MOLD BOTTOM WITH WIDE AIR VENTS FOR THE FORMING OF A CONTAINER
20170173845 ยท 2017-06-22
Inventors
Cpc classification
B29C49/4823
PERFORMING OPERATIONS; TRANSPORTING
B29C2049/4825
PERFORMING OPERATIONS; TRANSPORTING
B29C2049/4892
PERFORMING OPERATIONS; TRANSPORTING
B29C2949/0715
PERFORMING OPERATIONS; TRANSPORTING
B29K2067/003
PERFORMING OPERATIONS; TRANSPORTING
International classification
Abstract
Mold bottom for the manufacture by blow molding of a container that has a bottom that is equipped with a seat, with this mold bottom including a unit that has a molding face bearing the at least partial impression of the bottom of the container, with a pressure-release air vent being formed in the unit and emptying out, via an inner opening, on the molding face and, via an outer opening, into a pipe for exposure to air, with this mold bottom also including an insert that is provided with at least one projection housed in the air vent and that has a terminal face bearing the impression of at least one part of the seat of the container, with this insert being provided with an inner circuit for heat regulation of the projection and being mounted to move in relation to the unit.
Claims
1. Mold bottom (20) intended for a mold (1) for the manufacture, by blow molding or stretch blow molding of a parison (3) made of plastic material, of a container (2) that has a bottom (8) that is equipped with a peripheral seat (9), with this mold bottom (20) comprising a bottom unit (21) that has a molding face (22) in relief bearing the impression of at least a part of the bottom (8) of the container (2), with a pressure-release air vent (26) being formed in the unit (21) and emptying out, via an inner opening (27), on the molding face (22) and, via an outer opening (28), into a pipe (29, 30) for exposure to air, wherein the mold bottom (20) comprises an insert (34) that is provided with at least one projection (35) housed in the air vent (26) (or in each air vent (26)) and that has a terminal face (36) bearing the impression of at least one part of the seat (9) of the container (2), with this insert (34) being provided with an inner circuit (37) for heat regulation of the (or each) projection (35), with this insert (34) being in addition mounted to move, in relation to the bottom unit (21), between: A retracted position in which the terminal face (36) of the (or of each) projection (35) is separated from the inner opening (27) and lets the former communicate with the pipe (29, 30) for exposure to air, and A deployed position in which the terminal face (36) extends in the vicinity of the inner opening (27).
2. Mold bottom (20) according to claim 1, wherein in the deployed position, the terminal face (36) of the (or of each) projection (35) extends into the extension of the molding face (22).
3. Mold bottom (20) according to claim 1, wherein in the deployed position, the terminal face (36) of the (or of each) projection (35) extends in a setback manner, in relation to the inner opening (27), by a distance of between 0.5 mm and 5 mm.
4. Mold bottom (20) according to claim 1, wherein the terminal face (36) is concave.
5. Mold bottom (20) according to claim 1, wherein the terminal face (36) is convex.
6. Mold bottom (20) according to claim 1, wherein the insert (34) comprises a piston (38) that is mounted in translation in a jacket (40) that is integral with the bottom unit (21).
7. Mold bottom (20) according to claim 1, wherein the or each air vent (26) comprises an inner portion (26A), which extends to the inner opening (27), and an outer portion (26B) with a larger section, which extends into the extension of the inner portion (26A) by being separated from the former by a shoulder (51).
8. Mold bottom (20) according to claim 7, further comprising a primary pipe (29) for exposure to air, which empties into the air vent (26) in the area of the shoulder (51).
9. Mold bottom (20) according to claim 7, further comprising a secondary pipe (30) for exposure to air, which empties into the air vent (26) in the area of the outer portion (26B).
10. Mold bottom (20) according to claim 1, wherein the bottom unit (21) is provided with a number of air vents (26) that are spaced from one another, and the insert (34) comprises a peripheral series of projections (35) that are spaced from one another.
