Anode electrode composition of Li-ion battery cell
In an embodiment, a Li-ion battery cell comprises an anode electrode with an electrode coating that (1) comprises Si-comprising active material particles, (2) exhibits an areal capacity loading in the range of about 3 mAh/cm.sup.2 to about 12 mAh/cm.sup.2, (3) exhibits a volumetric capacity in the range from about 600 mAh/cc to about 1800 mAh/cc in a charged state of the cell, (4) comprises conductive additive material particles, and (5) comprises a polymer binder that is configured to bind the Si-comprising active material particles and the conductive additive material particles together to stabilize the anode electrode against volume expansion during the one or more charge-discharge cycles of the battery cell while maintaining the electrical connection between the metal current collector and the Si-comprising active material particles.
Composition for gel polymer electrolyte including fluoroalkylene oligomer, lithium salt, and phosphate or boran-based additive, gel polymer electrolyte prepared therefrom, and lithium secondary battery including the gel polymer electrolyte
The present invention provides a composition for a gel polymer electrolyte, the composition including: an oligomer represented by Formula 1; an additive; a polymerization initiator; a lithium salt; and a non-aqueous solvent, the additive including at least one compound selected from the group consisting of a substituted or unsubstituted phosphate-based compound and a substituted or unsubstituted benzene-based compound, a gel polymer electrolyte prepared using the same, and a lithium secondary battery.
Secondary battery and method for manufacturing the same
One of the objects of the present invention is to suppress a short circuit due to metal deposition in an insulating layer in a secondary battery in which a positive electrode and a negative electrode are disposed to face each other via the insulating layer. The secondary battery comprises a battery element including at least one positive electrode 11 and at least one negative electrode 12, and a casing that seals the battery element together with an electrolyte. At least one of the positive electrode 11 and the negative electrode 12 comprises a current collector, an active material layer formed on at least one surface of the current collector, and an insulating layer 112 formed on the surface of the active material layer. The electrolyte comprises an electrolyte component and a crosslinked gelling agent. The gelling agent exists at least between the active material layer of the positive electrode 11 and the active material layer of the negative electrode 12, and the ratio Rg of the gelling agent to 100% by mass of the electrolyte component in between the active material layer of the positive electrode 11 and the active material layer of the negative electrode 12 is 0<Rg≤5% by mass.
Secondary battery and method for manufacturing the same
One of the objects of the present invention is to suppress a short circuit due to metal deposition in an insulating layer in a secondary battery in which a positive electrode and a negative electrode are disposed to face each other via the insulating layer. The secondary battery comprises a battery element including at least one positive electrode 11 and at least one negative electrode 12, and a casing that seals the battery element together with an electrolyte. At least one of the positive electrode 11 and the negative electrode 12 comprises a current collector, an active material layer formed on at least one surface of the current collector, and an insulating layer 112 formed on the surface of the active material layer. The electrolyte comprises an electrolyte component and a crosslinked gelling agent. The gelling agent exists at least between the active material layer of the positive electrode 11 and the active material layer of the negative electrode 12, and the ratio Rg of the gelling agent to 100% by mass of the electrolyte component in between the active material layer of the positive electrode 11 and the active material layer of the negative electrode 12 is 0<Rg≤5% by mass.
Ethyl cellulose as a dispersant for lithium ion battery cathode production
The process of making a lithium ion battery cathode comprises the step of forming a slurry of an active material, a nano-size conductive agent, a binder polymer, a solvent and a dispersant. The solvent consists essentially of one or more of a compound of Formula 1, 2, or 3, and the dispersant comprises an ethyl cellulose.
Negative electrode slurry for lithium secondary battery, and preparation method thereof
A negative electrode slurry and a method of preparing the same. The negative electrode slurry includes lithium titanium oxide (LTO), a carboxylic acid-containing polymer dispersant, a binder, and an aqueous solvent. The carboxylic acid-containing polymer dispersant has a weight average molecular weight (Mw) of 2,500 g/mol to 500,000 g/mol and is present in an amount of 1.5 parts by weight to 20 parts by weight with respect to 100 parts by weight of the lithium titanium oxide.
Battery housing for a drive battery
A battery housing for a drive battery, comprising at least one housing shell, wherein the housing shell is formed at least partially or fully from a thermoplastic, wherein the housing shell has a receiving region for insertion of a drive battery, wherein the housing shell has a wall, wherein the wall has a two-layer or multi-layer sandwich structure, wherein at least a first layer of the sandwich structure, at least in some sections, is distanced from a second layer of the sandwich structure such that a wall cavity is formed between the first layer and the second layer, and wherein the wall cavity is designed to store a cooling medium.
NEGATIVE ELECTRODE INCLUDING OXIDIZED CURRENT COLLECTOR FOR LITHIUM SECONDARY BATTERIES AND METHOD OF MANUFACTURING THE SAME
A negative electrode for lithium secondary batteries and a method of manufacturing the same are provided. The negative electrode includes a negative electrode current collector and a lithiophilic material formed on at least one surface of the negative electrode current collector, wherein the lithiophilic material is an oxidized product of a coating material coated on the negative electrode current collector and includes at least one of a metal or a metal oxide, and an oxide layer is formed on a surface of the negative electrode current collector having the lithiophilic material formed thereon.
NEGATIVE ELECTRODE COATED WITH LITHIOPHILIC MATERIAL FOR LITHIUM SECONDARY BATTERIES AND METHOD OF MANUFACTURING THE SAME
A negative electrode for lithium secondary batteries is provided. The negative electrode comprises a negative electrode current collector including a porous structure having an inner pore or a through-hole formed therethrough from an upper surface to a lower surface thereof, wherein a lithiophilic material is applied to a surface of the porous structure or the through-hole excluding a first surface of the negative electrode current collector that faces a positive electrode.
POSITIVE ELECTRODE AND LITHIUM-SULFUR BATTERY COMPRISING SAME
A positive electrode comprising a current collector and a positive electrode active material layer disposed on at least one surface of the current collector, and a lithium-sulfur battery comprising the positive electrode are provided. The positive electrode active material layer comprises a positive electrode active material and an additive, and the additive comprises a transition metal-ferrocyanide compound.