Fiber-Based Food Containers
20220049429 · 2022-02-17
Inventors
Cpc classification
D21J5/00
TEXTILES; PAPER
D21H21/14
TEXTILES; PAPER
Y02W90/10
GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
Y02A40/90
GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
B65D85/34
PERFORMING OPERATIONS; TRANSPORTING
B65D1/42
PERFORMING OPERATIONS; TRANSPORTING
B65D65/466
PERFORMING OPERATIONS; TRANSPORTING
B65D81/3453
PERFORMING OPERATIONS; TRANSPORTING
B65D1/22
PERFORMING OPERATIONS; TRANSPORTING
D21H11/12
TEXTILES; PAPER
B29C41/50
PERFORMING OPERATIONS; TRANSPORTING
B65D25/34
PERFORMING OPERATIONS; TRANSPORTING
B65D1/26
PERFORMING OPERATIONS; TRANSPORTING
D21J7/00
TEXTILES; PAPER
B05D5/083
PERFORMING OPERATIONS; TRANSPORTING
International classification
B05D5/08
PERFORMING OPERATIONS; TRANSPORTING
B29C41/50
PERFORMING OPERATIONS; TRANSPORTING
B65D1/22
PERFORMING OPERATIONS; TRANSPORTING
B65D1/26
PERFORMING OPERATIONS; TRANSPORTING
B65D1/42
PERFORMING OPERATIONS; TRANSPORTING
B65D25/34
PERFORMING OPERATIONS; TRANSPORTING
B65D65/46
PERFORMING OPERATIONS; TRANSPORTING
B65D81/34
PERFORMING OPERATIONS; TRANSPORTING
B65D85/34
PERFORMING OPERATIONS; TRANSPORTING
D21H11/12
TEXTILES; PAPER
D21H21/14
TEXTILES; PAPER
D21J5/00
TEXTILES; PAPER
Abstract
Methods and apparatus for manufacturing a microwavable food container include: forming a wire mesh over a mold comprising a mirror image of the microwavable food container; immersing the wire mesh in a fiber-based slurry bath; drawing a vacuum across the wire mesh to cause fiber particles to accumulate at the wire mesh surface; and removing the wire mesh including the accumulated fiber particles from the slurry bath; wherein the slurry comprises one or more of a moisture barrier, an oil barrier, and a vapor barrier.
Claims
1. A food container obtained by: forming a mesh in the shape of a mold corresponding to the shape of the food container; immersing the mesh in a fiber-based slurry; drawing a vacuum across the mesh to cause fiber particles to accumulate at the mesh surface; and removing the mesh and the accumulated fiber particles from the slurry bath; wherein the slurry comprises a moisture barrier component in the range of 1%-10% by weight.
2. The food container of claim 1, wherein the slurry comprises a moisture barrier component in the range of about 4%.
3. The food container of claim 1, wherein the moisture barrier component comprises alkyl ketene dimer (AKD).
4. The food container of claim 1, wherein the moisture barrier component comprises alkyl ketene dimer (AKD) 80.
5. The food container of claim 1, wherein the moisture barrier component comprises long chain diketenes.
6. The food container of claim 1, wherein the slurry comprises a coloring agent comprising one of a cationic dye and a fiber reactive dye.
7. The food container of claim 1, wherein the slurry further comprises a dye absorption agent comprising one of salt and soda ash.
8. The food container of claim 1, further comprising processing the mesh having the accumulated fiber particles in one of a wet or dry process.
9. The food container of claim 1, wherein the slurry further comprises a starch component in the range of 1%-7% by weight.
10. The food container of claim 9, wherein the starch component comprises a cationic liquid starch.
11. The food container of claim 9, wherein the starch component comprises modified polyamines.
12. The food container of claim 9, wherein the starch component forms both hydrogen and ionic bonds with fibers.
13. The food container of claim 9, wherein the starch component comprises a polyamide epichlorohydrin (PAE) resin.
14. The food container of claim 1, further comprising drying the accumulated fiber particles.
15. The food container of claim 14, further comprising applying an oil barrier coating to a surface of the food container.
16. The food container of claim 15, wherein the oil barrier coating comprises a water-based emulsion.
17. The food container of claim 16, wherein the oil barrier coating is in the range of 0.5%-10% of the weight of the food container.
18. The food container of claim 14, further comprising applying a vapor barrier coating to a surface of the food container.
