B22D11/11
Method for continuously casting slab containing titanium or titanium alloy
The present invention provides a method for casting a slab having a good cast surface. The method includes heating the surface of molten metal on a metal inlet side of a mold by a first heat source so that the following formulas: q0.87 and c11.762q+0.3095 are satisfied where c is a cycle time [sec] of turning movement of the first heat source, and q is an average amount of heat input [MW/m.sup.2] determined by accumulating an amount of heat input applied by at least the first heat source to the contact region between the upper surface of the slab on the metal inlet side and the mold, along the path of turning movement of the first heat source, and dividing the resultant accumulated value by the cycle time c.
Method for continuously casting slab containing titanium or titanium alloy
The present invention provides a method for casting a slab having a good cast surface. The method includes heating the surface of molten metal on a metal inlet side of a mold by a first heat source so that the following formulas: q0.87 and c11.762q+0.3095 are satisfied where c is a cycle time [sec] of turning movement of the first heat source, and q is an average amount of heat input [MW/m.sup.2] determined by accumulating an amount of heat input applied by at least the first heat source to the contact region between the upper surface of the slab on the metal inlet side and the mold, along the path of turning movement of the first heat source, and dividing the resultant accumulated value by the cycle time c.
Continuous casting method
In a continuous casting apparatus 100 for casting a stainless steel billet 3c, a long nozzle 2 extending into a tundish 101 is provided at a ladle 1 for pouring a molten stainless steel 3 in the ladle 1 into the tundish 101. Further, a nitrogen gas 4 is supplied as a seal gas around the molten stainless steel 3 in the tundish 101, and continuous casting of the stainless steel billet 3c is performed, in which, while immersing the spout 2a of the long nozzle 2 into the molten stainless steel 3 in the tundish 101, the molten stainless steel 3 is poured through the long nozzle 2 into the tundish 101 and the molten stainless steel 3 in the tundish 101 is poured into a casting mold 105.
Continuous casting method
In a continuous casting apparatus 100 for casting a stainless steel billet 3c, a long nozzle 2 extending into a tundish 101 is provided at a ladle 1 for pouring a molten stainless steel 3 in the ladle 1 into the tundish 101. Further, a nitrogen gas 4 is supplied as a seal gas around the molten stainless steel 3 in the tundish 101, and continuous casting of the stainless steel billet 3c is performed, in which, while immersing the spout 2a of the long nozzle 2 into the molten stainless steel 3 in the tundish 101, the molten stainless steel 3 is poured through the long nozzle 2 into the tundish 101 and the molten stainless steel 3 in the tundish 101 is poured into a casting mold 105.
Continuous casting process of metal
A continuous casting process of a steel semi-product is provided. The process includes a step of casting using a hollow jet nozzle located between a tundish and a continuous casting mould. The nozzle includes, in its upper part, a dome for deflecting the liquid metal arriving at the inlet of the nozzle towards the internal wall of the nozzle, defining an internal volume with no liquid metal. A simultaneous step of injecting powder through a hole of the dome occurs. The powder has a particle size of 200 m or less. The dome includes a first device to inject the powder without any contact with the dome and a second device to avoid sticking or sintering of the powder onto the first device.
Continuous casting process of metal
A continuous casting process of a steel semi-product is provided. The process includes a step of casting using a hollow jet nozzle located between a tundish and a continuous casting mould. The nozzle includes, in its upper part, a dome for deflecting the liquid metal arriving at the inlet of the nozzle towards the internal wall of the nozzle, defining an internal volume with no liquid metal. A simultaneous step of injecting powder through a hole of the dome occurs. The powder has a particle size of 200 m or less. The dome includes a first device to inject the powder without any contact with the dome and a second device to avoid sticking or sintering of the powder onto the first device.
METAL MOLDED BODY MANUFACTURING APPARATUS BY ELECTROMAGNETIC STIRRING
There is provided a metal molded body manufacturing apparatus for electromagnetically stirring metallic molten metal and molding a metal molded body. The metal molded body manufacturing apparatus includes: a die having an inclined side wall; and a moving magnetic field generation section that stirs the molten metal in the die, wherein the moving magnetic field generation section includes a magnetic body, and a coil wound around the magnetic body as a center, and an end surface of the magnetic body is disposed in parallel to an inner surface of the side wall.
Method for continuously casting slab containing titanium or titanium alloy
The present invention provides a method for casting a slab with good cast surface quality. The method includes pouring molten metal 8 into a mold 2 from one of the paired shorter sides of the mold 2 while allowing superheat T [ C.], which is a temperature difference obtained by subtracting the melting point Tm [ C.] of the raw material from the temperature Tin [ C.] of the molten material on the surface of the molten metal in the mold and at the pouring point of the molten metal, to satisfy the following Formula (1) and Formula (2):
0.0014T.sup.2 +0.0144T+699.45>800 Formula (1)
0.0008T.sup.2 +0.2472T+853.02<1250 Formula (2)
Method for continuously casting slab containing titanium or titanium alloy
The present invention provides a method for casting a slab with good cast surface quality. The method includes pouring molten metal 8 into a mold 2 from one of the paired shorter sides of the mold 2 while allowing superheat T [ C.], which is a temperature difference obtained by subtracting the melting point Tm [ C.] of the raw material from the temperature Tin [ C.] of the molten material on the surface of the molten metal in the mold and at the pouring point of the molten metal, to satisfy the following Formula (1) and Formula (2):
0.0014T.sup.2 +0.0144T+699.45>800 Formula (1)
0.0008T.sup.2 +0.2472T+853.02<1250 Formula (2)
Continuous casting method
In a continuous casting method for casting aluminum-deoxidized molten stainless steel 1 by using a continuous casting apparatus 100 in which a long nozzle 3 extending into a tundish 101 is provided at a ladle 2, the molten stainless steel 1 is poured into the tundish 101 through the long nozzle 3, while the spout 3a of the long nozzle 3 is being immersed in the molten stainless steel 1 that has been poured, and the molten stainless steel 1 in the tundish 101 is poured into a casting mold 105. A TD powder 5 is sprayed so that the powder covers the surface of the molten stainless steel 1 in the tundish 101, and nitrogen gas is supplied around the molten stainless steel 1. A calcium-containing material is added to the molten stainless steel 1 in a state other than a state of retention in the tundish 101.