C10M2217/0443

Sliding shaft and steering device
10830282 · 2020-11-10 · ·

In a sliding shaft, an outer circumferential surface of a male shaft is coated with a resin coating layer formed by a fluidized bed powder coating method using a powder coating material containing a base resin and at least either a carbon black or a metal oxide as an antistatic agent. A steering device includes this sliding shaft as an intermediate shaft transmitting steering force.

Sliding member and bearing device using the same

A sliding member of the present embodiment includes a bearing alloy layer and a coating layer provided on a sliding surface side thereof. The coating layer has a resin binder with sulfide particles dispersed therein. A covering portion is provided over specific particles and is made of metal oxide comprising the same metal element as a metal element constituting the sulfide particles. When measured by an X-ray photoelectron spectroscopy and an X-ray diffraction method, a ratio of a peak height of the metal oxide to a peak height of metal sulfide by the X-ray photoelectron spectroscopy is from 0.10 to 0.50, and a ratio of the peak height of the metal oxide to the peak height of the metal sulfide by the X-ray diffraction method is 0.10 or less.

Razor cartridge with lubricating strip

The disclosure deals with a lubricative skin engaging member with progressive release of lubricating polymer from a water-insoluble matrix containing thermoplastic elastomer compound and maleic anhydride copolymer and lubricating polymer in concentration less than 30%. The disclosure lies in the use of the maleic anhydride in grafted form on polyethylene and the incorporation of water-soluble lubricating polymer in concentration less than 30% in the thermoplastic elastomer compound, leading to a lubricative mixture, and to a skin engaging member, with increased homogeneity and water absorption ability that assist in the lubricating polymer release in a progressive and controllable manner.

Polyamide resin molded body

A polyamide resin molded body is formed by a resin composition having a (B) fluorine series resin within a range from 1 to 15 parts by mass with respect to 100 parts by mass of a (A) polyamide resin. In the resin composition, the number average particle diameter of the fluorine series resin dispersed in the polyamide resin is 0.8 m or less. The resin composition includes particles of the (B) fluorine series resin having particle diameters of 0.8 m or greater. The percentage of particles having particle diameters of 0.8 m or greater which are secondary particles while maintaining the form of primary particles is 60% or greater, and/or the degree of crystallinity of the dispersed (B) fluorine series resin is 42 J/g or greater.

PHASE CHANGE MATERIAL COMPOSITIONS AND METHODS FOR THEIR USE TO LOWER SURFACE FRICTION AND WEAR

Phase change material compositions and methods for using the compositions to prepare substrate coatings or bulk blended polymers that advantageously lower friction between interacting substrate surfaces and lower substrate surface wear.

COATING COMPOSITION FOR PRODUCING ARTICLE HAVING SLIPPERY SURFACE

The present invention relates to a coating composition that can produce an article having an inner surface and an outer surface, both of which are slippery, and a method for preparing the same. By using the coating composition according to the present invention, it is possible to produce the article having the inner surface and the outer surface, both of which are slippery, only with a simple process of molding and curing a polymer resin by the technique of the prior art. The article produced using the coating composition of the present invention can solve an ice removal on a surface of the machinery such as an aircraft and an automobile, a biofouling problem in a blood vessel, a problem requiring self-cleaning, and the like, and thus can be used in various industries.

Mixed powder for powder metallurgy
10632532 · 2020-04-28 · ·

A mixed powder for powder metallurgy having excellent green compact strength and ejectability is provided. The mixed powder for powder metallurgy includes an iron-based powder; and a copolymerized polyamide, in an amount of 0.3 to 2.0 parts by mass per 100 parts by mass of the iron-based powder, having a melting point of 80 C. to 116 C.

SLIDING MEMBER AND BEARING DEVICE USING THE SAME
20200124099 · 2020-04-23 ·

A sliding member of the present embodiment includes a bearing alloy layer and a coating layer provided on a sliding surface side thereof. The coating layer has a resin binder with sulfide particles dispersed therein. A covering portion is provided over specific particles and is made of metal oxide comprising the same metal element as a metal element constituting the sulfide particles. When measured by an X-ray photoelectron spectroscopy and an X-ray diffraction method, a ratio of a peak height of the metal oxide to a peak height of metal sulfide by the X-ray photoelectron spectroscopy is from 0.10 to 0.50, and a ratio of the peak height of the metal oxide to the peak height of the metal sulfide by the X-ray diffraction method is 0.10 or less.

POLYAMIDE RESIN COMPOSITION, MOLDED ARTICLE, AND METHOD FOR MANUFACTURING POLYAMIDE RESIN PELLET
20200087459 · 2020-03-19 ·

Provided is a polyamide resin composition capable of providing a molded article having an excellent wear resistance while maintaining a high mechanical strength; a molded article; and a method for manufacturing a polyamide resin pellet. The polyamide resin composition includes a polyamide resin and an inorganic filler, wherein the polyamide resin includes diamine-derived constituent units and dicarboxylic acid derived constituent units; 70 mol % or more of the diamine-derived constituent units are derived from 1,4-bis(aminomethyl)cyclohexane; a molar ratio of cis:trans of the 1,4-bis(aminomethyl)cyclohexane is from 35:65 to 0:100; 70 mol % or more of the dicarboxylic acid-derived constituent units are derived from an ,-linear aliphatic dicarboxylic acid having from 8 to 12 carbons; and the polyamide resin includes phosphorus atoms in a ratio of from 20 to 100 mass ppm and comprises calcium atoms so as to be phosphorus atoms:calcium atoms of 1:0.3 to 0.7 in a molar ratio.

POLYAMIDE-BASED SLIDING MATERIAL
20200056039 · 2020-02-20 ·

The invention relates to a polyamide-based sliding material, having fillers that improve the tribological properties, wherein the fillers comprise at least one metal sulfide and/or calcium phosphate. The invention further relates to a plain-bearing composite material, having a metal support layer, in particular made of steel or bronze, optionally a porous carrier layer, in particular made of bronze, and a sliding material, which fills the pores in the carrier layer, and to a three-dimensional shaped body for sliding load, consisting of a sliding material, in particular produced as an injection-molded or extrusion part and/or by additive manufacturing. The invention further relates to a plain-bearing element produced from a plain-bearing composite material comprising a shaped body