C04B41/5058

High temperature oxidation protection for composites

An oxidation protection system disposed on a substrate is provided, which may comprise a boron layer comprising a boron compound disposed on the substrate; a silicon layer comprising a silicon compound disposed on the boron layer; and at least one sealing layer comprising monoaluminum phosphate and phosphoric acid disposed on the silicon layer.

METHOD FOR COATING A CERAMIC MATRIX COMPOSITE PART WITH AN ENVIRONMENTAL BARRIER
20230121823 · 2023-04-20 ·

A method for coating a ceramic matrix composite part with an environmental barrier, the method including a) applying, to a surface of the part, a coating composition including a first powder of a rare earth silicate and a second powder including boron, the coating composition having a ratio R=[mass of the second powder]/[mass of the first powder] of between 0.1% and 5%, and b) sintering the first and second powders to obtain the environmental barrier on the part.

METHOD FOR COATING A CERAMIC MATRIX COMPOSITE PART WITH AN ENVIRONMENTAL BARRIER
20230121823 · 2023-04-20 ·

A method for coating a ceramic matrix composite part with an environmental barrier, the method including a) applying, to a surface of the part, a coating composition including a first powder of a rare earth silicate and a second powder including boron, the coating composition having a ratio R=[mass of the second powder]/[mass of the first powder] of between 0.1% and 5%, and b) sintering the first and second powders to obtain the environmental barrier on the part.

HIGH TEMPERATURE OXIDATION PROTECTION FOR CARBON-CARBON COMPOSITES
20230150884 · 2023-05-18 · ·

A method for forming an oxidation protection system on a composite structure may comprise: applying a ceramic layer slurry to the composite structure, wherein the ceramic layer slurry comprises aluminum and silicon in a solvent or carrier fluid; and heating the composite structure in an environment comprising nitrogen gas and oxygen gas to form a ceramic layer on the composite structure, wherein the ceramic layer comprises aluminum nitride and alumina.

HIGH TEMPERATURE OXIDATION PROTECTION FOR CARBON-CARBON COMPOSITES
20230150884 · 2023-05-18 · ·

A method for forming an oxidation protection system on a composite structure may comprise: applying a ceramic layer slurry to the composite structure, wherein the ceramic layer slurry comprises aluminum and silicon in a solvent or carrier fluid; and heating the composite structure in an environment comprising nitrogen gas and oxygen gas to form a ceramic layer on the composite structure, wherein the ceramic layer comprises aluminum nitride and alumina.

HIGH TEMPERATURE OXIDATION PROTECTION FOR COMPOSITES

Systems and methods for forming an oxidation protection system on a composite structure are provided. In various embodiments, an oxidation protection system disposed on a substrate may comprise a boron-silicon-glass layer formed directly on the composite structure. The boron-silicon-glass layer may comprise a boron compound, a silicon compound, and a glass compound.

HIGH TEMPERATURE OXIDATION PROTECTION FOR COMPOSITES

Systems and methods for forming an oxidation protection system on a composite structure are provided. In various embodiments, an oxidation protection system disposed on a substrate may comprise a boron-silicon-glass layer formed directly on the composite structure. The boron-silicon-glass layer may comprise a boron compound, a silicon compound, and a glass compound.

Protecting parts made of carbon-containing composite material from oxidation

A method of protecting a part made of carbon-including composite material against oxidation, the method including a) applying a coating composition on at least a portion of the outside surface of the part, the coating composition being in the form of an aqueous suspension including: a metallic phosphate; a powder of a compound comprising titanium; and a B.sub.4C powder; and b) applying heat treatment to the coating composition applied during step a) with a treatment temperature lying in the range 330° C. to 730° C. being imposed during the heat treatment in order to obtain a coating on the outside surface of the part, the coating including a first phase in which the metallic phosphate is in crystalline form and a second phase in which the metallic phosphate is in amorphous form.

Protecting parts made of carbon-containing composite material from oxidation

A method of protecting a part made of carbon-including composite material against oxidation, the method including a) applying a coating composition on at least a portion of the outside surface of the part, the coating composition being in the form of an aqueous suspension including: a metallic phosphate; a powder of a compound comprising titanium; and a B.sub.4C powder; and b) applying heat treatment to the coating composition applied during step a) with a treatment temperature lying in the range 330° C. to 730° C. being imposed during the heat treatment in order to obtain a coating on the outside surface of the part, the coating including a first phase in which the metallic phosphate is in crystalline form and a second phase in which the metallic phosphate is in amorphous form.

METHOD OF REPAIRING CERAMIC COMPOSITE ARTICLES
20220228256 · 2022-07-21 ·

A method of repairing an article including cleaning a repair area, wherein the repair area comprises a ceramic matrix composite; and depositing a ceramic material in the cleaned repair area using laser assisted chemical vapor deposition. Also disclosed is a repaired ceramic composite produced by this method.