C22C45/00

Method and apparatus for supercooling of metal/alloy melts and for the formation of amorphous metals therefrom

A method and apparatus are described for creation of amorphous metals using electromagnetic supercooling of a metal/alloy without the utilization of rapid quenching or immaculate process environments. By exposing the cooling melt to electric currents, either induced by an alternating current (AC) magnetic field or supplied directly, crystallization is suppressed, and the melt can reach significant levels of supercooling. With sufficient current densities in the melt, the supercooling can extend all the way into the glass transition range for certain materials, at which point an amorphous metal/alloy is created.

Method and apparatus for supercooling of metal/alloy melts and for the formation of amorphous metals therefrom

A method and apparatus are described for creation of amorphous metals using electromagnetic supercooling of a metal/alloy without the utilization of rapid quenching or immaculate process environments. By exposing the cooling melt to electric currents, either induced by an alternating current (AC) magnetic field or supplied directly, crystallization is suppressed, and the melt can reach significant levels of supercooling. With sufficient current densities in the melt, the supercooling can extend all the way into the glass transition range for certain materials, at which point an amorphous metal/alloy is created.

Ejector for metal jetting bulk metallic glass compositions and methods thereof

A metal component is disclosed. The metal component has a first dimension greater than 5 mm, and a second dimension greater than 5 mm. The metal component may include where the alloy includes titanium, aluminum, vanadium, carbon, nitrogen, and oxygen. The alloy may include zirconium, titanium, copper, nickel, and beryllium. The metal component is not die-cast, melt-spun, or forged. An ejector and a method for jetting the metal component is also disclosed.

Amorphous alloy, molding die, and method for forming optical element

An amorphous alloy contains Ni and Nb and has a composition including at least one of: a composition containing Nb with a content in the range of 35.6 atomic % to 75.1 atomic %, Ir with a content in the range of 7.2 atomic % to 52.3 atomic %, and Ni with a content in the range of 4.0 atomic % to 48.5 atomic %; a composition containing Nb with a content in the range of 19.6 atomic % to 80.9 atomic %, Re with a content in the range of 7.4 atomic % to 59.2 atomic %, and Ni with a content in the range of 4.1 atomic % to 56.9 atomic %; and a composition containing Nb with a content in the range of 7.5 atomic % to 52.9 atomic %, W with a content in the range of 16.4 atomic % to 47.0 atomic %, and Ni with a content in the range of 22.0 atomic % to 53.3 atomic %.

Amorphous alloy, molding die, and method for forming optical element

An amorphous alloy contains Ni and Nb and has a composition including at least one of: a composition containing Nb with a content in the range of 35.6 atomic % to 75.1 atomic %, Ir with a content in the range of 7.2 atomic % to 52.3 atomic %, and Ni with a content in the range of 4.0 atomic % to 48.5 atomic %; a composition containing Nb with a content in the range of 19.6 atomic % to 80.9 atomic %, Re with a content in the range of 7.4 atomic % to 59.2 atomic %, and Ni with a content in the range of 4.1 atomic % to 56.9 atomic %; and a composition containing Nb with a content in the range of 7.5 atomic % to 52.9 atomic %, W with a content in the range of 16.4 atomic % to 47.0 atomic %, and Ni with a content in the range of 22.0 atomic % to 53.3 atomic %.

Powder for magnetic member

Provided is a powder suitable for a magnetic member capable of suppressing noise in a frequency range of 100 kHz to 20 MHz. The powder for a magnetic member contains a plurality of particles 2. The main part of the particle 2 is made of an alloy. The alloy contains B. The content of B in the alloy is 5.0 mass % or more and 8.0 mass % or less. The alloy may further contain one or more elements selected from the group consisting of Cr, Mn, Co, and Ni. The content of these elements is 0 mass % or more and 25 mass % or less. The balance of the alloy is Fe and unavoidable impurities. The alloy contains an Fe.sub.2B phase. The area percentage of the Fe.sub.2B phase in the alloy is 20 mass % or more and 80 mass % or less.

High-density thermodynamically stable nanostructured copper-based bulk metallic systems, and methods of making the same

High-density thermodynamically stable nanostructured copper-based metallic systems, and methods of making, are presented herein. A ternary high-density thermodynamically stable nanostructured copper-based metallic system includes: a solvent of copper (Cu) metal; that comprises 50 to 95 atomic percent (at. %) of the metallic system; a first solute metal dispersed in the solvent that comprises 0.01 to 50 at. % of the metallic system; and a second solute metal dispersed in the solvent that comprises 0.01 to 50 at. % of the metallic system. The internal grain size of the solvent is suppressed to no more than 250 nm at 98% of the melting point temperature of the solvent and the solute metals remain uniformly dispersed in the solvent at that temperature. Processes for forming these metallic systems include: subjecting powder metals to a high-energy milling process, and consolidating the resultant powder metal subjected to the milling to form a bulk material.

FOLDABLE DISPLAY STRUCTURES
20190352756 · 2019-11-21 ·

One embodiment provides a structure, comprising: a display; at least one structural component disposed over a portion of the display, wherein the at least on structural component comprises at least one amorphous alloy; and wherein a portion of the display is foldable.

FOLDABLE DISPLAY STRUCTURES
20190352756 · 2019-11-21 ·

One embodiment provides a structure, comprising: a display; at least one structural component disposed over a portion of the display, wherein the at least on structural component comprises at least one amorphous alloy; and wherein a portion of the display is foldable.

MAGNESIUM-BASED BULK METALLIC GLASS COMPOSITE AND SUTURE ANCHOR THEREOF

A magnesium-based bulk metallic glass composite includes a magnesium-based bulk metallic glass composite comprising a magnesium-based material and a TiZr alloy.