Patent classifications
H01L21/02562
Core-shell nanoplatelets and uses thereof
Disclosed is a formulation of semiconductor nanoplatelets, including at least one nanoplatelet including a nanoplatelet core and a shell on the surface of the nanoplatelet core, wherein the formulation is substantially free of molecular oxygen and/or molecular water, and uses thereof.
HETEROJUNCTION METERIAL AND METHOD OF PREPARING THE SAME
A method of preparing a heterojunction material, includes forming a first transition metal on a substrate, forming a second transition metal on the first transition metal, and performing a plasma process containing a chalcogen source on the substrate. The first transition metal and the second transition metal are different from each other.
USING A COMPLIANT LAYER TO ELIMINATE BUMP BONDING
Methods, systems, and apparatuses are described for a CMOS compatible substrate having multiple stacks of semiconductor layers. The multiple stacks, at least, each include i) a layer of a tellurium based semiconductor layer on top of ii) a porous silicon layer. The porous silicon layer is a compliant layer to accept structural defects from the tellurium based semiconductor layer into the porous silicon layer. The multiple stacks are grown on the CMOS compatible substrate.
Photonic curing of nanocrystal films for photovoltaics
Methods of making a semiconductor layer from nanocrystals are disclosed. A film of nanocrystals capped with a ligand can be deposited onto a substrate; and the nanocrystals can be irradiated with one or more pulses of light. The pulsed light can be used to substantially remove the ligands from the nanocrystals and leave the nanocrystals unsintered or sintered, thereby providing a semiconductor layer. Layered structures comprising these semiconductor layers with an electrode are also disclosed. Devices comprising such layered structures are also disclosed.
SYNTHESIS AND USE OF PRECURSORS FOR ALD OF TELLURIUM AND SELENIUM THIN FILMS
Atomic layer deposition (ALD) processes for forming Te-containing thin films, such as Sb—Te, Ge—Te, Ge—Sb—Te, Bi—Te, and Zn—Te thin films are provided. ALD processes are also provided for forming Se—containing thin films, such as Sb—Se, Ge—Se, Ge—Sb—Se, Bi—Se, and Zn—Se thin films are also provided. Te and Se precursors of the formula (Te,Se)(SiR.sup.1R.sup.2R.sup.3).sub.2 are preferably used, wherein R.sup.1, R.sup.2, and R.sup.3 are alkyl groups. Methods are also provided for synthesizing these Te and Se precursors. Methods are also provided for using the Te and Se thin films in phase change memory devices.
OPTIMIZED THICK HETEROEPITAXIAL GROWTH OF SEMICONDUCTORS WITH IN-SITU SUBSTRATE PRETREATMENT
A method of performing HVPE heteroepitaxy comprises exposing a substrate to a carrier gas, a first precursor gas, a Group II/III element, and ternary-forming gasses (V/VI group precursor), to form a heteroepitaxial growth of a binary, ternary, and/or quaternary compound on the substrate; wherein the carrier gas is H.sub.2, wherein the first precursor gas is HCl, the Group II/III element comprises at least one of Zn, Cd, Hg, Al, Ga, and In; and wherein the ternary-forming gasses comprise at least two or more of AsH.sub.3 (arsine), PH.sub.3 (phosphine), H.sub.2Se (hydrogen selenide), H.sub.2Te (hydrogen telluride), SbH.sub.3 (hydrogen antimonide, or antimony tri-hydride, or stibine), H.sub.2S (hydrogen sulfide), NH.sub.3 (ammonia), and HF (hydrogen fluoride); flowing the carrier gas over the Group II/III element; exposing the substrate to the ternary-forming gasses in a predetermined ratio of first ternary-forming gas to second ternary-forming gas (1tf:2tf ratio); and changing the 1tf:2tf ratio over time.
