H01L21/76862
Doping of metal barrier layers
Described are methods for doping barrier layers such as tantalum (Ta), tantalum nitride (TaN), tantalum carbide (TaC), niobium (Nb), niobium nitride (NbN), manganese (Mn), manganese nitride (MnN), titanium (Ti), titanium nitride (TiN), molybdenum (Mo), and molybdenum nitride (MoN), and the like. Dopants may include one or more of one or more of ruthenium (Ru), manganese (Mn), niobium (Nb), cobalt (Co), vanadium (V), copper (Cu), aluminum (Al), carbon (C), oxygen (O), silicon (Si), molybdenum (Mo), and the like. The doped barrier layer provides improved adhesion at a thickness of less than about 15 Å.
Methods Of Etching Metals In Semiconductor Devices
A semiconductor structure includes a conductive feature disposed over a semiconductor substrate, a via disposed in a first interlayer dielectric (ILD) layer over the conductive feature, and a metal-containing etch-stop layer (ESL) disposed on the via, where the metal-containing ESL includes a first metal and is resistant to etching by a fluorine-containing etchant. The semiconductor structure further includes a conductive line disposed over the metal-containing ESL, where the conductive line includes a second metal different from the first metal and is etchable by the fluorine-containing etchant, and where the via is configured to interconnect the conductive line to the conductive feature. Furthermore, the semiconductor structure includes a second ILD layer disposed over the first ILD layer.
Methods of etching metals in semiconductor devices
A semiconductor structure includes a conductive feature disposed over a semiconductor substrate, a via disposed in a first interlayer dielectric (ILD) layer over the conductive feature, and a metal-containing etch-stop layer (ESL) disposed on the via, where the metal-containing ESL includes a first metal and is resistant to etching by a fluorine-containing etchant. The semiconductor structure further includes a conductive line disposed over the metal-containing ESL, where the conductive line includes a second metal different from the first metal and is etchable by the fluorine-containing etchant, and where the via is configured to interconnect the conductive line to the conductive feature. Furthermore, the semiconductor structure includes a second ILD layer disposed over the first ILD layer.
Method and structure for barrier-less plug
A method includes receiving a structure having a dielectric layer over a conductive feature; etching a hole through the dielectric layer and exposing the conductive feature; depositing a first metal into the hole and in direct contact with the dielectric layer and the conductive feature; depositing a second metal over the first metal; and annealing the structure including the first and the second metals.
Method of forming an interconnect in a semiconductor device
A method of forming a semiconductor device includes patterning a dielectric layer to form a groove and depositing a plurality of conductive layers over the dielectric layer and in the groove. The first conductive layer is a liner layer, the second conductive layer is a metal film, and the third conductive layer is a capping layer. The first conductive layer is treated with a hydrogen plasma treatment to remove impurities. The first conductive layer is also treated with a hydrogen soak treatment to remove microvoids. The third conductive layer is treated with an ammonia plasma treatment to remove impurities. The third conductive layer is also treated with a hydrogen plasma treatment to remove additional impurities. The third conductive layer is also treated with a hydrogen soak treatment to remove microvoids.
Dielectric damage-free dual damascene Cu interconnects without barrier at via bottom
Techniques for dielectric damage-free interconnects are provided. In one aspect, a method for forming a Cu interconnect structure includes: forming a via and trench in a dielectric over a metal line M1; depositing a first barrier layer into the via and trench; removing the first barrier layer from the via and trench bottoms using neutral beam oxidation, and removing oxidized portions of the first barrier layer such that the first barrier layer remains along only sidewalls of the via and trench; depositing Cu into the via in direct contact with the metal line M1 to form a via V1; lining the trench with a second barrier layer; and depositing Cu into the trench to form a metal line M2. The second barrier layer can instead include Mn or optionally CuMn so as to further serve as a seed layer. A Cu interconnect structure is also provided.
Gap fill deposition process
Methods for forming an interconnections structure on a substrate in a cluster processing system and thermal processing such interconnections structure are provided. In one embodiment, a method for a device structure for semiconductor devices includes forming a barrier layer in an opening formed in a material layer disposed on a substrate, forming an interface layer on the barrier layer, forming a gap filling layer on the interface layer, and performing an annealing process on the substrate, wherein the annealing process is performed at a pressure range greater than 5 bar.
ULTRAVIOLET RADIATION ACTIVATED ATOMIC LAYER DEPOSITION
The present disclosure relates to a method of fabricating a semiconductor structure, the method includes forming an opening and depositing a metal layer in the opening. The depositing includes performing one or more deposition cycles, wherein each deposition cycle includes flowing a first precursor into a deposition chamber and performing an ultraviolet (UV) radiation process on the first precursor. The method further includes performing a first purging process in the deposition chamber to remove at least a portion of the first precursor, flowing a second precursor into the deposition chamber, and purging the deposition chamber to remove at least a portion of the second precursor.
SEMICONDUCTOR DEVICE AND FORMATION METHOD THEREOF
A semiconductor device includes a fin structure, a source/drain region, a first inter-layer dielectric (ILD) layer, a first contact plug, and a second contact plug. The fin structure extends above a substrate. The source/drain region is in the fin structure. The first ILD layer is over the source/drain region. The first contact plug extends through the first ILD layer to a silicide region of the source/drain region. The second contact plug is over the first contact plug. The first contact plug has a protruding portion extending above the first ILD layer and laterally surrounding a lower part of the second contact plug.
Enhanced cobalt agglomeration resistance and gap-fill performance by ruthenium doping
In one implementation, a method of forming a cobalt layer on a substrate is provided. The method comprises forming a barrier and/or liner layer on a substrate having a feature definition formed in a first surface of the substrate, wherein the barrier and/or liner layer is formed on a sidewall and bottom surface of the feature definition. The method further comprises exposing the substrate to a ruthenium precursor to form a ruthenium-containing layer on the barrier and/or liner layer. The method further comprises exposing the substrate to a cobalt precursor to form a cobalt seed layer atop the ruthenium-containing layer. The method further comprises forming a bulk cobalt layer on the cobalt seed layer to fill the feature definition.