D02G3/44
Filamentary core for an elastic yarn, elastic composite yarn, textile fabric and apparatus and method for manufacturing said elastic yarn
A filamentary core for an elastic composite yarn, particularly for an elastic textile composite yarn, comprising at least two elastic performance filaments, wherein each of the at least two elastic performance filaments is capable of being stretched at least about 2 times its package length and has at least 90% up to 100% elastic recovery after having being released from a stretching 2 times its package length.
Biosensing garment
Embodiments described herein relate generally to wearable electronic biosensing garments. In some embodiments, an apparatus comprises a biosensing garment and a plurality of electrical connectors that are mechanically fastened to the biosensing garment. A plurality of printed electrodes is disposed on the biosensing garment, each being electrically coupled, via a corresponding conductive pathway, to a corresponding one of the plurality of electrical connectors. The apparatus can further include an elongate member including a conductive member that is coupled to a plurality of elastic members in a curved pattern and that is configured to change from a first configuration to a second configuration as the elongate member stretches. The change from the first configuration to the second configuration can result in a change of inductance of the conductive member.
Material, method for producing the material, partially welded material, composite material, and method of producing molded product
To provide a novel material that maintains suppleness which is the advantage of a material using fibers and has a low thermal shrinkage ratio, and a method for producing the material, a partially welded material using the material, a composite material, and a method for producing a molded product. A material including: a first region, a fiber region, and a second region continuously in a thickness direction; the first region and the second region being each independently a resin layer including from 20 to 100 mass % of a thermoplastic resin component and from 80 to 0 mass % of reinforcing fibers; the fiber region including from 20 to 100 mass % of thermoplastic resin fibers and from 80 to 0 mass % of reinforcing fibers; the thermoplastic resin component included in the first region and the thermoplastic resin component included in the second region each independently having a crystallization energy during temperature increase of 2 J/g or greater, measured by differential scanning calorimetry; and the thermoplastic resin fibers included in the fiber region having a crystallization energy during temperature increase of less than 1 J/g, measured by differential scanning calorimetry; wherein the crystallization energy during temperature increase is a value measured by using a differential scanning calorimeter (DSC) in a nitrogen stream while heating is performed from 25° C. to a temperature that is 20° C. higher than a melting point of the thermoplastic resin component or the thermoplastic resin fibers at a temperature increase rate of 10° C./min.
Material, method for producing the material, partially welded material, composite material, and method of producing molded product
To provide a novel material that maintains suppleness which is the advantage of a material using fibers and has a low thermal shrinkage ratio, and a method for producing the material, a partially welded material using the material, a composite material, and a method for producing a molded product. A material including: a first region, a fiber region, and a second region continuously in a thickness direction; the first region and the second region being each independently a resin layer including from 20 to 100 mass % of a thermoplastic resin component and from 80 to 0 mass % of reinforcing fibers; the fiber region including from 20 to 100 mass % of thermoplastic resin fibers and from 80 to 0 mass % of reinforcing fibers; the thermoplastic resin component included in the first region and the thermoplastic resin component included in the second region each independently having a crystallization energy during temperature increase of 2 J/g or greater, measured by differential scanning calorimetry; and the thermoplastic resin fibers included in the fiber region having a crystallization energy during temperature increase of less than 1 J/g, measured by differential scanning calorimetry; wherein the crystallization energy during temperature increase is a value measured by using a differential scanning calorimeter (DSC) in a nitrogen stream while heating is performed from 25° C. to a temperature that is 20° C. higher than a melting point of the thermoplastic resin component or the thermoplastic resin fibers at a temperature increase rate of 10° C./min.
DEODORANT AND ANTIBACTERIAL COPPER NANOFIBER YARN AND MANUFACTURING METHOD THEREOF
A deodorant and antibacterial copper nanofiber yarn and a manufacturing method thereof are provided, the manufacturing method including: providing a raw material, including a polyblend slurry, a nano-metal solution, a plurality of inorganic particles, and a plurality of TPU rubber particles; stirring the raw material into a mixed material; making second metal contact the first metal ion fiber to cause the first metal ion to undergo a reduction reaction to obtain a copper nanofiber yarn; drying the mixed material; performing hot-melt spinning on the mixed material, the plurality of TPU rubber particles, after being hot-melted, being coated on an outer peripheral side of the spun wire to form a first-phase wire; forcibly cooling the first-phase wire; stretching the first-phase wire; air-cooling the first-phase wire to form a second-phase wire; and collecting the second-phase wire to make the wire into a finished deodorant and antibacterial copper nanofiber yarn.
Textile including bulking yarn
In one aspect, a textile component including bulking yarn is disclosed. In embodiments, the textile component is a knitted component. In one embodiment, an article of footwear includes a knitted component arch support configured to reduce the rate of pronation. A support structure may include a fusible yarn adjacent to an external surface of the arch support, a bulking yarn, and a nonfusible yarn. In certain embodiments, an arch support includes compartments and flex lines. In another aspect, an article having a knitted component includes a rigid material, a bulking yarn, and a flexible material. The rigid material may be fusible yarn. Methods for forming a textile component are provided. One embodiment involves knitting a first section comprising a fusible yarn, a second section comprising a bulking yarn, and a third section comprising a nonfusible yarn, and heating.
Textile including bulking yarn
In one aspect, a textile component including bulking yarn is disclosed. In embodiments, the textile component is a knitted component. In one embodiment, an article of footwear includes a knitted component arch support configured to reduce the rate of pronation. A support structure may include a fusible yarn adjacent to an external surface of the arch support, a bulking yarn, and a nonfusible yarn. In certain embodiments, an arch support includes compartments and flex lines. In another aspect, an article having a knitted component includes a rigid material, a bulking yarn, and a flexible material. The rigid material may be fusible yarn. Methods for forming a textile component are provided. One embodiment involves knitting a first section comprising a fusible yarn, a second section comprising a bulking yarn, and a third section comprising a nonfusible yarn, and heating.
TEXTILE PART PROVIDED WITH AN ELECTRONIC TAG COMPRISING A WIRED ELECTRONIC DEVICE AND METHOD FOR PRODUCING SUCH A PART
The invention relates to a method for making a textile part (A; A1, A2), comprising a step of forming a stitched seam (c1, c2, c3; C). The stitched seam step also aims to secure an electronic tag (1) to the textile part (A; A1, A2). The electronic tag (1) is formed from a strip comprising a wired electronic device comprising a chip (3a) associated with at least one antenna wire (3b), the chip (3a) and the antenna wire (3b) being arranged inside the stitched seam (c1, c2, c3; C). The invention also relates to the textile part provided with the tag.
THERMOPLASTIC COMPOSITE
A method of making a flexible pipe layer, which method comprises: commingling polymer filaments and carbon fibre filaments to form an intimate mixture, forming yarns of the commingled filaments, forming the yarns into a tape, and applying the tape to a pipe body to form a flexible pipe layer.
CONDUCTIVE BAND FOR BIOSENSING GARMENTS
Embodiments described herein relate generally to wearable electronic biosensing garments. In some embodiments, an apparatus comprises a biosensing garment and a plurality of electrical connectors that are mechanically fastened to the biosensing garment. A plurality of printed electrodes is disposed on the biosensing garment, each being electrically coupled, via a corresponding conductive pathway, to a corresponding one of the plurality of electrical connectors. The apparatus can further include an elongate member including a conductive member that is coupled to a plurality of elastic members in a curved pattern and that is configured to change from a first configuration to a second configuration as the elongate member stretches. The change from the first configuration to the second configuration can result in a change of inductance of the conductive member.