A mat structure includes a main body. The main body has a property of toughness. The main body includes a first face and a second face. The main body is formed with a cut line in a middle. The cut line is formed through cutting from the second face of the main body. The cut line has a depth that is smaller than a thickness of the main body. The main body is further provided with at least one surface layer. With the depth of the cut line being smaller than the thickness of the main body and the main body having a property of toughness, the main body can be folded without causing damage. Further, when a die cutter is applied to cut and make the cut line, an allowable tolerance range for the die cutter is enlarged.
Claims
1. A mat structure, comprising: a main body, the main body having a property of toughness, the main body comprising a first face and a second face, the second face of the main body being formed with a cut line in a middle, wherein the cut line has a depth that is smaller than a thickness of the main body.
2. The mat structure according to claim 1, wherein the main body comprises polypropylene (PP), or thermoplastic elastomer (TPE), or thermoplastic polyurethane (TPU).
3. The mat structure according to claim 1, wherein the first face of the main body is formed with a folding line.
4. The mat structure according to claim 1, wherein the first face of the main body is provided with a first surface layer.
5. The mat structure according to claim 4, wherein the first surface layer comprises a material of cutting resistance and toughness.
6. The mat structure according to claim 4, wherein the first surface layer is formed with a folding line in a middle.
7. The mat structure according to claim 1, wherein the second face the main body is provided with a second surface layer.
8. The mat structure according to claim 7, wherein the second surface layer comprises a material of cutting resistance and toughness.
9. The mat structure according to claim 1, wherein the cut line is of a straight configuration.
Description
BRIEF DESCRIPTION OF THE DRAWINGS
[0009]
[0010]
[0011]
[0012]
[0013]
DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0014] Referring to
[0016] In the above, the cut line 13 has a depth D2 that is smaller than a thickness D1 of the main body 1.
[0017] The first face 11 of the main body 1 is further provided with a first surface layer 2, so that connection and integration of the main body 1 during an operation of folding is enhanced by the first surface layer 2 to achieve an effect of extending the service life of the folding function.
[0018] In the above, the first face 11 of the main body 1 or the first surface layer 2 may be further formed with a folding line 14, and folding of the main body 1 can be easily carried out by means of the folding line 14 (as shown in
[0019] In the above, the second face 12 of the main body 1 is further provided with a second surface layer 3, as shown in
[0020] In the above, the main body 1 comprises polypropylene (PP), or thermoplastic elastomer (TPE), or thermoplastic polyurethane (TPU).
[0021] In the above, the first surface layer 2 comprises a cut-resistant and tough material.
[0022] In the above, the second surface layer 3 comprises a cut-resistant and tough material.
[0023] In the above, the cut line 13 is of a straight configuration.
[0024] For practical utilization, the first face 11 or the second face 12 of the main body 1 of the present invention can serve as a cutting surface for conducting cutting, or the first surface layer 2 or the second surface layer 3 provided on the first face 11 and the second face 12 of the main body 1 can be used as a cutting surface for conducting cutting. Further, due to the main body 1 being formed with the cut line 13, the main body 1 can be folded along the folding line 14 (as shown in
[0025] With the depth D2 of the cut line 13 being smaller than the thickness D1 of the main body 1 and the main body 1 having a property of toughness, the main body 1 can be folded along the folding line 14 without causing any damage. Compared with the prior art, the present invention does not need to cut off the main body 1, so that a die cutter, when applied to cutting and making the cut line 13, does not easily cut into and damage the first surface layer 2, and this allows for an enlarged allowable tolerance range for the die cutter. Further, since the present invention does not rely on the first surface layer 2 to connect and integrate the main body 1, the present invention allows the first surface layer 2 to be made thin, and an effect of saving material can be achieved. Further, the arrangement of the main body 1 in combination with the first surface layer 2 helps strengthen connection and integration of the main body 1 during an operation of folding, and an effect of extending service life for folding function is achieved.