Thermal insulation products for insulating buildings and other enclosed environments
09598857 ยท 2017-03-21
Assignee
Inventors
Cpc classification
E04B2001/742
FIXED CONSTRUCTIONS
F16L59/065
MECHANICAL ENGINEERING; LIGHTING; HEATING; WEAPONS; BLASTING
Y02A30/242
GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
F16L59/141
MECHANICAL ENGINEERING; LIGHTING; HEATING; WEAPONS; BLASTING
Y02B80/10
GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
International classification
F16L59/065
MECHANICAL ENGINEERING; LIGHTING; HEATING; WEAPONS; BLASTING
Abstract
High-efficiency thermal insulation products and methods for use thereof for use in insulating buildings, residential homes, and other enclosed environments. In one arrangement, a thermal insulation product includes a substantially gas-impermeable envelope having first and second opposing surfaces and a sealed interior portion between the first and second opposing surfaces, a support material within the sealed interior portion of the gas-impermeable envelope, and at least about 2 grams of a liquid per liter of a total volume of the sealed interior portion within the sealed interior portion. At least a portion of the liquid is operable to cyclically evaporate from adjacent one of the first and second opposing surfaces and subsequently condense adjacent the other of the first and second opposing surfaces depending on temperature differences between the first and second opposing surfaces.
Claims
1. A method of insulating a building, comprising: positioning a plurality of thermal insulation products relative to a frame of a building; wherein each thermal insulation product comprises a substantially gas-impermeable envelope including first and second opposing surfaces and a sealed interior portion between the first and second opposing surfaces, a support material within the sealed interior portion of the gas-impermeable envelope, and at least about 1 grams of a liquid per liter of a total volume of the sealed interior portion disposed within the sealed interior portion; wherein the positioning includes orienting the plurality of thermal insulation products so that the first opposing surface faces an interior of the building and the second opposing surface faces an outside ambient environment; wherein at least a portion of the liquid is operable to evaporate from adjacent the first opposing surface and subsequently condense adjacent the second opposing surface when a temperature of the interior of the building is greater than a temperature of the outside ambient environment; and wherein at least a portion of the liquid is operable to evaporate from adjacent the second opposing surface and subsequently condense adjacent the first opposing surface when a temperature of the interior of the building is less than a temperature of the outside ambient environment.
2. The method of claim 1, wherein the positioning step comprises: arranging at least some of the plurality of thermal insulation products relative to a plurality of structural members of the building frame.
3. The method of claim 2, wherein the arranging step comprises: disposing at least some of the plurality of thermal insulation products between adjacent one of the plurality of structural members.
4. The method of claim 3, further comprising: securing a plurality of sheathing members over opposing sides of the plurality of structural members, wherein the at least some of the plurality of thermal insulation products are disposed between adjacent one of the plurality of sheathing members.
5. The method of claim 4, wherein the sheathing members comprise at least one selected from drywall, particle board, plywood, siding, and brick.
6. The method of claim 2, wherein the plurality of structural members comprise at least one selected from studs, joists and rafters.
7. The method of claim 2, wherein the plurality of structural members are made of at least one of wood, metal, and composites.
8. The method of claim 1, wherein at least some of the plurality of thermal insulation products comprise portions of composite building products.
9. The method of claim 1, wherein the portion of the liquid is operable to evaporate from adjacent one of the first and second opposing surfaces and condense adjacent the other of the first and second opposing surfaces diurnally.
10. The method of claim 1, wherein the sealed interior portion comprises at least about 2 grams of the liquid per liter of a total volume of the sealed interior portion.
11. The method of claim 1, wherein the sealed interior portion comprises at least about 4 grams of the liquid per liter of a total volume of the sealed interior portion.
12. The method of claim 1, wherein the sealed interior portion comprises at least about 10 grams of the liquid per liter of a total volume of the sealed interior portion.
13. The method of claim 1, wherein at least about 10% of the liquid within the sealed interior portion is operable to evaporate from adjacent one of the first and second opposing surfaces and condense adjacent the other of the first and second opposing surfaces during each cycle.
14. The method of claim 1, wherein at least about 70% of the liquid within the sealed interior portion is operable to evaporate from adjacent one of the first and second opposing surfaces and condense adjacent the other of the first and second opposing surfaces during each cycle.
15. The method of claim 1, wherein at least about 50 g/m.sup.3 of the liquid within the sealed interior portion is operable to evaporate from adjacent one of the first and second opposing surfaces and condense adjacent the other of the first and second opposing surfaces during each cycle.
