INTEGRATED METAL-AND-PLASTIC MOLDED ARTICLE AND METHOD FOR MANUFACTURING INTEGRATED METAL-AND-PLASTIC MOLDED ARTICLE
20170200968 ยท 2017-07-13
Assignee
Inventors
Cpc classification
B32B3/266
PERFORMING OPERATIONS; TRANSPORTING
B29C2045/14975
PERFORMING OPERATIONS; TRANSPORTING
Y02P70/50
GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
B29C45/14819
PERFORMING OPERATIONS; TRANSPORTING
B29C2045/14327
PERFORMING OPERATIONS; TRANSPORTING
B29L2031/3468
PERFORMING OPERATIONS; TRANSPORTING
B29C45/14311
PERFORMING OPERATIONS; TRANSPORTING
B32B15/20
PERFORMING OPERATIONS; TRANSPORTING
B22D17/00
PERFORMING OPERATIONS; TRANSPORTING
H01M8/04201
ELECTRICITY
Y02E60/50
GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
B32B3/30
PERFORMING OPERATIONS; TRANSPORTING
B22D25/02
PERFORMING OPERATIONS; TRANSPORTING
International classification
B22D25/02
PERFORMING OPERATIONS; TRANSPORTING
B29C45/14
PERFORMING OPERATIONS; TRANSPORTING
Abstract
An integrated metal-and-plastic molded article includes a metal plate having a first surface and a second surface in the thickness direction, a first plastic portion on the first surface, a second plastic portion on the second surface, a through-hole that extends through the metal plate in the thickness direction and opens in the first surface and the second surface, and an intermediate plastic portion arranged to fill the through-hole and to be continuous with the first plastic portion and the second plastic portion.
Claims
1. An integrated metal-and-plastic molded article comprising: a metal plate having a first surface and a second surface in a thickness direction; a first plastic portion provided on the first surface; a second plastic portion provided on the second surface; a through-hole that extends through the metal plate in the thickness direction and opens in the first surface and the second surface; and an intermediate plastic portion that is arranged to fill the through-hole and be continuous with the first plastic portion and the second plastic portion.
2. The integrated metal-and-plastic molded article according to claim 1, wherein the metal plate is an end plate adapted to be attached to an end of a fuel cell stack at the first surface, and the first plastic portion insulates the fuel cell stack and the end plate from each other.
3. The integrated metal-and-plastic molded article according to claim 2, wherein the end plate includes a recess that is provided in the first surface, when the end plate is attached to the fuel cell stack, the recess configures a channel adapted to selectively supply fluid to and discharge fluid from the fuel cell stack, the through-hole opens in a bottom surface of the recess, and the first plastic portion is provided also on an inner wall of the recess and insulates the fluid flowing in the channel and the end plate from each other.
4. The integrated metal-and-plastic molded article according to claim 3, wherein the recess is a first recess, the end plate includes a second recess provided in the second surface, the through-hole opens in a bottom surface of the second recess, and the second plastic portion is provided on an inner wall of the second recess.
5. The integrated metal-and-plastic molded article according to claim 4, wherein the through-hole opens at a center of the bottom surface of the second recess.
6. The integrated metal-and-plastic molded article according to claim 1, wherein opposite ends of an inner wall of the through-hole in an axial direction of the through-hole are each curved into an arcuate shape in the axial direction.
7. A method for manufacturing an integrated metal-and-plastic molded article, wherein, after a metal plate that has been formed using a high-pressure die casting method and has a first surface and a second surface in a thickness direction is set in a mold, a molten plastic is injected into and solidified in the mold to form a plastic portion on the first surface, the method comprising: setting, in a mold, a metal plate that has been formed using the high-pressure die casting method and has a through-hole extending through the metal plate in a thickness direction; and when a molten plastic is injected into the mold, causing the plastic to flow from a side corresponding to a first surface in the thickness direction of the metal plate to a side corresponding to a second surface in the thickness direction via the through-hole.
Description
BRIEF DESCRIPTION OF THE DRAWINGS
[0010]
[0011]
[0012]
[0013]
[0014]
[0015]
[0016]
[0017]
DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0018] An embodiment of a stack manifold, which is an integrated metal-and-plastic molded article, and a method for manufacturing the stack manifold will hereafter be described with reference to
[0019] As illustrated in
[0020]
[0021] With reference to
[0022] In the stack manifold 2, the end plate 3 is attached to the fuel cell stack 1. More specifically, the end plate 3 is attached to the end of the fuel cell stack 1 at a first surface 3a, which is one of the opposite sides in the thickness direction of the end plate 3. The first surface 3a of the end plate 3 corresponds to the lower surface as viewed in
[0023] When the stack manifold 2 (the end plate 3) is attached to the fuel cell stack 1, the first recess 10 configures a channel adapted to selectively supply fluid to and discharge fluid from the fuel cell stack 1. In the present embodiment, the first recess 10 is connected to the discharge passage 7 and configures a channel adapted to discharge coolant water from the fuel cell stack 1. The first recesses 11 each serve as a thin section adapted to decrease the weight of the end plate 3.
[0024] A first plastic portion 12, which insulates the end plate 3 and the fuel cell stack 1 from each other, is provided on the first surface 3a. The first plastic portion 12 has a predetermined thickness and is formed like a coating covering the entire first surface 3a including the inner walls of the first recesses 10, 11. The first plastic portion 12 is arranged to cover the inner walls of the supply passages 4, 5, 6 and the discharge passages 7, 8, 9.
