WATER-SOLUBLE FOAMING AGENT FOR MAKING BUBBLE SOLUTION AND METHOD FOR PREPARING SAME

20250109336 ยท 2025-04-03

Assignee

Inventors

Cpc classification

International classification

Abstract

Disclosed are a water-soluble foaming agent for making a bubble solution and a method for preparing the same. The water-soluble foaming agent for making a bubble solution includes a solid foaming agent and a water-soluble coating wrapped around the solid foaming agent in a weight ratio of 10:1 to 20:1. The solid foaming agent includes the following raw materials in percentage by weight: 25 to 45% of surfactant, 4 to 8% of stabilizer, 4 to 12% of glycerol, 10 to 25% of starch, 2 to 6% of pH-sensitive adhesive and 4 to 20% of sugar. The water-soluble coating includes the following raw materials in percentage by weight: 65 to 85% of film former, 2 to 15% of plasticizer and the balance of one or more of colorant or auxiliary additive.

Claims

1. A water-soluble foaming agent for making a bubble solution, comprising a solid foaming agent and a water-soluble coating wrapped around the solid foaming agent in a weight ratio of 10:1 to 20:1; wherein the solid foaming agent comprises the following raw materials in percentage by weight: 25 to 45% of surfactant, 4 to 8% of stabilizer, 4 to 12% of glycerol, 10 to 25% of starch, 2 to 6% of pH-sensitive adhesive and 4 to 20% of sugar; and the water-soluble coating comprises the following raw materials in percentage by weight: 65 to 85% of film former, 2 to 15% of plasticizer and the balance of one or more of colorant or auxiliary additive.

2. The water-soluble foaming agent for making a bubble solution according to claim 1, wherein the surfactant is at least one of sodium lauryl sulfate, sodium dodecylbenzenesulfonate, alkenyl sulfonate, ammonium dodecyl sulfate, sodium lauroyl sarcosinate, alkyl glycoside and peregal.

3. The water-soluble foaming agent for making a bubble solution according to claim 1, wherein the stabilizer is at least one of methyl cellulose, hydroxyethyl cellulose, hydroxypropyl methylcellulose, sodium gluconate, polyvinyl alcohol (PVA) and sodium polyacrylate.

4. The water-soluble foaming agent for making a bubble solution according to claim 1, wherein the film former is at least one of hydroxypropyl methylcellulose, hydroxypropyl cellulose, PVA or copovidone.

5. The water-soluble foaming agent for making a bubble solution according to claim 1, wherein the plasticizer is at least one of ethylene glycol, propylene glycol, castor oil, acetylated monoglyceride or phthalate.

6. The water-soluble foaming agent for making a bubble solution according to claim 1, wherein the colorant is at least one of ferric oxide, edible pigment and titanium dioxide.

7. The water-soluble foaming agent for making a bubble solution according to claim 1, wherein the auxiliary additive is at least one of talcum powder, magnesium stearate, glycerol monostearate or silicon dioxide.

8. A method for preparing the water-soluble foaming agent for making a bubble solution according to claim 1, comprising the following steps: step 1: drying a surfactant, a stabilizer, glycerol, starch, a pH-sensitive adhesive and sugar; step 2: proportionally stirring and grinding the surfactant, the stabilizer, the glycerol, the starch, the pH-sensitive adhesive and the sugar that have been dried in step 1 until they are uniformly mixed to obtain mixed powder; step 3: granulating or tabletting the mixed powder in step 2 to form solid foaming agent granules; step 4: proportionally adding a film former, a plasticizer, and a colorant or/and an auxiliary additive into water, and stirring the mixture to form a coating solution; and step 5: drying the coating solution obtained in step 4 such that a film is formed and shaped so as to form a water-soluble coating bag with an inner cavity, putting the solid foaming agent granules obtained in step 3 into the inner cavity of the water-soluble coating bag, and sealing the water-soluble coating bag to finally obtain the water-soluble foaming agent.

Description

DETAILED DESCRIPTION OF THE EMBODIMENTS

[0023] The present disclosure will be further described in conjunction with specific examples.

Example I

[0024] A water-soluble foaming agent for making a bubble solution includes a solid foaming agent and a water-soluble coating wrapped around the solid foaming agent in a weight ratio of 20:1.

[0025] The solid foaming agent includes the following raw materials in percentage by weight: 38% of surfactant, 7% of stabilizer, 10% of glycerol, 25% of starch, 5% of pH-sensitive adhesive and 15% of sugar.

[0026] The water-soluble coating includes the following raw materials in percentage by weight: 75% of film former, 12% of plasticizer, 3% of colorant and 10% of auxiliary additive.

[0027] In this example, the surfactant in the solid foaming agent is sodium lauryl sulfate. In addition, the stabilizer for stabilizing and assisting foaming can increase a viscosity of the bubble solution and improve a toughness of bubbles. The stabilizer is hydroxyethyl cellulose.

[0028] Moreover, the film former of the water-soluble coating is hydroxypropyl methylcellulose and hydroxypropyl cellulose. The plasticizer is ethylene glycol. The colorant is ferric oxide. The auxiliary additive is magnesium stearate.

Example II

[0029] A water-soluble foaming agent for making a bubble solution includes a solid foaming agent and a water-soluble coating wrapped around the solid foaming agent in a weight ratio of 20:1.

[0030] The solid foaming agent includes the following raw materials in percentage by weight: 35% of surfactant, 6% of stabilizer, 10% of glycerol, 25% of starch, 6% of pH-sensitive adhesive and 18% of sugar.

[0031] The water-soluble coating includes the following raw materials in percentage by weight: 85% of film former, 10% of plasticizer and 5% of auxiliary additive.

[0032] In this example, the surfactant in the solid foaming agent is peregal. In addition, the stabilizer for stabilizing and assisting foaming can increase a viscosity of the bubble solution and improve a toughness of bubbles. The stabilizer is sodium polyacrylate.

[0033] Moreover, the film former of the water-soluble coating is polyvinyl alcohol (PVA). The plasticizer is acetylated monoglyceride. The auxiliary additive is silicon dioxide.

[0034] In addition, a method for preparing the water-soluble foaming agent for making a bubble solution includes the following steps:

[0035] Step 1: A surfactant, a stabilizer, glycerol, starch, a pH-sensitive adhesive and sugar are dried until a water content is less than or equal to 5%.

[0036] Step 2: The surfactant, the stabilizer, the glycerol, the starch, the pH-sensitive adhesive and the sugar that have been dried in step 1 are proportionally stirred and ground until they are uniformly mixed to obtain mixed powder.

[0037] Step 3: The mixed powder in step 2 is granulated or tabletted to form solid foaming agent granules.

[0038] Step 4: A film former, a plasticizer, and a colorant or/and an auxiliary additive are proportionally added into water, and the mixture is stirred to form a coating solution.

[0039] Step 5: The coating solution obtained in step 4 is dried such that a film is formed and shaped so as to form a water-soluble coating bag with an inner cavity, the solid foaming agent granules obtained in step 3 is put into the inner cavity of the water-soluble coating bag, and the water-soluble coating bag is sealed to finally obtain the water-soluble foaming agent.

[0040] The above example is only one of the preferred examples of the present disclosure, and it is not intended to limit the scope of implementation of the present disclosure. Therefore, all equivalent changes made according to the shape, structure and principle of the present disclosure shall fall into the scope of protection of the present disclosure.