16. The method of claim 1, wherein at least about 100 g/m.sup.3 of the liquid within the sealed interior portion is operable to evaporate from adjacent one of the first and second opposing surfaces and condense adjacent the other of the first and second opposing surfaces during each cycle.
17. The method of claim 1, wherein the pressure within the sealed interior portion is not greater than about 500 mbar at a temperature of about 20 C.
18. The method of claim 1, further comprising: a gas-permeable enclosure, wherein the support material is disposed within the gas-permeable enclosure.
19. The method of claim 18, wherein the gas-permeable enclosure is disposed between the support material and the gas-impermeable envelope.
20. The method of claim 19, further comprising: at least one desiccant disposed between the gas-permeable enclosure and the gas-impermeable envelope.
21. The method of claim 1, wherein the support material comprises a fine powder selected from at least one of silica powder and an aerogel powder.
22. The method of claim 21, wherein the fine powder comprises fumed silica.
23. The method of claim 21, wherein the support material comprises at least about 60 wt % of the fine powder.
24. The method of claim 21, wherein the support material comprises up to about 100 wt % of the fine powder.
25. The method of claim 1, wherein the support material comprises an infrared (IR) opacifier.
26. The method of claim 25, wherein the IR opacifier comprises at least one of titania, aluminum, iron oxide, silicon carbide, and carbon.
27. The method of claim 25, wherein the support material comprises at least about 5 wt % of said IR opacifier.
28. The method of claim 25, wherein the support material comprises not greater than about 25 wt % of the IR opacifier.
29. The method of claim 1, wherein the support material comprises not greater than about 0.1 wt % of fibrous materials.
30. The method of claim 1, wherein the support material comprises at least about 10 wt % of a structural filler.
31. The method of claim 1, wherein the support material comprises not greater than about 70 wt % of a structural filler.
32. The method of claim 30, wherein the structural filler comprises perlite.
33. The method of claim 1, wherein the support material comprises at least about 0.01 wt % of a getter.
34. The method of claim 1, wherein the support material comprises not greater than about 1 wt % of a getter.
35. The method of claim 33, wherein the getter comprises at least one of iron, barium, lithium, and zeolites.
36. The method of claim 1, wherein the support material comprises a total porosity of at least about 80%.
37. The method of claim 1, wherein the support material comprises a total porosity of not greater than about 98%.
38. The method of claim 1, wherein the support material comprises an average pore size of at least about 20 nanometers.
39. The method of claim 1, wherein the support material comprises an average pore size of not greater than about 2000 nanometers.
40. The method of claim 1, wherein the product comprises a density of at least about 80 g/l.
41. The method of claim 1, wherein the product comprises a density of not greater than about 280 g/l.
42. The method of claim 1, wherein the product comprises a thermal resistance of at least about 0.5 m.sup.2.Math.K/W.
43. The method of claim 1, wherein the gas-impermeable envelope comprises a thickness of at least about 25 microns.
44. The method of claim 1, wherein the gas-impermeable envelope comprises a thickness of not greater than about 300 microns.
45. The method of claim 1, wherein the gas-impermeable envelope comprises at least one of a polymeric film and a metallic foil.
46. The method of claim 45, wherein the gas-impermeable envelope comprises an Ethylene Vinyl Alcohol (EVOH) barrier film.
47. The method of claim 46, wherein the gas-impermeable envelope comprises a coextruded polyethylene (PE)/EVOH barrier film.
48. The method of claim 46, wherein the gas-impermeable envelope comprises a metalized EVOH barrier film.
49. The method of claim 1, wherein the liquid comprises water.
50. The method of claim 1, wherein the product comprises a substantially planar product having spaced apart first and second sidewalls.
51. The method of claim 50, wherein a distance between the first and second sidewalls is at least about 2 mm.
52. The method of claim 51, wherein the distance between the first and second sidewalls is at least about 20 mm.
53. The method of claim 51, wherein a distance between the first and second sidewalls is not greater than about 100 mm.
54. The method of claim 53, wherein the distance between the first and second sidewalls is not greater than about 50 mm.
Description
BRIEF DESCRIPTION OF THE DRAWINGS
(1)
(2)
(3)
(4)
(5)
(6)
(7)
(8)
(9)
(10)
(11)
DETAILED DESCRIPTION
(12) The present disclosure is generally directed to highly efficient thermal insulation products (e.g., panels, systems, methods of use, methods of manufacture, etc.) for use in insulating buildings and other enclosed environments where a temperature of the environment outside of the enclosed environments experiences temperature swings relative to the outside As will be discussed herein, the disclosed utilities allow for significant increases in thermal performance, increases in the range of operating conditions in which the disclosed utilities can be utilized, reductions in costs, and the like.