11. Mold bottom (20) according to claim 10, wherein the molding face (22) bears the impression of a petal-shaped bottom (8) of the container (2) and comprises alternating ribs (32) bearing the impression of valleys (13) of the petal-shaped bottom (8), which radiate from a central zone (33), and with recessed reserved places (31) bearing the impression of feet (12) of the petal-shaped bottom (8), which extend between the ribs (32), the air vents (26) are made in the recessed reserved places (31), and the terminal face (36) of each projection (35) bears the impression of the feet (12) of the container (2).
12. Mold (1) for the manufacture of a container (2) from a parison (3) made of plastic material, which comprises a side wall (16) bearing the impression of a body (4) of the container (2), and a mold bottom (20) according to claim 1, which completes the impression of the container (2) with the side wall (16).
13. Method for manufacturing a container (2), which comprises the operations that consist in: Introducing into a mold according to claim 12 a parison (3) made of plastic material, heated in advance to a temperature that is higher than the glass transition temperature of the material; In the retracted position of the insert (34), injecting a pressurized gas into the parison (3); While maintaining the pressure in the parison (3), moving the insert (34) toward its deployed position.
14. Mold bottom (20) according to claim 2, wherein the terminal face (36) is concave.
15. Mold bottom (20) according to claim 3, wherein the terminal face (36) is concave.
16. Mold bottom (20) according to claim 2, wherein the terminal face (36) is convex.
17. Mold bottom (20) according to claim 2, wherein the insert (34) comprises a piston (38) that is mounted in translation in a jacket (40) that is integral with the bottom unit (21).
18. Mold bottom (20) according to claim 3, wherein the insert (34) comprises a piston (38) that is mounted in translation in a jacket (40) that is integral with the bottom unit (21).
19. Mold bottom (20) according to claim 4, wherein the insert (34) comprises a piston (38) that is mounted in translation in a jacket (40) that is integral with the bottom unit (21).
20. Mold bottom (20) according to claim 5, wherein the insert (34) comprises a piston (38) that is mounted in translation in a jacket (40) that is integral with the bottom unit (21).
Description
BRIEF DESCRIPTION OF THE DRAWINGS
[0036] Other objects and advantages of the invention will become evident from the description of an embodiment, provided below with reference to the accompanying drawings in which:
[0037]
[0038]
[0039]
[0040]
[0041]
[0042]
[0043]
[0044]
[0045]
[0046]
[0047]
[0048]
[0049]
[0050]
DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0051]
[0052] The parison 3 can be an intermediate container that has undergone a first blow-molding operation starting from a preform. It can also be, as in the illustrated example, a crude injection preform. Also, hereinafter, the reference 3 will be used interchangeably to refer to any type of parison or preform.
[0053] The container 2 comprises an essentially cylindrical body 4 that extends along a main axis X, a shoulder 5 that extends, in narrowing, into the extension of the body 4 at an upper end of the former, a neck 6 that is open at an upper end of the shoulder 5 from which it is separated by a collar 7, and a bottom 8 that closes the body 4 at a lower end of the former. The bottom 8 has a peripheral seat 9 by which the container 2 is intended to rest on a flat surface such as a table, and a raised central zone 10 (where an injection button 11 of the preform 3 is located), to which the seat 9 is connected by an arch.
[0054] According to an embodiment that is illustrated in the figures (and more particularly in
[0055] The preform 3 comprises a body 14 with an essentially tubular shape, designed to form the body 4 and the shoulder 5 of the container 2, a neck 6 which is that of the container 2 and remains unchanged during the forming, and a hemispherical bottom 15 that is designed to form the bottom 8 of the container 2.
[0056] The mold 1 comprises a side wall 16 that defines a cavity 17 bearing the impression of the body 4 and the shoulder 5 of the container 2. The side wall 16 extends along a main axis that, when the container 2 is formed, is merged with the main axis X of the former. Below, the expression main axis interchangeably refers to the axis of the container or that of the side wall 16.
