plate to define a mold space therein, wherein when the second plate is superimposed on the first plate, the second plate is adapted to primarily contact the one or more projections of the first plate.
16. The method of molding of claim 15, further comprising: determining an amount of pressure needed to cure the fixed quantity of moldable compound within a predetermined period of time; determining an area of contact between the first plate and the second plate of the mold assembly; and determining a force to be applied by a mold press to the mold assembly based on the amount of pressure needed to cure the fixed quantity of moldable compound and the area of contact between the first plate and the second plate.
17. The method of molding of claim 16, wherein the amount of pressure needed to cure the fixed quantity of moldable compound is further determined based on a temperature within the mold space.
18. The method of molding of claim 14, wherein molding the article of footwear comprises: placing the fixed quantity of moldable compound in the mold cavity of the first plate; superimposing the second plate onto the first plate of the mold assembly; and applying the force to the mold assembly for the predetermined period of time to form the article of footwear.
19. The method of molding of claim 18, wherein placing the fixed quantity of moldable compound in the mold cavity comprises injecting the moldable compound into the mold cavity.
20. The method of molding of claim 18, wherein placing the fixed quantity of moldable compound in the mold cavity comprises placing a pellet form of the fixed quantity of moldable compound in the mold cavity.
Description
BRIEF DESCRIPTION OF THE DRAWING
[0011] The present invention is described in detail below with reference to the attached drawing figures, wherein:
[0012]
[0013]
[0014]
[0015]
[0016]
[0017]
[0018]
[0019]
[0020]
[0021]
[0022]
[0023]
[0024]
[0025]
DETAILED DESCRIPTION OF THE INVENTION
[0026] Aspects provide for a flash-free mold assembly for use in the manufacture of an article of footwear such as, for example, a midsole, an outsole, a combination midsole/outsole, and/or portions thereof. Such articles of footwear are generally formed by filling or injecting a mold space of a mold assembly with a moldable compound or mixture and generating a pressure needed to cure the moldable compound by utilizing a mold press to apply a predefined force to the mold assembly. The moldable compound may comprise natural or man-made materials such as rubber, polyurethane, thermoplastic polyurethane (TPU), ethylene vinyl acetate (EVA), other types of foams, and the like. As discussed above, typical molding techniques often create flash or flashing on the molded article at the intersection of the mold plates. As used throughout this disclosure, the term flash or flashing means excess material that is attached to a molded product and which usually must be removed in a post-processing step. The mold assembly described herein eliminates flash and produces a continuous or sealed skin on the molded article of footwear at the intersection of the plates of the mold assembly. The mold assembly described herein, moreover, is configured such that the amount of force that needs to be applied to the mold assembly by a mold press in order to generate the requisite amount of pressure needed to cure the moldable compound is reduced.
[0027] The exemplary mold assembly described herein may comprise a first plate having at least one mold cavity and a second plate that is operably coupled to the first plate. When superimposed over the mold cavity of the first plate, the first and second plates may define a mold space. The first plate may comprise one or more projections extending upward from the plate surface of the first plate and circumscribing or encircling the mold cavity. The plate surface, in turn, may completely surround the one or more projections. In an exemplary aspect, the first plate may further comprise one or more depressions extending downward from the plate surface and located at, for example, the corners of the first plate and/or along a front portion of the first plate.
[0028] In an exemplary aspect, the second plate may comprise one or more depressions adapted to receive the one or more projections of the first plate when the second plate is in an operative relationship with the first plate (i.e., when the second plate is superimposed on the first plate). Further, when the second plate is superimposed on the first plate, the second plate may be adapted to primarily contact the one or more projections of the first plate. In some exemplary aspects, the second plate may be adapted to only contact the one or more projections of the first plate. The second plate may also comprise one or more vent apertures that are in communication with the mold space when the second plate is superimposed on the first plate. The second plate may optionally comprise one or more projections extending upward from the surface of the second plate and adapted to be received into the one or more depressions of the first plate when the second plate is superimposed on the first plate.