19. The food container of claim 18, wherein the vapor barrier comprises a copolymer composition.
Description
BRIEF DESCRIPTION OF THE DRAWING FIGURES
[0015] Exemplary embodiments will hereinafter be described in conjunction with the appended drawing figures, wherein like numerals denote like elements, and:
[0016]
[0017]
[0018]
[0019]
[0020]
[0021]
[0022]
[0023]
[0024]
[0025]
[0026]
[0027]
[0028]
[0029]
[0030]
[0031]
[0032]
[0033]
[0034]
[0035]
[0036]
DETAILED DESCRIPTION OF PREFERRED EXEMPLARY EMBODIMENTS
[0037] The following detailed description of the invention is merely exemplary in nature and is not intended to limit the invention or the application and uses of the invention. Furthermore, there is no intention to be bound by any theory presented in the preceding background or the following detailed description.
[0038] Various embodiments of the present invention relate to fiber-based or pulp-base products for use both within and outside of the food and beverage industry. By way of non-limiting example, the present disclosure relates to particular chemical formulations of slurries adapted to address the unique challenges facing the food industry including oil barriers, moisture barriers, water vapor barriers, strengthening additives, and/or retention aids, the absence of which have heretofore impeded fiber-based products from displacing single use plastic containers and components in the food industry. The present disclosure further contemplates fiber-based containers having geometric and structural features for enhanced rigidity. Coupling these features with novel chemistries enables fiber-based products to replace their plastic counterparts in a wide variety of applications such as, for example: frozen, refrigerated, and non-refrigerated foods; medical, pharmaceutical, and biological applications; microwavable food containers; beverages; comestible and non-comestible liquids; substances which liberate water, oil, and/or water vapor during storage, shipment, and preparation (e.g., cooking); horticultural applications including consumable and landscaping/gardening plants, flowers, herbs, shrubs, and trees; chemical storage and dispensing apparatus (e.g., paint trays); produce (including human and animal foodstuffs such as fruits and vegetables); salads; prepared foods; packaging for meat, poultry, and fish; lids; cups; bottles; guides and separators for processing and displaying the foregoing; edge and corner pieces for packing, storing, and shipping electronics, mirrors, fine art, and other fragile components; buckets; tubes; industrial, automotive, marine, aerospace and military components such as gaskets, spacers, seals, cushions, and the like; and associated molds, wire mesh forms, recipes, processes, chemical formulae, tooling, slurry distribution, chemical monitoring, chemical infusion, and related systems, apparatus, methods, and techniques for manufacturing the foregoing components.
[0039] Referring now to
[0040] With continued reference to
[0041] In accordance with various embodiments the vacuum mold process is operated as a closed loop system, in that the unused slurry is re-circulated back into the bath where the product is formed. As such, some of the chemical additives (discussed in more detail below) are absorbed into the individual fibers, and some of the additive remains in the water-based solution. During vacuum formation, only the fibers (which have absorbed some of the additives) are trapped into the form, while the remaining additives are re-circulated back into the tank. Consequently, only the additives captured in the formed part must be replenished, as the remaining additives are re-circulated with the slurry in solution. As described below, the system maintains a steady state chemistry within the vacuum tank at predetermined volumetric ratios of the constituent components comprising the slurry.
[0042] Referring now to
[0043] In a typical wet press process, the Hot Press Temperature Range is around 150-250 degree C., with a Hot Press Pressure Range around 140-170 kg/cm.sup.2. The final product density should be around 0.5-1.5 g/cm.sup.3, and most likely around 0.9-1.1 g/cm.sup.3. Final product thickness is about 0.3-1.5 mm, and preferably about 0.5-0.8 mm.
[0044] With continued reference to
[0045] The pulp fiber used in 202 can also be mechanically grinded to improve fiber-to-fiber bonding and improve bonding of chemicals to the fiber. In this way the slurry undergoes a refining process which changes the freeness, or drainage rate, of fiber materials. Refining physically modifies fibers to fibrillate and make them more flexible to achieve better bonding. Also, the refining process can increase tensile and burst strength of the final product. Freeness, in various embodiments, is related to the surface conditions and swelling of the fibers. Freeness (csf) is suitably within the range of 200-700, and preferably about 220-250 for many of the processes and products described herein.