[0025] The other one of the opposite surfaces of the end plate 3 in the thickness direction, which is the surface opposite to the first surface 3a, configures a second surface 3b. As illustrated in
[0026] Through-holes 16, which extend through the end plate 3 in the thickness direction and open in the first surface 3a and the second surface 3b, are formed between the first recess 10 and the corresponding second recesses 13. More specifically, each of the through-holes 16 opens in a bottom surface 10a of the first recess 10 and a bottom surface 13a of the corresponding one of the second recesses 13. The opening of each through-hole 16 in the bottom surface 13a of the corresponding second recess 13 is located substantially at the center of the bottom surface 13a. The length of each through-hole 16 in the axial direction (the vertical direction as viewed in
[0027] With reference to
[0028] Through-holes 18, which extend through the end plate 3 in the thickness direction and open in the first surface 3a and the second surface 3b, are formed between the first recesses 11 and the corresponding second recesses 14. More specifically, each of the through-holes 18 opens in a bottom surface 11a of the corresponding one of the first recesses 11 and a bottom surface 14a of the associated one of the second recesses 14. The opening of each through-hole 18 in the bottom surface 14a of the corresponding second recess 14 is located substantially at the center of the bottom surface 14a. The length of each through-hole 18 in the axial direction (the vertical direction as viewed in
[0029] A method for manufacturing the stack manifold 2 will hereafter be described.
[0030] The end plate 3 of the stack manifold 2 is cast using the high-pressure die casting method, which has higher productivity than the gravity casting method. To manufacture the stack manifold 2 using the end plate 3, insert molding is performed as will be described. That is, the end plate 3, which has been cast using the high-pressure die casting method and has the through-holes 16, 18, is set in a mold for insert molding. Then, molten plastic is injected into and solidified in the mold.
[0031]
[0032] When plastic is injected into the molds 21, 22, the plastic flows into the first recess 10 in the first surface 3a of the end plate 3 shown in
[0033] After being injected into the molds 21, 22, the plastic also flows into the first recesses 11 in the first surface 3a of the end plate 3, which are illustrated in
[0034] As has been described, in insert molding, the plastic injected into the molds 21, 22 flows from the side corresponding to the first surface 3a to the side corresponding to the second surface 3b via the through-holes 16 (
[0035] The present embodiment, which has been described in detail, has the advantages described below.
[0036] (1) Despite the fact that the end plate 3 is formed to have a small thickness using the high-pressure die casting method, which is highly productive, the injection pressure of plastic acting on the end plate 3 in insert molding is decreased. This restrains deformation of the end plate 3 caused by action of the injection pressure, thus restraining lowering of the quality of the end plate 3 caused by the deformation of the end plate 3. As a result, the productivity of the stack manifold 2 is improved and high quality of the end plate 3 is ensured.
[0037] (2) When the stack manifold 2 (the end plate 3) is attached to the fuel cell stack 1, the first recess 10 configures a channel adapted to selectively supply fluid to and discharge fluid from the fuel cell stack 1. Since the first plastic portion 12 is provided to cover the inner wall of the first recess 10 including the bottom surface 10a, the fluid flowing in the aforementioned channel and the end plate 3 are insulated from each other by the first plastic portion 12.
[0038] (3) In the end plate 3, each through-hole 16 opens at the center of the bottom surface 13a of the corresponding second recess 13 and each through-hole 18 opens at the center of the bottom surface 14a of the corresponding second recess 14. This facilitates, in insert molding, uniform spreading of molten plastic in each of the second recesses 13, 14 at the time the plastic flows from the side corresponding to the first surface 3a of the end plate 3 to the side corresponding to the second surface 3b via the through-holes 16, 18, or, more specifically, the plastic flows from inside the first recesses 10, 11 into the second recesses 13, 14 via the through-holes 16, 18.
[0039] (4) The opposite ends 16a, 16b of the inner wall of each through-hole 16 in the axial direction of the through-hole 16 are each curved in an arcuate shape in the axial direction. The opposite ends 18a, 18b of the inner wall of each through-hole 18 in the axial direction of the through-hole 18 are each curved in an arcuate shape in the axial direction. This restrains breakage of the plastic portions 12, 15, 17 even if the ends 16a, 16b, 18a, 18b of the through-holes 16, 18 strike the first plastic portion 12, the second plastic portions 15, and the intermediate plastic portions 17 after the stack manifold 2 is manufactured.
[0040] The illustrated embodiment may be modified to the forms described below.
[0041] The opposite ends 16a, 16b of the inner wall of each through-hole 16 in the axial direction of the through-hole 16 do not necessarily have to be curved in an arcuate shape in the aforementioned axial direction. The opposite ends 18a, 18b of the inner wall of each through-hole 18 in the axial direction of the through-hole 18 do not necessarily have to be curved in an arcuate shape in the aforementioned axial direction.
[0042] The opening position of the through-hole 16 in the bottom surface 13a of each second recess 13 may be changed as needed.
[0043] The opening position of the through-hole 18 in the bottom surface 14a of each second recess 14 may be changed as needed.
[0044] The second recesses 13, 14 do not necessarily have to be provided. In this case, the second plastic portions 15 are arranged in the portions of the second surface 3b that are continuous at least with the through-holes 16, 18.
[0045] When the stack manifold 2 is attached to the end of the fuel cell stack 1, the first recess 10 does not necessarily have to configure the channel for flow of the fluid selectively supplied to and discharged from the fuel cell stack 1.
[0046] The present invention may be used for any integrated metal-and-plastic molded article other than the stack manifold 2. In this case, the first recesses 10, 11 do not necessarily have to be provided in the first surface 3a or the second recesses 13, 14 do not necessarily have to be provided in the second surface 3b.