C04B2235/444

FUNCTIONALIZED CERAMIC ARTICLE

The present invention relates to a method for additive manufacturing of a position sensitive colored ceramic article comprising: a) providing at least one flowable ceramic component; b) forming a green body by sequential deposition of the ceramic component provided in step a) and optionally a support material not intended to be part of the final article; c) position sensitive application of a coloring substance in a solvent to at least a part of the surface of the green body formed in step b), wherein the coloring substance is applied simultaneously to the sequential deposition; d) heat treatment or curing of at least a part of the green body surface obtained in step c); wherein the method steps a)-d) are at least performed once; e) optionally removing the support material from the green body; and f) sintering the green body to obtain the ceramic article; wherein the coloring substance is a dyestuff according to ISO 18451-1:2019(E). In addition, the present invention relates to a system adapted to perform the method and a control data set configured, when implemented in an additive manufacturing system, to cause the system to execute the steps of the inventive method.

LITHIUM ION-CONDUCTING GARNET TYPE OXIDE
20230064947 · 2023-03-02 · ·

An oxide-based solid electrolyte with a high lithium ion conductance is provided. A lithium ion-conducting garnet type oxide includes Li, La, Ga, Zr, a halogen element, and oxygen. A lithium ion conductivity at room temperature is not lower than 1.0×10.sup.−3 S/cm. A proportion of Ga with respect to 1 mole of the oxide may be not larger than 0.5 moles.

The halogen element may be at least one type selected from the group consisting of Cl, Br, and I, and a proportion of Li with respect to 1 mole of the oxide may be not smaller than 6.1 moles and smaller than 6.5 moles.

Thermoelectric material, thermoelectric device, powder for thermoelectric material, and method for producing thermoelectric material

A thermoelectric material of the present invention includes copper, tin, and sulfur, wherein a ratio A/B of the number A of copper atoms to the number B of tin atoms is 0.5 to 2.5 and a content of a metal element other than copper and tin is 5 mol % or less with respect to total metal elements. Additionally, the thermoelectric material of the present invention has a thermal conductivity less than 1.0 W/(m.Math.K) at 200 to 400° C.

Nitrogen-doped sulfide-based solid electrolyte for all-solid batteries

The present invention relates to a nitrogen-doped sulfide-based solid electrolyte for all-solid batteries. The a nitrogen-doped sulfide-based solid electrolyte for all-solid batteries includes a compound with an argyrodite-type crystal structure represented by the following Formula 1:
Li.sub.aPS.sub.bN.sub.cX.sub.d  [Formula 1] wherein 6≤a≤7, 3<b<6, 0<c≤1, 0<d≤2, and each X is the same or different halogen atom selected from the group consisting of chlorine (Cl), bromine (Br), and iodine (I).

ALUMINUM-CONTAINING NITRIDE CERAMIC MATRIX COMPOSITE, METHOD OF MAKING, AND METHOD OF USE
20230111390 · 2023-04-13 ·

Embodiments of disclosure may provide a method for forming an aluminum-containing nitride ceramic matrix composite, comprising heating a green body, an aluminum-containing composition, ammonia and a mineralizer composition in a sealable container to a temperature between about 400 degrees Celsius and about 800 degrees Celsius and a pressure between about 10 MPa and about 1000 MPa, to form an aluminum-containing nitride ceramic matrix composite characterized by a phosphor-to-aluminum nitride (AlN) ratio, by volume, between about 1% and about 99%, by a porosity between about 1% and about 50%, and by a thermal conductivity between about 1 watt per meter-Kelvin and about 320 watts per meter-Kelvin. The green body comprises a phosphor powder comprising at least one phosphor composition, wherein the phosphor powder particles are characterized by a D50 diameter between about 100 nanometers and about 500 micrometers, and the green body has a porosity between about 10% and about 80%. The aluminum-containing composition has a purity, on a metals basis, between about 90% and about 99.9999%. The fraction of free volume within the sealable container contains between about 10% and about 95% of liquid ammonia prior to heating the green body, the aluminum-containing composition, ammonia and the mineralizer composition in the sealable container.