(13)
(14) The gas-impermeable envelope 120 may be constructed from any appropriate material(s) such as plastic laminates, metallized plastics, metals, metal-foils, electroplated metals, and/or the like. Depending upon the particular sealing process utilized, the gas-impermeable envelope 120 may have a number of flaps such as first and second flaps 128, 132 that may, if desired, be folded and secured onto the first or second surfaces 104, 108 of the product 100, at least partially cut off and removed, and/or the like. While the product 100 has been shown in
(15) Turning now to
(16) As discussed previously, the support material may be in the form of an adsorbent material (e.g., powder(s), particulate(s), blend(s), and/or the like) having a relatively low thermal conductivity and pores sized to facilitate the Knudsen effect (e.g., a fine powder such as fumed silica, silica aerogels, etc.). In some situations, one or more additives may be mixed in with the adsorbent material (and thereby form part of the support material) to add one or more desired properties or qualities to the support material (and thereby the product 100 to be formed). For instance, one or more of an IR opacifier (to limit radiative heat transfer through the support material), a lightweight fibrous material and/or a structural filler material (to enhance the structural integrity of the product 100 to be formed), a getter (to maintain the low pressure or evacuated state within the product 100 to be formed), and/or the like may be included.
(17) Furthermore, many vapors and/or vaporous mixtures are envisioned that may be disposed and sealed within the gas-permeable enclosure along with the support material. The vapor may be a vapor with relatively low thermal conductivity (e.g., lower than that of nitrogen/air) and/or may be a vapor whose pressure drops by a desired amount along with a particular reduction in temperature. As discussed herein, the vapor is, once sealed within a gas-impermeable envelope, cooled and condensed to reduce the pressure within the gas-impermeable envelope. In this regard, it may be advantageous to utilize vapors that have a boiling point above the operating temperatures of the environment in which the product 100 to be formed is to be used so that the vapor remains condensed and the inside of the product 100 remains in the low pressure state during use of the product 100.
(18) In addition to or other than steam (i.e., water), vapors that may be sealed within the gas-permeable envelope include, but are not limited to, paraffins such as n-pentane, chlorohydrocarbons such as carbon tetrachloride, CFCs, HCFCs, oxygenated organics such as acetone and ethylene glycol, and/or a wide range of vapors.
(19) With reference to
(20) As discussed, the at least one vapor, once sealed within the gas-impermeable envelope 120, will be eventually cooled down to a temperature below a boiling point of the at least one vapor (e.g., at or above an ambient temperature) to reduce the pressure within the gas-impermeable envelope 120 (as well as to eliminate or at least reduce the need to maintain the product 100 in contact with a cold source to maintain the vapor in the condensed, low-pressure state). In this regard, at least a portion of the assembly line 300, such as between and including the injection of the support material/gas mixture from the chamber 316 into the gas-permeable enclosure 136 up to the sealing of the sealed gas-permeable enclosure 136 within the gas-impermeable envelope 120 (e.g., at station 320, discussed below), may be maintained within any appropriate heating zone 328 that is configured to maintain the at least one vapor at a temperature above its boiling point and limit premature condensation of the vapor. For instance, the heating zone 328 may be in the form of an enclosure made up of vinyl drapes, plastic walls, insulated walls, air curtains, and/or the like.
(21) The support material and at least one vapor need not necessarily be injected substantially simultaneously into the chamber 316 or even into the interior portion of the gas-permeable enclosure 136. In one arrangement, the support material may be injected from the enclosure 308 into the gas-permeable enclosure 136 (e.g., with or without passing through the chamber 316), and then the at least one vapor may be injected from the enclosure 312 into the gas-permeable enclosure 136 (e.g., also with or without passing through the chamber 316). In another arrangement, the support material may be injected or otherwise disposed into the gas-permeable enclosure 136; a liquid (e.g., water) may be applied over the support material (either before or after the support material is injected into the gas-permeable enclosure 136); and then the support material may be heated above the boiling point of the liquid to convert at least some of the liquid into the at least one vapor and thereby drive some or all air out of the gas-permeable enclosure 136. Other manners of disposing and sealing the support material and at least one vapor into the interior portion of the gas-permeable enclosure 136 are also envisioned and included within the scope of the present disclosure.
