Patent classifications
C23C16/24
METHODS FOR SELECTIVELY DEPOSITING AN AMORPHOUS SILICON FILM ON A SUBSTRATE
A method for selectively depositing an amorphous silicon film on a substrate comprising a metallic nitride surface and a metallic oxide surface is disclosed. The method may include; providing a substrate within a reaction chamber, heating the substrate to a deposition temperature, contacting the substrate with silicon iodide precursor, and selectively depositing the amorphous silicon film on the metallic nitride surface relative to the metallic oxide surface. Semiconductor device structures including an amorphous silicon film deposited by selective deposition methods are also disclosed.
Semiconductor Device and Method of Forming Sacrificial Heteroepitaxy Interface to Provide Substantially Defect-Free Silicon Carbide Substrate
A semiconductor device has a first substrate made of a first semiconductor material, such as silicon. A sacrificial layer is formed over a first surface of the first substrate. A seed layer is formed over the sacrificial layer. A compliant layer is formed over a second surface of the first substrate opposite the first surface of the first substrate. A first semiconductor layer made of a second semiconductor material, such as silicon carbide, dissimilar from the first semiconductor material is formed over the sacrificial layer. The first substrate and sacrificial layer are removed leaving the first semiconductor layer substantially defect-free. The first semiconductor layer containing the second semiconductor material is formed at a temperature greater than a melting point of the first semiconductor material. A second semiconductor layer is formed over the first semiconductor layer with an electrical component formed in the second semiconductor layer.
Semiconductor Device and Method of Forming Sacrificial Heteroepitaxy Interface to Provide Substantially Defect-Free Silicon Carbide Substrate
A semiconductor device has a first substrate made of a first semiconductor material, such as silicon. A sacrificial layer is formed over a first surface of the first substrate. A seed layer is formed over the sacrificial layer. A compliant layer is formed over a second surface of the first substrate opposite the first surface of the first substrate. A first semiconductor layer made of a second semiconductor material, such as silicon carbide, dissimilar from the first semiconductor material is formed over the sacrificial layer. The first substrate and sacrificial layer are removed leaving the first semiconductor layer substantially defect-free. The first semiconductor layer containing the second semiconductor material is formed at a temperature greater than a melting point of the first semiconductor material. A second semiconductor layer is formed over the first semiconductor layer with an electrical component formed in the second semiconductor layer.
MICROFLUIDIC MEMS DEVICE COMPRISING A BURIED CHAMBER AND MANUFACTURING PROCESS THEREOF
Process for manufacturing a microfluidic device, wherein a sacrificial layer is formed on a semiconductor substrate; a carrying layer is formed on the sacrificial layer; the carrying layer is selectively removed to form at least one release opening extending through the carrying layer; a permeable layer of a permeable semiconductor material is formed in the at least one release opening; the sacrificial layer is selectively removed through the permeable layer to form a fluidic chamber; the at least one release opening is filled with non-permeable semiconductor filling material, forming a monolithic body having a membrane region; an actuator element is formed on the membrane region and a cap element is attached to the monolithic body and surrounds the actuator element.
MICROFLUIDIC MEMS DEVICE COMPRISING A BURIED CHAMBER AND MANUFACTURING PROCESS THEREOF
Process for manufacturing a microfluidic device, wherein a sacrificial layer is formed on a semiconductor substrate; a carrying layer is formed on the sacrificial layer; the carrying layer is selectively removed to form at least one release opening extending through the carrying layer; a permeable layer of a permeable semiconductor material is formed in the at least one release opening; the sacrificial layer is selectively removed through the permeable layer to form a fluidic chamber; the at least one release opening is filled with non-permeable semiconductor filling material, forming a monolithic body having a membrane region; an actuator element is formed on the membrane region and a cap element is attached to the monolithic body and surrounds the actuator element.
SYSTEMS AND METHODS FOR PURGING REACTOR LOWER CHAMBERS WITH ETCHANTS DURING FILM DEPOSITION
A semiconductor processing system includes a gas delivery module, and a chamber body connected to the gas delivery module. The divider has an aperture, is fixed within an interior of the chamber body, and separates an interior of the chamber body into upper and lower chambers, the aperture fluidly coupling the lower chamber to the upper chamber. A susceptor is arranged within the aperture. A controller is operably connected to the gas delivery module to purge the lower chamber with a first purge flow including an etchant while etching the upper chamber, purge the lower chamber with a second purge flow including the etchant while depositing a precoat in the upper chamber, and purge the lower chamber with a third purge flow including the etchant while depositing a film onto a substrate in the upper chamber. Film deposition methods and lower chamber etchant purge kits are also described.
SYSTEMS AND METHODS FOR PURGING REACTOR LOWER CHAMBERS WITH ETCHANTS DURING FILM DEPOSITION
A semiconductor processing system includes a gas delivery module, and a chamber body connected to the gas delivery module. The divider has an aperture, is fixed within an interior of the chamber body, and separates an interior of the chamber body into upper and lower chambers, the aperture fluidly coupling the lower chamber to the upper chamber. A susceptor is arranged within the aperture. A controller is operably connected to the gas delivery module to purge the lower chamber with a first purge flow including an etchant while etching the upper chamber, purge the lower chamber with a second purge flow including the etchant while depositing a precoat in the upper chamber, and purge the lower chamber with a third purge flow including the etchant while depositing a film onto a substrate in the upper chamber. Film deposition methods and lower chamber etchant purge kits are also described.
SELECTIVE SILICON DEPOSITION
Exemplary semiconductor processing methods may include providing a silicon-containing precursor to a processing region of a semiconductor processing chamber. A substrate may be disposed within the processing region. The substrate may include one or more patterned features separated by exposed regions of the substrate. The methods may include providing a hydrogen-containing precursor to the processing region of the semiconductor processing chamber. The methods may include forming a plasma of the silicon-containing precursor and the hydrogen-containing precursor. Forming the plasma of the silicon-containing precursor and the hydrogen-containing precursor may be performed at a plasma power of less than or about 1,000 W. The methods may include depositing a silicon-containing material on the one or more patterned features along the substrate. The silicon-containing material may be deposited on the patterned features at a rate of at least 2:1 relative to deposition on the exposed regions of the substrate.
SELECTIVE SILICON DEPOSITION
Exemplary semiconductor processing methods may include providing a silicon-containing precursor to a processing region of a semiconductor processing chamber. A substrate may be disposed within the processing region. The substrate may include one or more patterned features separated by exposed regions of the substrate. The methods may include providing a hydrogen-containing precursor to the processing region of the semiconductor processing chamber. The methods may include forming a plasma of the silicon-containing precursor and the hydrogen-containing precursor. Forming the plasma of the silicon-containing precursor and the hydrogen-containing precursor may be performed at a plasma power of less than or about 1,000 W. The methods may include depositing a silicon-containing material on the one or more patterned features along the substrate. The silicon-containing material may be deposited on the patterned features at a rate of at least 2:1 relative to deposition on the exposed regions of the substrate.
BIOPHARMACEUTICAL MANUFACTURING PROCESS AND PRODUCT
Pharmaceutical manufacturing processes and products are disclosed. A pharmaceutical manufacturing process includes flowing a liquid through a pathway. The liquid contacts a non-polymeric coating on a substrate within the pathway. The substrate is a metal or metallic substrate. A pharmaceutical product is produced by flowing a liquid through a pathway. The liquid contacts a non-polymeric coating on a substrate within the pathway. The substrate is a metal or metallic substrate.