[0046] The chemical formulae (sometimes referred to herein as “chemistries”) and product configurations for various fiber-based packages and containers, as well as their methods for manufacture, will now be described in conjunction with
Produce Containers
[0047]
[0048]
[0049] As briefly mentioned above, the various slurries used to vacuum mold containers according to the present invention comprises a fiber base mixture of pulp and water, with added chemical components to impart desired performance characteristics tuned to each particular product application. The base fiber may include any one or combination of at least the following materials: softwood (SW), bagasse, bamboo, old corrugated containers (OCC), and newsprint (NP). Alternatively, the base fiber may be selected in accordance with the following resources, the entire contents of which are hereby incorporated by this reference: “Lignocellulosic Fibers and Wood Handbook: Renewable Materials for Today's Environment,” edited by Mohamed Naceur Belgacem and Antonio Pizzi (Copyright 2016 by Scrivener Publishing, LLC) and available at books.google.com/books?id=jTL8CwAAQBAJ&printsec=frontcover#v=onepage&q&f=false; “Efficient Use of Fluorescent Whitening Agents and Shading Colorants in the Production of White Paper and Board” by Liisa Ohlsson and Robert Federe, Published Oct. 8, 2002 in the African Pulp and Paper Week and available at tappsa.co.za/archive/APPW2002/Title/Efficient_use_of fluorescent_w/efficient_use_of fluoresce ntw.html; Cellulosic Pulps, Fibres and Materials: Cellucon '98 Proceedings, edited by J F Kennedy, G O Phillips, P A Williams, copyright 200 by Woodhead Publishing Ltd. and available at books.google.com/books?id=xO2iAgAAQBAJ&printsec=frontcover#v=onepage&q&f=false; and U.S. Pat. No. 5,169,497 A entitled “Application of Enzymes and Flocculants for Enhancing the Freeness of Paper Making Pulp” issued Dec. 8, 1992.
[0050] For vacuum molded produce containers manufactured using either a wet or dry press, a fiber base of OCC and NP may be used, where the OCC component is between 50%-100%, and preferably about 70% OCC and 30% NP, with an added moisture/water repellant in the range of 1%-10% by weight, and preferably about 1.5%-4%, and most preferably about 4%. In a preferred embodiment, the moisture/water barrier may comprise alkyl ketene dimer (AKD) (for example, AKD 80) and/or long chain diketenes, available from FOBCHEM at fobchem.com/html_products/Alkyl-Ketene-Dimer%EF%BC%88AKD-WAX%EF%BC%89.html#.VOzozvkrKUk; and Yanzhou Tiancheng Chemical Co., Ltd. at yztianchengchem.com/en/index.php?m=content&c=index&a=show&catid=38&id=124&gclid=CPbn65aUg80CFRCOaQod0JUGRg.
[0051] In order to yield specific colors for molded pulp products, cationic dye or fiber reactive dye may be added to the pulp. Fiber reactive dyes, such as Procion MX, bond with the fiber at a molecular level, becoming chemically part of the fabric. Also, adding salt, soda ash and/or increase pulp temperature will help the absorbed dye to be furtherly locked in the fabric to prevent color bleeding and enhance the color depth.
[0052] To enhance structural rigidity, a starch component may be added to the slurry, for example, liquid starches available commercially as Topcat® L98 cationic additive, Hercobond, and Topcat® L95 cationic additive (available from Penford Products Co. of Cedar Rapids, Iowa). Alternatively, the liquid starch can also be combined with low charge liquid cationic starches such as those available as Penbond® cationic additive and PAF 9137 BR cationic additive (also available from Penford Products Co., Cedar Rapids, Iowa).
