C04B20/1037

REINFORCED BUILDING BLOCK MADE OF AUTOCLAVED AERATED CONCRETE (AAC)

The present invention is directed to a reinforced building block made of autoclaved aerated concrete (AAC) comprising rebars formed essentially from A) at least one fibrous carrier and B) and a hardened composition formed from B1) at least one epoxy compound and B2) at least one diamine and/or polyamine in a stoichiometric ratio of the epoxy compound B1) to the diamine and/or polyamine component B2) of 0.8:1 to 2:1, as matrix material, and C) optionally further auxiliaries and additives and to methods of production thereof

High-strength geopolymer hollow microsphere, preparation method thereof and phase change energy storage microsphere

A high-strength geopolymer hollow microsphere, a preparation method thereof and a phase change energy storage microsphere are provided, including: dissolving sodium hydroxide, sodium silicate and spheroidizing aid in water to form a solution A, and adding active powder to the solution A, stirring and uniformly mixing to form a slurry B, adding the slurry B to an oil phase, stirring and dispersing into balls, filtering to obtain geopolymer microspheres I, washing the geopolymer microspheres I, and then carrying out a high-temperature calcination to obtain the high-strength geopolymer hollow microspheres II; using the high-strength geopolymer hollow microsphere as a carrier, absorbing a phase change material into the carrier, and mixing a microsphere carrying the phase change material with an epoxy resin, adding a powder dispersant and stirring to disperse the microsphere, after the epoxy resin is solidified, screening the superfluous powder dispersant to obtain the phase energy storage microsphere.

High-strength geopolymer hollow microsphere, preparation method thereof and phase change energy storage microsphere

A high-strength geopolymer hollow microsphere, a preparation method thereof and a phase change energy storage microsphere are provided, including: dissolving sodium hydroxide, sodium silicate and spheroidizing aid in water to form a solution A, and adding active powder to the solution A, stirring and uniformly mixing to form a slurry B, adding the slurry B to an oil phase, stirring and dispersing into balls, filtering to obtain geopolymer microspheres I, washing the geopolymer microspheres I, and then carrying out a high-temperature calcination to obtain the high-strength geopolymer hollow microspheres II; using the high-strength geopolymer hollow microsphere as a carrier, absorbing a phase change material into the carrier, and mixing a microsphere carrying the phase change material with an epoxy resin, adding a powder dispersant and stirring to disperse the microsphere, after the epoxy resin is solidified, screening the superfluous powder dispersant to obtain the phase energy storage microsphere.

CATIONIC LATEX MODIFIED HYDROCARBON BINDER EMULSIONS AND THEIR USE IN THE PREPARATION OF BITUMINOUS PRODUCTS

A process for preparing a cationic latex modified hydrocarbon binder emulsion comprising the steps of: (a) preparing a cationic copolymer latex emulsion by an emulsion polymerisation of polymerizable monomers, said polymerizable monomers comprising A—one or more non-ionic acrylate ester and/or methacrylate ester monomer(s), and B—optionally styrene monomer and/or one or more non-ionic styrene derivative monomer(s), C—optionally one or more cross-linking monomer(s) having two or more ethylenically unsaturated (C═C) double bonds susceptible to free radical copolymerisation, D—optionally one or more epoxy functional monomer(s) having one C═C double bond susceptible to free radical copolymerisation and one epoxide functional group, wherein said polymerizable monomers do not comprise any aliphatic conjugated diene monomer, in presence of a cationic stabilizing surfactant, and (b) adding the cationic copolymer latex emulsion resulting from step (a) to a cationic hydrocarbon binder emulsion, or (b′) adding the cationic copolymer latex emulsion resulting from step (a) to an emulsifier solution, said emulsifier solution comprising water, one or more cationic surfactant(s), one or more acid(s) and optionally additives to provide a mixture, and adding the resulting mixture to hydrocarbon binder; to form a cationic latex modified hydrocarbon binder emulsion.

ADDITIVE OF CELLULOSE NANOFIBRILS OR NANOCRYSTALS AND A SECOND POLYMER

A wellbore treatment fluid comprising: a base fluid; and an additive comprising: a first polymer bundle selected from the group consisting of cellulose nanofibrils, cellulose nanocrystals, and combinations thereof; and a second polymer, wherein the second polymer attaches to the first polymer bundle by a non-covalent mechanism. A method of treating a portion of a wellbore comprising: introducing the treatment fluid into the wellbore.

ADDITIVE OF CELLULOSE NANOFIBRILS OR NANOCRYSTALS AND A SECOND POLYMER

A wellbore treatment fluid comprising: a base fluid; and an additive comprising: a first polymer bundle selected from the group consisting of cellulose nanofibrils, cellulose nanocrystals, and combinations thereof; and a second polymer, wherein the second polymer attaches to the first polymer bundle by a non-covalent mechanism. A method of treating a portion of a wellbore comprising: introducing the treatment fluid into the wellbore.

FIBER MATERIAL FOR CEMENT REINFORCEMENT

Provided is a fiber material for cement reinforcement, configured such that a resin A containing an isocyanate compound as a constituent component is present inside a fiber bundled body, and a resin B containing an epoxy resin as a constituent component is present on a surface of the fiber bundled body. Further, it is preferable that the resin A contains a polyol or an epoxy compound as a constituent component in addition to the isocyanate compound, the resin B contains an acrylic-modified epoxy resin or a bisphenol-A epoxy resin as a main component, the fiber bundled body has a tensile strength of 7 cN/dtex or more, and the fiber bundled body includes 50 to 3,000 single fibers. The invention is also addressed to a concrete or mortar molded article using the above fiber material for reinforcement.

FIBER MATERIAL FOR CEMENT REINFORCEMENT

Provided is a fiber material for cement reinforcement, configured such that a resin A containing an isocyanate compound as a constituent component is present inside a fiber bundled body, and a resin B containing an epoxy resin as a constituent component is present on a surface of the fiber bundled body. Further, it is preferable that the resin A contains a polyol or an epoxy compound as a constituent component in addition to the isocyanate compound, the resin B contains an acrylic-modified epoxy resin or a bisphenol-A epoxy resin as a main component, the fiber bundled body has a tensile strength of 7 cN/dtex or more, and the fiber bundled body includes 50 to 3,000 single fibers. The invention is also addressed to a concrete or mortar molded article using the above fiber material for reinforcement.

LOW-DUST FILLER FOR COMPOSITE BUILDING PRODUCT

A low-dust composite building product is provided. The low-dust composite building product includes a binder system comprising one or more of a thermoset resin, a diluent, and a hardener; and a low-dust filler material comprising filler particles that have been pre-coated with a coating agent comprising one or more of the thermoset resin, the diluent, and the hardener from the binder system.

LOW-DUST FILLER FOR COMPOSITE BUILDING PRODUCT

A low-dust composite building product is provided. The low-dust composite building product includes a binder system comprising one or more of a thermoset resin, a diluent, and a hardener; and a low-dust filler material comprising filler particles that have been pre-coated with a coating agent comprising one or more of the thermoset resin, the diluent, and the hardener from the binder system.