C04B35/62821

Surface-treated ceramic powder and applications thereof

A surface-treated ceramic powder includes a plurality of ceramic particles and a surface-treating material. Each of the ceramic particles is at least partially coated by the surface-treating material, wherein the ceramic particles have an average particle diameter ranging from 10 micrometer (m) to 100 m, and the surface-treating material is made of metal, metal oxide or the combination thereof.

NON-STICK CERAMIC COATING COMPRISING DIAMONDS AND COLOURED MICA

The present invention relates to an enhanced ceramic coating composition comprising a base non-stick ceramic coating composition and 0.2 wt %-2 wt % diamond additive (DA) with wt % compared with the total weight compared of the ceramic coating composition, wherein the diamond additive comprises diamond and mica particles, and wherein said mica particles comprise coloured mica particles, such as red and/or green and/or blue coloured mica particles. It also relates to a method of coating an artefact with the improved ceramic coating, and an artefact provided with a dry film coating containing an improved ceramic coating prepared using an improved ceramic coating composition of the invention. An artefact coated with the improved ceramic coating has the combined advantages of durable non-stick, scratch resistance and abrasion resistance.

MAGNETIC NANOPARTICLE
20200124592 · 2020-04-23 ·

Disclosed herein are magnetic nanoparticles, compositions and kits comprising the magnetic nanoparticles, methods of making the magnetic nanoparticles, and methods of using the magnetic nanoparticles to enrich biological targets.

SINTERED BODY, SUBSTRATE, CIRCUIT BOARD, AND MANUFACTURING METHOD OF SINTERED BODY

A sintered body includes a crystal grain containing silicon nitride, and a grain boundary phase. If dielectric losses of the sintered body are measured while applying an alternating voltage to the sintered body and continuously changing a frequency of the alternating voltage from 50 Hz to 1 MHz, an average value .sub.A of dielectric losses of the sintered body in a frequency band from 800 kHz to 1 MHz and an average value .sub.B of dielectric losses of the sintered body in a frequency band from 100 Hz to 200 Hz satisfy an expression |.sub.A.sub.B|0.1.

Ferrite particles having outer shell structure used for filtering medium
10603614 · 2020-03-31 · ·

An object of the present invention is to provide ferrite particles for a filtering medium excellent in filtration ability having a small apparent density, capable of various properties maintained in the controllable state and filling a specified volume with a small amount, and a filtering medium made from the ferrite particles. In order to achieve the object, ferrite particles provided an outer shell structure containing Ti oxide for a filtering medium, and a filtering medium made from the ferrite particles are employed.

Dielectric composition and multilayer ceramic capacitor containing the same

A multilayer ceramic capacitor includes: a ceramic body including dielectric layers and first and second internal electrodes disposed to face each other with respective dielectric layers interposed therebetween; and first and second external electrodes disposed on an external surface of the ceramic body, wherein the dielectric layer contains a barium titanate-based powder particle having a core-shell structure including a core and a shell around the core, the shell having a structure in which titanium is partially substituted with an element having the same oxidation number as that of the titanium in the barium titanate-based powder particle and having an ionic radius different from that of the titanium in the barium titanate-based powder particle, and the shell covers at least 30% of a surface of the core.

Dielectric composition and multilayer ceramic capacitor containing the same

A multilayer ceramic capacitor includes: a ceramic body including dielectric layers and first and second internal electrodes disposed to face each other with respective dielectric layers interposed therebetween; and first and second external electrodes disposed on an external surface of the ceramic body, wherein the dielectric layer contains a barium titanate-based powder particle having a core-shell structure including a core and a shell around the core, the shell having a structure in which titanium is partially substituted with an element having the same oxidation number as that of the titanium in the barium titanate-based powder particle and having an ionic radius different from that of the titanium in the barium titanate-based powder particle, and the shell covers at least 30% of a surface of the core.

Dielectric powder and multilayer ceramic electronic component using the same

A multilayer ceramic electronic component includes: a body part including dielectric layers and internal electrodes disposed to face each other with respective dielectric layers interposed therebetween; and external electrodes disposed on an outer surface of the body part and electrically connected to the internal electrodes. The dielectric layer includes grains including: a semiconductive or conductive grain core region containing a base material represented by ABO.sub.3, where A is at least one of Ba, Sr, and Ca, and B is at least one of Ti, Zr, and Hf, and a doping material including a rare earth element; and an insulating grain shell region enclosing the grain core region.

LITHIUM-MIXED OXIDE PARTICLES ENCAPSULATED IN ALUMINUM OXIDE AND TITANIUM DIOXIDE, AND METHOD FOR USING SAME
20200010367 · 2020-01-09 · ·

Process for producing coated mixed lithium oxide particles, in which mixed lithium oxide particles and a mixture comprising aluminium oxide and titanium dioxide are subjected to dry mixing by means of a mixing unit having a specific power of 0.1-1 kW per kg of mixed lithium oxide particles and mixture used, in total, under shearing conditions.

Coated mixed lithium oxide particles comprising a mixture of aluminium oxide and titanium dioxide as coating material, wherein the aluminium oxide and the titanium dioxide are in the form of aggregated primary particles and the weight ratio of aluminium oxide to titanium dioxide is 10:90-90:10.

PERFORMANCE OF TECHNICAL CERAMICS

Disclosed herein are a ceramic particle comprising a ceramic core substrate and a conformal coating of a sintering aid film on a surface of the core substrate, wherein the conformal coating includes a plurality of distributed islands of the sintering aid film across the surface of the core substrate; methods for producing the ceramic particle by ALD or MLD; and methods of using the coated ceramic particles in additive manufacturing or in solid oxide fuel cells. In one example, the film may have a thickness of less than three nanometers. The disclosed ceramic particle may be non-reactive with water.