Patent classifications
H01L2224/81211
SOLDER REFLOW APPARATUS AND METHOD OF MANUFACTURING AN ELECTRONIC DEVICE
A method of manufacturing an electronic device includes: providing a vapor generating chamber that accommodates a heat transfer fluid; providing a substrate stage within the vapor generating chamber, the substrate stage including a seating surface and suction passages penetrating the substrate stage to be open to the seating surface; loading a substrate on the substrate stage, wherein electronic components are disposed on the substrate via bumps; generating at least a partial vacuum in the suction holes to suction-support the substrate on the seating surface; heating the heat transfer fluid to generate saturated vapor within the vapor generating chamber; and soldering the bumps using the saturated vapor.
STRUCTURES TO ENABLE A FULL INTERMETALLIC INTERCONNECT
A method forming an interconnect structure includes depositing a first solder bump on a chip; depositing a second solder bump on a laminate, the second solder bump including a nickel copper colloid surrounded by a nickel or copper shell and suspended in a tin-based solder; aligning the chip with the laminate; performing a first reflow process to join the chip to the laminate; depositing an underfill material around the first solder bump and the second solder bump; and performing a second reflow process at a temperature that is lower than the first reflow process to convert the first solder bump and the second solder bump to an all intermetallic interconnect; wherein depositing the underfill material is performed before or after performing the second reflow process.
STRUCTURES AND METHODS TO ENABLE A FULL INTERMETALLIC INTERCONNECT
A method forming an interconnect structure includes depositing a first solder bump on a chip; depositing a second solder bump on a laminate, the second solder bump including a nickel copper colloid surrounded by a nickel or copper shell and suspended in a tin-based solder; aligning the chip with the laminate; performing a first reflow process to join the chip to the laminate; depositing an underfill material around the first solder bump and the second solder bump; and performing a second reflow process at a temperature that is lower than the first reflow process to convert the first solder bump and the second solder bump to an all intermetallic interconnect; wherein depositing the underfill material is performed before or after performing the second reflow process.
Electrical apparatus
An electrical apparatus includes a first electrical component; a second electrical component; and an InSnAg alloy connecting the first electrical component and the second electrical component, the InSnAg alloy containing AgIn.sub.2 and Ag.sub.2In, a Ag.sub.2In content being lower than a AgIn.sub.2 content.
Semiconductor device having connection terminal of solder
A method of manufacturing a semiconductor device includes forming a barrier metal film on a surface of at least one of a first electrode of a wiring board and a second electrode of a semiconductor element, providing a connection terminal between the first and second electrodes, the connection terminal being made of solder containing tin, bismuth and zinc, and bonding the connection terminal to the barrier metal film by heating the connection terminal and maintaining the temperature of the connection terminal at a constant temperature not lower than a melting point of the solder for a certain period of time.
Semiconductor die assembly
A semiconductor die assembly having a solderball wirebonded to a substrate. As an example, the semiconductor die assembly may include the solderball attached to a bond pad on a face surface of a memory die. A non-face surface of the memory die can be attached to the substrate. A wire can be wirebonded to the solderball at a first end of the wire and connected to the substrate at a second end of the wire.
LOW COST PACKAGE WARPAGE SOLUTION
Embodiments of the invention include device packages and methods of forming such packages. In an embodiment, the method of forming a device package may comprise forming a reinforcement layer over a substrate. One or more openings may be formed through the reinforcement layer. In an embodiment, a device die may be placed into one of the openings. The device die may be bonded to the substrate by reflowing one or more solder bumps positioned between the device die and the substrate. Embodiments of the invention may include a molded reinforcement layer. Alternative embodiments include a reinforcement layer that is adhered to the surface of the substrate with an adhesive layer.
FLIP CHIP BONDING ALLOYS
A method of bonding a plurality of die having first and second metal layers on a die surface to a board, comprising placing a first die onto a board comprising one of a ceramic or substrate board or metal lead frame having a solderable surface and placing the first die and the board into a reflow oven. The method includes reflowing at a first reflow temperature for a first period until the first metal board layer and at least one of the first and second metal die layers of the first die form an alloy to adhere the first die to the board. The newly formed alloy has a higher melting temperature than the first reflow temperature. Accordingly, additional die may be reflowed and attached to the board without causing the bonding of the first die to the board to fail if the same reflow temperature is used.
Apparatus and method for wafer oxide removal and reflow treatment
The present invention relates to an apparatus and method for wafer oxide removal and reflow treatment. In particular, the present invention relates to an apparatus for wafer oxide removal and reflow treatment, comprising: a heating plate, a sample plate for supporting a wafer sample above the heating plate, and an electron attachment pin plate above the sample plate, wherein the heating plate is configured to be capable of moving up and down, and contacting and heating the sample plate.