H01L21/022
MIM CAPACITOR WITH A SYMMETRICAL CAPACITOR INSULATOR STRUCTURE
Various embodiments of the present application are directed towards a metal-insulator-metal (MIM) capacitor. The MIM capacitor comprises a bottom electrode disposed over a semiconductor substrate. A top electrode is disposed over and overlies the bottom electrode. A capacitor insulator structure is disposed between the bottom electrode and the top electrode. The capacitor insulator structure comprises at least three dielectric structures vertically stacked upon each other. A bottom half of the capacitor insulator structure is a mirror image of a top half of the capacitor insulator structure in terms of dielectric materials of the dielectric structures.
GAPFILL OF VARIABLE ASPECT RATIO FEATURES WITH A COMPOSITE PEALD AND PECVD METHOD
Provided herein are methods and apparatus for filling one or more gaps on a semiconductor substrate. The disclosed embodiments are especially useful for forming seam-free, void-free fill in both narrow and wide features. The methods may be performed without any intervening etching operations to achieve a single step deposition. In various implementations, a first operation is performed using a novel PEALD fill mechanism to fill narrow gaps and line wide gaps. A second operation may be performed using PECVD methods to continue filling the wide gaps.
High-K Dielectric and Method of Manufacture
A semiconductor device and method of manufacturing same are described. A first hafnium oxide (HfO.sub.2) layer is formed on a substrate. A titanium (Ti) layer is formed over the first hafnium oxide layer. A second hafnium oxide layer is formed over the titanium layer. The composite device structure is thermally annealed to produce a high-k dielectric structure having a hafnium titanium oxide (Hf.sub.xTi.sub.1-xO.sub.2) layer interposed between the first hafnium oxide layer and the second hafnium oxide layer.
Multi-layer filled gate cut to prevent power rail shorting to gate structure
A method of forming a power rail to semiconductor devices that includes forming a gate structure extending from a first active region to a second active region of a substrate, and removing a portion of the gate structure forming a gate cut trench separating the first active region from the second active region. A fill material of an alternating sequence of at least two different composition conformally deposited dielectric layers is formed within the gate cut trench. A power rail is formed in the gate cut trench. An aspect ratio of the vertically orientated portions of the alternating sequence of the at least two different composition conformally deposited dielectric layer obstructs lateral etching of the gate cut trench during etching to form a power rail opening for housing the power rail.
Nitride Light Emitting Diode and Fabrication Method Thereof
A nitride light-emitting diode (LED) fabrication method includes: providing a glass substrate; stacking a buffer layer structure composed of circular SiAlN layers and AlGaN layers with the number of cycles 1-5; growing a non-doped GaN layer, an N-type layer, a quantum well layer and a P-type layer. By using the low-cost glass the substrate that has a mature processing technology, and growing a SiAlN and an AlGaN buffer layer thereon, lattice mismatch constant between the substance and the epitaxial layer can be improved. Therefore, photoelectric property of the LED can be improved.
METHOD OF MAKING SEMICONDUCTOR FERROELECTRIC MEMORY ELEMENT, AND SEMICONDUCTOR FERROELECTRIC MEMORY TRANSISTOR
[Object] To provide a FeFET and a method of its manufacture, the FeFET having a ferroelectric whose film thickness (dr) is made small and so nanofine as to range in: 59 nm<dr<150, without impairing the data retention property of not less than 10.sup.5 seconds and the data rewrite withstand property of not less than 10.sup.8 times, of those that have hitherto been developed, and the FeFET allowing data to be written with a writing voltage whose absolute value is not more than 3.3 volts.
[Means for Solving] In methods of making a device in which an insulator, a film made of constituent elements of a bismuth layered perovskite crystalline ferroelectric and a metal are sequentially formed in the indicated order on a semiconductor substrate and thereafter are annealed for ferroelectric crystallization, thereby preparing the device composed of the semiconductor, insulator, ferroelectric and metal, a method of making a semiconductor ferroelectric memory element in which the film is composed of Ca. Sr, Bi, Ta and oxygen atoms, the metal is Ir or Pt or an alloy of Ir and Pt, or Ru, and the annealing for ferroelectric crystallization is performed in a mixed gas having oxygen added to nitrogen or a mixed gas having oxygen added to argon.
METHODS FOR FORMING A LAMINATE FILM BY CYCLICAL PLASMA-ENHANCED DEPOSITION PROCESSES
Methods for forming a laminate film on substrate by a plasma-enhanced cyclical deposition process are provided. The methods may include: providing a substrate into a reaction chamber, and depositing on substrate a metal oxide laminate film by alternatingly depositing a first metal oxide film and a second metal oxide film different from the first metal oxide film, wherein depositing the first metal oxide film and the second metal oxide film comprises, contacting the substrate with sequential and alternating pulses of a metal precursor and an oxygen reactive species generated by applying RF power to a reactant gas comprising at least nitrous oxide (N.sub.2O).
METHOD OF MANUFACTURING SEMICONDUCTOR DEVICE AND FILM FORMING APPARATUS
A method of manufacturing a semiconductor includes adjusting a temperature of a substrate having a recess formed therein and accommodated in a container to a temperature within a range of 200 degrees C. or higher and 280 degrees or lower, and laminating a polyurea film in the recess in the substrate by supplying isocyanate gas and amine gas into the container.
Sonos stack with split nitride memory layer
A semiconductor device and method of manufacturing the same are provided. In one embodiment, method includes forming a first oxide layer over a substrate, forming a silicon-rich, oxygen-rich, oxynitride layer on the first oxide layer, forming a silicon-rich, nitrogen-rich, and oxygen-lean nitride layer over the oxynitride layer, and forming a second oxide layer on the nitride layer. Generally, the nitride layer includes a majority of charge traps distributed in the oxynitride layer and the nitride layer. Optionally, the method further includes forming a middle oxide layer between the oxynitride layer and the nitride layer. Other embodiments are also described.
Conformal low temperature hermetic dielectric diffusion barriers
Conformal hermetic dielectric films suitable as dielectric diffusion barriers over 3D topography. In embodiments, the dielectric diffusion barrier includes a dielectric layer, such as a metal oxide, which can be deposited by atomic layer deposition (ALD) techniques with a conformality and density greater than can be achieved in a conventional silicon dioxide-based film deposited by a PECVD process for a thinner contiguous hermetic diffusion barrier. In further embodiments, the diffusion barrier is a multi-layered film including a high-k dielectric layer and a low-k or intermediate-k dielectric layer (e.g., a bi-layer) to reduce the dielectric constant of the diffusion barrier. In other embodiments a silicate of a high-k dielectric layer (e.g., a metal silicate) is formed to lower the k-value of the diffusion barrier by adjusting the silicon content of the silicate while maintaining high film conformality and density.