(22) Once the support material and at least one vapor have been sealed within the interior portion of the gas-permeable enclosure 136, the method 200 of
(23) In one arrangement, the sealed gas-permeable enclosure 136 may be moved along the assembly line 300 by the conveyor belt 304 from the position shown in
(24) After the sealing 212, the method 200 of
(25) Turning now to
(26) In one arrangement, the sealed interior portion may have at least about 2 grams of a liquid per liter of a total volume of the sealed interior portion of the gas-impermeable envelope 120 after the condensing/cooling 216. For instance, the sealed interior portion may have at least about 3 grams of a liquid per liter of a total volume of the sealed interior portion of the gas-impermeable envelope 120 after the condensing/cooling 216 (e.g., at least about 4 grams of a liquid per liter). As another example, the sealed interior portion may have not greater than about 7 grams of a liquid per liter of a total volume of the sealed interior portion of the gas-impermeable envelope 120 after the condensing/cooling 216, such as not greater than about 6 grams of a liquid per liter (e.g., not greater than about 5 grams of a liquid per liter).
(27) As another example, the grams of liquid per liter of the total volume of the sealed interior portion of the gas-impermeable envelope 120 may be at least about two times greater (e.g., three times greater, four times greater, etc.) after the condensing/cooling 216 as compared to before the condensing/cooling 216 (e.g., such as just after the sealing 212). It is noted that the liquid has been illustrated as being concentrated at the bottom of the interior portion of the gas-impermeable envelope 120 for purposes of facilitating the reader's understanding of the present disclosure and that the liquid may in reality be more disbursed within the support material throughout the interior portion of the gas-impermeable envelope 120.
(28) For instance, imagine that the at least one vapor was steam and that it was sealed along with the support material within the interior portion of the gas-impermeable envelope 120 at a temperature of just over about 100 C. In this regard, the pressure within the interior portion of the gas-impermeable envelope 120 may be about 1000 mbar (e.g., at or close to ambient pressure). Upon cooling of the gas-impermeable envelope 120 (and the steam and support material thereinside) down to a temperature at about ambient temperature (e.g., down to about 20 C.), the pressure within the interior portion of the gas-impermeable envelope 120 may drop to only about 20 mbar. The pressure within the gas-impermeable envelope 120 may thus advantageously substantially remain at the 20 mbar level (or other low pressure level) for uses of the resulting product 100 in temperatures substantially the same as the ambient temperature at which the product 100 was cooled 212.
(29) For other vapors (e.g., n-pentane), the interior portion of the gas-impermeable envelope 120 may have a first temperature during the sealing step different (e.g., less) than that at which steam was sealed 212 within the envelope 120, such as about 70 C., and/or a second temperature after the cooling step 216 different (e.g., greater) than that to which the envelope 120 was cooled 216, such as about 40 C. Of course, further pressure reductions within the product 100 may result in cold applications (e.g., refrigeration, shipping containers) in which the product 100 is disposed adjacent a cold source that causes further condensation of vapor remaining within the product 100. Additional pressure reductions may result from the use of different types of support material, pore sizes or overall porosities thereof, getters, and/or the like.
(30) Before referring back to the method 200 and assembly line 300, a further advantage of the finished/resulting thermal insulation products 100 will now be discussed. For instance, transient thermal performance of insulation products (e.g., the ability to resist temperature equilibration between first and second sides of an insulation product) can become important for applications in which the hot and cold temperatures respectively adjacent the opposing first and second surfaces of the products are not temporally independent of each other (e.g., construction, refrigerated trucking, and/or the like). Stated differently, transient performance of an insulation product becomes important when at least one of the first and second surfaces of the insulation product experiences temperature swings relative to the other surface.
(31) Specifically, thermal diffusivity is a measure of transient performance governing the timescale for a material to equilibrate to a change in conditions and depends upon the thermal conductivity, density and heat capacity of the material or product (where thermal diffusivity () is equal to the thermal conductivity () divided by the density () and heat capacity (C.sub.p)). For instance, the characteristic time (i.e., for the temperatures on the first and second surfaces of the product to equilibrate, where characteristic time increases with the square of the insulation product thickness) for a 25 mm thick piece of Expanded Polystyrene (EPS) foam insulation is on the order of a few minutes while that of current VIPs is on the order of an hour or two. Generally, transient thermal performance increases with increasing characteristic time.
