Patent classifications
C04B41/5096
Coated member and method of manufacturing the same
Provided are a coated member in which damage of a coating film can be suppressed in a high temperature environment and the coating may be performed at low cost, and a method of manufacturing the same. A coated member includes a bond coat and a top coat sequentially laminated on a substrate made of a Si-based ceramic or a SiC fiber-reinforced SiC matrix composite, wherein the top coat includes a layer composed of a mixed phase of a (Y.sub.1-aLn.sub.1a).sub.2Si.sub.2O.sub.7 solid solution (here, Ln.sub.1 is any one of Nd, Sm, Eu, and Gd) and Y.sub.2SiO.sub.5 or a (Y.sub.1-bLn.sub.1′.sub.b).sub.2SiO.sub.5 solid solution (here, Ln.sub.1′ is any one of Nd, Sm, Eu, and Gd), or a mixed phase of a (Y.sub.1-cLn.sub.2c).sub.2Si.sub.2O.sub.7 solid solution (here, Ln.sub.2 is any one of Sc, Yb, and Lu) and Y.sub.2SiO.sub.5 or a (Y.sub.1-dLn.sub.2′.sub.d).sub.2SiO.sub.5 solid solution (here, Ln.sub.2′ is any one of Sc, Yb, and Lu).
Coated member and method of manufacturing the same
Provided are a coated member in which damage of a coating film can be suppressed in a high temperature environment and the coating may be performed at low cost, and a method of manufacturing the same. A coated member includes a bond coat and a top coat sequentially laminated on a substrate made of a Si-based ceramic or a SiC fiber-reinforced SiC matrix composite, wherein the top coat includes a layer composed of a mixed phase of a (Y.sub.1-aLn.sub.1a).sub.2Si.sub.2O.sub.7 solid solution (here, Ln.sub.1 is any one of Nd, Sm, Eu, and Gd) and Y.sub.2SiO.sub.5 or a (Y.sub.1-bLn.sub.1′.sub.b).sub.2SiO.sub.5 solid solution (here, Ln.sub.1′ is any one of Nd, Sm, Eu, and Gd), or a mixed phase of a (Y.sub.1-cLn.sub.2c).sub.2Si.sub.2O.sub.7 solid solution (here, Ln.sub.2 is any one of Sc, Yb, and Lu) and Y.sub.2SiO.sub.5 or a (Y.sub.1-dLn.sub.2′.sub.d).sub.2SiO.sub.5 solid solution (here, Ln.sub.2′ is any one of Sc, Yb, and Lu).
Airfoil having environmental barrier topcoats that vary in composition by location
An airfoil includes an airfoil wall that defines a leading end, a trailing end, and suction and pressure sides that join the leading end and the trailing end. The airfoil wall is formed of a silicon-containing ceramic. A first environmental barrier topcoat is disposed on the suction side of the airfoil wall, and a second, different environmental barrier topcoat is disposed on the pressure side of the airfoil wall. The first topcoat is vaporization-resistant and the second topcoat is resistant to calcium-magnesium-aluminosilicate.
Airfoil having environmental barrier topcoats that vary in composition by location
An airfoil includes an airfoil wall that defines a leading end, a trailing end, and suction and pressure sides that join the leading end and the trailing end. The airfoil wall is formed of a silicon-containing ceramic. A first environmental barrier topcoat is disposed on the suction side of the airfoil wall, and a second, different environmental barrier topcoat is disposed on the pressure side of the airfoil wall. The first topcoat is vaporization-resistant and the second topcoat is resistant to calcium-magnesium-aluminosilicate.
EBC with mullite bondcoat that includes an oxygen getter phase
A coated component, along with methods of its formation and use, is provided. The coated component includes a ceramic matrix composite (CMC) substrate comprising silicon carbide and having a mullite bondcoat on its surface. The mullite bondcoat includes an oxygen getter phase contained within a mullite phase. For example, the mullite bondcoat may include 60% to 98% by volume of the mullite phase. An environmental barrier coating is on the mullite bondcoat.
EBC with mullite bondcoat that includes an oxygen getter phase
A coated component, along with methods of its formation and use, is provided. The coated component includes a ceramic matrix composite (CMC) substrate comprising silicon carbide and having a mullite bondcoat on its surface. The mullite bondcoat includes an oxygen getter phase contained within a mullite phase. For example, the mullite bondcoat may include 60% to 98% by volume of the mullite phase. An environmental barrier coating is on the mullite bondcoat.
High temperature oxidation protection for composites
An oxidation protection system disposed on a substrate is provided, which may comprise a boron layer comprising a boron compound disposed on the substrate; a silicon layer comprising a silicon compound disposed on the boron layer; and at least one sealing layer comprising monoaluminum phosphate and phosphoric acid disposed on the silicon layer.
High temperature oxidation protection for composites
An oxidation protection system disposed on a substrate is provided, which may comprise a boron layer comprising a boron compound disposed on the substrate; a silicon layer comprising a silicon compound disposed on the boron layer; and at least one sealing layer comprising monoaluminum phosphate and phosphoric acid disposed on the silicon layer.
METHOD FOR COATING A CERAMIC MATRIX COMPOSITE PART WITH AN ENVIRONMENTAL BARRIER
A method for coating a ceramic matrix composite part with an environmental barrier, the method including a) applying, to a surface of the part, a coating composition including a first powder of a rare earth silicate and a second powder including boron, the coating composition having a ratio R=[mass of the second powder]/[mass of the first powder] of between 0.1% and 5%, and b) sintering the first and second powders to obtain the environmental barrier on the part.
METHOD FOR COATING A CERAMIC MATRIX COMPOSITE PART WITH AN ENVIRONMENTAL BARRIER
A method for coating a ceramic matrix composite part with an environmental barrier, the method including a) applying, to a surface of the part, a coating composition including a first powder of a rare earth silicate and a second powder including boron, the coating composition having a ratio R=[mass of the second powder]/[mass of the first powder] of between 0.1% and 5%, and b) sintering the first and second powders to obtain the environmental barrier on the part.