STRUCTURE AND METHOD FOR STABILIZING LEADS IN WIRE-BONDED SEMICONDUCTOR DEVICES
A semiconductor device having a leadframe including a pad (101) surrounded by elongated leads (110) spaced from the pad by a gap (113) and extending to a frame, the pad and the leads having a first thickness (115) and a first and an opposite and parallel second surface; the leads having a first portion (112) of first thickness near the gap and a second portion (111) of first thickness near the frame, and a zone (114) of reduced second thickness (116) between the first and second portions; the second surface (112a) of the first lead portions is coplanar with the second surface (111a) of the second portions. A semiconductor chip (220) with a terminal is attached the pad. A metallic wire connection (230) from the terminal to an adjacent lead includes a stitch bond (232) attached to the first surface of the lead.
STRUCTURE AND METHOD FOR STABILIZING LEADS IN WIRE-BONDED SEMICONDUCTOR DEVICES
A semiconductor device having a leadframe including a pad (101) surrounded by elongated leads (110) spaced from the pad by a gap (113) and extending to a frame, the pad and the leads having a first thickness (115) and a first and an opposite and parallel second surface; the leads having a first portion (112) of first thickness near the gap and a second portion (111) of first thickness near the frame, and a zone (114) of reduced second thickness (116) between the first and second portions; the second surface (112a) of the first lead portions is coplanar with the second surface (111a) of the second portions. A semiconductor chip (220) with a terminal is attached the pad. A metallic wire connection (230) from the terminal to an adjacent lead includes a stitch bond (232) attached to the first surface of the lead.
BONDING WIRE FOR SEMICONDUCTOR DEVICE
There is provided a Cu bonding wire having a Pd coating layer on a surface thereof, that improves bonding reliability of a ball bonded part in a high-temperature and high-humidity environment and is suitable for on-vehicle devices.
The bonding wire for a semiconductor device includes a Cu alloy core material and a Pd coating layer formed on a surface of the Cu alloy core material, and the bonding wire contains In of 0.011 to 1.2% by mass and has the Pd coating layer of a thickness of 0.015 to 0.150 μm. With this configuration, it is able to increase the bonding longevity of a ball bonded part in a high-temperature and high-humidity environment, and thus to improve the bonding reliability. When the Cu alloy core material contains one or more elements of Pt, Pd, Rh and Ni in an amount, for each element, of 0.05 to 1.2% by mass, it is able to increase the reliability of a ball bonded part in a high-temperature environment of 175° C. or more. When an Au skin layer is further formed on a surface of the Pd coating layer, wedge bondability improves.
BONDING WIRE FOR SEMICONDUCTOR DEVICE
There is provided a Cu bonding wire having a Pd coating layer on a surface thereof, that improves bonding reliability of a ball bonded part in a high-temperature and high-humidity environment and is suitable for on-vehicle devices.
The bonding wire for a semiconductor device includes a Cu alloy core material and a Pd coating layer formed on a surface of the Cu alloy core material, and the bonding wire contains In of 0.011 to 1.2% by mass and has the Pd coating layer of a thickness of 0.015 to 0.150 μm. With this configuration, it is able to increase the bonding longevity of a ball bonded part in a high-temperature and high-humidity environment, and thus to improve the bonding reliability. When the Cu alloy core material contains one or more elements of Pt, Pd, Rh and Ni in an amount, for each element, of 0.05 to 1.2% by mass, it is able to increase the reliability of a ball bonded part in a high-temperature environment of 175° C. or more. When an Au skin layer is further formed on a surface of the Pd coating layer, wedge bondability improves.
METHOD FOR FABRICATING A SEMICONDUCTOR DEVICE USING WET ETCHING AND DRY ETCHING AND SEMICONDUCTOR DEVICE
A method for fabricating a semiconductor device comprises depositing a TiW layer on a semiconductor substrate, depositing a Ti layer on the TiW layer, depositing a Ni alloy layer on the Ti layer, depositing an Ag layer on the Ni alloy layer, at least partially covering the Ag layer with photoresist, wet etching the Ag layer and the Ni alloy layer, and dry etching the Ti layer and the TiW layer.
METHOD FOR FABRICATING A SEMICONDUCTOR DEVICE USING WET ETCHING AND DRY ETCHING AND SEMICONDUCTOR DEVICE
A method for fabricating a semiconductor device comprises depositing a TiW layer on a semiconductor substrate, depositing a Ti layer on the TiW layer, depositing a Ni alloy layer on the Ti layer, depositing an Ag layer on the Ni alloy layer, at least partially covering the Ag layer with photoresist, wet etching the Ag layer and the Ni alloy layer, and dry etching the Ti layer and the TiW layer.
Bump structure to prevent metal redeposit and to prevent bond pad consumption and corrosion
Various embodiments of the present disclosure are directed towards a semiconductor device structure including a bump structure overlying a bond pad. The bond pad is disposed over a semiconductor substrate. An etch stop layer overlies the bond pad. A buffer layer is disposed over the bond pad and separates the etch stop layer and the bond pad. The bump structure includes a base portion contacting an upper surface of the bond pad and an upper portion extending through the etch stop layer and the buffer layer. The base portion of the bump structure has a first width or diameter and the upper portion of the bump structure has a second width or diameter. The first width or diameter being greater than the second width or diameter.
HYBRID MANUFACTURING FOR INTEGRATED CIRCUIT DEVICES AND ASSEMBLIES
Microelectronic assemblies fabricated using hybrid manufacturing, as well as related devices and methods, are disclosed herein. As used herein, “hybrid manufacturing” refers to fabricating a microelectronic assembly by arranging together at least two IC structures fabricated by different manufacturers, using different materials, or different manufacturing techniques. For example, a microelectronic assembly may include a first IC structure that includes first interconnects and a second IC structure that includes second interconnects, where at least some of the first and second interconnects may include a liner and an electrically conductive fill material, and where a material composition of the liner/electrically conductive fill material of the first interconnects may be different from a material composition of the liner/electrically conductive fill material of the second interconnects.
HYBRID MANUFACTURING FOR INTEGRATED CIRCUIT DEVICES AND ASSEMBLIES
Microelectronic assemblies fabricated using hybrid manufacturing, as well as related devices and methods, are disclosed herein. As used herein, “hybrid manufacturing” refers to fabricating a microelectronic assembly by arranging together at least two IC structures fabricated by different manufacturers, using different materials, or different manufacturing techniques. For example, a microelectronic assembly may include a first IC structure that includes first interconnects and a second IC structure that includes second interconnects, where at least some of the first and second interconnects may include a liner and an electrically conductive fill material, and where a material composition of the liner/electrically conductive fill material of the first interconnects may be different from a material composition of the liner/electrically conductive fill material of the second interconnects.
SEMICONDUCTOR DIE STACKS AND ASSOCIATED SYSTEMS AND METHODS
Semiconductor die stacks, and associated methods and systems are disclosed. The semiconductor die stack may include a first die with a memory array and a second die with CMOS circuitry configured to access the memory array. The first die may not have circuitry for accessing the memory array. Further, the first and second dies may be bonded to function as a single memory device, and front surfaces of the first and second dies are conjoined to form electrical connections therebetween. The second die may include a portion uncovered by the first die, where bond pads of the semiconductor die stack are located. The first die may provide a space for bond wires to connect to the bond pads without interfering with another die attached above the semiconductor die stack. Multiple semiconductor die stacks may be stacked on top of and in line with each other.