B29K2033/20

MALEIMIDE-BASED COPOLYMER, METHOD FOR PRODUCING SAME, AND RESIN COMPOSITION OBTAINED USING SAME

The present invention provides a maleimide-based copolymer, a method for producing same, and a resin composition obtained using same.

This maleimide-based copolymer contains 40-60 mass % of aromatic vinyl monomer units, 5-20 mass % of vinyl cyanide monomer units, and 35-50 mass % of maleimide monomer units, and is such that a 4 mass % tetrahydrofuran solution of the copolymer has a transmittance of 90% or more for light having a wavelength of 450 nm at an optical path length of 10 mm, and the residual maleimide-based monomer amount is less than 300 ppm. This maleimide-based copolymer preferably further contains 0-10 mass % of unsaturated dicarboxylic acid anhydride monomer units, and preferably has a glass transition temperature of 165 C. or higher.

FABRICATION OF PURE TRAGACANTH NANOFIBROUS WEBS AND APPLICATIONS THEREOF IN WATER-ABSORBENT FILTERS

A fabrication method for a water-absorbent filter includes obtaining a homogenized tragacanth suspension by dissolving tragacanth in a solvent, where the solvent may include distilled water, ethyl acetate, acetic acid, and formic acid, obtaining a support layer by coating a stainless steel mesh with a thin layer of a hydrophobic polymer, coating a stainless steel mesh with the thin layer of the hydrophobic polymer comprising electrospinning a hydrophobic polymer solution onto the stainless steel mesh, forming a tragacanth nanofibrous web on the support layer by electrospinning the homogenized tragacanth suspension onto the support layer, and cross-linking the tragacanth nanofibrous web by exposing the tragacanth nanofibrous web to a saturated vapor of a cross-linking agent.

FABRICATION OF TRAGACANTHIN-PVA NANOFIBROUS WEBS AND APPLICATIONS THEREOF IN WATER-ABSORBENT FILTERS

A fabrication method for a filter containing tragacanthin-polyvinyl alcohol (PVA) nanofibers includes obtaining a homogenous tragacanthin-PVA solution by obtaining a PVA solution by dissolving PVA in distilled water, and adding tragacanthin to the PVA solution. The method may further include obtaining a support layer by coating a stainless steel mesh with a thin layer of a hydrophobic polymer, coating a stainless steel mesh with the thin layer of the hydrophobic polymer comprising electrospinning a hydrophobic polymer solution onto the stainless steel mesh, and forming a tragacanthin-PVA nanofibrous web on the support layer by electrospinning the homogenous tragacanthin-PVA solution onto the support layer.

Primer compositions for injection molding

Curable compositions, such as by way of exposure to radiation in the electromagnetic spectrum, for use as a primer composition for injection molding applications, are provided.

MASTER BATCH FOR EXPANSION MOLDING AND FOAM MOLDED BODY
20200231763 · 2020-07-23 · ·

The present invention aims to provide a masterbatch for foam molding which can be suitably used in molding involving high shear force or molding requiring low molding temperature and which can provide a foam molded article having a high expansion ratio and good appearance quality. The present invention also aims to provide a foam molded article formed from the masterbatch for foam molding. Provided is a masterbatch for foam molding, containing: a base resin; and a thermally expandable microcapsule, the masterbatch having a true specific gravity of 0.80 g/cm.sup.3 or more, the base resin containing an olefin elastomer, the masterbatch containing the thermally expandable microcapsule in an amount of 40 to 300 parts by weight relative to 100 parts by weight of the base resin.

POLYMERIC FOAM LAYER AND METHODS OF MAKING THE SAME

Polymeric foam layer having a thickness up to 25,700 micrometers, having first and second opposed major surfaces, and comprising foam features extending from or into the first major surface by at least 100 micrometers, and having a T.sub.g in a range from 125 C. to 150 C., wherein the first and second opposed major surfaces are free of exposed internal porous cells (i.e., less than 10 percent of the surface area of each of the first and second major surface has any exposed porous cells) and wherein at least 40 percent by area of each major surface has an as-cured surface; and methods of making the same. Exemplary uses of polymeric foam layers described herein including a finishing pad for silicon wafers and vibration damping.

Latex composition for dip molding, and molded product manufactured therefrom
10717851 · 2020-07-21 · ·

The present invention relates to a latex composition for dip-molding comprising a mixture of latex pigment and carboxylic acid-modified nitrile based copolymer latex which are two types of latex having Tg different to each other, and a dip-molded article produced therefrom. The dip-molded article according to the present invention does not use sulfur and a vulcanization accelerator and thus has a low risk of allergies and can have excellent elasticity, while maintaining the physical properties such as tensile strength and modulus in the trade-off relationship opposite to each other at the levels equal to or higher than those of the prior art, so that the dip-molded article can be easily applied to industries in need thereof, such as industry of rubber gloves, etc.

Glass and polymer film assemblies and methods of making

A glass and polymer film assembly including a glass film and a polymer film bonded to a surface of the glass film. The polymer film is directly bonded to the glass film by applying the polymer to the glass film when the glass film is above a bonding temperature of the polymer film. The glass film may have a thickness less than about 1 mm and the polymer film may be an oriented semicrystalline homopolymer which is permanently bonded to a major surface of the glass film.

Glass and polymer film assemblies and methods of making

A glass and polymer film assembly including a glass film and a polymer film bonded to a surface of the glass film. The polymer film is directly bonded to the glass film by applying the polymer to the glass film when the glass film is above a bonding temperature of the polymer film. The glass film may have a thickness less than about 1 mm and the polymer film may be an oriented semicrystalline homopolymer which is permanently bonded to a major surface of the glass film.

Methods of making plastic-metal junctions via laser

Various embodiments relate to plastic-metal junctions and methods of making the same via laser-assisted joining. The present invention provides a method of forming a junction between a metal form and a solid plastic. The method can include laser treating a surface of a metal form to generate a feature (e.g., a plurality of at least one of pores and grooves) in the surface of the metal, wherein the laser has an angle of incidence with the surface of the metal of other than 0 degrees. The method can include contacting the metal surface including the feature with a flowable resin composition. The method can include curing the flowable resin composition to form the solid plastic, to provide the junction between the metal form and the solid plastic.