C08K5/5317

POLYETHYLENE POLYMER COMPOSITIONS AND ARTICLES MADE FROM THE SAME
20220348741 · 2022-11-03 ·

A polymer composition comprises a polyethylene polymer having a Melt Relaxation Ratio of 1.5 or greater and a salt of a branched alkyl phosphonic acid. A method for molding a thermoplastic polymer composition comprises the steps of (a) providing an apparatus comprising a die and a mold cavity; (b) providing the polymer composition described above; (c) heating the polymer composition to melt the polymer composition; (d) extruding the molten polymer composition through the die to form a parison; (e) capturing the parison in the mold cavity; (f) blowing a pressurized fluid into the parison to inflate the parison and conform it to the interior surface of the mold cavity; (g) allowing the molded article to cool so that the molded article retains its shape; and (h) removing the molded article from the mold cavity.

Methods relating to polyurethane foam-containing and degradable foam-containing tires, and degradable foam-containing tires

Disclosed herein are methods for degrading polyurethane foam from mounted polyurethane foam-containing tires, methods for separating a wheel from a mounted polyurethane foam-containing tire, methods for preparing a degradable foam-containing tire, and degradable foam-containing tires. The methods include applying a solution comprising at least one phosphorous oxoacid or an ester thereof to the polyurethane foam inside of a tire, incorporating a degradant comprising at least one phosphorous oxoacid or an ester thereof into the polyurethane foam, or both, and then heating to degrade the foam. Degradation of the foam allows for separation of the wheel from the rubber carcass of the tire.

Methods relating to polyurethane foam-containing and degradable foam-containing tires, and degradable foam-containing tires

Disclosed herein are methods for degrading polyurethane foam from mounted polyurethane foam-containing tires, methods for separating a wheel from a mounted polyurethane foam-containing tire, methods for preparing a degradable foam-containing tire, and degradable foam-containing tires. The methods include applying a solution comprising at least one phosphorous oxoacid or an ester thereof to the polyurethane foam inside of a tire, incorporating a degradant comprising at least one phosphorous oxoacid or an ester thereof into the polyurethane foam, or both, and then heating to degrade the foam. Degradation of the foam allows for separation of the wheel from the rubber carcass of the tire.

Foaming composition
11643518 · 2023-05-09 · ·

This invention relates to a foaming composition, comprising at least one ethylene-vinyl acetate (EVA) copolymer; at least one foaming agent; at least one peroxide compound; at least one polyamine; at least one crosslinking enhancer; at least one primary antioxidant; and at least one secondary antioxidant; the content of the crosslinking enhancer is from 0.1 to 3% by weight based on the total weight of the composition. A foaming article cured from the foaming composition under the temperature range of 80 to 120° C. according to the present invention exhibits high initial volume expansion ratio at the baking window from 130 to 200° C. and shows excellent stability after storage.

Flame retardant resin composition and flame retardant resin molded article manufactured therefrom

The present invention relates to a flame retardant resin composition having excellent flame retardancy and improved thermal deformation properties, and a flame retardant resin molded article manufactured therefrom, and provides a flame retardant resin composition including a) a base resin including a polyarylene ether-based polymer; an aromatic vinyl-based polymer and a copolymer of vinylcyan monomer-conjugated diene monomer-aromatic vinyl monomer; b) an organophosphorus-based flame retardant; c) a hypophosphite compound; and d) a sulfur-containing compound including at least two sulfur atoms, wherein b) the organophosphorus-based flame retardant, c) the hypophosphite compound and d) the sulfur-containing compound are included in a weight ratio of 15 to 24:2 to 4:2 to 5.

Flame retardant resin composition and flame retardant resin molded article manufactured therefrom

The present invention relates to a flame retardant resin composition having excellent flame retardancy and improved thermal deformation properties, and a flame retardant resin molded article manufactured therefrom, and provides a flame retardant resin composition including a) a base resin including a polyarylene ether-based polymer; an aromatic vinyl-based polymer and a copolymer of vinylcyan monomer-conjugated diene monomer-aromatic vinyl monomer; b) an organophosphorus-based flame retardant; c) a hypophosphite compound; and d) a sulfur-containing compound including at least two sulfur atoms, wherein b) the organophosphorus-based flame retardant, c) the hypophosphite compound and d) the sulfur-containing compound are included in a weight ratio of 15 to 24:2 to 4:2 to 5.

FIBRE-MATRIX SEMIFINISHED PRODUCT

A flame-retardant single-, or multi-layered, fibre-matrix semi-finished product has a polyamide-based fibre-matrix that includes at least one organic phosphinic acid salt and/or a diphosphinic acid salt. A process for the production thereof includes impregnating a fibre ply, or plies, and consolidating the ply or plies into a composite.

Adhesion promoters and compositions for containers and other articles

This invention provides a coating composition that contains an aromatic adhesion promoter. Containers and other articles comprising the coatings and methods of making such containers and other articles are also provided. The invention further provides compositions including the adhesion promoter, which have utility in a variety of coating end uses, including, for example, valve and pipe coatings.

Adhesion promoters and compositions for containers and other articles

This invention provides a coating composition that contains an aromatic adhesion promoter. Containers and other articles comprising the coatings and methods of making such containers and other articles are also provided. The invention further provides compositions including the adhesion promoter, which have utility in a variety of coating end uses, including, for example, valve and pipe coatings.

Solventless functionalization, milling, and compounding process with reactive diluents

Methods of compounding nanoparticles with a resin, e.g., a curable resin and one or more surface modifying agents are described. The methods use wet milling technology, including both continuous and batch milling processes, and can be used to functionalize the nanoparticles and disperse the functionalized nanoparticles into the resin system in a single process. Methods of compounding curable resin systems containing reactive diluents are also disclosed.