[0053] For dry press processes, Topcat L95 may be added as a percent by weight in the range of 0.5%-10%, and preferably about 1%-7%, and particularly for products which need maintain strength in a high moisture environment most preferably about 6.5%; otherwise, most preferably about 1.5-2.0%. For wet press processes, dry strength additives such as Topcat L95 or Hercobond which are made from modified polyamines that form both hydrogen and ionic bonds with fibers and fines. Dry strength additives help to increase dry strength, as well as drainage and retention, and are also effective in fixing anions, hydrophobes and sizing agents into fiber products. Those additives may be added as a percent by weight in the range of 0.5%-10%, and preferably about 1%-6%, and most preferably about 3.5%. In addition, both wet and dry processes may benefit from the addition of wet strength additives, for example solutions formulated with polyamide-epichlorohydrin (PAE) resin such as Kymene 577 or similar component available from Ashland Specialty Chemical Products at ashland.com/products. In a preferred embodiment, Kymene 577 may be added in a percent by volume range of 0.5%-10%, and preferably about 1%-4%, and most preferably about 2% or approximately equal amounts with dosing of dry strength additives. Kymene 577 is of the class of polycationic materials containing an average of two or more amino and/or quaternary ammonium salt groups per molecule. Such amino groups tend to protonate in acidic solutions to produce cationic species. Other examples of polycationic materials include polymers derived from the modification with epichlorohydrin of amino containing polyamides such as those prepared from the condensation adipic acid and dimethylene triamine, available commercially as Hercosett 57 from Hercules and Catalyst 3774 from Ciba-Geigy.
[0054] In some packaging applications it is desired to allow air to flow through the container, for example, to facilitate ripening or avoid spoliation of the contents (e.g. tomatoes). However, conventional vacuum tooling typically rinses excess fiber from the mold using a downwardly directed water spry, thereby limiting the size of the resulting vent holes in the finished produce. The present inventor has determined that re-directing the spray facilitates greater fiber removal during the rinse cycle, producing a larger vent hole in the finished product for a given mold configuration.
[0055] More particularly,
[0056] Referring now to
[0057] With continued reference to
Vent Hole Tooling
[0058]
[0059] With momentary reference to
[0060] As seen in
Microwavable Containers
[0061] Building on knowledge obtained from the development of the aforementioned produce containers, the present inventor has determined that molded fiber containers can be rendered suitable as single use food containers suitable for use in microwave, convection, and conventional ovens by optimizing the slurry chemistry. In particular, the slurry chemistry should advantageously accommodate one or more of the following three performance metrics: i) moisture barrier; ii) oil barrier; and iii) water vapor (condensation) barrier to avoid condensate due to placing the hot container on a surface having a lower temperature than the container. In this context, the extent to which water vapor permeates the container is related to the porosity of the container, which the present invention seeks to reduce. That is, even if the container is effectively impermeable to oil and water, it may nonetheless compromise the user experience if water vapor permeates the container, particularly if the water vapor condenses on a cold surface, leaving behind a moisture ring. The present inventor has further determined that the condensate problem is uniquely pronounced in fiber-based applications because water vapor typically does not permeate a plastic barrier.
[0062] Accordingly, for microwavable containers the present invention contemplates a fiber or pulp-based slurry including one or more of a water barrier, oil barrier, and water vapor barrier, and optional strengthening and/or retention aids. In an embodiment, a fiber base of softwood (SW)/bagasse at a ratio in the range of about 10%-90%, and preferably about 7:3 may be used. As a water/moisture barrier, AKD may be used in the range of about 0.5%-10%, and preferably about 1.5%-4%, and most preferably about 3.5%. As an oil barrier, the grease and oil repellent additives are usually water based emulsions of fluorine containing compositions of fluorocarbon resin or other fluorine-containing polymers such as UNIDYNE TG 8111 or UNIDYNE TG-8731 available from Daikin or World of Chemicals at worldofchemicals.com/chemicals/chemical-properties/unidyne-tg-8111.html. The oil barrier component of the slurry (or topical coat) may comprise, as a percentage by weight, in the range of 0.5%-10%, and preferably about 1%-4%, and most preferably about 2.5%. As a retention aid, an organic compound such as Nalco 7527 available from the Nalco Company of Naperville, Ill. May be employed in the range of 0.1%-1% by volume, and preferably about 0.3%. Finally, to strengthen the finished product, a dry strength additive such as an inorganic salt (e.g., Hercobond 6950 available at: solenis.com/en/industries/tissue-towel/innovations/hercobond-dry-strength-additives; see also sfin.state.or.us/CR2K_SubDB/MSDS/HERCOBOND 6950.PDF) may be employed in the range of 0.5%-10% by weight, and preferably about 1.5%-5%, and most preferably about 4%.
[0063] As mentioned, vapor barrier performance is directly impacted by porosity of the fiber tray. Reducing the porosity of the fiber tray and, hence, improving vapor barrier performance can be achieved using at least two approaches. One is by improving freeness of the tray material by grinding the fibers. The second way is by topical spray coating using, for example, Daikin S2066, which is a water based long chain Flourione-containing polymer. Spray coating may be implemented using in the range of about 0.1%-3% by weight, and preferably about 0.2%-1.5%, and most preferably about 1%.
