G03G9/1138

ELECTROSTATIC-IMAGE DEVELOPING TONER, ELECTROSTATIC-IMAGE DEVELOPER, TONER CARTRIDGE, PROCESS CARTRIDGE, IMAGE FORMING APPARATUS, AND IMAGE FORMING METHOD

An electrostatic-image developing toner includes toner particles, layered compound particles, and inorganic particles. The inorganic particles have an average circularity of 0.910 or more and 0.995 or less. A ratio Da/Db of a number-average particle size Da of the layered compound particles to a number-average particle size Db of the inorganic particles is 1.2 or more and 43 or less.

ELECTROSTATIC IMAGE DEVELOPING TONER, ELECTROSTATIC IMAGE DEVELOPER, TONER CARTRIDGE, PROCESS CARTRIDGE, IMAGE FORMING APPARATUS, AND IMAGE FORMING METHOD

An electrostatic image developing toner includes toner particles, layered compound particles, and inorganic particles. The content of titanium in the electrostatic image developing toner is 0.1 ppm or more and less than 1,500 ppm.

ELECTROSTATIC IMAGE DEVELOPING TONER, ELECTROSTATIC IMAGE DEVELOPER, TONER CARTRIDGE, PROCESS CARTRIDGE, IMAGE FORMING APPARATUS, AND IMAGE FORMING METHOD

An electrostatic image developing toner includes toner particles, layered compound particles, and inorganic particles. The proportion of irregular-shaped inorganic particles having a circularity of 0.5 or more and 0.9 or less and a size of 0.015 m or more and 0.350 m or less to the entire inorganic particles is 2% by number or more and 70% by number or less.

Carrier and two-component developer
10852654 · 2020-12-01 · ·

A carrier includes carrier particles. The carrier particles include first carrier particles and second carrier particles. The first carrier particles each include a first carrier core and a first coat layer covering a surface of the first carrier core. The second carrier particles each include a second carrier core and a second coat layer covering a surface of the second carrier core. The first coat layers contain no fatty acid metal salt. The second coat layer contains a coat layer binder resin and a fatty acid metal salt. The second coat layers contain the fatty acid metal salt in a proportion of from 85 mass % to 95 mass % relative to a total mass of the second coat layers. The second carrier particles are contained in a proportion of from 7 mass % to 15 mass % relative to a total mass of the first carrier particles and the second carrier particles.

Electrostatic-image developer and process cartridge

An electrostatic-image developer includes a toner and a resin-coated carrier. The toner includes toner particles including a binder resin, a release agent, and a non-ionic surfactant. The resin-coated carrier includes magnetic particles and a resin layer covering the magnetic particles. The resin-coated carrier has an absolute specific gravity of 3 g/cm.sup.3 or more and 4 g/cm.sup.3 or less.

TONER EXTERNAL ADDITIVE AND TONER
20200301303 · 2020-09-24 ·

Provided is a toner external additive containing a base material, wherein the base material is surface-treated with an isocyanurate ring-bearing silane coupling agent, and a toner including a toner particle and a toner external additive on a surface of the toner particle, wherein the toner external additive is the aforementioned toner external additive.

ELECTROSTATIC-IMAGE DEVELOPER AND PROCESS CARTRIDGE

An electrostatic-image developer includes a toner and a resin-coated carrier. The toner includes toner particles including a binder resin, a release agent, and a non-ionic surfactant. The resin-coated carrier includes magnetic particles and a resin layer covering the magnetic particles. The resin-coated carrier has an absolute specific gravity of 3 g/cm.sup.3 or more and 4 g/cm.sup.3 or less.

CARRIER AND TWO-COMPONENT DEVELOPER
20200159140 · 2020-05-21 · ·

A carrier includes carrier particles. The carrier particles include first carrier particles and second carrier particles. The first carrier particles each include a first carrier core and a first coat layer covering a surface of the first carrier core. The second carrier particles each include a second carrier core and a second coat layer covering a surface of the second carrier core. The first coat layers contain no fatty acid metal salt. The second coat layer contains a coat layer binder resin and a fatty acid metal salt. The second coat layers contain the fatty acid metal salt in a proportion of from 85 mass % to 95 mass % relative to a total mass of the second coat layers. The second carrier particles are contained in a proportion of from 7 mass % to 15 mass % relative to a total mass of the first carrier particles and the second carrier particles.

Toner and two-component developer
11947313 · 2024-04-02 · ·

The peak top molecular weight of the tetrahydrofuran-soluble component of the toner, as measured by gel permeation chromatography, is 4,000 or more and 6,500 or less. The tetrahydrofuran-insoluble component of the toner is 10% by weight or more and 30% by weight or less. When the endothermic peak temperature T1 in the heating process and the exothermic peak temperature T2 during the cooling process originating from the ester wax is measured using a differential scanning calorimeter, the value T1-T2 is 15? C. or more and 30? C. or less.

ELECTROSTATIC IMAGE DEVELOPER, PROCESS CARTRIDGE, IMAGE FORMING APPARATUS, AND IMAGE FORMING METHOD

An electrostatic image developer includes: a toner A to which silica particles (A) containing an elemental nitrogen-containing compound containing elemental molybdenum are externally added; and a carrier B including a core material and a coating resin layer that covers the core material and contains inorganic particles. In the silica particles (A), the ratio N.sub.Mo/N.sub.Si of a Net intensity N.sub.Mo of elemental molybdenum that is measured by X-ray fluorescence analysis to a Net intensity N.sub.Si of elemental silicon that is measured by the X-ray fluorescence analysis is from 0.035 to 0.45 inclusive.