Patent classifications
C08F291/00
CURABLE COMPOSITION AND CURED PRODUCT THEREOF
A curable composition includes an olefin-aromatic vinyl compound-aromatic polyene copolymer satisfying conditions (1) to (4) and an additive resin, which is at least one of a hydrocarbon-based elastomer, polyphenylene ether, olefin-aromatic vinyl compound-aromatic polyene copolymerized oligomer, and aromatic polyene-based resin. (1) The number average molecular weight of the copolymer is 5000 to 100000. (2) The aromatic vinyl compound monomer has 8 to 20 carbon atoms, and the content of the unit of the monomer is 0 to 70 mass %. (3) The aromatic polyene is selected from polyenes having 5 to 20 carbon atoms and a plurality of vinyl and/or vinylene groups in the molecule, and the content of the groups is 1.5 to 20 pieces per number average molecular weight. (4) The olefin is selected from olefins having 2 to 20 carbon atoms, and the total monomer units of the olefin, aromatic vinyl compound, and aromatic polyene is 100 mass %.
CURABLE COMPOSITION AND CURED PRODUCT THEREOF
A curable composition includes an olefin-aromatic vinyl compound-aromatic polyene copolymer satisfying conditions (1) to (4) and an additive resin, which is at least one of a hydrocarbon-based elastomer, polyphenylene ether, olefin-aromatic vinyl compound-aromatic polyene copolymerized oligomer, and aromatic polyene-based resin. (1) The number average molecular weight of the copolymer is 5000 to 100000. (2) The aromatic vinyl compound monomer has 8 to 20 carbon atoms, and the content of the unit of the monomer is 0 to 70 mass %. (3) The aromatic polyene is selected from polyenes having 5 to 20 carbon atoms and a plurality of vinyl and/or vinylene groups in the molecule, and the content of the groups is 1.5 to 20 pieces per number average molecular weight. (4) The olefin is selected from olefins having 2 to 20 carbon atoms, and the total monomer units of the olefin, aromatic vinyl compound, and aromatic polyene is 100 mass %.
Negative photosensitive resin composition, cured film, element provided with cured film, organic EL display provided with cured film, and method for producing same
The invention aims to provide a cured film that is high in sensitivity, able to form a pattern having a small-tapered shape after a development step and after a heat curing step, helpful to depress the difference in the width of patterned openings between before and after the heat curing step, and high in light-shielding capability and also aims to provide a negative type photosensitive resin composition that serves for the production thereof. The negative type photosensitive resin composition includes an alkali-soluble resin (A), a radical polymerizable compound (B), a photo initiator (C1), and a black colorant (Da); the alkali-soluble resin (A) including a first resin (A1) containing one or more selected from the group consisting of polyimide (A1-1), polyimide precursor (A1-2), polybenzoxazole (A1-3), polybenzoxazole precursor (A1-4), and polysiloxane (A1-5); and the radical polymerizable compound (B) including one or more selected from the group consisting of a fluorene backbone-containing radical polymerizable compound (B1) and an indane backbone-containing radical polymerizable compound (B2).
AQUEOUS DISPERSION AND IMAGE RECORDING METHOD
An ink including particles including a polymer P and a polymerizable monomer M and water, wherein the polymer P includes a salt of an anionic group, and of the salt, a content of a salt derived from a neutralizer having a solubility in water at 20° C. of 12.5 g/100 mL or less is more than 90 mol %, and an image recording method.
Self-wetting adhesive composition
A self-wetting adhesive composition is described comprising the reaction product of a low T.sub.g (meth)acrylate solute copolymer component; a low T.sub.g solvent monomer solvent monomer component comprising low T.sub.g monomers, a multifunctional acrylate; and a polymerizable siloxane copolymer having at least one polydiorganosiloxane segment and at least on oxyalkylene segment.
Self-wetting adhesive composition
A self-wetting adhesive composition is described comprising the reaction product of a low T.sub.g (meth)acrylate solute copolymer component; a low T.sub.g solvent monomer solvent monomer component comprising low T.sub.g monomers, a multifunctional acrylate; and a polymerizable siloxane copolymer having at least one polydiorganosiloxane segment and at least on oxyalkylene segment.
PHOTOCURABLE RESIN COMPOSITION, INK, AND COATING
An object of the present invention is to provide a photocurable resin composition that has excellent adhesion to plastic substrates and can form a composition with good compatibility. The present invention relates to a photocurable resin composition containing: an allylic polymer (A) produced by polymerization of an allylic compound represented by the formula (I) below; and a tackifier resin (B),
##STR00001##
SURFACE MODIFICATION METHOD
Provided are methods for surface-modifying a tubular object of a rubber vulcanizate or a thermoplastic elastomer. The methods allow these objects to have at least a lubricating inner surface layer chemically fixed thereon, instead of having a resin coating which has drawbacks such as reduction in lubricity due to e.g. separation or peeling of the coating during movement within a vessel or tract. Included is a method for surface-modifying a tubular object made of a rubber vulcanizate or a thermoplastic elastomer whose side wall may have an opening, the method including: step 1 of forming polymerization initiation points on at least the outer surface of the object; and step 2 of irradiating the outer surface of the object with ultraviolet light of 300-400 nm to radically polymerize a monomer using radicals generated from the polymerization initiation points to grow polymer chains on at least the inner surface of the object.
SURFACE MODIFICATION METHOD
Provided are methods for surface-modifying a tubular object of a rubber vulcanizate or a thermoplastic elastomer. The methods allow these objects to have at least a lubricating inner surface layer chemically fixed thereon, instead of having a resin coating which has drawbacks such as reduction in lubricity due to e.g. separation or peeling of the coating during movement within a vessel or tract. Included is a method for surface-modifying a tubular object made of a rubber vulcanizate or a thermoplastic elastomer whose side wall may have an opening, the method including: step 1 of forming polymerization initiation points on at least the outer surface of the object; and step 2 of irradiating the outer surface of the object with ultraviolet light of 300-400 nm to radically polymerize a monomer using radicals generated from the polymerization initiation points to grow polymer chains on at least the inner surface of the object.
THERMOPLASTIC ELASTOMER COMPOSITION
Provided is a thermoplastic elastomer composition excellent in mechanical characteristics, abrasion resistance, etc., comprising: a crosslinked composition (X) obtained by heat-treating, under molten condition, a composition containing 100 pars of a block copolymer or a hydrogenated product thereof, the block copolymer including a polymer block A mainly derived from an aromatic vinyl compound containing 1% by mass or more of an alkylstyrene and a polymer block B mainly derived from a diene compound, 10 to 300 parts of an olefin-based resin, 0.01 to 20 parts of a crosslinking agent, 1 to 50 parts of a crosslinking adjuvant, and 30 to 250 parts of a softener for rubber; and a hydrogenated block copolymer (Y) obtained by hydrogenating a block copolymer having at least two polymer blocks of an aromatic vinyl compound and at least one polymer block of a conjugated diene compound, with the mass ratio of (X)/(Y)=10/90 to 90/10.