Patent classifications
C04B2237/124
LIGHT-EMITTING CERAMIC AND LIGHT-EMITTING DEVICE
A light-emitting ceramic and a light-emitting device. The light-emitting ceramic comprises a YAG substrate and light-emitting centers and diffusion particles evenly dispersed in the YAG substrate. The light-emitting centers are lanthanide-doped YAG fluorescent powder particles of 10-20 m in grain size. The particle size of the scattering particles is 20-50 nm. The YAG substrate is a lanthanide-doped YAG ceramic. Also, the grain size of the YAG substrate is less than the grain size of the YAG fluorescent powder particles.
Method for manufacturing active metal-brazed nitride ceramic substrate with excellent joining strength
A method for manufacturing active metal-brazed a nitride ceramics substrate having excellent joining strength, includes: a step of preparing a mixed raw material; a step of forming a green sheet of the mixed raw material by a tape casting method; a step of removing a binder by performing degreasing; a step of performing sintering; a step of forming an aluminum nitride sintered substrate by performing gradual cooling; and a step of printing a conductive wiring pattern with active metal paste on the aluminum nitride sintered substrate.
Power module substrate
A power module substrate of the present invention includes a ceramic substrate and a circuit layer having a circuit pattern. In an interface between the circuit layer and the ceramic substrate, a CuSn layer and a Ti-containing layer are laminated in this order from the ceramic substrate side. In a cross-sectional shape of an end portion of the circuit pattern of the circuit layer, an angle formed between a surface of the ceramic substrate and an end face of the CuSn layer is set in a range equal to or greater than 80 and equal to or smaller than 100, and a maximum protrusion length L of the CuSn layer or the Ti-containing layer from an end face of the circuit layer is set in a range equal to or greater than 2m and equal to or smaller than 15 m.
JOINING METHOD FOR OPTICAL PART
A method for joining an optical part made of quartz glass and a supporting part made of ceramic includes forming a metal layer on a surface of the supporting part by electroless plating, polishing the formed metal layer with a polishing pad to form a first smoothed face on the supporting part surface, polishing a surface of the optical part with the polishing pad to form a second smoothed face, cleaning the first smoothed face and the second smoothed face with ultrasonic cleaning water, forming a first metal film on the first smoothed face by vapor deposition and forming a second metal film on the second smoothed face by vapor deposition, and joining the first metal film and the second metal film to each other by interatomic joining by atomic diffusion between the faces at which the first metal film and the second metal film contact with each other.
Method for producing a composite material
A method for producing a composite material comprising a planar base material to which an additional layer is applied on one side or both sides via a solder layer, characterized by: providing the base material, wherein the base material has a first surface on at least one side; providing the additional layer and arranging the solder layer between a second surface of the additional layer and the first surface such that when the additional layer is deposited on the first surface, the first surface of the base material is covered by the solder layer in a planar manner; wherein a thickness of the solder layer between the base material and the additional layer is smaller than 12 m; heating the base material and the additional layer on the first surface to at least partially melt the solder layer; and connecting the base material to the at least one additional layer.
Joined body and method for producing the same
A joined body 20 according to the present invention includes a first member 22 made of a porous ceramic, a second member 24 made of a metal, and a joint 30 formed of an oxide ceramic of a transition metal, the joint 30 joining the first member 22 to the second member 24. Alternatively, a joined body may include a first member made of a dense material, a second member made of a dense material, and a joint formed of an oxide ceramic of a transition metal, the joint joining the first member to the second member.
Ceramic circuit board
It is an object of the present invention to obtain a ceramic circuit substrate having high bonding strength, excellent heat cycle resistance, enhanced reliability of operation as an electronic device, and excellent heat dissipation properties. The present invention provides a ceramic circuit substrate in which metal plates, particularly copper plates, and both main surfaces of a ceramic substrate are bonded vial silver-copper brazing material layers. The silver-copper brazing material layers are formed from a silver-copper brazing material including i) 0.3-7.5 parts by mass of carbon fibers, and ii) 1.0-9.0 parts by mass of at least one active metal selected from titanium, zirconium, hafnium, niobium, tantalum, vanadium, and tin; with respect to iii) a total of 100 parts by mass of a) 75-98 parts by mass of silver powder and b) 2-25 parts by mass of copper powder. The carbon fibers having an average length of 15-400 m, an average diameter of 5-25 m and an average aspect ratio of 3-28.
Light converter assemblies with enhanced heat dissipation
The present disclosure is directed to light converter assemblies with enhanced heat dissipation. A light converter assembly may comprise a confinement material applied to at least a first substrate and a phosphor material also deposited on the first substrate so as to be surrounded by the confinement material. The first substrate may be hermetically sealed to a second substrate using the confinement material so that the phosphor material is confined between the substrates and protected from atmospheric contamination. The substrates may comprise, for example, sapphire to allow for light beam transmission and heat conductance. Confinement materials that may be employed to seal the first substrate to the second substrate may include, for example, silicon or a metal (e.g., silver, copper, aluminum, etc.) The phosphor material may comprise, for example, at least one quantum dot material.
Process for producing bonded body and process for producing power module substrate
Disclosed is provided a process for producing a bonded body by bonding a ceramic member made of a ceramic to a Cu member made of Cu or a Cu alloy, the process including: a laminating step of laminating the Cu member on a first surface side of the ceramic member via a brazing material containing Cu and a eutectic element which has a eutectic reaction with Cu, and via an active metal; and a heating step of heating the ceramic member and the Cu member which are laminated together.
Power module substrate, power module substrate with heat sink, power module, method of manufacturing power module substrate, and copper member-bonding paste
This power module substrate includes a copper plate that is formed of copper or a copper alloy and is laminated on a surface of a ceramic substrate 11; a nitride layer 31 that is formed on the surface of the ceramic substrate 11 between the copper plate and the ceramic substrate 11; and an AgCu eutectic structure layer 32 having a thickness of 15 m or less that is formed between the nitride layer and the copper plate.