B22F3/1025
SUPERALLOY POWDER, PART AND METHOD FOR MANUFACTURING THE PART FROM THE POWDER
A nickel-based superalloy powder comprising, by mass percent, 14.00 to 15.25% chromium, 14.25 to 15.75% cobalt, 3.9 to 4.5% molybdenum, 4.0 to 4.6% aluminum, 3.0 to 3.7% titanium, 0 to 200 ppm carbon, the remainder consisting of nickel and unavoidable impurities. Component made from the powder and manufacturing process of the component.
Polymer ammunition having an overmolded primer insert
One embodiment of the present invention provides a polymeric ammunition cartridge and methods of making and using the same. The cartridge includes a substantially cylindrical insert connected to a substantially cylindrical polymeric middle body. The substantially cylindrical insert includes a top surface opposite a bottom surface and a substantially cylindrical coupling element that extends from the bottom surface, a primer recess in the top surface that extends toward the bottom surface, a primer flash hole positioned in the primer recess to extend through the bottom surface, and a flange that extends circumferentially about an outer edge of the top surface. The substantially cylindrical polymeric middle body includes a substantially cylindrical polymeric bullet-end and a substantially cylindrical polymeric coupling end connected by a powder chamber, wherein the substantially cylindrical polymeric coupling end extends over the substantially cylindrical coupling element and covers a circumferential surface of the primer flash hole.
Polymer ammunition having an overmolded primer insert
One embodiment of the present invention provides a polymeric ammunition cartridge and methods of making and using the same. The cartridge includes a substantially cylindrical insert connected to a substantially cylindrical polymeric middle body. The substantially cylindrical insert includes a top surface opposite a bottom surface and a substantially cylindrical coupling element that extends from the bottom surface, a primer recess in the top surface that extends toward the bottom surface, a primer flash hole positioned in the primer recess to extend through the bottom surface, and a flange that extends circumferentially about an outer edge of the top surface. The substantially cylindrical polymeric middle body includes a substantially cylindrical polymeric bullet-end and a substantially cylindrical polymeric coupling end connected by a powder chamber, wherein the substantially cylindrical polymeric coupling end extends over the substantially cylindrical coupling element and covers a circumferential surface of the primer flash hole.
Debinder for 3D objects
A debinder provides for debinding printed green parts in an additive manufacturing system. The debinder can include a storage chamber, a process chamber, a distill chamber, a waste chamber, and a condenser. The storage chamber stores a liquid solvent for debinding the green part. The process chamber debinds the green part using a volume of the liquid solvent transferred from the storage chamber. The distill chamber collects a solution drained from the process chamber and produces a solvent vapor from the solution. The condenser condenses the solvent vapor to the liquid solvent and transfer the liquid solvent to the storage chamber. The waste chamber collects a waste component of the solution.
Debinder for 3D objects
A debinder provides for debinding printed green parts in an additive manufacturing system. The debinder can include a storage chamber, a process chamber, a distill chamber, a waste chamber, and a condenser. The storage chamber stores a liquid solvent for debinding the green part. The process chamber debinds the green part using a volume of the liquid solvent transferred from the storage chamber. The distill chamber collects a solution drained from the process chamber and produces a solvent vapor from the solution. The condenser condenses the solvent vapor to the liquid solvent and transfer the liquid solvent to the storage chamber. The waste chamber collects a waste component of the solution.
Debinding of 3D objects
3D-printed parts may include binding agents to be removed following an additive manufacturing process. A debinding process removes the binding agents by immersing the part in a solvent bath causing chemical dissolution of the binding agents. The time of exposure of the 3D-printed part to the solvent is determined based on the geometry of the part, wherein the geometry is applied to predict the diffusion of the solvent through the 3D-printed part. The 3D-printed part is then immersed in the solvent bath to remove the binding agent, and is removed from the solvent bath after the time of exposure.
Primer Insert Having a Primer Pocket Groove
The present invention provides a primer insert for use in a polymeric ammunition cartridge includes atop surface opposite a bottom surface and a extraction flange that extends circumferentially about an outer edge of the top surface; a coupling element that extends from the bottom surface, wherein the substantially cylindrical coupling element is adapted to receive a polymer overmolding; a primer recess in the top surface that extends toward the bottom surface, wherein the primer recess comprises a recess bottom and a circular recess side wall; a primer flash aperture through the recess bottom that extends through the bottom surface, wherein the primer flash aperture is adapted to receive a polymer overmolding to form a flash hole; and one or more pads positioned on the recess bottom; a groove in the primer recess positioned around the primer flash aperture to extend at least partially over the recess bottom and adapted to receive a polymer overmolding.
Primer Insert Having a Primer Pocket Groove
The present invention provides a primer insert for use in a polymeric ammunition cartridge includes atop surface opposite a bottom surface and a extraction flange that extends circumferentially about an outer edge of the top surface; a coupling element that extends from the bottom surface, wherein the substantially cylindrical coupling element is adapted to receive a polymer overmolding; a primer recess in the top surface that extends toward the bottom surface, wherein the primer recess comprises a recess bottom and a circular recess side wall; a primer flash aperture through the recess bottom that extends through the bottom surface, wherein the primer flash aperture is adapted to receive a polymer overmolding to form a flash hole; and one or more pads positioned on the recess bottom; a groove in the primer recess positioned around the primer flash aperture to extend at least partially over the recess bottom and adapted to receive a polymer overmolding.
Polymer ammunition and cartridge primer insert
The present invention provides polymer ammunition having a primer insert having: a top surface; a bottom surface opposite the top surface; a coupling element that extends from the bottom surface, wherein the coupling element comprises an interior surface and an exterior surface, wherein the interior surface comprises: a transition region that transitions from the bottom surface to a second segment wherein the transition region has a radius of from 0.02 to 0.08; a first segment extending from the second segment and terminates at a tip, wherein the first segment has a first segment distance from 0.05 to 0.09 inches and the second segment has a second segment distance from 0.05 to 0.09 inches, wherein the second segment has a second segment angle from +3 to −3 degrees relative to the first segment angle and the first segment has a first segment angle from +6 to −6 degrees from perpendicular to the top surface; a primer recess in the top surface that extends toward the bottom surface; a primer flash aperture positioned in the primer recess through the bottom surface; and a flash aperture groove in the primer recess and positioned around the primer flash aperture and adapted to receive a polymer overmolding through the primer flash aperture.
Polymer ammunition and cartridge primer insert
The present invention provides polymer ammunition having a primer insert having: a top surface; a bottom surface opposite the top surface; a coupling element that extends from the bottom surface, wherein the coupling element comprises an interior surface and an exterior surface, wherein the interior surface comprises: a transition region that transitions from the bottom surface to a second segment wherein the transition region has a radius of from 0.02 to 0.08; a first segment extending from the second segment and terminates at a tip, wherein the first segment has a first segment distance from 0.05 to 0.09 inches and the second segment has a second segment distance from 0.05 to 0.09 inches, wherein the second segment has a second segment angle from +3 to −3 degrees relative to the first segment angle and the first segment has a first segment angle from +6 to −6 degrees from perpendicular to the top surface; a primer recess in the top surface that extends toward the bottom surface; a primer flash aperture positioned in the primer recess through the bottom surface; and a flash aperture groove in the primer recess and positioned around the primer flash aperture and adapted to receive a polymer overmolding through the primer flash aperture.