(32) Before accounting for any phase changing effects of materials/components in the core of an insulation product (e.g., occurring during a temperature change adjacent a first side of an insulation product relative to an opposing second side of the insulation product) on transient performance of the insulation product, current VIPs and the present thermal insulation products 100 may have comparable transient performance (e.g., both on the order of about an hour or two). However, the increased water content of the present thermal insulation products 100 (e.g., about 4 g/l, such as at least about 6 g/l, or higher) compared to that of current VIPs (e.g., 0.5 g/l or less) may result in a greater degree of phase changing of liquid into a vapor during temperature swings adjacent one side of the products 100 and corresponding increased transient performance of the present thermal insulation products 100 relative to current VIPs. In one arrangement, at least about 50 g/m.sup.3 (e.g., at least about 80 g/m.sup.3, 100 g/m.sup.3, 150 g/m.sup.3, etc.) of the liquid within the sealed interior portion of the disclosed thermal insulation product is operable to evaporate from adjacent one of the first and second opposing surfaces or sides and condense adjacent the other of the first and second opposing surfaces or sides during each temperature fluctuation cycle. In another arrangement, at least about 10% (e.g., such as at least about 30%, 50%, 70%, etc.) of the liquid within the sealed interior portion may be operable to evaporate from adjacent one of the first and second opposing sides or surfaces of the disclosed thermal insulation product and condense adjacent the other of the first and second opposing surfaces during each temperature fluctuation cycle.
(33) Assume that each of a current VIP and a present thermal insulation product 100 was independently used as insulation for an outside wall of a building. For instance,
(34) However, the phase changing of the liquid in the present thermal insulation product 100 into vapor during the temperature swings of the outside ambient environment 600 serves to increase the transient performance of the thermal insulation product 100 by further cooling the first or second side of the thermal insulation product 100 during evaporation of the liquid depending upon which of the first and second sides is the hot side and which is the cold side. For instance, imagine that the first and second surfaces 104, 108 of the thermal insulation product 100 were respectively adjacent the inside and outside of the building 400 as shown in
(35) However, as the second surface 108 of the thermal insulation product 100 heats owing to the outside ambient environment 600 increasing from 5 C. to 35 C. in this example, at least some of the liquid formerly condensed adjacent the second surface 108 on the inside of the thermal insulation product 100 evaporates (e.g., 100 g/m.sup.3) and subsequently condenses on the inside of the thermal insulation product 100 adjacent the first surface 104 (e.g., because the inside/enclosed environment 500 of the building 400 near or adjacent the first surface 104 is now colder (20 C.) than is the outside ambient environment 600 near or adjacent the second surface 108 (35 C.)). As the condensed liquid adjacent the second surface 108 of the thermal insulation product 100 absorbs energy (e.g., heat) from the second surface 108 to evaporate into a vapor, the net result is a cooling effect adjacent the second surface 108 of the thermal insulation product 100 and a corresponding increase in transient thermal performance of the thermal insulation product 100 (e.g., due to the aforementioned cooling effect tending to increase the characteristic time of the thermal insulation product 100 or, in other words, the time to temperature equilibrium between the first and second surfaces 104, 108 of the thermal insulation product 100).
(36) Once the outside ambient environment 600 begins cooling again (e.g., down to the 5 C. temperature in this example), the above discussed process reverses whereby condensed liquid adjacent the first surface 104 of the thermal insulation product 100 evaporates and condenses adjacent the second surface 108 of the thermal insulation product 100 (e.g., due to the relatively hotter temperature (20 C.) of the enclosed environment 500 relative to outside ambient environment 600 (5 C.)) resulting in a cooling effect adjacent the first surface 104 of the thermal insulation product 100. In the event that the time required to pump the fluid from the first surface 108 to the second surface 104 (and vice versa) approaches the diurnal timescales, transient thermal performance can be greatly increased in relation to current VIPs.
