B29C47/06

Coextrusion feedblock, coextrusion profiling insert assembly, and methods of operation
09808980 · 2017-11-07 · ·

The invention provides a coextrusion feedblock having a flow adjuster, a viscosity compensation device, an actuator, a central extrusion conduit, and a coextrusion conduit. The invention also provides a coextrusion profiling insert assembly constructed to be mounted in a coextrusion feedblock. The insert assembly has a flow adjuster, a viscosity compensation device, and an actuator. The insert assembly when mounted in the feedblock has a coextrusion conduit extending between the flow adjuster and the viscosity compensation device. The actuator is adjustable to apply force to bend the viscosity compensation device and thereby adjust a gap height of the coextrusion conduit. Also provided is a method of operating a feedblock having a viscosity compensation device comprising a flex region, a central extrusion conduit, and a coextrusion conduit. Force is applied to bend the flex region of the viscosity compensation device and thereby adjust a gap height of the coextrusion conduit.

POLYMER COMPOSITIONS, SHRINK FILMS, AND METHODS OF MAKING THEREOF

A polyethylene-based polymer composition suitable for use in a shrink film, the polyethylene-based polymer composition comprising a low density polyethylene having a density of from 0.917 g/cc to 0.935 g/cc and melt index, I.sub.2, of from 0.1 g/10 min to 5 g/10 min, a linear low density polyethylene having a density of from 0.900 g/cc to 0.965 g/cc and melt index, I.sub.2, of from 0.05 g/10 min to 15 g/10 min, or combinations thereof, a material that absorbs radiation in the near-infrared, visible, and ultraviolet spectral wavelength ranges, and optionally, a medium density polyethylene, a high density polyethylene, or combinations thereof.

MULTILAYER TUBE
20170261133 · 2017-09-14 · ·

Provided is a multilayer tube that has a layer containing an aliphatic polyamide (such as Polyamide 11 or Polyamide 12), a layer containing a Polyamide 6 composition or Polyamide 6/66/12 composition, a layer containing a saponified ethylene-vinyl acetate copolymer, and a layer containing a semi-aromatic polyamide composition that contains a semi-aromatic polyamide having a specific structure, and further has a fluorine-containing polymer in which a functional group having reactivity with an amino group is introduced into the molecular chain thereof.

COEXTRUSION ADAPTER
20170259483 · 2017-09-14 ·

A coextrusion adapter, including a central conduit having an inlet end and an outlet end and having bottom and top walls that define the height of the central conduit and side walls that define the width of the central conduit, as well as at least one coextrusion conduit having an inlet end and an outlet end. The outlet end feeds into the central conduit near or in the vicinity of the bottom and/or top wall thereof, downstream of the inlet end of the central conduit, and adjusting devices are provided, which are allocated to each outlet end of the at least one coextrusion conduit and are composed of a plurality of adjusting elements, which collectively extend across the width of the outlet end and by actuating drives, are adjustable independently of one another so that it is possible to change the inner width of the respective width section of the outlet end. Adjacent to the outlet end at least one of the side walls has a receiving bore into which it is possible to insert a displacing element that protrudes beyond the side wall into the central conduit.

Printing Utilizing A Virtual Mask
20170259500 · 2017-09-14 ·

A method and apparatus for printing on an article are disclosed. An embodiment of a method may include the generation of a virtual mask that can designate areas for printing and/or designate areas to exclude from printing. A method may include utilization of the virtual mask during either 2D or 3D printing such that a print design is printed in areas designated for printing by the virtual mask.

APPARATUS FOR PERFORMING THREE-DIMENSIONAL PRINTING
20170259482 · 2017-09-14 ·

A three-dimensional (3D) printer is disclosed. The 3D printer can print viscous material such as plastisol, polymer clay, melted sugar and melted chocolate. The 3D printer utilizes an extruder that can prevent dripping of viscous material from a nozzle. The 3D printer includes a control circuit for controlling the movement of the extruder and the air flow within a pneumatic system.

FACE FILMS AND PRESSURE SENSITIVE LAMINATES FOR PRINTING
20170259604 · 2017-09-14 ·

Microporous structures in face films are described for improving printability of the films. Also described are laminates and pressure sensitive adhesive laminates including the microporous structured face films. Various related methods are additionally described.

POLYOLEFIN-BASED ELASTIC FILM STRUCTURES, LAMINATES AND METHODS THEREOF

A stretch-modified elastomeric multilayer film comprising a core layer comprising a first ethylene-α-olefin block copolymer, wherein the first ethylene-α-olefin block copolymer comprises at least 50 mol. % ethylene, has a melt index (12) from 0.5 g/10 min to 5 g/10 min, and has a density of 0.850 g/cc to 0.890 g/cc, and at least one outer layer independently comprising a second ethylene-α-olefin block copolymer and from 2.5 to 30 wt. % of an antiblock agent, wherein the second ethylene-α-olefin block copolymer comprises at least 50 mol. % ethylene, has a melt index (12) from 0.5 g/10 min to 25 g/10 min, and has a density of 0.850 g/cc to 0.890 g/cc, wherein the density of the first ethylene-α-olefin block copolymer is equal to or greater than the density of the second ethylene-α-olefin block copolymer.

OPTICAL FILM
20170254925 · 2017-09-07 · ·

An optical film including an olefin resin layer that contains a cyclic olefin polymer and an ester compound. The ratio of the ester compound in the olefin resin layer is 0.1% by weight to 10% by weight. An average light absorbance of the optical film in a wavelength range of 9 μm to 11 μm is 0.1% or more.

OPTICAL FILM, SHAPING FILM, METHOD FOR MANUFACTURING OPTICAL FILM, AND METHOD FOR MANUFACTURING STRETCHED FILM
20170254937 · 2017-09-07 · ·

The present invention provides an optical film containing an additive. The optical film includes a high concentration portion containing the additive, and a low concentration portion containing the additive at a concentration lower than the high concentration portion. The low concentration portion is provided on both sides of the high concentration portion in a thickness direction of the optical film, and the low concentration portion is provided on both sides of the high concentration portion in a width direction of the optical film.