[0064] Referring now to
Meat Containers
[0065] Presently known meat trays, such as those used for the display of poultry, beef, pork, and seafood in grocery stores, are typically made of plastic based materials such as polystyrene and Styrofoam, primarily because of their superior moisture barrier properties. The present inventor has determined that variations of the foregoing chemistries used for microwavable containers may be adapted for use in meat trays, particularly with respect to the moisture barrier (oil and porosity barriers are typically not as important in a meat tray as they are in a microwave container).
[0066] Accordingly, for meat containers the present invention contemplates a fiber or pulp-based slurry including a water barrier and an optional oil barrier. In an embodiment, a fiber base of softwood (SW)/bagasse and/or bamboo/bagasse at a ratio in the range of about 10%-90%, and preferably about 7:3 may be used. As a moisture/water barrier, AKD may be used in the range of about 0.5%-10%, and preferably about 1%-4%, and most preferably about 4%. As an oil barrier, a water based emulsion may be employed such as UNIDYNE TG 8111 or UNIDYNE TG-8731. The oil barrier component of the slurry (or topical coat) may comprise, as a percentage by weight, in the range of 0.5%-10%, and preferably about 1%-4%, and most preferably about 1.5%. Finally, to strengthen the finished product, a dry strength additive such as Hercobond 6950 may be employed in the range of 0.5%-10% by weight, and preferably about 1.5%-4%, and most preferably about 4%.
[0067] As discussed above in connection with the produce containers, the slurry chemistry may be combined with structural features to provide prolonged rigidity over time by preventing moisture/water from penetrating into the tray.
[0068]
[0069]
Beverage Lids
[0070] Although fiber and pulp based paper cups are widely known, the beverage industry still needs a sustainable fiber-based lid solution. A significant impediment to the widespread adoption of fiber-based lids surrounds the ability to incorporate a zero or negative draft into the lid, in a manner which allows it to be conveniently removed from the mold. In addition, the fiber-based chemistry must be adapted to provide an adequate moisture/water barrier so that the rigidity of the lid is not compromised in the presence of liquid. The methods, chemical formulae, and tooling contemplated by the present invention addresses both of these issues in a manner heretofore not address by the prior art.
[0071] In particular, the chemistry for lids is similar to meat trays and microwave bowls discussed above. Specifically, for beverage container lids the present invention contemplates a fiber or pulp-based slurry including a water/moisture barrier and an optional retention aid. In an embodiment, a fiber base of softwood (SW)/bagasse and/or bamboo/bagasse at a ratio in the range of about 10%-90%, and preferably about 7:3 may be used. As a moisture/water barrier, AKD may be used in the range of about 0.5%-10%, and preferably about 1%-4%, and most preferably about 4%. Rigidity may be enhanced by Hercobond 6950 in the range of 0.5%-10% by weight, and preferably about 1%-4%, and most preferably about 2% or, alternatively, an equal amount as dry strength additives used in the system. Kymene may also be added in the range of 0.5%-10%, and preferably about 1%-4%, and most preferably about 3%. In various embodiments, the Hercobond and/or the Kymene (or functionally analogous additives) may be added to the slurry before addition of the AKD.
[0072] Referring now to
[0073]
Lid Tooling
[0074] A tool for making a fiber-based lid having a zero or negative draft comprises a retractable piston having a shape which generally to a mirror image of the lid, and which is configured to extend to unlock the finished lid from that part of the mold which the lid locks to.
[0075] Referring now to
[0076]
[0077]
Utility and Shipping Containers
[0078]
[0079] While the present invention has been described in the context of the foregoing embodiments, it will be appreciated that the invention is not so limited. For example, the various geometric features and chemistries may be adjusted to accommodate additional applications based on the teachings of the present invention.
[0080] A method is thus provided for manufacturing a produce container. The method includes: forming a wire mesh over a mold comprising a mirror image of the produce container; immersing the wire mesh in a fiber-based slurry bath; drawing a vacuum across the wire mesh to cause fiber particles to accumulate at the wire mesh surface; and removing the wire mesh from the slurry bath; wherein the slurry comprises a moisture/water barrier component in the range of 1.5%-4% by weight.