[0057] According to a conventional embodiment, the side wall 16 is subdivided into two half-molds that can move in relation to one another (for example by being articulated around a hinge that is parallel to the main axis X), between an open position in which the two half-molds are separated angularly from one another to make possible the introduction of the preform 3 and the evacuation of the container 2, and a closed position in which the two half-molds are flattened against one another to define together the cavity 17, as described in, for example, the French patent application FR 2 856 333 or the corresponding international application WO 05/002820 (Sidel).
[0058] The side wall 16 defines an upper opening 18, by which the preform 3 is suspended by its collar 7, and an opposite lower opening 19. Since the line of
[0059] The mold 1 is also equipped with a mold bottom 20 that comprises, firstly, a bottom unit 21 (for example made of steel or in an aluminum alloy) having a molding face 22 in relief bearing the impression of at least one part of the bottom 8 of the container 2, and which completes the impression of the former with the side wall 16.
[0060] The bottom unit 21 is attached to a support 23 that is itself mounted (for example by means of a screw 24) on a stand 25 that can move in translation in relation to the side wall 16 between a loading/unloading position in which the unit 21 is separated from the cavity 17 to make possible the evacuation of the container 2 that is formed and the installation of a new preform 3, and a forming position (illustrated in
[0061] The mold bottom 20 is equipped with at least one pressure-release air vent 26 that is formed in the mold unit 21 and that empties, via an inner opening 27, onto the molding face 22 and, via an outer or peripheral opening 28, into at least one pipe 29, 30 for exposure to air. The air vent 26 (or each air vent 26) is formed by a scalloping made in the unit 21 in a direction that is essentially parallel to the main axis X, in a seating zone corresponding to the seat 9 of the container 2 and formed by recessed reserved places 31.
[0062] According to an embodiment that is illustrated in the figures, where the container 2 has a petal-shaped bottom 8, the molding face 22, bearing the impression of the former, comprises alternating ribs 32 (bearing the impression of the valleys 13), which radiate from a central zone 33 (bearing the impression of the central zone 10 of the bottom 8), and recessed reserved places 31 (each forming the above-mentioned seating zone) bearing the impression of the feet 12 (here, five in number), which extend between the ribs 32. In this case, the bottom unit 21 comprises a series of air vents 26 (here, five in number) that are spaced (here, distributed over a circular sector), made in the recessed reserved places 31. More specifically, as in the illustrated example, an air vent 26 is made in the bottom of each recessed reserved place 31.
[0063] Secondly, the mold bottom 20 comprises an insert 34 that is provided with at least one projection 35 that is housed in the air vent 26 (when there is only one of them) or in each air vent 26 (when there are several of them, as in the illustrated example) and that has a terminal face 36 bearing the impression of at least a part of the seat 9 of the container 2.
[0064] According to an embodiment that is illustrated in the figures, in which the container 2 has a petal-shaped bottom 8, the insert 34 comprises a number of spaced air vents 26 (here, distributed in a circular sector). In this case, the terminal face 36 of each projection 35 has an impression of the end of a foot 12. The terminal faces 36 of the projections 35 then form the impression of the entire seat 9 of the container 2, consisting of all of the ends of the feet 12. In this case, the terminal face 36 is concave.
[0065] The insert 34 is provided with an internal circuit 37 for heat regulation of the (or of each) projection 35, in such a way that the former is kept at a moderate temperature (between 5 C. and 30 C., and preferably between 10 C. and 20 C.).
[0066] The insert 34 is mounted to move, in relation to the bottom unit 21, between: [0067] A retracted position (
[0069] According to a first embodiment, illustrated in
[0070] According to a second embodiment that is illustrated in
[0071] According to a third embodiment that is illustrated in
[0072] It is preferable that the terminal face 36 be solid, i.e., have no perforations. However, it can be considered to provide in the terminal face 36 one or more air vents of small width (or diameter) that contribute to facilitating the evacuation of air without, however, running the risk of forming hot points on the container 2.
[0073] According to an embodiment that is illustrated in the figures, the insert 34 comprises a base that is shaped like a piston 38. This piston 38 has an upper face 39 from which the projections 35 emerge axially.