[0029] The configuration thus described helps to eliminate the formation of flash on the article of footwear at the intersection of the first and second plates when the mold space is filled/injected with a moldable compound and force is applied to the mold assembly by a mold press to form the article of footwear. Further, by generally limiting the area of contact between the first plate and the second plate to that of the projections on the first plate, a greater amount of pressure may be generated in response to a fixed force being applied to the mold assembly by the mold press. One result of this is that the amount of force applied to the mold assembly by the mold press can be reduced while still generating the pressure needed to cure the moldable composition. By decreasing the amount of force applied by the mold press, the lifespan of both the mold assembly and the mold press may be prolonged. As well, because a decreased amount of force is being applied to the mold assembly, the mold assembly may be constructed in part from softer, more-deforming metals such as aluminum and/or bronze which may help to reduce the costs associated with making the mold assembly along with possibly reducing the weight of the mold assembly.
[0030] Turning now to
[0031] The first plate 110 may have a generally square or rectangular shape and be constructed from materials having a high degree of hardness such as, for example, steel or ceramics. The term hardness as used herein means a measure of how resistant solid matter is to various kinds of shape changes when a compressive force is applied. The first plate 110 may comprise a plate surface 114 (indicated by the hash marks), one or more mold cavities 116 and 118, a first projection 120, and a second projection 122. The first plate 110 may optionally further comprise pin receiving holes 126 and 130, corner depressions 124 and 128, and a midline depression 152 located at a front edge of the first plate 110 and situated between the mold cavity 116 and the mold cavity 118.
[0032] The mold cavities 116 and 118 may comprise depressions extending downward from the plate surface 114 into the body of the first plate 110. In an exemplary aspect, the mold cavities 116 and 118 may be shaped so as to mold a midsole, an outsole, a combination midsole/outsole, and/or portions thereof. As such, the mold cavities 116 and 118 may be in the general shape of these articles of footwear. Further, the mold cavities 116 and 118, in an exemplary aspect, may comprise a mold cavity for an article of footwear configured for a right foot (e.g., mold cavity 118) and an article of footwear configured for a left foot (e.g., mold cavity 116). The mold cavities 116 and 118 may be sized for a particular shoe size. In other exemplary aspects, the first plate 110 may comprise a single mold cavity or multiple mold cavities which may be used to mold other articles of footwear such as inserts, heel cups, and the like. Any and all such aspects, and any variation thereof, are contemplated as being within the scope herein.
[0033] The first projection 120 may extend generally perpendicularly upward from the plate surface 114 when the mold assembly 100 is in an as-used configuration. Using the mold cavity 116 as a representative example, the first projection 120 may circumscribe the mold cavity 116 and be in the same general shape configuration as the mold cavity 116. To put it another way, the first projection 120 may form a continuous ridge surrounding and partially contiguous with the mold cavity 116.
[0034] Likewise, the second projection 122 may be spaced apart from the first projection 120 and extend generally perpendicularly upward from the plate surface 114. The second projection 122 may circumscribe the first projection 120 and it also may circumscribe the mold cavity 116. To put it another way, the second projection 122 may form a continuous ridge surrounding both the first projection 120 and the mold cavity 116 and be in the same general shape configuration as the first projection 120 and the mold cavity 116. In turn, as illustrated in
[0035] The use of two projections, as opposed to just one projection, may help to disperse the force transmitted by the mold press to the mold assembly 100 when the second plate 112 is superimposed on the first plate 110 such that the second plate 112 contacts the projections 120 and 122. This, in turn, helps to prevent excess wear-and-tear on the projections 120 and 122 and may prolong the lifespan of the mold assembly 100. Although two projections are shown in
[0036] As mentioned, the first plate 110 may also comprise pin receiving holes 126 and 130 located at the front corners of the first plate 110. The pin receiving holes 126 and 130 are adapted to receive pins 144 and 148 located on the second plate 112 when the second plate 112 is superimposed on the first plate 110. More specifically, the pin receiving hole 126 is adapted to receive the pin 144 and the pin receiving hole 130 is adapted to receive the pin 148. This helps to secure and align the plates 110/112 together and prevent movement between the plates 110/112 during the molding process.
