C03B37/0253

Spun round core fiber
10838141 · 2020-11-17 · ·

Optical waveguide cores having refractive index profiles that vary angularly about a propagation axis of the core can provide single-mode operation with larger core diameters than conventional waveguides. In one representative embodiment, an optical waveguide comprises a core that extends along a propagation axis and has a refractive index profile that varies angularly about the propagation axis. The optical waveguide can also comprise a cladding disposed about the core and extending along the propagation axis. The refractive index profile of the core can vary angularly along a length of the propagation axis.

Optical and functional metrology of microstructured optical fibers

Described are systems and techniques for characterizing optical fibers. Disclosed systems and techniques employ optical metrology, functional metrology, or both to characterize microstructured optical fibers and determine fiber characteristics, errors, and quality control metrics. The characteristics, errors, and quality control metrics are useful for improving the manufacturing of optical fibers.

OPTICAL FIBER, COATED OPTICAL FIBER, AND OPTICAL TRANSMISSION SYSTEM
20200333528 · 2020-10-22 ·

The optical fiber has an effective area that is greater than or equal to 110 m.sup.2 and less than or equal to 180 m.sup.2 at a wavelength of 1550 nm and a cable cut-off wavelength of less than or equal to 1530 nm. An average value of a glass outer diameter in a longitudinal direction is 1250.5 m. When is a standard deviation of the glass outer diameter in the longitudinal direction, 3 is greater than or equal to 0.1 m and less than or equal to 0.5 m.

LIGHT DIFFUSING OPTICAL FIBERS HAVING UNIFORM ILLUMINATION ALONG DIFFUSION LENGTHS AND METHODS OF FORMING THE SAME
20200264359 · 2020-08-20 ·

A light diffusing optical fiber includes a core, a cladding surrounding the core, an outer surface, and a plurality of scattering structures positioned within the core, the cladding, or both the core and the cladding. The plurality of scattering structures are configured to scatter guided light towards the outer surface, such that light including a wavelength of from about 450 nm to about 650 nm diffusing through the outer surface along a diffusion length of the light diffusing optical fiber includes a spectral attenuation percent relative range of about 15% or less.

Method of manufacturing optical fiber, optical fiber manufacturing apparatus, and control apparatus therefor
10745314 · 2020-08-18 · ·

A method of manufacturing an optical fiber of the invention includes: preparing a direction changer; drawing a bare optical fiber from an optical fiber preform, thereby forming the bare optical fiber; providing a coated layer made of a resin on a periphery of the bare optical fiber; obtaining an optical fiber by curing the coated layer; changing a direction of the bare optical fiber by use of the direction changer; measuring a drawing velocity of the optical fiber; and adjusting a length of the bare optical fiber from a drawing unit to a coating unit by controlling a position of the direction changer based on a measurement value of the drawing velocity, the drawing unit forming the bare optical fiber, the coating unit providing the coated layer on the periphery of the bare optical fiber.

Optical fiber production method
10710924 · 2020-07-14 · ·

An optical fiber production method includes: drawing an optical fiber from an optical fiber preform in a drawing furnace; cooling the optical fiber in an annealing furnace; and delivering the optical fiber into the annealing furnace, and controlling a temperature difference between a temperature of the optical fiber and a fictive temperature of glass forming a core included in the optical fiber to be higher than 20 C. and lower than 100 C.

MANUFACTURING METHOD OF OPTICAL FIBER

A method for manufacturing an optical fiber is disclosed. The method for manufacturing an optical fiber includes: drawing an optical fiber by heating an optical fiber preform inside a drawing furnace into which a first gas is introduced; and annealing the optical fiber by causing the optical fiber to pass through an annealing furnace disposed downstream of the drawing furnace and adjusted to a temperature lower than a temperature at which the optical fiber preform is heated. In the annealing, a second gas having a lower heat conductivity than the first gas is introduced into the annealing furnace through one or more gas introduction ports such that a total flow rate becomes 3 slm or higher, and a flow rate of the second gas per gas introduction port is adjusted to 30 slm or lower.

THERMALLY RESISTANT RADIATION CURABLE COATINGS FOR OPTICAL FIBER

Described herein are coated optical fibers including an optical fiber portion, wherein the optical fiber portion includes a glass core and cladding section that is configured to possesses certain mode-field diameters and effective areas, and a coating portion including a primary and secondary coating, wherein the primary coating is the cured product of a composition that possesses specified liquid glass transition temperatures, such as below 82 C., and/or a viscosity ratios, such as between 25 C. and 85 C., of less than 13.9. Also described are radiation curable coating compositions possessing reduced thermal sensitivity, methods of coating such radiation curable coating compositions to form coated optical fibers, and optical fiber cables comprising the coated optical fibers and/or radiation curable coating compositions elsewhere described.

Rayleigh scattering based distributed fiber sensors with optimized scattering coefficients

A fiber sensor includes an optical fiber configured for operation at a wavelength from about 800 nm to about 1600 nm. The optical fiber includes a cladding that is defined by a fiber outer diameter and a core that is surrounded by the cladding. The core of the optical fiber has a Rayleigh scattering coefficient, .sub.s, that is controlled by controlling a concentration of one or more dopants in the core. The Rayleigh scattering coefficient is tuned to be within a predetermined range of an optimum Rayleigh scattering coefficient for a given total length, L, of the optical fiber. The predetermined range is from about 70% of the optimum .sub.s to about 130% of the optimum .sub.s.

Optical fiber manufacturing apparatus and method of starting optical fiber manufacturing apparatus
10641945 · 2020-05-05 · ·

An optical fiber manufacturing apparatus includes a heating furnace configured to heat and melt an optical fiber preform; a pulling mechanism configured to adjust an outer diameter of a glass optical fiber by drawing out the glass optical fiber from the optical fiber preform melted through the heating by the heating furnace, and to draw the glass optical fiber that has been adjusted in outer diameter; a coating mechanism configured to apply a predetermined resin on an outer circumference of the glass optical fiber that has been adjusted in outer diameter; and a transport mechanism configured to returnably retract the coating mechanism from a passage route of the glass optical fiber.