B32B2329/00

DECORATIVE SHEET WITH ADHESIVE
20200122428 · 2020-04-23 ·

A decorative sheet with adhesive according to the present disclosure comprises a decorative plate layer and an adhesive layer. The decorative plate layer includes a decorative layer and a mixed paper layer which includes a magnesium silicate mixed paper with bound water.

Interlayer for laminated glass and laminated glass
10596784 · 2020-03-24 · ·

There is provided an interlayer film for laminated glass with which double images in laminated glass can be considerably suppressed. The interlayer film for laminated glass according to the present invention has one end and the other end being at the opposite side of the one end, makes the thickness of the other end larger than the thickness of the one end, has a display corresponding region corresponding to a display area of the head-up display, and when a position apart from an end part at the one end side of the display corresponding region by 4 cm toward the other end is set to a start point, a position apart from an end part at the other end side of the display corresponding region by 4 cm toward the one end is set to an end point, spots are selected at 2-mm intervals from the start point to the end point, and the interlayer film is measured for the amount of change in the thickness within respective segments, centered on the respective spots, of 80 mm in a direction connecting the one end and the other end, makes the absolute value of a difference between the largest value among values of the amount of change in the thickness and the smallest value among values of the amount of change in the thickness 32 m or less.

POLY(VINYL ACETAL) RESIN COMPOSITIONS, LAYERS, AND INTERLAYERS HAVING ENHANCED PROPERTIES
20190381772 · 2019-12-19 · ·

Resin compositions, layers, and interlayers comprising a poly(vinyl acetal) resin that includes residues of an aldehyde other than n-butyraldehyde are provided. Such compositions, layers, and interlayers can exhibit enhanced or optimized properties as compared to those formulated with comparable poly(vinyl n-butyral) resins.

MANUFACTURING METHOD FOR GLASS FILM WITH RESIN TAPE, AND MANUFACTURING METHOD FOR GLASS FILM

Provided is a method comprises: continuously forming an elongated, glass film having marginal portions from molten glass into a given shape having two marginal portions, in width-directional opposite edge regions thereof, wherein the glass film having marginal portions has the marginal portions, and an effective portion formed in a width-directional central region of the glass film having marginal portions; annealing the glass film having marginal portions; continuously forming resin tapes on the glass film having marginal portions at positions adjacent to and away by a given distance from the respective marginal portions, to extend in a length direction of the glass film having marginal portions; and continuously removing each of the marginal portions from the glass film having marginal portions, along a position between the marginal portion and a corresponding one of the resin tapes, or at a given width-directional position within the corresponding resin tape.

Poly(vinyl acetal) resin compositions, layers, and interlayers having enhanced properties
10391749 · 2019-08-27 · ·

Resin compositions, layers, and interlayers comprising a poly(vinyl acetal) resin that includes residues of an aldehyde other than n-butyraldehyde are provided. Such compositions, layers, and interlayers can exhibit enhanced or optimized properties as compared to those formulated with comparable poly(vinyl n-butyral) resins.

TECHNIQUES TO MOLD PARTS WITH INJECTION-FORMED APERTURE IN GATE AREA
20190255748 · 2019-08-22 ·

Methods and systems for co-extruding multiple polymeric material flow streams into a mold cavity to produce a molded plastic article having an injection-formed aperture in gate region of the article are disclosed herein. A method includes providing a valve pin having a distal portion with a first diameter and a mid-portion with a second diameter smaller than the first diameter and providing a mold defining a cavity corresponding to a shape of a resulting molded plastic article. The mold has a recess aligned with a gate region of the mold, extending into the mold and configured to receive the distal portion of the valve pin when the distal portion of the valve pin extends beyond the gate region. The method includes advancing the distal portion of the valve pin into the recess until the mid-portion of the valve pin at least partially extends into the gate region, thereby establishing a flow path for a combined polymeric stream into the cavity at the gate region for forming a molded plastic article having at least one layer of a first polymeric material and at least one layer of a second polymeric material. The method also includes withdrawing the mid-portion of the valve pin from the gate region, thereby forming an injection-molded aperture in the resulting molded plastic article at the gate region.

FILLING-BONDING MATERIAL, PROTECTIVE SHEET-EQUIPPED FILLING-BONDING MATERIAL, LAMINATED BODY, OPTICAL DEVICE, AND PROTECTIVE PANEL FOR OPTICAL DEVICE

The present invention aims to provide a filling-bonding material that is suitably used to fill a space between parts, while bonding the parts, in optical devices in various shapes not limited to flat shapes. The present invention also aims to provide a protective sheet-equipped filling-bonding material, a laminate, an optical device, and a protective panel for an optical device each including the filling-bonding material. Provided is a filling-bonding material having a shape with an uneven thickness.

GLASS LAMINATES WITH IMPROVED FLATNESS AND METHODS FOR FORMING THE SAME
20190184683 · 2019-06-20 ·

A glass laminate includes a non-glass substrate with a first surface and a second surface opposite the first surface. A glass sheet is laminated to the first surface of the non-glass substrate. A barrier film is laminated to the second surface of the non-glass substrate and includes a first surface adjacent to the non-glass substrate, a second surface opposite the first surface. A thickness of the barrier film can be at most about 0.5 mm. The second surface of the barrier film can define an outer surface of the glass laminate. The barrier film can be a multi-layer barrier film with a metal layer and a polymer layer. An absolute value of a flatness of the glass laminate determined according to European Standard EN 438 after exposure to 23 C. and 90% relative humidity for 7 days can be at most about 3 mm/m.

Manufacturing method for glass film with resin tape, and manufacturing method for glass film

Provided is a method comprises: continuously forming an elongated, glass film having marginal portions from molten glass into a given shape having two marginal portions, in width-directional opposite edge regions thereof, wherein the glass film having marginal portions has the marginal portions, and an effective portion formed in a width-directional central region of the glass film having marginal portions; annealing the glass film having marginal portions; continuously forming resin tapes on the glass film having marginal portions at positions adjacent to and away by a given distance from the respective marginal portions, to extend in a length direction of the glass film having marginal portions; and continuously removing each of the marginal portions from the glass film having marginal portions, along a position between the marginal portion and a corresponding one of the resin tapes, or at a given width-directional position within the corresponding resin tape.

INTERLAYER FOR LAMINATED GLASS AND LAMINATED GLASS
20190143649 · 2019-05-16 ·

There is provided an interlayer film for laminated glass with which double images in laminated glass can be considerably suppressed. The interlayer film for laminated glass according to the present invention has one end and the other end being at the opposite side of the one end, makes the thickness of the other end larger than the thickness of the one end, has a display corresponding region corresponding to a display area of the head-up display, and when a position apart from an end part at the one end side of the display corresponding region by 4 cm toward the other end is set to a start point, a position apart from an end part at the other end side of the display corresponding region by 4 cm toward the one end is set to an end point, spots are selected at 2-mm intervals from the start point to the end point, and the interlayer film is measured for the amount of change in the thickness within respective segments, centered on the respective spots, of 80 mm in a direction connecting the one end and the other end, makes the absolute value of a difference between the largest value among values of the amount of change in the thickness and the smallest value among values of the amount of change in the thickness 32 m or less.