[0037] The first plate 110 may further comprise the triangular-shaped depressions 124 and 128 located at the two rear corners of the first plate 110 and extending downward from the plate surface 114 into the body of the first plate 110. In an exemplary aspect, the depressions 124 and 128 may be adapted to receive corresponding triangular-shaped projections located on the second plate 112. This aspect is shown in more detail with respect to
[0038] As well, the first plate 110 may comprise the midline depression 152. In aspects, the midline depression 152 extends downward from the plate surface 114 into the body of the first plate 110 and may be located along a front portion of the first plate 110 at a position midway between the mold cavities 116 and 118. The midline depression 152 may be generally triangular shaped with the base of the triangle intersecting the front edge of the first plate 110 and the apex of the triangle extending towards the center of the first plate 110. In aspects, the apex may not comprise a true pointed apex but, instead, be more rounded or squared-off as shown in
[0039] The second plate 112 may also have a generally square or rectangular shape that is substantially congruent with the shape of the first plate 110. The second plate 112 may be constructed from materials similar to the first plate 110 such as, for example, steel or ceramic. Alternatively, the second plate 112 may be constructed, in total or in part, of materials, such as bronze, aluminum, or alloys of each, that deform to a greater degree than the materials used to construct the first plate 110 in response to the application of force. Any and all such aspects, and any variation thereof, are contemplated as being within the scope herein. The benefits of using these types of metals will be explained in greater depth below with respect to
[0040] The mold surfaces 134 and 136 of the second plate 112 are complementary to the mold cavities 116 and 118 of the first plate 110. When the second plate 112 is superimposed on the first plate 110, the mold surface 134 in combination with the mold cavity 116 form a first complete mold space for an article of footwear (i.e., an article of footwear configured for a left foot). Likewise, the mold surface 136 in combination with the mold cavity 118 of the first plate 110 form a second complete mold space for an article of footwear (i.e., an article of footwear configured for a right foot). As explained above, the article of footwear may comprise a midsole, an outsole, a combination midsole/outsole, portions of a midsole and/or outsole, inserts, heel cups, and the like.
[0041] The mold surfaces 134 and 136 may each comprise the plurality of vent apertures 142 that extend from the mold surfaces 134 and 136 to an exterior surface of the second plate 112 (not shown in
[0042] The first and second depressions 138 and 140 of the second plate 112 may be complementary to the first and second projections 120 and 122 of the first plate 110. As such, the first depression 138 may comprise a recess or groove on the plate surface 132 and may be adapted to receive the first projection 120 of the first plate 110 when the mold assembly 100 is in an as-used configuration. Using the mold surface 134 as a representative example, the first depression 138 may circumscribe the mold surface 134 and have the same general shape configuration as the mold surface 134. In other words, the first depression 138 may form a continuous depression surrounding the mold surface 134 and partially contiguous with the mold surface 134. Likewise, the second depression 140 may be spaced apart from the first depression 138 and may also comprise a recess or groove on the plate surface 132. The second depression 140 may be adapted to receive the second projection 122 of the first plate 110 when the mold assembly 100 is in an as-used configuration. The second depression 140 may circumscribe the first depression 138 and it may also circumscribe the mold surface 134. To put it another way, the second depression 140 may form a continuous depression surrounding both the first depression 138 and the mold surface 134 and have the same general shape configuration as the first depression 138 and the mold surface 134. In turn, the plate surface 132 completely surrounds (i.e., without disruptions) both the first and second depressions 138 and 140. Although two depressions are shown in
[0043] The pin 144 and the pin 148 may be located at the two front corners of the second plate 112 and may extend perpendicularly out from the plate surface 132. The pins 144 and 148 are adapted to be received into the pin receiving holes 126 and 130 of the first plate 110 when the second plate 112 is superimposed on the first plate 110. This configuration helps to secure the plates 110 and 112 together and prevent movement of the plates 110 and 112 when a force is applied to the mold assembly 100.
[0044] The triangular-shaped projections 146 and 150 extend out from the plate surface 132 and are generally located at the two rear corners of the second plate 112. As explained above, the projections 146 and 150 are adapted to be received into the depressions 124 and 128 when the second plate 112 is superimposed on the first plate 110. Although a triangular shape is shown for the projections 146 and 150, it is contemplated that the projections 146 and 150 may have different shapes such as a square, a rectangle, a circle, and the like. The shape of the projections 146 and 150 of the second plate 112 should generally correspond to the shape of the depressions 124 and 128 of the first plate 110.