(37) The thermal insulation products 100 disclosed herein may be incorporated into a building and/or components thereof (e.g., walls, frames, panels, etc.) in numerous manners for purposes of insulating the same. Turning now to
(38) As shown, the wall structure 700 may include a number of framing members 704 (e.g., studs, channels, joists, rafters, etc. of any appropriate material(s) such as wood, metals, composites, etc.) spaced by any appropriate distance. One or more thermal insulation products 100 may be appropriately disposed or arranged relative to the framing members 704 for purposes of limiting heat transfer through the wall structure 700 from an outside ambient environment 900 into an inside enclosed environment 800 of the building and vice versa. For instance, one or more thermal insulation products 100 may be appropriately disposed between adjacent ones of the framing members 704. In one arrangement, a number of sheathing members 708 (e.g., gypsum board, drywall, particle board, plywood, etc.) may be appropriately disposed over and/or secured to opposite sides of the framing members 704 so as to enclose the thermal insulation products 100 therebetween. Any other appropriate number and/or type of additional sheathing members or components 712 may also be disposed over and/or secured to one or more of the sheathing members 708 such as flashing, spray foam insulation, masonry (e.g., bricks, stone, marble, etc.), siding (e.g., vinyl, metal, etc.), and/or the like. While not shown, the wall structure 700 may be one of a number of interconnected wall structures of one or more buildings, where each interconnected wall structure includes one or more thermal insulation products 100 disposed therein or relative thereto for purposes of limiting heat transfer into and out of the interior of the building(s).
(39) In one arrangement, the one or more thermal insulation products 100 may be disposed over the framing members 704 in addition to or as an alternative to positioning thermal insulation products between adjacent framing members 704 as shown in
(40) With reference back to the assembly line 300 of
(41) For instance, the first and second surfaces may lightly contact or press the first and second sides 104, 108 of the product 100 to simultaneously cool the vapor below its boiling point (e.g., down to an ambient temperature) and form the product 100 into more precise or exact dimensions, but need not exert any substantial amounts of pressure against the first and second sides 104, 108 of the product 100 (e.g., because only minimal pressure may be required to maintain thermal contact and guide shrinkage into a desired final shape). In one embodiment, at least one of the opposing surfaces may have a depression, cavity, or the like, the shape of which is a desired shape of the product 100 to be formed (e.g., similar to a mold cavity).
(42) For instance, movement of at least one of the surfaces towards the other of the surfaces may cause the product 100 to fill and expand in the cavity until the product 100 has assumed the shape of the cavity. As a result, the product 100 may be able to achieve increased dimensional stability and/or tighter tolerances. In another arrangement, the cooling station 324 may be configured to spray a cooling liquid such as water or another liquid (e.g., having a temperature below the boiling point of the gas) over the outside of the product 100 to accelerate condensation of the vapor therewithin. In any event, the conveyor belt 304 may eventually move the finished product 100 out of the cooling station 324 as shown in
(43) Thus, the present disclosure contemplates new methods of producing thermal insulation products that have significant advantages over previous/current manners of making VIPs as well as the resulting thermal insulation products themselves. The resulting thermal insulation products may be used in a variety of applications, such as in the insulation of pipes, electronics, energy sources, apparel, shipping containers, appliances, and other uses for which high thermal efficiency and/or space savings is desirable. The thermal insulation products may be produced in any suitable shape, size, form and/or arrangement, as desired for the application to which it will be applied.
(44) It will be readily appreciated that many additions and/or deviations may be made from the specific embodiments disclosed in the specification without departing from the spirit and scope of the invention. In one arrangement, the gas-impermeable envelope and vapor thereinside may be cooled 216 (e.g., by the cooling station 324 of
EXAMPLE
(45) A thermal insulation panel is manufactured by way of disposing a support material (including 90 wt. % fumed silica and 10 wt. % silicon carbide) and steam at a temperature of about 100 C. within a gas-permeable enclosure (Imperial RB1, product 39317 manufactured by Hanes Engineered Materials) at ambient pressure, sealing the sealed gas-permeable enclosure within a gas-impermeable envelope (Cryovak PFS8155 manufactured by the Sealed Air Corporation) at ambient pressure and with the steam maintained at the temperature of about 100 C., and then cooling the gas-impermeable envelope (including the steam thereinside) for about 5 min down to a temperature of about 35 C.
(46) After the temperature inside the gas-impermeable envelope drops down to about 20 C., the pressure within the resulting thermal insulation panel is about 8 mbar.
(47) When measured with a cold side temperature of about 5 C. and a hot side temperature of about 25 C., the thermal conductivity of the thermal insulation panel is about 0.004 W/mK.
(48) The bulk density of the thermal insulation panel is about 140 g/l.
(49) As will be appreciated, the embodiments described above are for exemplary purposes only and are not intended to limit the scope of the present invention. Various adaptations, modifications and extensions of the described method will be apparent to those skilled in the art and are intended to be within the scope of the invention as defined by the claims that follow.