[0081] In an embodiment the slurry comprises a moisture barrier component in the range of about 4%.
[0082] In an embodiment the moisture barrier component comprises alkyl ketene dimer (AKD).
[0083] In an embodiment the moisture barrier component comprises alkyl ketene dimer (AKD) 80.
[0084] In an embodiment the slurry comprises a fiber base of OCC/NP at a ratio in the range of 0.5/9.5.
[0085] In an embodiment the slurry further comprises a dry strength component in the range of 1%-7% by weight.
[0086] In an embodiment the starch component comprises a cationic liquid starch.
[0087] In an embodiment the slurry further comprises a wet strength component such as Kymene (e.g., Kymene 577) in the range of 1%-4% by weight.
[0088] In an embodiment the mold comprises a rolled edge including a vertically descending skirt.
[0089] In an embodiment the moisture/water barrier comprises AKD in the range of about 4%, wherein the AKD may be added to the pulp slurry as a diluted solution (e.g., 1:10 ADK:Water); the slurry comprises a cationic liquid starch component in the range of 1%-7%; and the mold comprises a rolled edge including a vertically descending skirt, at least one bottom rib, and at least one sidewall rib.
[0090] A produce container manufactured according to the foregoing methods is also provided.
[0091] In a vacuum mold assembly of the type including a wire mesh surrounding a mold form having a substantially vertical insert configured to provide a vent hole in a finished container, a directional rinse assembly is provided. The directional rinse assembly includes: a water supply conduit; a manifold connected to the water supply conduit; and a spray nozzle connected to the manifold and configured to direct a spray of water at the insert along a vector having a horizontal component.
[0092] In an embodiment the mold includes a plurality of substantially vertical inserts, and the directional rinse assembly further includes a plurality of spray nozzles, each configured to direct a spray of water at respective inserts along respective vectors each having a horizontal component.
[0093] A method is also provided for manufacturing a zero or nearly zero porosity food container. This method includes a wet press procedure as the first step, followed by an extra surface coating procedure for applying a thin layer of water based long chain fluorine-containing polymers such as Daikin S 2066, in the range of about 0.5%-6% by weight, and preferably about 1%-5%, and most preferably about 4%.
[0094] A method is also provided for manufacturing a microwavable and/or oven worthy food container. The method includes: forming a wire mesh over a mold comprising a mirror image of the microwavable food container; immersing the wire mesh in a fiber-based slurry bath; drawing a vacuum across the wire mesh to cause fiber particles to accumulate at the wire mesh surface; and removing the wire mesh from the slurry bath; wherein the slurry comprises a moisture barrier component in the range of 0.5%-10% by weight, an oil barrier in the range of 0.5%-10% by weight, and a retention aid in the range of 0.05%-5% by weight.
[0095] In an embodiment the moisture/water barrier component is in the range of about 1.5%-4%, the oil barrier is in the range of about 1%-4%, and the retention aid is in the range of about 0.1%-0.5%.
[0096] In an embodiment the moisture barrier component comprises alkyl ketene dimer (AKD).
[0097] In an embodiment the moisture barrier component comprises alkyl ketene dimer (AKD) 79.
[0098] In an embodiment the slurry comprises a fiber base of SW/bagasse at a ratio in the range of 0.5/9.5.
[0099] In an embodiment the slurry further comprises a rigidity component in the range of 1%-5% by weight.
[0100] In an embodiment the rigidity component comprises a dry inorganic salt.
[0101] In an embodiment the oil barrier comprises a water based emulsion.
[0102] In an embodiment the oil barrier comprises TG 8111.
[0103] In an embodiment the retention aid comprises an organic compound.
[0104] In an embodiment the retention aid comprises Nalco 7527.
[0105] In an embodiment the moisture/water barrier comprises AKD in the range of about 4%; the slurry comprises bagasse and a dry inorganic salt; the oil barrier comprises a water based emulsion; and the vapor barrier comprises an organic compound.
[0106] A microwavable container manufactured according to the foregoing methods is also provided.
[0107] A method of manufacturing a meat tray is provided, the method including: forming a wire mesh over a mold comprising a mirror image of the meat tray; immersing the wire mesh in a fiber-based slurry bath; drawing a vacuum across the wire mesh to cause fiber particles to accumulate at the wire mesh surface; and removing the wire mesh from the slurry bath; wherein the slurry comprises a moisture/water barrier component in the range of 0.5%-10% by weight and an oil barrier in the range of 0.5%-10% by weight.