[0045] The midline projection 154 extends out from the plate surface 132 and is generally located along a front portion of the second plate 112. The midline projection 154 may have a shape corresponding to the midline depression 152 of the first plate 110. As such, the projection 154 may be generally triangular-shaped with the base of the projection 154 being aligned with the front edge of the second plate 112 and the apex of the projection 154 extending towards the center of the plate 112. As with the midline depression 152, the apex may be rounded or squared-off as shown in
[0046] The relationship between the triangular-shaped depressions 124 and 128 of the first plate 110 and the corresponding projections 146 and 150 of the second plate 112 along with the midline depression 152 of the first plate 110 and the midline projection 154 of the second plate 112 helps to align the first and second plates 110 and 112 when the second plate 112 is superimposed on the first plate 110. Having the plates 110 and 112 properly aligned prior to a mold press applying force to the mold assembly 100 helps to prevent the force from being unevenly applied to the projections 120 and/or 122 which could potentially cause permanent deformation of these structures.
[0047] In an optional aspect, the relationship between these depressions and projections, moreover, may help to slightly increase the area of contact between the first plate 110 and the second plate 112 when the second plate 112 is superimposed on the first plate 110. By slightly increasing the area of contact between the first and second plates 110 and 112, the force applied by the mold press to the mold assembly 100 may be more dispersed instead of being limited only to the projections 120 and/or 122 thereby prolonging the life of the projections 120 and 122. The depressions 124, 128 and 152 of the first plate 110 and the projections 146, 150, and 154 of the second plate 112 may be optional in certain situations. For example, if the mold assembly 100 comprises only one mold space, these depressions/projections may not be present. This also may hold true if the mold press is configured such that it is consistently centered on the mold assembly 100 and consistently applies a uniform force to the projections 120 and 122.
[0048] Thus, when the mold assembly 100 is in an as-used configuration (e.g., when the second plate 112 is superimposed on the first plate 110), the areas of contact between the first plate 110 and the second plate 112 may generally comprise: 1) the first projections 120 and the first depressions 138; 2) the second projections 122 and the second depressions 140; and, optionally 3) the pins 144 and 148 and the pin receiving holes 126 and 130 respectively; 4) the triangular-shaped projections 146 and 150 and the corresponding triangular-shaped depressions 124 and 128; and/or 5) the midline projection 154 and the midline depression 152. When the mold assembly 100 is in an as-used configuration, the plate surface 114 of the first plate 110 generally does not come into contact with the plate surface 132 of the second plate 112.
[0049] Turning now to
[0050] As seen in
[0051] The second projection 122 may be offset or spaced apart from the first projection 120 by a distance C. In exemplary aspects, the distance C may be between 12 mm and 14 mm, between 11 mm and 13 mm, and/or between 10 mm and 12 mm. The second projection 122 may be contiguous with and extend perpendicularly upward from the plate surface 114 by a height A that is generally equal to the height A of the first projection 120. Further, the second projection 122 may have a flat surface or top that has a width B generally equal to the width B of the first projection 120. The width B of the projections 120 and 122 may be selected so as to facilitate a tight seal being formed between the projections 120 and 122 and the depressions 138 and 140 when a mold press applies a force to the mold assembly 100 as explained in greater depth below with respect to
[0052]
[0053] As shown in
[0054] The second depression 140 may be offset or spaced apart from the first depression 138 by a distance C, which may be generally equal to the distance C between the first projection 120 and the second projection 122 as illustrated in
[0055] Continuing with respect to
[0056] The second portion 314 of the vent aperture 142 may transition the first portion 312 into the third portion 316. As such, it may generally be funnel-shaped. The third portion 316 of the vent aperture 142 generally extends vertically upward for a predetermined distance before opening up into the fourth portion 318 as shown in
[0057] Turning now to
[0058] The midline depression 152 extends from the plate surface 114 into the body of the first plate 110 by a depth J. In exemplary aspects, the depth J may be between 0.3 cm and 1.2 cm, and/or between 0.5 cm and 1.0 cm. As shown in
[0059]
[0060]
[0061] The midline projection 154 extends outward from the plate surface 132 by a distance N. In exemplary aspects, the distance N may be approximately equal to the depth J of the midline depression 152 of the first plate 110 such that the surface of the projection 154 may contact the bottom of the depression 152 when the first plate 110 is superimposed on the second plate 112. As shown, the sides of the projection 154 angle inward towards each other to form a beveled edge.
