Patent classifications
C23C14/08
Recording layer for optical data recording medium, optical data recording medium, and sputtering target
A recording layer for an optical data recording medium according to one embodiment of the present invention makes it possible to record an information signal by irradiation with laser beam. The recording layer for an optical data recording medium comprises metal oxides including a Mn oxide, a W oxide, and a Sn oxide. The atomic ratio of Mn with respect to the total number of atoms of metal elements constituting the metal oxides is 3-40 atm %.
LENS ASSEMBLY, CAMERA MODULE HAVING A LENS ASSEMBLY FOR MOTOR VEHICLES, AND A METHOD FOR MAKING LENS ASSEMBLY
The camera module has a lens assembly comprising a body and a heating element with an optically transparent coating applied to the body for heating it as electric current flows for removing water-based obstructions. The module includes a power supply for supplying electric current to the optically transparent coating through conductors, and a lens barrel (for receiving the body comprising a passageway for the conductors extending within the lens barrel towards the lens body. The method comprises applying to the lens body, high- and low-refractive index layers and an aluminium-doped zinc oxide layer.
Metal oxide film formation method
In a metal oxide film formation method of the present invention, the following steps are performed. In a solution vessel, a raw-material solution including aluminum as a metallic element is turned into a mist so that a raw-material solution mist is obtained. In a solution vessel provided independently of the solution vessel, a reaction aiding solution including a reaction aiding agent for formation of aluminum oxide is turned into a mist so that an aiding-agent mist is obtained. Then, the raw-material solution mist and the aiding-agent mist are fed to a nozzle provided in a reactor vessel via paths. Thereafter, the raw-material solution mist and the aiding-agent mist are mixed in the nozzle so that a mixed mist is obtained. Then, the mixed mist is fed onto a back surface of a heated P-type silicon substrate.
Innovation In High Performance Electro-Chromic Device Manufacturing Method
The invention relates to the manufacturing method of high performance electro-chromic devices containing transition metal oxide based compounds, wherein it comprises the steps of enlarging of the metal contact with Pt (Platinum) (1) sputtering method on one edge of the 80-150 nm thick Indium-Tin oxide alloy (ITO) (2), which was previously enlarged on the glass (3) by the sputter method, growing vertical nano-wall structures at 15-25 mTorr, 300-500° C. substrate temperature and at 3-45 minutes intervals on glass (3) with sputter method, by using transition metal chalcogen targets on previously enlarged ITO (2) with a thickness of 80-150 nm, oxidizing the grown structures in the oxidizing furnace for 10-60 minutes under oxygen gas in the temperature range 300-450° C., preparing the electro-chromic device by placing a counter glass/ITO (80-150 nm) in propylene carbonate (PC) to face 1 Mole/Liter Lithium perchlorate (LiClO4) ion-conducting electrolyte (6) with a 0.5-1 mm distance between them and closing it.
MIXED METAL OXIDE
In an aspect, a mixed metal oxide comprises or consists essentially of: a mixture comprises or consisting essentially of 0.30 to 0.69 parts by mole Mg, 0.20 to 0.69 parts by mole Zn, 0.01 to 0.30 parts by mole of a third element selected from Al and Ga, and, either, when the third element is Al, 0.00 to 0.31 parts by mole of other elements selected from metals and metalloids, or, when the third element is Ga, 0.00 to 0.15 parts by mole of other elements selected from metals and metalloids, wherein the sum of all parts by mole of Mg, Zn, the third element, and the other elements amounts to 1.00, wherein the amount in parts by mole of the other elements is lower than the amount in parts by mole of Mg and is lower than the amount in parts by mole of Zn; oxygen; and less than 0.01 parts by mole of non-metallic and non-metalloid impurities.
Object in a lithographic apparatus
An object, such as a sensor for an immersion lithographic apparatus, has an outer layer which comes in contact with immersion liquid and wherein the outer layer has a composition including a rare earth element. There is also provided an immersion lithographic apparatus having such an object and a method for manufacturing such an object.
Object in a lithographic apparatus
An object, such as a sensor for an immersion lithographic apparatus, has an outer layer which comes in contact with immersion liquid and wherein the outer layer has a composition including a rare earth element. There is also provided an immersion lithographic apparatus having such an object and a method for manufacturing such an object.
Electrochromic devices
Conventional electrochromic devices frequently suffer from poor reliability and poor performance. Improvements are made using entirely solid and inorganic materials. Electrochromic devices are fabricated by forming an ion conducting electronically-insulating interfacial region that serves as an IC layer. In some methods, the interfacial region is formed after formation of an electrochromic and a counter electrode layer. The interfacial region contains an ion conducting electronically-insulating material along with components of the electrochromic and/or the counter electrode layer. Materials and microstructure of the electrochromic devices provide improvements in performance and reliability over conventional devices. In various embodiments, a counter electrode is fabricated to include a base anodically coloring material and one or more additives.
ION BEAM SPUTTERING WITH ION ASSISTED DEPOSITION FOR COATINGS ON CHAMBER COMPONENTS
An article comprises a body and a conformal protective layer on at least one surface of the body. The conformal protective layer is a plasma resistant rare earth oxide film having a thickness of less than 1000 μm, wherein the plasma resistant rare earth oxide film is selected from a group consisting of an Er—Y composition, an Er—Al—Y composition, an Er—Y—Zr composition, and an Er—Al composition.
ION BEAM SPUTTERING WITH ION ASSISTED DEPOSITION FOR COATINGS ON CHAMBER COMPONENTS
An article comprises a body and a conformal protective layer on at least one surface of the body. The conformal protective layer is a plasma resistant rare earth oxide film having a thickness of less than 1000 μm, wherein the plasma resistant rare earth oxide film is selected from a group consisting of an Er—Y composition, an Er—Al—Y composition, an Er—Y—Zr composition, and an Er—Al composition.