[0074] The piston 38 is mounted in translation in a jacket 40 that is integral with the mold unit 21. More specifically, in the illustrated example, the jacket 40 is formed in the support 23; this jacket 40 extends in an annular manner around a central shaft 41 and is delimited axially by an upper wall 42 that belongs to the support 23 and by a lower opposite wall 43 that belongs to the stand 25. The upper wall 42 is pierced by openings 44 that partly define the air vents 26 and in which are housed the projections 35 when the piston 38, also in annular form, is mounted in the jacket 40.
[0075] In the jacket 40, the piston 38 delimits an upper chamber 45, from the side of the upper wall 42, and a lower chamber 46, from the side of the lower wall 43. A fluid intake pipe 47 is formed in the stand 25 and empties, via the lower wall 43, into the lower chamber 46, to inject into the former a pressurized fluid (such as air or oil) that pushes back the piston 38 toward the upper wall 42, and therefore the insert 34 toward its deployed position. In the illustrated example, the jack that is constituted by the piston 38 and the jacket 40 is of the single-action type, and the mold bottom 20 comprises one (or multiple) return spring(s) 48 inserted between the upper wall 42 and the piston 38, and which permanently stress the former toward the inside wall 43, and therefore the insert 34 toward its retracted position. In the illustrated example, five return springs 48 are provided, cf.
[0076] Thus, to place the insert 34 in its deployed position, a pressurized fluid (such as air or oil) is injected into the lower chamber 46, via the intake pipe 47 (and by means of, for example, a branched hose on the stand by means of a connector 49partially shown in
[0077] The travel of the insert 34 between its retracted position and its deployed position is between 5 mm and 15 mm, and advantageously approximately 10 mm.
[0078] The sealing between the two chambers 45, 46 is advantageously carried out by means of annular segments 50 housed in grooves made in a peripheral manner in the piston 38.
[0079] As a variant, the movement of the insert 34 can be controlled by mechanical and non-pneumatic (or hydraulic) means, for example by a cam. For this purpose, a lower end of the insert can carry a cam follower (such as a roller), which works with a cam groove, with the permanent contact of the cam follower with the cam groove being ensured by, for example, a return spring. The cam groove has an upper section that moves the cam follower toward the top (and therefore the insert 34 toward its deployed position) and a lower section that makes it possible for the cam follower to come down (and therefore the insert 34 to return toward its retracted position).
[0080] In the illustrated example, where the container 2 has a petal-shaped bottom 8, each air vent 26 has in cross-section a profile of an essentially oval shape, of which the angular extension (measured in a transverse plane from the main axis X) is denoted A, the radial extension (also called small width) is denoted B, and the perimeter extension (also called large width, and measured perpendicularly to the radius passing through the geometric center of the inner opening 27) is denoted C.
[0081] Furthermore, the diameter of the pitch circle that passes through the points of the terminal faces 36 of the projections 35 corresponding to the ends of the feet 12 (also called seat circle) is denoted D1, and the outer diameter of the molding face 22, corresponding to the overall diameter of the bottom 8 of the container 2, is denoted D2.
[0082] The air vents 26, indicated in
10A45 [0084] Advantageously, for a petal-shaped bottom:
17A35 [0085] And, for example,
A35 [0086] The small width B of each air vent 26 is between 20% and 60% of the radius of the pitch circle, and advantageously, for a petal-shaped bottom 8 as illustrated, approximately 40% of the radius of the pitch circle:
BC2.Math.B [0089] And advantageously, for a petal-shaped bottom 8:
C1.45.Math.B [0090] The individual surface, denoted Su, of each air vent 26 on a transverse plane, is between 1% and 4% of the projected surface of the bottom 8 (i.e., the surface of the disk of diameter D2), and advantageously, in the case of a petal-shaped bottom 8, approximately 3% of the former:
[0095] Each projection 35 has, in cross-section (i.e., in a plane that is perpendicular to the main axis X), a profile that is complementary to that of the air vent 26 in which the projection 35 is housed, by taking into account an operational play necessary to its sliding.
[0096] In the deployed position of the insert 34, this play is approximately 0.25 mm in the area of the inner opening 27.
