B29C48/2565

QUICK-CHANGE FUSED FILAMENT FABRICATION NOZZLE ASSEMBLY
20190375141 · 2019-12-12 · ·

The present invention provides a system and method for quickly removing and installing a filament tube and nozzle in an FFF extrusion system. The system utilizes a primary manifold that includes a cooling block, a heating block and a quick-change mechanism. This primary manifold is adapted to mate a filament tube/nozzle assembly. The quick-change mechanism, which in a particular embodiment utilizes a recessed biased-bearing arrangement, enables the filament/nozzle assembly to be removed and inserted without the use of any tools, and without causing any significant downtime for the FFF extrusion system. Once removed, the filament tube/nozzle assembly can be refurbished by a technician, trained so as not to over torque the tube/nozzle threaded interface. This refurbishment (typically consisting of a cleaning and the installation of a new nozzle) could be accomplished off-line, without any impact on the continued use of FFF extrusion system.

Single and twin screw extruders with ultrasound horns for decrosslinking and devulcanization
10465059 · 2019-11-05 · ·

Processes for decrosslinking crosslinked plastic and devulcanizing vulcanized rubber include advancing such materials through single screw or twin screw extruders including special ultrasonic treatment zones wherein threadless shaft (single screw) or shafts (twin screw) rotate under an ultrasonic horn having a distal end aligned with the shaft or shafts and being shaped complimentary thereto. Special arcuate (single screw) or double-arcuate ultrasonic treatment flow paths confine the materials to flow under the horn where the material is subjected to ultrasonic waves to decrosslink the material, in the case of crosslinked plastic, or devulcanize the material, in the case of vulcanized rubber, with the extrudate leaving the die as a continuous stream or rope as is typical of virgin plastic or rubber.

Liner-type barrel

A barrel main body, a sleeve, and a fixing mechanism (a fastening hole and a fastening device) are provided. The barrel main body includes a barrel hole having a cylindrical shape and a slit dividing an inner circumferential surface of the barrel hole. The sleeve having a hollow cylindrical shape is removably incorporated into the barrel hole. The slit includes two cutout surfaces facing each other with a space between. The fixing mechanism brings the inner circumferential surface of the barrel hole into close contact with the sleeve without any gap by narrowing the space between the cutout surfaces and deforming the barrel main body.

Planetary Roller Extruder with Improved Cooling During the Extrusion of Melts
20190263044 · 2019-08-29 · ·

The disclosure relates to various measures for increasing the cooling effect on a planetary roller extruder section/module. Those measures include a choke being arranged at an outlet of the planetary roller extruder section or module, a distance between centerlines of adjacent planetary spindles being at least equal to an outer diameter of the planetary spindles, providing a pressurized melt supply, having a cooling section composed of several sections/modules, providing at least one section/module in which a flow, during melt supply is converse to the conveying direction of the extruder, and providing cooling tubes arranged within the central spindle.

Barrel assembly and method of setting up an extrusion system utilizing the barrel assembly

A barrel assembly through which flowable material is delivered to a die assembly through which the flowable material is delivered to form a sheet layer. The barrel assembly has: a conduit having a body with a length defining a lengthwise flow passage between upstream and downstream ends; and a support assembly for the conduit. The support assembly has: a) a conduit engaging assembly; and b) a guide assembly through which the conduit body and conduit engaging assembly are moved guidingly relative to a base, to which the guide assembly is mounted, in a path that is substantially parallel to the length of the conduit body.

BARREL BLOCK FOR TWIN-SCREW EXTRUDER AND TWIN-SCREW EXTRUDER
20190202086 · 2019-07-04 · ·

A barrel block for a twin-screw extruder constitutes a barrel including a cylinder and has joints at both ends. A first joint includes a first inner joint face on a peripheral edge of a first hole of an insertion hole for screws, and includes a first flank face and a first outer joint face on an outer periphery of the first inner joint face. The first outer joint face is located in the outer periphery of a plurality of first bolt holes. The first outer joint face is more recessed toward a second block end face than the first inner joint face.

METHOD FOR PRODUCING A THERMOPLASTIC MOULDING COMPOUND
20190193302 · 2019-06-27 ·

A method for producing a thermoplastic moulding compound by means of an extruder (10), which comprises at least one feed zone (20), at least one mixing section (30), at least one venting section (40) and at least one discharge zone (50), wherein in the at least one feed zone (20) a water-containing first component and a second component are supplied, in the at least one mixing section (30) the thermoplastic moulding compound is mixed and contained water is evaporated, in the at least one venting section (40) water vapour is removed from the moulding compound and in the at least one discharge zone (50) the moulding compound is discharged. At least one of the mixing housings (31, 32) is kept at a temperature that is equal to or lower than the temperature of the moulding compound within the mixing section (30).

SCREW MACHINE AND METHOD FOR THE PROCESSING OF MATERIAL TO BE PROCESSED
20180326646 · 2018-11-15 ·

A screw machine includes an inductive heating device for processing of material to be processed. The inductive heating device is used to heat the material in a heating zone. In the heating zone, at least one housing portion is made of an electromagnetically transparent material at least partly, the material being non-magnetic and electrically non-conductive, whereas at least one treatment element shaft is made of an electrically conductive material at least partly. The inductive heating device includes at least one coil formed integrally with a component of the at least one housing portion, in particular in such a way as to form a hybrid component. During the processing of the material, the inductive heating device generates an alternating magnetic field that produces eddy current losses in the at least one treatment element shaft, the eddy current losses leading to a temperature increase of the at least one treatment element shaft.

Integrated single and twin screw extruder

An extruder is disclosed, and more particularly, to an integrated single screw extruder and a twin screw extruder for mixing, compounding, kneading and/or extruding of materials. The integrated extruder includes a first barrel assembly and a second barrel assembly. The integrated extruder further includes a first screw having a first threaded portion and a second threaded portion. The first threaded portion is housed within the first barrel assembly and is configured to provide upstream material processing. The second threaded portion is housed within the second barrel assembly and is configured to provide downstream material processing. The integrated extruder further includes a second screw having a non-threaded shaft portion and a threaded portion. The threaded portion of the second screw is housed within the second barrel assembly and is configured to provide the downstream material processing with the second threaded portion of the first screw.

Device and method for the homogenisation of plastics material melts
10093034 · 2018-10-09 · ·

A device, to homogenise plastics material melts, has a homogenising element with a plurality of flow channels, which differ with respect to at least one feature from the group length, cross sectional area and cross sectional shape. When flowing through the homogenising element, the plastics material melt is divided into a plurality of part streams, which, in each case, flow through an associated flow channel. When leaving the respective flow channel the part streams have different flow speeds so the plastics material melt is expanded and sheared on transition to a uniform flow. As a result, a homogenisation of the plastics material melt takes place in a simple, efficient and effective manner.