CURABLE COMPOSITION FOR THE MANUFACTURE, BY STEREOLITHOGRAPHY, OF GREEN PARTS OF CERAMIC OR METALLIC MATERIAL BY PHOTO-THERMAL ROUTE

Disclosed is a curable composition for the manufacture, by stereolithography, of a green part made of a ceramic or metallic material, the curable composition including at least one ceramic and/or metallic powder; at least one polymerizable monomer and/or oligomer; at least one initiator for the polymerization of the polymerizable monomer(s) and/or oligomer(s). The initiator(s) are selected from iodonium, sulphonium and diazonium salts and onium salts in combination with at least one amine and/or at least one phosphine to form a charge transfer complex. The initiator(s) may generate the initiation of a thermal polymerization under the exposure to at least one source of UV, visible or IR irradiation.

METHOD AND COMPOSITION OF SCALABLE, INFILTRATION FREE CERAMIC MATRIX COMPOSITE

A ceramic matrix composite has fibers, a ceramic matrix bonded to the fibers, and ceramic particles, distributed throughout the matrix. A method includes mixing a high char ceramic resin precursor with ceramic particles, adding a catalyst to create a mixture, heating the mixture to produce functionalized ceramic particles, and cooling the mixture to produce a resin having functionalized particles.

PROCESS FOR COLD SINTERING OF CALCIUM CARBONATE FOR PRECAST CONSTRUCTION MATERIALS
20230150883 · 2023-05-18 ·

Embodiments relate to use of a solution having low molarity to form a mixture with a ceramic compound that will facilitate formation of a sintered ceramic compact exhibiting grain boundary formation, low porosity, adequate compressive strength, and adequate hardness to be used as a precast block 108 for cement.

ION CONDUCTOR, AND POSITIVE ELECTRODE, SOLID ELECTROLYTE, AND LITHIUM BATTERY EACH INCLUDING THE ION CONDUCTOR, AND METHOD OF PREPARING THE ION CONDUCTOR
20230142448 · 2023-05-11 ·

A lithium battery includes: a positive electrode having a positive active material; a negative electrode including lithium metal; and a solid electrolyte disposed therebetween. The solid electrolyte contains at least one oxide represented by Li.sub.4±xM.sub.1-x′M′.sub.x′O.sub.4 (Formula 1), Li.sub.4-yM″O.sub.4-yA′.sub.y (Formula 2), or Li.sub.4+4zM′″.sub.1-zO.sub.4 (Formula 3), wherein and 0≤x23 1 and 0≤x′≤1, M is a Group 4 element, and M′ is an element of Group 2, 3, 5, 12, or 13, a vacancy, or a combination thereof, with the proviso that when M is Zr, then x≠0, x′≠0 and M′ is Be, Ca, Sr, Ba, Ra, Cd, Hg, Cn, Ga, In, TI, an element of Group 3 or 5, or a combination thereof; 0≤y≤1, M″ is a Group 4 element, and A′ includes at least one halogen, with the proviso that when M″ is Zr, then y≠0; and 0<z<1, and M′″ is a Group 4 element.

Magnesium-based raw material with low thermal conductivity and low thermal expansion and preparation method thereof

The present disclosure relates to a magnesium-based raw material and a preparation method thereof. According to the technical solution, 40-60 wt % fused magnesia particles, 30-40 wt % fine monoclinic zirconia powder, 5-20 wt % fine zirconium oxychloride powder, 0.5-1.5 wt % calcium hydroxide nanopowder, 0.2-0.5 wt % calcium hydroxide nanopowder, and 0.1-0.3 wt % maleic acid are stirred for 15 min to mix well in a high-speed mixing mill at a constant temperature of 25° C. to obtain a mixed powder; and the mixed powder is mixed through a ball mill at a constant temperature of 25° C. for 3 min, roasted in a high temperature furnace at 250-400° C. for 0.5-3 h, and finally cooled to room temperature.