H10D30/0212

Method of manufacturing a semiconductor device to prevent occurrence of short-channel characteristics and parasitic capacitance

Occurrence of short-channel characteristics and parasitic capacitance of a MOSFET on a SOI substrate is prevented. A sidewall having a stacked structure obtained by sequentially stacking a silicon oxide film and a nitride film is formed on a side wall of a gate electrode on the SOI substrate. Subsequently, after an epitaxial layer is formed beside the gate electrode, and then, the nitride film is removed. Then, an impurity is implanted into an upper surface of the semiconductor substrate with using the gate electrode and the epitaxial layer as a mask, so that a halo region is formed in only a region of the upper surface of the semiconductor substrate which is right below a vicinity of both ends of the gate electrode.

NiPt AND Ti INTERSECTING SILICIDE PROCESS AND STRUCTURE

A method includes forming a first silicide on a substrate after patterning a gate and spacer onto the substrate. A film is deposited over the substrate. A portion of the dielectric film is removed to expose the first silicide. A portion of the first silicide is removed to form a punch through region. A liner is deposited in the punch through region. A metal layer is deposited on the liner. The substrate is annealed to form a second silicide on the substrate.

Controlled ion implantation into silicon carbide using channeling and devices fabricated using controlled ion implantation into silicon carbide using channeling
09768259 · 2017-09-19 · ·

Methods of forming a semiconductor structure include the use of channeled implants into silicon carbide crystals. Some methods include providing a silicon carbide layer having a crystallographic axis, heating the silicon carbide layer to a temperature of about 300 C. or more, implanting dopant ions into the heated silicon carbide layer at an implant angle between a direction of implantation and the crystallographic axis of less than about 2, and annealing the silicon carbide layer at a time-temperature product of less than about 30,000 C.-hours to activate the implanted ions.

METHOD FOR FABRICATING A METAL HIGH-K GATE STACK FOR A BURIED RECESSED ACCESS DEVICE
20170263458 · 2017-09-14 ·

A method for fabricated a buried recessed access device comprising etching a plurality of gate trenches in a substrate, implanting and activating a source/drain region in the substrate, depositing a dummy gate in each of the plurality of gate trenches, filling the plurality of gate trenches with an oxide layer, removing each dummy gate and depositing a high-K dielectric in the plurality of gate trenches, depositing a metal gate on the high-K dielectric in each of the plurality of gate trenches, depositing a second oxide layer on the metal gate and forming a contact on the source/drain.

SEMICONDUCTOR DEVICE

The present examples relate to a semiconductor device used in an electric device or high voltage device. The present examples improve R.sub.sp by minimizing drift region resistance by satisfying breakdown voltage by improving the structure of a drift region through which current flows in a semiconductor device to provide optimal results. Moreover, a high frequency application achieves useful results by reducing a gate charge Q.sub.g for an identical device pitch to that of an alternative technology.

Performance optimized gate structures having memory device and logic device, the memory device with silicided source/drain regions that are raised with respect to silicided source/drain regions of the logic device

A performance optimized CMOS FET structure and methods of manufacture are disclosed. The method includes forming source and drain regions for a first type device and a second type device. The method further includes lowering the source and drain regions for the first type device, while protecting the source and drain regions for the second type device. The method further includes performing silicide processes to form silicide regions on the lowered source and drain regions for the first type device and the source and drain regions for the second type device.

Method of fabricating semiconductor device with tilted preamorphized implant
09761688 · 2017-09-12 · ·

A method for fabricating a semiconductor device may include: preparing a semiconductor substrate including a doping region; performing tilt implantation using a first additional dopant to form an amorphous region in the doping region; doping a second additional dopant in the amorphous region; forming a metal layer on the doped amorphous region; and reacting the doped amorphous region with the metal layer to form metal silicide.

SEMICONDUCTOR DEVICE AND MANUFACTURING METHOD THEREOF
20170256613 · 2017-09-07 ·

A semiconductor device includes an isolation layer, first and second fin structures, a gate structure and a source/drain structure. The isolation layer is disposed over a substrate. The first and second fin structures are disposed over the substrate, and extend in a first direction in plan view. Upper portions of the first and second fin structures are exposed from the isolation layer. The gate structure is disposed over parts of the first and second fin structures, and extends in a second direction crossing the first direction. The source/drain structure is formed on the upper portions of the first and second fin structures, which are not covered by the first gate structure and exposed from the isolation layer, and wraps side surfaces and a top surface of each of the exposed first and second fin structures. A void is formed between the source/drain structure and the isolation layer.

Source and drain stressors with recessed top surfaces

An integrated circuit structure includes a gate stack over a semiconductor substrate, and a silicon germanium region extending into the semiconductor substrate and adjacent to the gate stack. The silicon germanium region has a top surface, with a center portion of the top surface recessed from edge portions of the top surface to form a recess. The edge portions are on opposite sides of the center portion.

High voltage device fabricated using low-voltage processes

A method for fabricating a high-voltage transistor on a semiconductor substrate includes defining and forming shallow trench isolation regions for all of the transistors, defining and forming well regions for all of the transistors, forming a gate oxide layer in the well regions for all of the transistor, forming gates for all of the transistors over the gate oxide layer, implanting a dopant to form lightly-doped drain regions for all of the transistors, the lightly-doped drain regions for at least drains of the high-voltage transistors being spaced apart from an inner edge of the shallow trench isolation regions, forming gate spacers at sides of the gates of all of the transistors, and implanting a dopant to form sources and drains for all of the transistors, the drains of the high-voltage transistors being formed completely surrounded by the lightly-doped drain regions of the high-voltage transistors.