C03C2217/475

COMPOSITION, LAMINATE AND WINDOW

The present disclosure provides a composition through which a laminate which is aesthetically excellent is formed by exhibiting a blue-based color, which is a general window color, and through which a laminate having high visible light transmittance and an excellent thermochromic property is formed while enabling mass production, and the present disclosure further provides a laminate formed through the above composition and a window including the laminate.

ARTICLE WITH AN OPTICAL SURFACE WITH ENGINEERED FUNCTIONS

An article including a coating including a plurality of particles dispersed in a host material; and a plurality of optical elements embedded on a surface of the coating is disclosed. A method of making the coating, and the article is disclosed.

GLASS ELEMENT COMPRISING ENAMEL COATING AND USE THEREOF, COATING AGENT FOR MAKING SAME, AND METHOD FOR PRODUCING THE COATING AGENT

Glass elements are provided that include a coating and a sheet-like glass substrate. The sheet-like glass substrate has a first surface and a second surface opposite the first surface. The coating is disposed in at least some areas of at least one of the first and second surfaces. The coating is an inorganic glass-based coating that includes at least one glassy component; at least one pigment comprising pigment particles; and a filler. The filler is inorganic and includes filler particles with a d.sub.50 value, based on an equivalent diameter, of at least 0.1 μm and less than 10 μm.

ULTRAVIOLET LIGHT-BLOCKING COATED PHARMACEUTICAL PACKAGES

According to one or more embodiments disclosed herein, a coated pharmaceutical package may comprise a glass container comprising a first surface and a second surface opposite the first surface, wherein the first surface is an outer surface of the glass container, and wherein the glass container in an uncoated state has an average light transmittance in the UVB and UVC spectrum of at least 50% through a single wall of the coated package. The coated pharmaceutical package may further comprise a coating positioned over at least a portion of the first surface of the glass container, wherein the coated pharmaceutical package has an average light transmittance in the UVC spectrum of less than 50% through a single wall of the coated package.

COATING AND COATING FORMULATION

A coated substrate comprising a coating layer comprising inorganic oxide and pores, the coating layer demonstrates improved durability properties. The coated substrate may for example be used in solar modules. Further a coating formulation and use of the coating formulation are disclosed

Coating Liquid Used For Forming Ultraviolet Absorption Coating And Ultraviolet Absorption Glass
20210261798 · 2021-08-26 ·

Provided is an ultraviolet absorption glass comprising: a glass substrate, and an ultraviolet absorption coating arranged on at least one surface of the glass substrate, wherein the ultraviolet absorption coating comprises silicon dioxide, an ultraviolet absorber, and MOz used for storing and releasing electrons excited by ultraviolet light in the ultraviolet absorber. The ultraviolet absorption glass is low cost and has good resistance to discoloration and devitrification.

Electroconductive particle, visible light transmitting particle-dispersed electrical conductor and manufacturing method thereof, transparent electroconductive thin film and manufacturing method thereof, transparent electroconductive article that uses the same, and infrared-shielding article

An infrared-shielding nanoparticle dispersion has a property whereby visible light is adequately transmitted, and light in the near-infrared region is adequately shielded. The infrared-shielding nanoparticles include a plural aggregate of electroconductive particles composed of a tungsten oxide expressed by the general formula WyOz (where W is tungsten, O is oxygen, and 2.2≤z/y≤2.999), and/or a composite tungsten oxide expressed by the general formula MxWyOz (where M is one or more elements selected from H, alkali metals, alkaline-earth metals, rare earth elements, Mg, Zr, Cr, Mn, Fe, Ru, Co, Rh, Ir, Ni, Pd, Pt, Cu, Ag, Au, Zn, Cd, Al, Ga, In, Tl, Si, Ge, Sn, Pb, Sb, B, F, P, S, Se, Br, Te, Ti, Nb, V, Mo, Ta, Re, Be, Hf, Os, Bi, and I; W is tungsten; O is oxygen; 0.001≤x/y≤1.1; and 2.2≤z/y≤3.0).

Method of manufacturing a bendable substrate coated with a coating layer of adjacent heterogeneous coatings bonded along boundaries thereof useful for foldable displays

Disclosed herein are a method of manufacturing a heterogeneous coating solution bonded coating layer, and a coating layer and a cover window produced thereby. More particularly, there are provided a method of manufacturing a heterogeneous coating solution bonded coating layer, in which a step difference at the boundary between different types of coating solutions is controllable by controlling a difference in capillary number during discharge of the different types of coating solutions using a slot die coater, and a coating layer and a cover window produced thereby. Therefore, the method of manufacturing a heterogeneous coating solution bonded coating layer can produce a cover window that is excellent in all the properties including durability, optical characteristics, and flexibility.

Digital ink

A method including digital printing a heat curable aqueous composition onto a substrate, wherein the composition includes: (a) at least one water soluble synthetic alkali metal silicate; and (b)(i) at least one pigment or (b)(ii) at least one additive selected from aluminum oxide, ceramic microspheres, recycled ground glass, or calcium carbonate; wherein the composition is substantially free of any organic solvent; and heating the composition bearing substrate thereby curing the composition, and wherein the substrate includes a material selected from glass, ceramic, textile, polymeric, metal, wood, or a combination thereof.

HEAT-TREATABLE ANTIMICROBIAL GLASS
20210246069 · 2021-08-12 · ·

A coated glass substrate is disclosed. The coated glass substrate includes a coating containing at least one metal oxide containing a zinc oxide. The zinc of the zinc oxide is present in an amount of from 5 wt. % to 50 wt. % as determined according to XPS. The coated glass substrate has area surface roughness Sa or Sq of from about 5 nm to about 1,500 nm as determined via atomic force microscopy.