C03C2217/48
MAGNETIC ADHESION TO THE HOUSEHOLD DEVICE
A device, in particular a household device, includes a device housing (1), wherein the device housing (1) is at least partially made of glass (2a). The glass (2a) has a glass outer surface (2h) and a glass inner surface (2g). The device housing (1) is adapted such that a permanent magnet (7) magnetically adheres to the glass outer surface (2h).
LITHIUM ION CONDUCTING SULFIDE GLASS FABRICATION
A standalone lithium ion-conductive sulfide solid electrolyte can include a freestanding inorganic vitreous sheet of sulfide-based lithium ion conducting glass capable of high performance in a lithium metal battery by providing a high degree of lithium-ion conductivity while being highly resistant to the initiation and/or propagation of lithium dendrites. Such an electrolyte is also itself manufacturable, and readily adaptable for battery cell and cell component manufacture, in a cost-effective, scalable manner. Methods of making and using the electrolyte, and battery cells and cell components incorporating the electrolyte are also disclosed.
SURFACE-TREATED INFRARED-ABSORBING FINE PARTICLES, SURFACE-TREATED INFRARED-ABSORBING FINE PARTICLE POWDER, INFRARED-ABSORBING FINE PARTICLE DISPERSION IN WHICH SAID SURFACE-TREATED INFRARED-ABSORBING FINE PARTICLES ARE USED, INFRARED-ABSORBING FINE PARTICLE DISPERSOID, AND INFRARED-ABSORBING SUBSTRATE
Provided are surface-treated infrared-absorbing fine particles that are infrared-absorbing fine particles each having a crystallite size greater than or equal to 30 nm and a surface that is coated with a coating layer that contains at least one selected from a hydrolysis product of a metal chelate compound, a polymer of the hydrolysis product of the metal chelate compound, a hydrolysis product of a metal cyclic oligomer compound, and a polymer of the hydrolysis product of the metal cyclic oligomer compound.
GLASS ELEMENT COMPRISING ENAMEL COATING AND USE THEREOF, COATING AGENT FOR MAKING SAME, AND METHOD FOR PRODUCING THE COATING AGENT
Glass elements are provided that include a coating and a sheet-like glass substrate. The sheet-like glass substrate has a first surface and a second surface opposite the first surface. The coating is disposed in at least some areas of at least one of the first and second surfaces. The coating is an inorganic glass-based coating that includes at least one glassy component; at least one pigment comprising pigment particles; and a filler. The filler is inorganic and includes filler particles with a d.sub.50 value, based on an equivalent diameter, of at least 0.1 μm and less than 10 μm.
ULTRAVIOLET LIGHT-BLOCKING COATED PHARMACEUTICAL PACKAGES
According to one or more embodiments disclosed herein, a coated pharmaceutical package may comprise a glass container comprising a first surface and a second surface opposite the first surface, wherein the first surface is an outer surface of the glass container, and wherein the glass container in an uncoated state has an average light transmittance in the UVB and UVC spectrum of at least 50% through a single wall of the coated package. The coated pharmaceutical package may further comprise a coating positioned over at least a portion of the first surface of the glass container, wherein the coated pharmaceutical package has an average light transmittance in the UVC spectrum of less than 50% through a single wall of the coated package.
Light-control panel with layered optical components
Light-control panels including layered optical components are described in this application. An example of a light-control panel includes first and second glazing layers and first and second switchable components extending between the first and second glazing layers. The light-control panel also includes a thermal coating extending between the first switchable component and the first glazing layer and a filter extending between the first and second switchable components.
COATING AND COATING FORMULATION
A coated substrate comprising a coating layer comprising inorganic oxide and pores, the coating layer demonstrates improved durability properties. The coated substrate may for example be used in solar modules. Further a coating formulation and use of the coating formulation are disclosed
Coating Liquid Used For Forming Ultraviolet Absorption Coating And Ultraviolet Absorption Glass
Provided is an ultraviolet absorption glass comprising: a glass substrate, and an ultraviolet absorption coating arranged on at least one surface of the glass substrate, wherein the ultraviolet absorption coating comprises silicon dioxide, an ultraviolet absorber, and MOz used for storing and releasing electrons excited by ultraviolet light in the ultraviolet absorber. The ultraviolet absorption glass is low cost and has good resistance to discoloration and devitrification.
Method of manufacturing a bendable substrate coated with a coating layer of adjacent heterogeneous coatings bonded along boundaries thereof useful for foldable displays
Disclosed herein are a method of manufacturing a heterogeneous coating solution bonded coating layer, and a coating layer and a cover window produced thereby. More particularly, there are provided a method of manufacturing a heterogeneous coating solution bonded coating layer, in which a step difference at the boundary between different types of coating solutions is controllable by controlling a difference in capillary number during discharge of the different types of coating solutions using a slot die coater, and a coating layer and a cover window produced thereby. Therefore, the method of manufacturing a heterogeneous coating solution bonded coating layer can produce a cover window that is excellent in all the properties including durability, optical characteristics, and flexibility.
Glass fluorescent powder slice with multi-layer structure and preparation method therefor, and light-emitting device
A multi-layer glass phosphor powder sheet and its preparation method, and a light-emitting device. The preparation method for the multi-layer glass phosphor powder sheet includes: mixing a first optical functional material, a glass powder and an organic carrier to obtain a first slurry, and mixing a second optical functional material, the glass powder and the organic carriers to obtain a second slurry; coating the first slurry on a first substrate, and drying it at a first temperature so that at least some of the organic carrier is volatilized, to obtain a first functional layer, the first temperature being lower than a softening point of the glass powder; coating the second slurry on the surface of the first functional layer, to obtain a second functional layer; and sintering the first substrate on which the functional layers are coated at a second temperature, to obtain the multi-layer glass phosphor powder sheet.