[0062]
[0063]
[0064]
[0065]
[0066] Exemplary aspects described herein allow for a tight seal to be formed between at least the first projection 120 and the first depression 138, which, in turn, prevents moldable compound from exiting the mold space at the intersection of the first plate 110 and the second plate 112. This is because, as previously described, the mold assembly 100 may be configured such that the area of contact between the first plate 110 and the second plate 112 is generally limited to the projections of the first plate 110 and the depressions of the second plate 112. Based on the formula, Pressure=Force/Area, this configuration enables a lesser amount of force to be applied to the mold assembly 100 by the mold press 612 while still generating the amount of pressure needed to cure the moldable compound. In other words, the curing pressure can still be reached even though the force applied to the mold assembly 100 by the mold press 612 is reduced, because the area of contact between the first plate 110 and the second plate 112 is small. This can be contrasted with traditional mold assemblies where the area of contact between the mold plates is much greater because essentially the entire plate surface of one plate (excluding the mold cavity) is in contact with the entire plate surface of the opposing plate when the mold assembly is being used. In this situation, a greater amount of force needs to be applied to the mold assembly by the mold press in order to generate the needed curing pressure.
[0067] Continuing, decreasing the force applied to the mold assembly 100 by the mold press 612 enables the second plate 112 to be formed, in total or in part, of softer, more deforming metals such as, for example, bronze, aluminum, and/or alloys of each. Therefore, as long as the force applied by the mold press 612 is below the plastic point of these metals, the depressions 138 and 140 of the second plate 112 will elastically deform to a small degree when they come into contact with the harder metal (e.g., steel) of the projections 120 and 122 of the first plate 120. The result of this elastic deformation is the formation of a tight seal between the projections 120 and 122 and the depressions 138 and 140 and a lack of egress for the moldable compound from the mold space 610 except through the vent apertures 142. More particularly, with respect to
[0068] The result of using a mold assembly such as the mold assembly 100 to mold an article of footwear is shown in
[0069] The side surface 1014 of the article 1000 may be adjacent to the intersection of the first plate 110 and the second plate 112 of the mold assembly 100. As explained above with respect to
[0070]
[0071]
[0072]
[0073] As shown in
[0074] Turning now to
[0075]
[0076] At a step 1216, the fixed quantity of moldable compound may be placed in the mold space(s) formed between the first and second plates of the mold assembly. The moldable compound may, in exemplary aspects, comprise pellets or pre-form that is placed in the mold cavity of the first plate prior to superimposing the second plate on the first plate. In another exemplary aspect, the moldable compound may be injected into the mold space. Any and all such aspects are contemplated as being within the scope herein.
[0077] At a step 1218, the second plate may be superimposed on the first plate. Depending on whether the moldable compound is in the form of pellets or pre-form, or whether it is injected into the mold space, the step 1218 may occur before the step 1216. Any and all such aspects are contemplated as being within the scope herein. At a step 1220, the force determined at step 1214 is applied to the mold assembly for the predetermined period of time to form the article of footwear.
[0078] Many different arrangements of the various components depicted, as well as components not shown, are possible without departing from the scope of the claims below. Aspects of our technology have been described with the intent to be illustrative rather than restrictive. Alternative aspects will become apparent to readers of this disclosure after and because of reading it. Alternative means of implementing the aforementioned can be completed without departing from the scope of the claims below. Certain features and subcombinations are of utility and may be employed without reference to other features and subcombinations and are contemplated within the scope of the claims.
[0079] As used herein and in connection with the claims listed hereinafter, the terminology any of claims or similar variations of said terminology is intended to be understood to include any combination of claims, including 2 or more, and so is also understood to include any one of.