[0108] In an embodiment the moisture/water barrier component is in the range of about 1%-4% and the oil barrier is in the range of about 1%-4.
[0109] In an embodiment the moisture barrier component comprises alkyl ketene dimer (AKD).
[0110] In an embodiment the moisture barrier component comprises alkyl ketene dimer (AKD) 79.
[0111] In an embodiment the slurry comprises a fiber base of SW/bagasse at a ratio in the range of 1/9.
[0112] In an embodiment the slurry includes a rigidity component in the range of 1.5%-4% by weight.
[0113] In an embodiment the rigidity component comprises a dry inorganic salt.
[0114] In an embodiment the oil barrier comprises a water based emulsion.
[0115] In an embodiment the oil barrier comprises TG 8111 in the range of about 1.5% by weight; the TG8111 may be added to the pulp slurry as a diluted solution (e.g., 1:5, TG8111: Water).
[0116] In an embodiment the moisture/water barrier comprises AKD in the range of about 4%; the slurry comprises bagasse and a dry inorganic salt; and the oil barrier comprises a water based emulsion.
[0117] A meat tray manufactured according to the foregoing methods is also provided.
[0118] In an embodiment the meat tray includes at least one sidewall rib and at least one bottom rib.
[0119] A method of manufacturing a lid for a beverage container is also provided. The method includes: forming a wire mesh over a mold comprising a mirror image of the lid; immersing the wire mesh in a fiber-based slurry bath; drawing a vacuum across the wire mesh to cause fiber particles to accumulate at the wire mesh surface; and removing the wire mesh from the slurry bath; wherein the slurry comprises a moisture/water barrier component in the range of 0.5%-10% by weight, a rigidity component in the range of 1%-4% by weight, and a polycationic component in the range of about 1%-4%.
[0120] In an embodiment the moisture/water barrier component is in the range of about 1%-4% and the oil barrier is in the range of about 1%-4.
[0121] In an embodiment the moisture barrier component comprises alkyl ketene dimer (AKD).
[0122] In an embodiment the moisture barrier component comprises alkyl ketene dime (AKD) 80.
[0123] In an embodiment the slurry comprises a fiber base of SW/bagasse at a ratio in the range of 1/9.
[0124] In an embodiment the slurry further comprises a rigidity component in the range of 1%-4% by weight.
[0125] In an embodiment the rigidity component comprises a dry inorganic salt.
[0126] In an embodiment the moisture/water barrier comprises AKD in the range of about 4%; the slurry comprises bagasse and a dry inorganic salt; and the slurry comprises a polycationic material in the range of about 1%-4% by weight.
[0127] A lid manufactured according to the foregoing methods is also provided.
[0128] In an embodiment the lid further includes a lock ring having a non-positive draft.
[0129] A vacuum tool is also provided for manufacturing a fiber-based beverage lid having a crown and a lock ring including a negative draft. The tool includes: a mold block supporting a lock ring mold portion corresponding to the lid lock ring; a retractable piston assembly comprising a crown mold portion corresponding to the lid crown and a piston shaft; and a pneumatic actuator configured to extend the piston shaft to thereby remove the lid lock ring from the lock ring mold portion.
[0130] In an embodiment the vacuum tool further includes a wire mesh removably surrounding the crown mold portion and the lock ring mold portion.
[0131] A shipping container kit is also provided for a flat screen TV. The kit includes: a top cover; a screen protector; four corrugated pulp corner pieces configured to fit over respective corresponding corners of the flat screen TV; a bottom tray configured to nest with the top cover; and a pallet strap configured to secure the TV, screen protector, corrugated pulp corner pieces within the nested top cover and bottom tray.
[0132] As used herein, the word “exemplary” means “serving as an example, instance, or illustration.” Any implementation described herein as “exemplary” is not necessarily to be construed as preferred or advantageous over other implementations, nor is it intended to be construed as a model that must be literally duplicated.
[0133] While the foregoing detailed description will provide those skilled in the art with a convenient road map for implementing various embodiments of the invention, it should be appreciated that the particular embodiments described above are only examples, and are not intended to limit the scope, applicability, or configuration of the invention in any way. To the contrary, various changes may be made in the function and arrangement of elements described without departing from the scope of the invention.