High-strength and tear-resistant leather materials and methods of manufacture

A leather substrate formed from waste leather and its method of production, particularly a leather substrate made up substantially of a collagen fibril matrix.

Apparatus for treating waste leather

An apparatus for treating leather waste includes: a main body having an inlet and an outlet; a sorting unit rotatably installed in the main body and comprising a plurality of treatment parts having processing components to sort leather inserted into the main body through the inlet; and a power unit configured to rotate the sorting unit.

Apparatus for treating waste leather

An apparatus for treating leather waste includes: a main body having an inlet and an outlet; a sorting unit rotatably installed in the main body and comprising a plurality of treatment parts having processing components to sort leather inserted into the main body through the inlet; and a power unit configured to rotate the sorting unit.

RECYCLED LEATHER, AND APPARATUS FOR DRY-MANUFACTURING RECYCLED LEATHER
20220002825 · 2022-01-06 ·

Disclosed is an apparatus for dry-manufacturing recycled leather comprising air-laid material; and recycled leather manufactured using the apparatus for dry-manufacturing recycled leather. The apparatus for dry-manufacturing recycled leather molds leather fibers and general fibers, which are mixed using air-laid material, and thus a conventional carding process is not required, and recycled leather manufactured thereby has a high tensile strength.

High-strength and tear-resistant leather materials and methods of manufacture

A leather substrate formed from waste leather and its method of production, particularly a leather substrate made up substantially of a collagen fibril matrix.

PROCESS FOR MANUFACTURING RECONSTITUTED LEATHER PRODUCT
20220282343 · 2022-09-08 · ·

A reconstituted-leather-manufacturing process includes a progressively increasing application of pressure to an aqueous leather solution to form a web of leather fibers. The solution/web may be dewatered to an extent before the first application of a pressure so that the solution/web consistency is on the order 29-55% (fiber to web/solution, by weight) when the first pressure of the progressive sequence of pressures is applied. Tannin (and various chemicals) may be added to the solution. The progressive pressing of the solution/web may be followed by a progressive drying of the web by application of a sequence of increasing temperatures via drying vessels.

METHOD FOR OBTAINING A MODIFIED COLLAGEN ABSORBENT PRODUCT FROM LEATHER
20220072507 · 2022-03-10 ·

The invention relates to a method for obtaining a modified collagen absorbent product from leather, which comprises aerating flat pieces of leather during a time period of between 15 and 45 days; collecting the pieces with an initial relative humidity value of 45% or less; grading the pieces by size; obtaining pieces with a maximum final length of between 0.5 and 1.5 mm; placing the pieces in a drying oven; applying heat in the drying oven so that the pieces are exposed to a temperature of 285° C. or less during a time period; controlling the temperature applied during the time period so that the relative humidity is reduced to a final value of between 0.5% and 5% in the pieces; reducing the temperature of the pieces to an ambient temperature; and obtaining the modified collagen absorbent product from leather.

Recycled leather, and apparatus for dry-manufacturing recycled leather
12018339 · 2024-06-25 · ·

An apparatus for dry-manufacturing recycled leather comprises air-laid material; and recycled leather manufactured using the apparatus for dry-manufacturing recycled leather. The apparatus for dry-manufacturing recycled leather molds leather fibers and general fibers, which are mixed using air-laid material, and thus a conventional carding process is not required, and recycled leather manufactured thereby has a high tensile strength.

Recycled leather, and apparatus for dry-manufacturing recycled leather
12018339 · 2024-06-25 · ·

An apparatus for dry-manufacturing recycled leather comprises air-laid material; and recycled leather manufactured using the apparatus for dry-manufacturing recycled leather. The apparatus for dry-manufacturing recycled leather molds leather fibers and general fibers, which are mixed using air-laid material, and thus a conventional carding process is not required, and recycled leather manufactured thereby has a high tensile strength.

APPARATUS FOR TREATING WASTE LEATHER

An apparatus for treating leather waste includes: a main body having an inlet and an outlet; a sorting unit rotatably installed in the main body and comprising a plurality of treatment parts having processing components to sort leather inserted into the main body through the inlet; and a power unit configured to rotate the sorting unit.