[0097] So as to facilitate the evacuation of the air during the blow molding of the container 2, the or each air vent 26 comprises an inner portion 26A, which extends axially up to the inner opening 27, and an outer portion 26B with a larger section, which extends axially into the extension of the inner portion 26A by being separated from the former by a shoulder 51. The height of the inner portion 26A of the air vent 26 is less than the travel of the insert 34 in such a way that in the retracted position of the former, the terminal face 36 of the projection 35 is located in the outer portion 26B, set back in relation to the shoulder 51. The result is an increase in the section of passage for the air around the projection 35, and therefore an increase in the evacuation flow rate of the air. The play between the projection and the outer portion 26B of the air vent 26 is advantageously greater than or equal to 0.5 mm, and, for example, on the order of 0.7 mm.
[0098] According to an embodiment that is illustrated in
[0099] The mold bottom 20 also advantageously comprises a secondary pipe 30 for exposure to air that empties into the air vent 26 in the area of the outer portion 26B. When the insert 34 is in its retracted position, the secondary pipe 30 empties opposite the projection 35, but the relatively significant play between the projection 35 and the outer portion 26B makes it possible for the air to circulate easily from the inner opening 27 to the secondary pipe 30. It will be noted that the secondary pipe 30, furthermore, produces the exposure to air (and therefore the holding at atmospheric pressure) of the upper chamber 45.
[0100] The heat regulation circuit 37 of the insert is, for example, of the fluid type and in this case comprises channels 52 formed in a closed circuit in each projection 35, in which a refrigerating fluid (such as water) circulates. In the example that is illustrated in
[0101] To form the container 2 from the preform (or more generally from a parison) 3, the procedure is as follows.
[0102] With the insert 34 being in the retracted position, the preform 3 (illustrated in dotted lines in
[0103] A pressurized gas (such as air) is then injected into the preform 3 while stretching it, preferably by means of an elongation rod. The pressure is increased during injection, from a pre-blow-molding pressure of approximately 7 bars to a blow-molding pressure on the order of 17 bars. The material flattens against the side wall 16 and against the molding face 22 of the mold bottom 20. The air between the material during deployment and the bottom 20 is evacuated via the air vents 26 by being free to escape via the pipes 29, 30 for exposure to air in communication with the inner opening 27.
[0104] The insert 34 is always in its retracted position when the blow molding begins at 17 bars.
[0105] Under these conditions, the material faithfully takes the impression of the molding face 22, with the evacuation of the air continuing via the air vents 26.
[0106] Under the blow-molding pressure, the material first penetrates into each air vent 26 to form a bump 55 there (in solid lines in
[0107] While maintaining the blow-molding pressure, the insert 34 is moved toward its deployed position. Each projection 35 then pushes back the bump 55 to give it the impression of the terminal face 36, either in the extension of the molding face 22 (the case of
[0108] The material of the bottom 8 of the container 2 that is thus formed is quickly cooled not only in the zones in contact with the molding face 22 of the unit 21 (by means of a cooling circuit 56 that is visible in particular in
[0109] In this way, the material that supplies the zones where the air vents 26 are positioned sets and does not undergo any subsequent uncontrolled deformation. It is consequently possible to make the air vents 26 wide by providing them with a significant scope in relation to the projected surface of the bottom 20, as is evident from the examples that are provided above for the angular amplitude A, the widths B and C, and the surface S.
[0110] The result is a better blowability of the container 2 (blowability of a container is defined as its capacity to be formed by blow molding) thanks to the increased flow of air through air vents 26, which are released when the insert 34 is in the retracted position, with the openings 27, 28 being in free communication with the pipes 29, 30 for exposure to air.
[0111] This likewise makes it possible to reduce the blow-molding pressure on the order of 2 to 3 bars, enhancing energy savings. Thus, a container that requires a blow-molding pressure of 20 bars to be formed in a mold that is equipped with standard air vents only requires a blow-molding pressure on the order of 17 to 18 bars, or a savings of 10 to 15%, to be formed in the mold 1 that was just described (with equal impression).