C03C2217/734

GLASS LAMINATE AND PORTABLE ELECTRONIC DEVICE

A glass laminate includes a glass substrate; and an anti-reflection layer laminated on the glass substrate and a minimum of absorbances of the glass laminate in wavelengths of 380 to 780 nm is 0.01 or more.

IG WINDOW UNIT HAVING TRIPLE SILVER COATING AND DIELECTRIC COATING ON OPPOSITE SIDES OF GLASS SUBSTRATE

An insulating glass (IG) window unit including first and second glass substrates that are spaced apart from each other. At least one of the glass substrate has a triple silver low-emissivity (low-E) coating on one major side thereof, and a dielectric coating for improving angular stability on the other major side thereof

INSULATED GLAZING UNIT

Insulated glazing units comprising first and second sheets of glazing material with a low pressure space there between are described. The major surface of the second sheet of glazing material not facing the low pressure space has a low emissivity coating comprising at least one layer of fluorine doped tin oxide thereon. There is a first anti-iridescence coating between the low emissivity coating and the second sheet of glazing material. Also described are insulated glazing units comprising three (first, second and third) sheets of glazing material with a low pressure space between first and second sheets of glazing material, and a second space between the first and third sheets of glazing material. There is a low emissivity coating on one or both major surfaces facing the low pressure space. The third sheet of glazing material has a low emissivity coating on both opposed major surfaces thereof.

LAMINATED WINDOW ASSEMBLY

A laminated window assembly has a first glass pane with a coating formed thereon, a second glass pane, and a polymeric interlayer provided between the first glass pane and the second glass pane. The coating includes a first layer deposited over a major surface of the glass pane, wherein the first layer has a refractive index of 1.6 or more and a thickness of 50 nm or less, a second layer deposited over the first layer, wherein the second layer has a refractive index that is less than the refractive index of the first layer and a thickness of 50 nm or less, a third layer deposited over the second layer, wherein the third layer has a refractive index that is greater than the refractive index of the second layer and a thickness of less than 500 nm, and a fourth layer deposited over the third layer, wherein the fourth layer has a refractive index that is less than the refractive index of the third layer and a thickness of 100 nm or less.

Scratch-resistant and optically transparent materials and articles
11203179 · 2021-12-21 · ·

Embodiments of a scratch-resistant and optically transparent material comprising silicon, aluminum, nitrogen, and optionally oxygen are disclosed. In one or more embodiments, the material exhibits an extinction coefficient (k) at a wavelength of 400 nm of less than about 1×10.sup.−3, and an average transmittance of about 80% or greater, over an optical wavelength regime in the range from about 380 nm to about 780 nm, as measured through the material having a thickness of about 0.4 micrometer. In one or more embodiments, the material comprises an intrinsic maximum hardness of about 12 GPa or greater as measured on a major surface of the material having a thickness of about 400 by a Berkovich Indenter Hardness Test along an indentation depth of about 100 nm or greater, low compressive stress and low roughness (Ra). Articles and devices incorporating the material are also disclosed.

BEAM SPLITTER WITH PHOTOCATALYTIC COATING AND FABRICATION METHOD THEREOF

A method for making a beam splitter with photocatalytic coating is disclosed. First, a TiO.sub.2—SiO.sub.2 sol, a SiO.sub.2 sol, and an anatase TiO.sub.2 preform sol are prepared. A glass substrate having two opposite surfaces is provided. The two opposite surfaces of the glass substrate is coated with the TiO.sub.2—SiO.sub.2 sol, the SiO.sub.2 sol, and the anatase TiO.sub.2 preform sol by dip-coating, thereby forming a coated glass substrate with a multi-layer optical coating on each of the two opposite surfaces. The multi-layer optical coating comprises a TiO.sub.2—SiO.sub.2 coating, a SiO.sub.2 coating, and an anatase TiO.sub.2 preform coating. The coated glass substrate is subjected to an anneal process. The coated glass substrate is cut, thereby forming the beam splitter with photocatalytic coating.

METHOD OF REDUCING THE EMISSIVITY OF A COATED GLASS ARTICLE

A method of reducing the emissivity of a coated glass article includes the following steps in sequence: (a) forming a coated glass article, the coated glass article comprising a glass substrate and a coating formed on the glass substrate, the coating having a first layer deposited over the glass substrate and a second layer, the second layer being provided between the first layer and the glass substrate, wherein the coated glass article exhibits a first emissivity; and (b) heating the coated glass article in an environment set to a predetermined temperature and for a predetermined period of time. After step (b), the coated glass article exhibits a second emissivity, the second emissivity being less than the first emissivity.

WINDOW HAVING METAL LAYER THAT TRANSMITS MICROWAVE SIGNALS AND REFLECTS INFRARED SIGNALS

A window structure includes a metal layer that transmits microwave signals and reflects infrared signals. A microwave signal is a signal that has a frequency in the microwave spectrum of frequencies (a.k.a. the microwave frequency spectrum). The microwave frequency spectrum extends from 300 megahertz (MHz) to 300 gigahertz (GHz). An infrared signal is a signal that has a frequency in the infrared spectrum of frequencies (a.k.a. the infrared frequency spectrum, which extends from 300 GHz to 430 terahertz (THz)). The metal layer may be a discontinuous metal layer that's an electrically discontinuous metal layer and/or a physically discontinuous metal layer.

SYSTEM FOR FORMING NANO-LAMINATE OPTICAL COATING
20220185726 · 2022-06-16 ·

A processing system for forming an optical coating on a substrate is provided, wherein the optical coating including an anti-reflective coating and an oleophobic coating, the system comprising: a linear transport processing section configured for processing and transporting substrate carriers individually and one at a time in a linear direction; at least one evaporation processing system positioned in the linear transport processing system, the evaporation processing system configured to form the oleophobic coating; a batch processing section configured to transport substrate carriers in unison about an axis; at least one ion beam assisted deposition processing chamber positioned in the batch processing section, the ion beam assisted deposition processing chamber configured to deposit layer of the anti-reflective coating; a plurality of substrate carriers for mounting substrates; and, means for transferring the substrate carriers between the linear transport processing section and the batch processing section without exposing the substrate carrier to atmosphere.

Partially-reflective cover for a smart home device

Various embodiments of smart devices are determined herein. A smart device can include a housing and an electronic display. The smart device can further include a cover, housed by the housing, through which the electronic display is visible. The cover can include a glass layer, wherein the glass layer is the outermost layer of the cover that is adjacent an ambient environment of the smart home device. The cover can further include an optical coating layer, deposited directly onto a surface of the glass layer, that comprises a plurality of sublayers. The optical coating layer can include alternating non-metallic oxide layers having different refractive indexes. The sublayers can vary in thickness such that the optical coating layer reflects light from the ambient environment through the glass layer.