Method for the Production of a Closed Hollow Profile for a Vehicle Axle
20170066036 · 2017-03-09
Inventors
- Michael Brüggenbrock (Rosendahl, DE)
- Thomas FLEHMIG (Ratingen, DE)
- Thomas Flöth (Duisburg, DE)
- Thomas Grosserüschkamp (Duisburg, DE)
- Norbert Niggemeyer (Paderborn, DE)
- Andreas Frehn (Delbruck, DE)
Cpc classification
B21D22/26
PERFORMING OPERATIONS; TRANSPORTING
B21D5/06
PERFORMING OPERATIONS; TRANSPORTING
B21D22/02
PERFORMING OPERATIONS; TRANSPORTING
B21D53/88
PERFORMING OPERATIONS; TRANSPORTING
International classification
B21D53/88
PERFORMING OPERATIONS; TRANSPORTING
B21D22/26
PERFORMING OPERATIONS; TRANSPORTING
Abstract
A method for the production of a closed hollow profile for a vehicle axle including the following steps: a) provision of a board made out of a sheet of metal, wherein the board has at least a length in a longitudinal direction and at least a width in a transverse direction, b) forming of the board, creating an open profile with a channel running in a longitudinal direction of the board, c) forming the lateral surfaces of the board, creating a hollow profile with a circumference and a longitudinal gap and d) joining together the longitudinal gap.
Claims
1. A method for the production of a closed hollow profile for a vehicle axle comprising the following steps: a) Providing a board made of sheet metal, wherein the board has at least a length (L) in a longitudinal direction and at least a width (B) or a mould contour in a transverse direction, b) Forming the board, wherein an open profile having a channel extending in the longitudinal direction of the board is created, c) Forming the lateral surfaces of the board, wherein a hollow profile having a circumference (U) and having a longitudinal gap is created, and d) Joining of the longitudinal gap, wherein the board is formed such that a compressive stress is generated at least in the region of the longitudinal gap.
2. The method according to claim 1, wherein the width (B) or the mould contour of the board is larger in at least one place than the circumference (U) of the same point on the hollow profile generated during the forming.
3. The method according to claim 1, wherein the board comprises a high-strength or super high-strength steel.
4. The method of claim 1, wherein the board has a thickness in the range from 0.5 mm to 4.0mm.
5. The method of claim 1, wherein the board has an elongation at break of less than 21%.
6. The method of claim 1, wherein the board is formed by any of the following methods: deep drawing, and/or stretch forming, and/or stamping and raising.
7. The method of claim 1, wherein the board is formed such that a butt joint or a lap joint is created.
8. The method of claim 1, wherein the board is formed such that the cross section on both ends of the open profile is substantially U-formed.
9. The method of claim 1, wherein the board is formed such that the cross section in the centre of the profile which is open on one side is substantially W-formed.
10. The method of claim 1, wherein the longitudinal gap is joined by any of the following methods: welding, soldering, adhesion or a mechanical joining process.
Description
BRIEF DESCRIPTION OF THE DRAWINGS
[0020] The invention is described in greater detail below using a drawing which merely shows one preferred embodiment of the invention, in which:
[0021]
[0022]
[0023]
[0024]
[0025]
[0026]
[0027]
[0028]
[0029]
DETAILED DESCRIPTION OF THE INVENTION
[0030]
[0031]
[0032] In step I, a flat board 1 made out of sheet metal is provided. The board 1 was cut on the longitudinal edges and corresponds to the board 1 shown in
[0033]
[0034] Finally,
LIST OF REFERENCE NUMERALS
[0035] 1: Board [0036] 2: Closed hollow profile [0037] 3: End (of board 1) [0038] 4: Indentation [0039] 5: Channel [0040] 6, 7: Lateral surfaces (of board 1) [0041] 8: Hollow profile [0042] 9: Longitudinal gap [0043] 10: Welded seam [0044] L: Length (of board 1) [0045] B: Width (of board 1) [0046] U: Circumference (of the hollow profile 8)