Optimized Heteroepitaxial Growth of Semiconductors
A method of performing HVPE heteroepitaxy comprises exposing a substrate to a carrier gas, a first precursor gas, a Group II/III element, and ternary-forming gasses (V/VI group precursor), to form a heteroepitaxial growth of a binary, ternary, and/or quaternary compound on the substrate; wherein the carrier gas is H.sub.2, wherein the first precursor gas is HCl, the Group II/III element comprises at least one of Zn, Cd, Hg, Al, Ga, and In; and wherein the ternary-forming gasses comprise at least two or more of AsH.sub.3 (arsine), PH.sub.3 (phosphine), H.sub.2Se (hydrogen selenide), H.sub.2Te (hydrogen telluride), SbH.sub.3 (hydrogen antimonide, or antimony tri-hydride, or stibine), H.sub.2S (hydrogen sulfide), NH.sub.3 (ammonia), and HF (hydrogen fluoride); flowing the carrier gas over the Group II/III element; exposing the substrate to the ternary-forming gasses in a predetermined ratio of first ternary-forming gas to second ternary-forming gas (1tf:2tf ratio); and changing the 1tf:2tf ratio over time.
Optimized Heteroepitaxial Growth of Semiconductors
A method of performing HVPE heteroepitaxy comprises exposing a substrate to a carrier gas, a first precursor gas, a Group II/III element, and ternary-forming gasses (V/VI group precursor), to form a heteroepitaxial growth of a binary, ternary, and/or quaternary compound on the substrate; wherein the carrier gas is Hz, wherein the first precursor gas is HCl, the Group II/III element comprises at least one of Zn, Cd, Hg, Al, Ga, and In; and wherein the ternary-forming gasses comprise at least two or more of AsH.sub.3 (arsine), PH.sub.3 (phosphine), H.sub.2Se (hydrogen selenide), H.sub.2Te (hydrogen telluride), SbH.sub.3 (hydrogen antimonide, or antimony tri-hydride, or stibine), H.sub.2S (hydrogen sulfide), NH.sub.3 (ammonia), and HF (hydrogen fluoride); flowing the carrier gas over the Group II/III element; exposing the substrate to the ternary-forming gasses in a predetermined ratio of first ternary-forming gas to second ternary-forming gas (1tf:2tf ratio); and changing the 1tf:2tf ratio over time.
Optimized Heteroepitaxial Growth of Semiconductors
A method of performing HVPE heteroepitaxy comprises exposing a substrate to a carrier gas, a first precursor gas, a Group II/III element, and ternary-forming gasses (V/VI group precursor), to form a heteroepitaxial growth of a binary, ternary, and/or quaternary compound on the substrate; wherein the carrier gas is H.sub.2, wherein the first precursor gas is HCl, the Group II/III element comprises at least one of Zn, Cd, Hg, Al, Ga, and In; and wherein the ternary-forming gasses comprise at least two or more of AsH.sub.3 (arsine), PH.sub.3 (phosphine), H.sub.2Se (hydrogen selenide), H.sub.2Te (hydrogen telluride), SbH.sub.3 (hydrogen antimonide, or antimony tri-hydride, or stibine), H.sub.2S (hydrogen sulfide), NH.sub.3 (ammonia), and HF (hydrogen fluoride); flowing the carrier gas over the Group II/III element; exposing the substrate to the ternary-forming gasses in a predetermined ratio of first ternary-forming gas to second ternary-forming gas (1tf:2tf ratio); and changing the 1tf:2tf ratio over time.
Optimized Heteroepitaxial Growth of Semiconductors
A method of performing heteroepitaxy comprises exposing a substrate to a carrier gas, a first precursor gas, a Group II/III element, and a second precursor gas, to form a heteroepitaxial growth of one of GaAs, AlAs, InAs, GaP, InP, ZnSe, GaSe, CdSe, InSe, ZnTe, CdTe, GaTe, HgTe, GaSb, InSb, AlSb, CdS, GaN, and AlN on the substrate; wherein the substrate comprises one of GaAs, AlAs, InAs, GaP, InP, ZnSe, GaSe, CdSe, InSe, ZnTe, CdTe, GaTe, HgTe, GaSb, InSb, AlSb, CdS, GaN, and AlN; wherein the carrier gas is H.sub.2, wherein the first precursor is HCl, the Group II/III element comprises at least one of Zn, Cd, Hg, Al, Ga, and In; and wherein the second precursor is one of AsH.sub.3 (arsine), PH.sub.3 (phosphine), H.sub.2Se (hydrogen selenide), H.sub.2Te (hydrogen telluride), SbH.sub.3 (hydrogen antimonide), H.sub.2S (hydrogen sulfide), and NH.sub.3 (ammonia). The process may be an HVPE (hydride vapor phase epitaxy) process.